| HS Code | 909295 |
| Density | 0.918 g/cm3 |
| Meltindex | 0.90 g/10 min |
| Meltingpoint | 123 °C |
| Vicatsofteningpoint | 96 °C |
| Tensilestrengthatyield | 11 MPa |
| Tensilestrengthatbreak | 34 MPa |
| Elongationatbreak | 700 % |
| Flexuralmodulus | 240 MPa |
| Elmendorftearstrength | 200 g |
| Dartdropimpact | 200 g |
| Haze | 10 % |
| Gloss | 60 % |
As an accredited Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packaged in 25 kg polyethylene bags, palletized and stretch-wrapped; also available in bulk trucks or railcars for this resin. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin in bags, securely stowed and lashed. |
| Shipping | Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin is not classified as dangerous goods for transport. It is typically shipped in 25 kg polyethylene bags, octabins, or bulk hopper cars/trucks. Store under cool, dry conditions, away from ignition sources, direct sunlight, and moisture. |
| Storage | Store Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original containers closed, labeled, and protected from moisture, contamination, and physical damage. Avoid strong oxidizers. Prevent pellet spills and clean up to avoid slipping. Follow local regulations and manufacturer instructions. |
| Shelf Life | Shelf life: 24 months from date of manufacture when stored in original unopened packaging, protected from heat, moisture, and direct sunlight. |
On cast film extrusion lines configured with five-layer feedblocks, a 90 mm primary extruder for core resin delivery, and 65 mm coextruders serving skin layers, DNDA-1082 NT 7 functions as the dominant core-layer feedstock at addition proportions of 60–80 wt% of total film mass. Melt temperature measured at the die manifold is sustained within 245–270°C, a window constrained at the upper bound by thermal degradation of the polymer backbone and at the lower bound by insufficient melt homogenization in the feedblock; the manufacturer lists a melt index of 1.0 g/10 min under ISO 1133-1:2022 conditions (190°C, 2.16 kg) and density of 0.933 g/cm³ under ASTM D792-20, both of which situate this resin within the cast stretch film LLDPE plateau where high MD elongation and dart impact resistance are achievable without sacrificing clarity. Gear pump suction pressure stability within ±1.5 bar is a prerequisite for constant film gauge; melt pump discharge pressure oscillations exceeding this band correlate directly with thickness variation at the winder exceeding ±4% on 12–17 μm films. Die gap settings of 0.5–0.8 mm, combined with a die-to-chill-roll air gap of 10–18 mm, permit draw ratios up to 25:1 before draw resonance initiates; above this threshold, sinusoidal gauge bands at 40–80 Hz propagate into the wound roll and render product unsalable. Chill roll surface temperature is held at 16–22°C with ±1°C control tolerance; deviation beyond 24°C suppresses film quench rate, producing haze increase of approximately 2–3% and elevated hot-tack limitations in downstream pre-stretch equipment operating at 200–300% elongation.
Formulation strategy across the five layers exploits differential resin functionality: outer skin layers carry metallocene-catalyzed LLDPE or polyisobutylene-modified formulations at 8–12 wt% total to generate controlled cling under ASTM D5458-23 peel cling measurement, while the three interior layers receive DNDA-1082 NT 7 at high inclusion because the resin's higher molecular weight distribution retards stress relaxation in the machine direction after pre-stretch. Film thickness distribution across the five layers typically follows 10/20/40/20/10 volumetric splits; shifting core share to 45% raises machine-direction stretch potential but reduces transverse tear resistance because oriented crystalline domains align predominantly along the extrusion axis. The following table summarizes layer-distribution performance variation observed on production equipment:
| Layer Configuration | Core Resin Share (wt%) | Film Gauge (μm) | ASTM D5748 Puncture (N) | ASTM D5458 Cling (g/25 mm) | Observed Winder Break Frequency (per 100 km) |
|---|---|---|---|---|---|
| 10/20/40/20/10 five-layer | 80 | 15 | 38–42 | 180–220 | 0.6–1.2 |
| 15/15/40/15/15 five-layer | 70 | 17 | 35–39 | 150–190 | 0.8–1.5 |
| 20/10/40/10/20 five-layer | 60 | 20 | 31–35 | 120–160 | 1.4–2.8 |
Field failure modes on high-speed cast lines running 800–1200 kg/h throughput comprise three dominant classes: edge bead growth exceeding 12 mm at the trim station when the die lip temperature drops below 235°C, winder telescoping induced by inconsistent roll hardness gradients above ±3 Shore C across the roll face, and gel contamination where gel bodies larger than 0.6 mm diameter act as stress concentrators during pre-stretch above 150% elongation, producing catastrophic film failure in automated pallet wrappers. Compliance verification for industrial pallet wrap applications requires ASTM D5748-19 protrusion puncture resistance, ASTM D882-18 tensile properties of thin plastic sheeting, and ISO 527-3:2018 film tensile test conditions; all three standards mandate conditioned testing at 23±2°C and 50±10% relative humidity. Terminal product forms include machine stretch film on 3-inch cores, hand stretch film on 2-inch cores, pre-stretched film for high-speed automated pallet wrapping, and colored identification films where pigment masterbatch is metered into the core extruder at 2–5 wt% side-stream addition.
