Dow Dnda 1149 Nt 7 Linear Low Density Polyethylene Resin

Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 550294
    Density 0.920 g/cm³
    Melt Index 2.0 g/10 min (190°C/2.16 kg)
    Melting Point 124°C
    Vicat Softening Point 97°C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 700%
    Flexural Modulus 241 MPa
    Haze 13%
    Gloss 60%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 500 g

    As an accredited Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg, securely stacked and stretch-wrapped for shipping.
    Container Loading (20′ FCL) 20′ FCL loaded with Dow DNDA-1149 NT 7 LLDPE resin, 25 kg bags, palletized and secured for ocean freight.
    Shipping Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin is generally non-hazardous and not regulated for transport. It is shipped in 25 kg bags, octabins, or bulk trucks/railcars. Keep packaging dry, clean, closed, and protected from direct sunlight, excessive heat, moisture, and contamination. Handle with care to avoid bag damage.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed to prevent moisture, dust, and contamination. Use first-in, first-out rotation. Avoid prolonged UV exposure and extreme temperatures. Maintain clean, labeled packaging; stack securely to prevent damage and spills. Store separately from incompatible or odorous materials. Follow supplier SDS and local rules.
    Shelf Life Shelf life for Dow DNDA-1149 NT 7 LLDPE resin is typically 24 months in cool, dry, unopened original packaging.
    Application of Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin

    On three-layer blown-film lines with a 65 mm grooved-feed extruder and a 250 mm spiral mandrel die, DNDA-1149 NT 7 is run as the core layer in heavy-duty industrial sacks at 60–90 µm total thickness. The nominal melt index of 1.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022 and density of 0.919 g/cm³ per ISO 1183-1:2019 place the resin in a processing window where bubble stability competes with melt fracture. A die gap of 1.8–2.3 mm combined with a blow-up ratio of 2.0–2.5:1 keeps the frost-line height at 6–8 die diameters. Frost lines below 5 die diameters increase transverse direction tear but reduce gauge uniformity on wide webs. Screw speeds above 90 min⁻¹ on a 30:1 L/D barrier screw can push melt temperature beyond 210°C; this narrows external bubble cooling capacity and raises blocking risk when the resin is not blended. At 100 µm monolayer thickness, output becomes heat-transfer-limited rather than extruder-limited. A dual-lip air ring with internal bubble cooling maintains line speed above 20 m/min only when die lip set temperature is held at 190–200°C. Addition of 10–20 wt% of a high-pressure LDPE with melt index 2.0 g/10 min improves bubble stability and dart-drop energy measured by ASTM D1709-16ae1, but reduces secant modulus measured by ASTM D882-18 at 1% strain. Finished sacks for fertilizers and resin pellets are tested at 50 kg drop cycles; puncture energy is monitored per ASTM D3420-21 after conditioning at 23°C and 50% RH for 48 h.

    What limits haze development in thin-gauge frozen-food films made from butene LLDPE?

    Because haze below 60 µm is governed by quench rate rather than additive content, the extrusion setup for frozen-food packaging uses a high-stalk geometry with a die gap of 1.5–1.8 mm, a blow-up ratio of 2.8:1, and melt temperature of 185–195°C. The elongated, unstretched stalk aligns crystallites axially before the bubble expands, lowering wide-angle scattering measured per ASTM D1003-13. Frost-line height is kept between 8 and 10 die diameters. If the stalk is shortened below 6 die diameters, average spherulite size increases and the film loses gloss at 60° per ASTM D2457-21. Frozen vegetable, seafood, and poultry bags at 40–60 µm require subzero puncture resistance; the property is tested per ASTM D3420-21 after conditioning at -20°C for 24 h. Food-contact compliance is assessed under FDA 21 CFR 177.1520(c) 3.1a and Commission Regulation (EU) No 10/2011, with migration of primary antioxidants checked at 40°C for 10 days in 3% acetic acid and 10% ethanol simulants. On single-screw extruders without internal bubble cooling, output drops 15–25% relative to a comparable LDPE film because the shear-thinning index of this resin is lower. A grooved-feed section increases throughput but also raises melt pressure at the screen changer above 350 bar when 60/100/60 mesh packs are used. If the base grade is not formulated with slip or antiblock, a coextruded sealant ply may contain 3–5 wt% slip/antiblock masterbatch to reduce blocking without shifting seal initiation temperature determined by ASTM F1921-12.