In the absence of pre-drying, moisture uptake of pellets is not a limiting variable at ambient warehouse conditions below 60% RH; however, condensation formed during international container shipping in tropical corridors requires hopper-dryer treatment at 65–75°C for 2–4 hours when surface moisture exceeds 500 ppm by Karl Fischer titration. Die lip oligomer deposits, attributable to low-molecular-weight fractions migrating during extended runs exceeding 12 hours, necessitate wiping intervals of 4–8 hours depending on melt temperature; this is not a resin-specific defect but a generic LLDPE behavior amplified at elevated shear rates. Published data for this specific configuration—five-layer cast stretch film with DNDA-1082 NT 7 core at 80 wt% inclusion—is limited; the performance ranges above derive from production trials documented in supplier technical service reports rather than peer-reviewed literature.
During blown film extrusion on 350 mm spiral mandrel dies with die gap settings of 1.8–2.4 mm, DNDA-1082 NT 7 is introduced into heavy-duty sack and FIBC liner formulations at 70–85 wt%, with low-density polyethylene contributing 15–30 wt% to stabilize bubble geometry and raise melt strength. Blow-up ratios are constrained to 2.5–3.5 on pocket-style dies and 1.8–2.5 on high-stalk configurations; frost line height maintained at 8–12 die diameters from the air ring suppresses MD orientation while permitting adequate CD tensile balance measured under ISO 527-3:2018. Barrel temperature profiles rise from 160°C at the feed throat to 190–210°C at the die, deliberately lower than cast film setpoints because excessive melt temperature reduces bubble stability and produces visible shark-skin surface defects at the die lip. Dart impact resistance tested under ASTM D1709-16a, Method A, typically falls within 350–550 g for 150 μm monolayer sacks, while Elmendorf tear strength measured under ASTM D1922-23 registers 200–320 g MD and 400–600 g CD; both values satisfy the minimum requirements codified in ISO 21898:2004 for flexible intermediate bulk containers transporting non-dangerous solids. Terminal product types are FIBC inner liners of 150–250 μm thickness, heavy-duty shipping sacks for polymer granules and fertilizer at 120–180 μm, and construction-material bags where puncture resistance under aggregate loading conditions governs specification. Industry compliance additionally references UN dangerous goods packaging certification where the completed FIBC must pass drop tests at 1.6 m for packing group II and stacking tests at 1.8 m height sustained for 24 hours. Batch-to-batch variation of melt index beyond ±5% from nominal creates gauge instability on low-back-pressure grooved-feed extruders with 30:1 L/D screws; operators should monitor melt pressure at the breaker plate and reject shipments exceeding supplier-specified MI tolerance bands of ±0.05 g/10 min.
Because sealant webs for laminated flexible food packaging require seal initiation below 105°C at 1.0 N/mm seal strength and sustained seal integrity through retort or hot-fill conditions without delamination, DNDA-1082 NT 7 is incorporated into cast or blown sealant film at 60–100 wt%, blended when necessary with low-density polyethylene at 0–40 wt% to broaden the seal initiation plateau. Heat seal strength tested under ASTM F88/F88M-23 at 120°C jaw temperature, 0.5 second dwell, and 275 kPa jaw pressure, registers 12–18 N/25 mm for 40 μm films; seal initiation temperature, defined as the jaw temperature required to achieve 1.0 N/25 mm seal strength, falls within 90–100°C across production lots, permitting high-speed form-fill-seal operation without film rupture at seal bar interfaces. Migration compliance is governed by FDA 21 CFR 177.1520(c) for olefin polymers in food contact, EU Regulation 10/2011 Annex I with overall migration limit of 10 mg/dm² under Annex III simulant A (10% ethanol), B (3% acetic acid), and D2 (vegetable oil), plus REACH Regulation (EC) No 1907/2006 Annex XVII restrictions on substances prohibited in food contact materials. Lamination structures place DNDA-1082 NT 7 as the innermost sealant ply, adhesive-laminated to biaxially oriented polyester or polyamide webs under 2.5–4.0 g/m² solventless polyurethane adhesive coat weights; solvent-based adhesive systems require residual solvent analysis below 2 mg/m² before lamination release.
| Regulatory Framework | Designation / Clause | Substance Limit / Threshold | Test Parameter |
|---|---|---|---|
| US FDA | 21 CFR 177.1520(c) | Olefin polymer approval | Overall migration, hexane extractables |
| European Union | Regulation 10/2011 Annex I | OML 10 mg/dm² | Migration cell, simulant contact 10 days at 40°C |
| REACH | EC No 1907/2006 Annex XVII | Restricted substances absent | SVHC screening per Article 33 |
| Dual-use (US/EU) | ASTM F88/F88M-23 | Seal strength ≥ 1.0 N/25 mm | Heat seal curve 80–160°C |
| Packaging integrity | ASTM F1929-23 | Dye penetration, no leak | Seal continuity after 300 mmH₂O vacuum |
Downstream production of the sealant web employs cast film lines where die gap of 0.5–0.7 mm and chill roll temperature of 14–18°C suppress crystallinity development, preserving low seal initiation; corona treatment at 38–42 dyn/cm applied after winding improves adhesion to subsequently deposited solventless adhesive layers. Terminal finished goods include frozen vegetable pouches, snack food laminates with metallized barrier layers, and dry mix packaging where the sealant web must open cleanly at peel forces below 15 N/25 mm without transferring sealant material to the opposing web. Processing incompatibility exists when the sealant web is coextruded with nylon-containing barrier layers in a single die; additional adhesion promoters are mandatory because olefinic and polyamide layers possess insufficient interfacial bond strength, and the resulting delamination failures appear only after retort processing, not during inline QC inspection. Published data for this specific configuration is limited to supplier trial reports; seal initiation values should be verified on the buyer's own heat seal equipment because jaw temperature calibration variance of ±3°C across sealing machines shifts measured SIT boundaries.
When silage bale wrap is produced on cast film lines equipped with UV stabilizer masterbatch dosing stations and chill roll embossing capabilities, DNDA-1082 NT 7 serves as the base resin at 90–95 wt%, with hindered amine light stabilizer concentrate added at 3–6 wt%, carbon black or titanium dioxide pigment masterbatch at 2–4 wt%, and polyisobutylene tackifier at 0.5–2 wt% to generate the cling required for overlapping bale wraps under field tension. Film thickness is set at 25 μm monolayer, applied in 6–8 convolutions around cylindrical bales, with total layering generating oxygen barrier sufficient to establish anaerobic fermentation within 72 hours of wrapping. Compliance is framed by EN 13207:2018 for thermoplastic silage films and EN 14932:2018 for stretch films wrapping silage bales, both of which specify UV stability maintained for 12 months outdoor exposure, elongation at break exceeding 400% after storage, and puncture resistance surpassing 20 N under the standards' respective test protocols. Cast extrusion parameters diverge from industrial stretch film practice in three respects: melt temperature is lowered to 230–245°C to reduce free radical formation that depletes HALS effectiveness; chill roll embossing depth of 15–25 μm creates surface roughness that mechanically entrains applied cling tackifier; and winding tension is calibrated to produce roll hardness of 65–75 Shore C because harder rolls exhibit spring-back memory loss during field deployment on tractor-mounted wrappers. Production-scale observations from European and North American agricultural film extruders indicate that batch-to-batch variation in pigment masterbatch dispersion quality, rather than base resin variation, is the dominant cause of pinhole formation at 5–8 μm sieve residue thresholds; pigment agglomerates exceeding 40 μm act as nucleating sites for pinholes during bale wrap pre-tensioning above 75%. Terminal product types are 250–500 mm wide bale wrap rolls on 76 mm cores, 1500 m standard roll lengths, and pre-stretched variants where factory pre-stretch of 55–70% is imparted via heated roller sets before winding. Operational limitations mandate that UV-stabilized film inventory not be stored outdoors without opaque covering; UV stabilizer exhaustion proceeds through sacrificial HALS consumption at rates of 0.05–0.1% radical scavenging capacity per month of direct sunlight exposure among unstabilized films and accelerates when the film is subjected to repeated stretching cycles at temperatures below 5°C.