    Indicative blown-film processing windows for DNDA-1149 NT 7 across three converting configurations
    ParameterHeavy-duty sack 75 µmFrozen-food film 45 µmSilage cover 125 µm
    Melt temperature190–210°C185–195°C190–220°C
    Die gap1.8–2.3 mm1.5–1.8 mm2.0–2.5 mm
    Blow-up ratio2.0–2.5:12.5–3.0:12.8–3.2:1
    Frost-line height6–8 die diameters8–10 die diameters8–12 die diameters
    Air ring configurationdual-lip + IBCsingle-lip high-stalkdual-lip + IBC

    When a silage cover is coextruded with a pigmented polyolefin skin

    The coextrusion of a black or white pigmented skin layer places DNDA-1149 NT 7 in the core layer at 100–150 µm total film thickness. The outer skin usually carries 4–6 wt% carbon black or titanium dioxide masterbatch at 8–12 wt% pigment loading, while the core remains unpigmented to preserve tear resistance. On a 1,200 mm blown-film die, gauge variation is monitored with a non-contact capacitance gauge; deviations above ±5% at 100 µm nominal thickness indicate insufficient die thermal uniformity or inconsistent melt pressure from the barrier screw. The primary mechanical requirement is slow puncture and tear propagation under outdoor storage conditions, evaluated by ASTM D1922-15 and ASTM D3420-21. UV resistance is not inherent in the base resin; hindered amine light stabilizers at 0.15–0.30 wt% and a benzotriazole UV absorber at 0.10–0.20 wt% are compounded into the skin layer. Xenon-arc or UVA-340 weathering per ISO 4892-2:2013 at 0.76 W/m²/nm and 1,000 h is used to track retained elongation at break. Published data for this specific formulation are limited, so converters must generate lot-specific ageing curves. The butene copolymer backbone limits long-term creep resistance under sustained hoop stress; silage bags with diameters above 1.5 m should not be stored beyond 24 months without side-wall support. Skin-to-core adhesion is verified by a peel test at 15 mm/min after coextrusion. Cohesive failure should occur within the core layer, not at the interface.

    In tandem extrusion lamination, DNDA-1149 NT 7 is metered as a sealant web at 20–25 µm coat weight against aluminium foil, metallised PET, or oriented PP. Because the resin has a relatively broad molecular-weight distribution for a butene LLDPE, it is blended with 20–30 wt% of an autoclave LDPE with melt index 7.5 g/10 min to reduce neck-in below 50 mm on a 150 mm slot die at 150–250 m/min line speed. The blend is processed at 280–320°C melt temperature. Above 320°C, oxidative gel formation increases and is visible as pinholes after chill-roll cooling. Chill-roll temperature is maintained between 15°C and 18°C to increase adhesion and prevent blocking on rewind. Adhesion to primed aluminium foil is tested per ASTM F904-16 with a bond strength target above 2.5 N/15 mm; the failure mode must be cohesive in the polyethylene layer. For food packaging laminates, the sealant web must satisfy FDA 21 CFR 177.1520(c) 3.1a and EU No 10/2011, with overall migration below 10 mg/dm² after 10 days at 40°C in 3% acetic acid. The density of 0.919 g/cm³ gives a lower sealing initiation temperature by 2–4°C in a jaw sealer compared with LDPE; plateau seal strength after 0.5 s dwell is governed by the coextruded tie layer and not by this resin alone. When the base grade is not formulated with slip or antiblock, a converter must add 5–8 wt% of silica-based masterbatch to prevent roll blocking at 30°C and 70% RH beyond 30 days storage.

    Blown stretch film core layer and pallet unitization

    Blown stretch film lines running 17–25 µm finished gauge use DNDA-1149 NT 7 as a core layer in three-layer A/B/A structures at 30–40 wt% of total thickness. The core contributes puncture resistance but lowers extensibility compared with a higher alpha-olefin LLDPE. On a high-speed rotary die with 2.0 mm die gap and 2.2:1 blow-up ratio, melt temperature is kept at 190–205°C. Above 210°C, film blocking and flow marks become more frequent. Pre-stretch performance at 200–250% elongation is measured per ASTM D5459-17. Film containing this resin typically retains 80–85% of original puncture force after 200% pre-stretch, but published data for this specific configuration are limited. Edge fold defects on pallet wrappers with power pre-stretch occur when the frost-line height is below 7 die diameters. Increasing the frost line to 9 die diameters improves bubble stability without reducing output. The cling layer is excluded from DNDA-1149 NT 7; polyisobutylene or ultra-low-density PE with high tackifier loading is coextruded at 5–8% of total thickness. Distribution packaging certification typically follows ASTM D3951-18 for bundling and ISO 527-3:2018 for machine-direction tensile properties.

    Collation shrink film is a minor-use application. DNDA-1149 NT 7 may be included at 20–30 wt% with LDPE to raise puncture resistance, but transverse shrink at 130°C should be measured per ISO 14616:2015 and the resin is not recommended as the sole layer when machine-direction shrink exceeds 40%.

    Free Quote

    Competitive Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin is a pelletized, high-flow ethylene copolymer characterized by a nominal melt mass-flow rate of 50 g/10 min when measured at 190 °C under a 2.16 kg load in accordance with ASTM D1238, and a nominal density of 0.919 g/cm³ when tested under ASTM D792. The material belongs to the linear low density polyethylene class rather than to high-pressure low density polyethylene or high-density polyethylene; its linear backbone and controlled short-chain branching give it a different combination of toughness, environmental stress-crack resistance, and melt processability. The suffix NT 7 identifies the natural-grade formulation and stabilizer package defined in the manufacturer’s product stewardship documentation. Published application fields for this melt flow class include injection molding of thin-wall parts, masterbatch carrier resin, and high-speed compounding, where the reduction in melt viscosity is more important than film bubble stability or drawdown.

    At 0.919 g/cm³, the density places the resin near the lower end of conventional LLDPE molding and film grades. A two-phase density estimate using 0.855 g/cm³ for amorphous polyethylene and 1.000 g/cm³ for crystalline polyethylene yields a room-temperature volume-fraction crystallinity of approximately 44%. This crystallinity level produces lower flexural modulus and hardness than HDPE injection-molding grades with densities from 0.945 g/cm³ to 0.965 g/cm³, but it retains enough stiffness for many thin-wall containers, overcaps, and closures. The 50 g/10 min melt flow indicates a relatively low molecular weight and low melt viscosity; it separates the product from standard butene-LLDPE film grades that are commonly supplied at 0.5 g/10 min to 2.0 g/10 min.

    What Distinguishes a 50 g/10 min LLDPE from Blown-Film Butene Grades?

    The primary variable is melt viscosity rather than density. A blown-film LLDPE with a melt index near 1.0 g/10 min is selected for bubble stability, dart impact strength, and machine-direction tear resistance in thin films. DNDA-1149 NT 7 is selected for cavity filling and carrier function, where melt strength is subordinate to pressure drop and flow length. The lower molecular weight reduces injection pressure and improves flow-length capability, but it also lowers the onset of melt fracture and reduces extrudate melt strength, which must be managed with wider die gaps or lower shear rates in any extrusion operation. In film lines, a 50 g/10 min grade cannot sustain the same stalk bubble geometry as a 1.0 g/10 min film grade; published data for this specific configuration is limited because the resin is not designed for blown-film bubble stability. In injection molding, the same high flow shortens fill time and improves replication of microtexture, but low melt viscosity can produce flash at the parting line if clamp force is insufficient or if the tool is not shut with adequate accuracy.

    Published nominal physical properties and method references
    PropertyTest methodNominal value
    Melt mass-flow rateASTM D123850 g/10 min at 190 °C/2.16 kg
    DensityASTM D7920.919 g/cm³
    Estimated crystallinityTwo-phase density model44%

    Injection Molding Process Window, Mold Shrinkage, and Gate Freeze Considerations

    Process development for DNDA-1149 NT 7 on a reciprocating-screw injection molding machine should begin with a melt temperature in the 204 °C to 232 °C range and a mold temperature from 15 °C to 40 °C. Polyethylene is not hygroscopic, and hopper drying is not generally required; however, condensation on cold pellets stored below ambient temperature can introduce surface moisture and should be avoided. Melt temperatures above 260 °C for extended residence times are an operational boundary, because thermal-oxidative degradation can increase color generation and reduce molecular weight. The high 50 g/10 min melt flow permits thin-wall filling at lower hydraulic injection pressure than would be required for an 8 g/10 min or 20 g/10 min LLDPE molding grade, but pack pressure and gate seal time must be re-established for each tool. Because the resin solidifies rapidly once the melt front contacts the cold mold wall, gate freeze may occur before sufficient packing is transferred to the core of a thicker section, increasing the risk of sink marks and dimensional variability.