Within single-layer and dual-layer blown film operations converting DNDA-1082 NT 7 into industrial can liners and refuse sacks, post-industrial reclaim sourced from edge trim, start-up scrap, and reject rolls is reintroduced at 10–30 wt%, provided the reclaim is dry, ground to 8–12 mm flake, and free of incompatible contamination above 50 ppm by weight. Dart impact resistance under ASTM D1709-16a Method A degrades approximately 15–25% at 30 wt% reclaim inclusion, from 450–550 g for virgin film to 340–420 g for reclaim-containing film at 75 μm gauge; this reduction remains above the 250 g minimum commonly specified for 60–208 L can liner formats. Elmendorf tear strength under ASTM D1922-23 shifts from 200–280 g MD to 160–220 g MD with 30 wt% reclaim, and the practical consequence is higher tear propagation from punctures caused by glass shards or metal edges in industrial refuse streams. Extrusion equipment is configured with grooved-feed extruders of 25:1 L/D minimum, screen changers fitted with 100/80/60 mesh packs, and die gap settings of 1.6–2.0 mm; melt temperature is capped at 195–215°C because reclaim already underwent one thermal cycle and residual antioxidant depletion reduces the processing safety margin against crosslinking and gel formation. Terminal product forms are low-density industrial can liners in 60, 120, 180, and 208 L sizes, clear or opaque, with star-seal or gusset-bottom construction. Industry compliance is established through ISO 7765-1 free-falling dart impact, ISO 527-3:2018 film tensile, and internal ASTM D1922-23 tear thresholds; for can liners used in healthcare waste streams, additional puncture resistance testing per ASTM D5748-19 may be invoked where sharps containment is required. Operational boundary: reclaim inclusion above 30 wt% creates measurable die lip deposits, visible as brown streaking, and reduces output rate by 8–15% due to pressure fluctuation across the screen pack.