    Shrinkage allowances in unfilled LLDPE at this density generally fall in the 0.015 mm/mm to 0.025 mm/mm range, but the exact value is geometry-dependent and must be derived from the production tool, not from a generic resin datasheet. Mold-flow simulation should use measured pressure-volume-temperature data for the specific lot; published data for this exact grade in molded parts with wall thicknesses below 0.8 mm are limited. The part designer should validate post-mold shrinkage after 48 h at 23 °C and after conditioning at the intended service temperature.

    On a co-rotating twin-screw compounding line with an L/D ratio of 40:1, DNDA-1149 NT 7 is frequently considered as a masterbatch carrier resin because the low melt viscosity reduces torque and permits high pigment or mineral loadings. However, the reduced viscosity also lowers the shear stress available to break pigment agglomerates, a processing conflict that is not visible from melt index alone. Dispersion quality should be assessed by pressure rise across a 25 μm screen pack or by film speck count, not by assuming that high melt flow equals good distributive mixing. In masterbatch production, the carrier should be matched to the let-down resin; a 50 g/10 min carrier dispersed into a 1.0 g/10 min film resin may require higher let-down ratios or extended distributive mixing to avoid local viscosity inhomogeneity and gel-like defects in the final article.

    When Regulatory Compliance Is Required, the Certificate Must Be Checked Separately

    Food-contact status for polyethylene in the United States may be supported under FDA 21 CFR 177.1520, which covers olefin polymers for repeated food-contact use, provided the finished article complies with extractive limitations and end-use constraints. The European framework requires compliance with Regulation (EU) No 10/2011 and subsequent amendments, including overall migration limits and specific migration limits for additives. The RoHS Directive 2011/65/EU restricts lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers in electrical and electronic equipment; natural polyethylene is generally expected to meet these heavy-metal restrictions, but lot-level documentation is required. REACH registration obligations and SVHC disclosure are separate and must be confirmed with current supplier documentation. Published data for this specific configuration is limited, and a resin datasheet alone is not a compliance certificate.

    Compared with high-pressure LDPE at a similar 0.919 g/cm³ density and 8 g/10 min melt index, the linear backbone of DNDA-1149 NT 7 generally provides higher tensile yield strength and environmental stress-crack resistance, but lower melt strength and poorer drawdown in extrusion coating. The absence of long-chain branching in conventional LLDPE restricts its use as a neat extrusion-coating resin; blending with LDPE is common to restore neck-in and drawdown performance. Compared with a metallocene-catalyzed LLDPE of the same melt index, the comonomer distribution may be broader, which can affect low-temperature impact, organoleptic performance, and seal initiation temperature. The manufacturer does not publish enough catalyst-structure data in standard datasheets to permit a quantitative comparison of short-chain branching distribution; therefore, seal performance and extractables must be evaluated in the final article under the relevant ASTM or ISO method.

    The rheological profile of a 50 g/10 min LLDPE is strongly shear-thinning but less strain-hardening than high-pressure LDPE. In capillary rheometry under ASTM D3835, the apparent shear viscosity at 190 °C and 100 s⁻¹ is expected to be much lower than that of a 1.0 g/10 min LLDPE, but the exact curve is lot-dependent. This behavior reduces screw torque and melt temperature rise in single-screw injection units, permitting higher screw recovery rates. However, the reduced viscosity also lowers the pressure available for compacting the melt in front of the screw, which can extend cushion requirements and make shot-to-shot consistency sensitive to check-ring wear. Processors should monitor cushion stability and check-ring leakage; a worn check ring produces more visible shot-weight variation in a high-flow resin than in a higher-viscosity resin because the backflow path has lower flow resistance.