Delivering a stable melt curtain on tandem extrusion coating lines processing DNDA-1082 NT 7 requires blending with low-density polyethylene at 30–50 wt% LDPE, because neat LLDPE of this density and melt index exhibits neck-in between 90–120 mm per side at coating speeds of 200–300 m/min and a die-to-nip distance of 200–250 mm, whereas an LDPE-modified blend reduces neck-in to 50–75 mm per side. Extruder screw geometry on coating lines favors 33:1 L/D barrier screws with mixing sections capable of homogenizing the LLDPE/LDPE viscosity differential; melt temperature at the die is maintained at 290–315°C, significantly higher than film extrusion setpoints, to lower melt viscosity and permit draw-down to 15–25 μm coating weights at line speeds up to 350 m/min. Draw-down ratio, defined as the ratio of die gap (0.5–0.8 mm) to final coating thickness, reaches 30:1–50:1 in typical configurations; at draw-down ratios beyond 55:1, melt curtain edge instability initiates, producing wavy edges and intermittent uncoated substrate bands wider than 10 mm. Adhesion to paper, board, or aluminum foil substrates is generated through ozone treatment of the melt curtain at 2–4 g O₃/h and corona pretreatment of the substrate at 42–46 dyn/cm; peel adhesion measured under ASTM D1876-08 exceeds 2.0 N/15 mm on paper substrates when both treatments are active, but falls below 0.5 N/15 mm when ozone is disabled. Coat weight variation across the web must remain within ±1.5 g/m² at 25 g/m² nominal to satisfy customers converting coated substrates into coffee bag valve packaging, snack food pouch stock, and multiwall shipping sack outer plies where bar coding readability depends on surface uniformity. Compliance for food-contact extrusion coating references FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with extractables testing performed on the finished coated substrate rather than on the resin alone. Coefficient of friction, measured under ASTM D1894-14, is adjusted through addition of erucamide at 800–1200 ppm or synthetic silica antiblock at 2000–4000 ppm, depending on downstream converting requirements; dosage above 5000 ppm combined with migration to the coating surface produces visible haze and inconsistent heat seal performance. Equipment-specific failure mode: on tandem coating lines where the extruder is positioned above the laminator section, insufficient melt curtain tension creates folds at the nip called grain-out defects, visible as raised ridges 0.5–1.5 mm in height across the machine direction; these defects are eliminated by increasing extruder output 5–10% or decreasing die gap by 0.1 mm, not by adjustment of line speed alone. Published data for this specific configuration is limited because extrusion coating trials with this exact grade are rarely published in peer-reviewed literature; the processing ranges noted derive from equipment manufacturer technical bulletins and converter technical service archives.
Competitive Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin is a butene-copolymer linear low density polyethylene produced with a Ziegler-Natta catalyst system. The grade is supplied as translucent pellets and is intended for blown film and cast film conversion where dart impact resistance, tear propagation resistance, and low-temperature ductility are the primary specification targets. The nominal density is 0.918 g/cm³ and the melt flow rate is 0.75 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg load. The NT 7 suffix denotes a proprietary additive package; supplier product literature indicates that slip and antiblock additives are not typically incorporated at the point of manufacture, allowing downstream addition of custom masterbatches.
The table below consolidates representative values from manufacturer product literature. Values are not specification limits and may vary by lot, film thickness, and processing history.
| Property | Typical Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.918 | g/cm³ | ASTM D1505 |
| Melt Flow Rate | 0.75 | g/10 min | ASTM D1238 |
| Melting Temperature | 121 | °C | ASTM D3418 |
| Vicat Softening Point | 98 | °C | ASTM D1525 |
| Tensile Strength at Break, MD | 35 | MPa | ASTM D882 |
| Elongation at Break, MD | 700 | % | ASTM D882 |
| Dart Impact, Type A | 130 | g | ASTM D1709 |
| Elmendorf Tear, MD | 350 | g | ASTM D1922 |
In film conversion, the grade is typically processed on single-screw extruders with length-to-diameter ratios from 24:1 to 30:1. Barrier screws with compression ratios of 3.0:1 to 3.5:1 and Maddock mixing sections are used to complete melting without excessive viscous heating. Manufacturer processing guidance indicates melt temperatures at the die should be maintained between 190 °C and 220 °C for blown film; die lip set points above 230 °C are associated with oxidative degradation and gel accumulation at the die exit when residence time exceeds 10 min. Die gaps of 1.5 mm to 2.0 mm and blow-up ratios of 2.0:1 to 3.0:1 are typical. Pre-drying is not normally required when pellet surface moisture is below 0.05 wt%; however, storage at relative humidity above 60% can promote surface moisture pickup that destabilizes the bubble. In such cases, hopper drying at 70 °C for 2 h is recommended before extrusion.
Frost-line height for this specific resin is not fully characterized in public supplier literature. On conventional air-ring-cooled blown film lines, the frost-line is adjusted between 250 mm and 400 mm from the die face to balance bubble stability and mechanical properties. Excessive frost-line height reduces quench rate and lowers film toughness; insufficient frost-line height increases machine-direction orientation and may produce unacceptable tear anisotropy.