    Gate and runner design for DNDA-1149 NT 7 should account for its low melt strength. Hot-runner systems with valve gates are preferred when the material is used for high-cavitation thin-wall packaging, because thermal gating reduces freeze-off at small gate diameters. Cold-runner tools with subgates below 0.6 mm may require elevated melt temperature or increased injection velocity to prevent premature freeze-off, but raising melt temperature above 232 °C reduces viscosity further and can increase flashing at the parting line. The exact gate size should be determined by spiral-flow testing using the production grade and colorant package. Structural parts with wall thicknesses above 2.5 mm are generally not the most predictable use for a 50 g/10 min LLDPE because the packing window is narrow; published data for this specific configuration is limited, but the low viscosity and fast cooling rate favor thin-wall applications.

    For multi-cavity thin-wall tools, mold temperature uniformity must be maintained within ±5 °C across the cavity because differential shrinkage creates warpage and part sticking. Mold cooling circuits should be designed for turbulent flow; a Reynolds number above 10 000 in cooling channels is commonly specified for consistent heat removal. Injection velocity profiling should be used to limit shear heating at the gate, particularly when color concentrates or fillers are added, because local temperature spikes can degrade the low-molecular-weight fraction and create visible streaks. Shot-size variation should be plotted against melt cushion over at least 50 cycles after start-up; the high-flow resin reaches stable processing more quickly than higher-viscosity grades but can expose check-ring wear earlier.

    Published mechanical property expectations for a 0.919 g/cm³ LLDPE include moderate tensile yield strength, high elongation at break, and higher puncture resistance relative to a high-flow LDPE of similar density. However, the 50 g/10 min melt index lowers notched Izod impact and tensile strength relative to lower-melt-index LLDPE grades of the same density. The correct comparison is not with a 1.0 g/10 min film grade but with other high-flow molding resins. Testing should be performed on molded plaques conditioned at 23 °C and 50% relative humidity for 40 h under ASTM D618 before tensile data are generated per ASTM D638 or ISO 527-2. Notched Izod impact data from ASTM D256 and flexural modulus from ASTM D790 should be supplemented by instrumented impact testing when the part is used below −20 °C, because high-flow LLDPE grades can show a ductile-to-brittle transition that is not visible in single-point Izod values.

    Environmental stress-crack resistance is generally higher for linear low density polyethylene than for high-pressure LDPE at similar density, but it decreases as melt index increases. A 50 g/10 min LLDPE should not be specified for aggressive surfactant- or solvent-contact service without testing under ASTM D1693 or the notched constant ligament stress test of ISO 16770. The high flow and lower molecular weight reduce slow-crack-growth resistance compared with a 1.0 g/10 min LLDPE, and this limitation is an expected trade-off for processability. Published data for this specific configuration is limited; service life predictions should be based on fractured-surface inspection and not on density or melt index alone.

    Clamp force requirements for thin-wall molds run with a 50 g/10 min resin are controlled by projected area and cavity pressure, not by melt index alone. The lower packing pressure needed for high-flow LLDPE can reduce the required clamp tonnage compared with a 20 g/10 min grade, but this is not a fixed percentage and must be confirmed with in-mold cavity pressure sensors. A cavity pressure transducer located near the gate and another near the end of fill should be used to establish the intensification ratio and switch-over point. Maintaining peak cavity pressure within the toolmaker’s limit is necessary to avoid flash in thin-wall multi-cavity tools. This measurement is preferable to setting machine hydraulic pressure alone because the low melt viscosity decreases pressure drop through the nozzle and runner; the hydraulic setting may not correlate with cavity conditions.

    Use of color concentrates and slip/antiblock masterbatches with a 50 g/10 min carrier should be evaluated for melt flow mismatch. A concentrate based on a 20 g/10 min carrier can create local viscosity differences if blended at very low let-down ratios. High-shear mixing at the screw tip or static mixers in the nozzle improves uniformity. The resin’s high flow enables high pigment loadings in masterbatch, but too high a loading can reduce the effective melt flow of the final blend and negate the processing advantage. A spiral-flow test on the let-down blend is recommended before cutting production tools.

    Regulatory standards and scope relevant to olefin polymers
    StandardScope
    FDA 21 CFR 177.1520US food-contact clearance for olefin polymers
    Regulation (EU) No 10/2011EU plastic food-contact materials
    RoHS Directive 2011/65/EUHeavy metal and brominated flame retardant restrictions