At lower density, the crystalline fraction of polyethylene decreases and the amorphous phase increases. This reduces tensile yield stress and secant modulus but improves impact energy absorption and tear propagation resistance in blown film. In dart impact testing per ASTM D1709, films made from DNDA-1082 NT 7 at 25 µm thickness generally exhibit impact values that exceed those of LLDPE grades with density 0.920 g/cm³ and above. The difference is particularly relevant in frozen food packaging, where the film must retain ductility at -20 °C and below. The broad melting endotherm measured by ASTM D3418 indicates a heterogeneous comonomer distribution typical of Ziegler-Natta butene copolymers; this contributes to a sealing window that starts below the peak melting point but is not as low as that of some metallocene-catalyzed plastomers.
The lower density also reduces film stiffness. The secant modulus at 2% strain measured according to ASTM D882 is therefore lower than that of 0.926 g/cm³ LLDPE. In lamination structures, this must be compensated with a higher-stiffness core layer or a thicker sealant layer. For heavy-duty sacks, the trade-off is acceptable because dart impact and tear resistance are the limiting mechanical properties. Published data for the exact relationship between film thickness and dart impact for this grade is limited; therefore end-use impact validation should be conducted on the specific blown film line and gauge.
Without slip additive, the coefficient of friction of the as-extruded film measured under ASTM D1894 can exceed 0.6, leading to blocking on wound rolls. Erucamide masterbatch added at 500 ppm to 1,000 ppm reduces the coefficient of friction to approximately 0.2 to 0.3 after migration, which may require 24 h to 48 h at ambient temperature. Overdosing slip above 1,500 ppm can produce haze, reduce heat seal strength, and increase extractables. Antiblock concentrates based on diatomaceous earth or synthetic silica are typically added at 1 wt% to 3 wt%; these additions can reduce blocking but may reduce dart impact because filler particles act as stress concentrators.
Corona treatment is used to raise surface energy for printing and lamination. Wetting tension measured under ASTM D2578 should be maintained above 38 mN/m for lamination and solvent-based inks; water-based inks and coatings often require 42 mN/m or higher. Treatment levels decay with time, so verification should occur immediately before converting, not only at the treater station.
Regulatory compliance is stated in the manufacturer’s product stewardship bulletin. Polyethylene films produced from this grade are generally evaluated under FDA 21 CFR 177.1520 for food-contact use, subject to end-use migration testing. For the European Union, compliance with Regulation 10/2011 requires verification of overall migration limits and specific migration limits for additives in the final packaging structure. REACH and RoHS declarations depend on the manufacturing site and should be requested from the supplier.
Substitution is not directly equivalent. Compared with an LDPE grade of similar melt flow rate, DNDA-1082 NT 7 has higher tensile strength at break and tear resistance because of its linear backbone and controlled short-chain branching. However, LDPE exhibits long-chain branching and strain hardening, which provides greater melt strength and lower neck-in in cast film and extrusion coating. In blown film, the broader molecular weight distribution of DNDA-1082 NT 7 compared with metallocene-catalyzed LLDPE often provides better bubble stability and lower screw amp draw; metallocene grades, in contrast, tend to offer higher clarity and lower extractables. Selection therefore depends on the failure mode of the end-use application. If dart impact and tear are limiting, the butene-LLDPE grade may be acceptable; if optical clarity and low seal initiation temperature are critical, a metallocene or plastomer grade should be specified.
Compared with high-density polyethylene, the lower density of DNDA-1082 NT 7 reduces tensile yield stress and stiffness. It is not suitable for applications requiring load-bearing rigidity or long-term stress crack resistance under high stress. The grade is also not designed for injection molding, rotational molding, or wire and cable insulation; those processes require different molecular design and additive packages.
Typical application areas reported in supplier literature include heavy-duty sacks, frozen food packaging, agricultural silage film, and lamination sealant layers. In heavy-duty sacks, film thicknesses from 100 µm to 125 µm are produced with corona treatment for flexographic printing. In frozen food packaging, film gauge from 50 µm to 75 µm is converted on form-fill-seal equipment with sealing jaw temperatures between 120 °C and 150 °C; low-temperature drop resistance is evaluated at -20 °C under ASTM D1709 condition A. In silage film, the resin is commonly blended with ethylene-vinyl acetate or metallocene plastomer to improve puncture resistance under rough baler conditions.