Dow Bynel 41e865 Anhydride Modified Lldpe

Dow Bynel® 41E865 Anhydride Modified LLDPE

    • Product Name: Dow Bynel® 41E865 Anhydride Modified LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 190014
    Material Type Anhydride Modified LLDPE
    Graft Monomer Maleic Anhydride
    Density 0.93 g/cm3
    Melt Index 190 C 2 16 Kg 5.0 g/10 min
    Melting Point 125 °C
    Vicat Softening Point 93 °C
    Tensile Strength At Break 17 MPa
    Elongation At Break 600%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Processing Temperature 230-260 °C
    Adhesion To Evoh Excellent
    Adhesion To Polyamide Excellent
    Adhesion To Polyethylene Excellent

    As an accredited Dow Bynel® 41E865 Anhydride Modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Bynel 41E865 pellets are typically supplied in 25 kg (55 lb) polyethylene-lined bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) Dow Bynel® 41E865 Anhydride Modified LLDPE, palletized pellet bags loaded in a 20′ FCL, shrink-wrapped and secured for ocean freight.
    Shipping Dow Bynel® 41E865 ships as non-hazardous, moisture-sensitive solid pellets in sealed bags, boxes, or bulk containers. Keep cool, dry, and away from heat, sunlight, and moisture. No special transport classification; follow local regulations and keep containers closed during shipping.
    Storage Store Dow Bynel® 41E865 in a cool, dry, well-ventilated area at ambient temperature. Keep containers tightly closed to prevent moisture ingress, contamination, and dust. Protect from direct sunlight, heat, sparks, flames, and oxidizing agents. Use labeled, compatible containers. Avoid incompatible materials and prolonged storage in humid conditions. Follow the supplier’s SDS and local regulations.
    Shelf Life Typically 2 years from manufacture when stored unopened in original packaging below 30°C under dry conditions.
    Application of Dow Bynel® 41E865 Anhydride Modified LLDPE

    In five-layer blown film coextrusion for modified atmosphere packaging of processed meat and cheese, Bynel® 41E865 anhydride-modified LLDPE is introduced as a 100% resin tie layer in a dedicated extruder between the polyethylene skin and the EVOH core. The structure assigns 8% to 12% of total film gauge to each tie layer, translating to 3–8 µm tie thickness in a 50–90 µm finished film; when tie thickness falls below 3 µm, converters specifying ASTM D1876 T-peel testing routinely detect interfacial delamination under 23°C and 50% RH conditioning. The production line employs a grooved-feed extruder with L/D ratio 30:1, die gap 1.8–2.4 mm, and die lip melt temperature 210–240°C. Food-contact compliance is verified under 21 CFR 175.105 for the adhesive component and 21 CFR 177.1520 for olefin polymer constituents; European converters verify overall migration according to Regulation (EU) No 10/2011 using EN 1186-1 protocols. Terminal product types include vacuum skin packs, MAP lidding films, and thermoformed base webs for fresh pasta, processed meat, and dairy applications.

    Regulation/StandardScopeTest methodTypical control point
    21 CFR 175.105Adhesive component in food-contact articlesEnd-use food-contact complianceIndirect contact via polyolefin skin
    21 CFR 177.1520Olefin polymer baseEnd-use food-contact complianceOlefin polymer constituents
    Regulation (EU) No 10/2011Plastic materials in food contactEN 1186-1Overall migration limit 10 mg/dm²
    REACH Regulation EC 1907/2006EU chemical registrationSVHC declarationNo SVHC above 0.1% w/w

    When Does Dry-Blending Tie Resin into Polyethylene Skins Fail in Cast Barrier Sheet?

    Dry blending of the anhydride-modified LLDPE into the polyethylene skin is not routinely performed in cast barrier sheet because the grafted maleic anhydride concentration at the interface governs adhesion development. The dedicated tie layer addition ratio is 8% to 15% of total sheet thickness, with tie thickness 25–120 µm for 300–800 µm sheet. Converter trials with 10% to 20% tie resin diluted into the polyethylene skin have produced T-peel reductions greater than 40% relative to a continuous tie layer at equal total gauge; published data for this specific configuration is limited, but production-scale twin-screw compounding indicates that dispersed tie resin domain size below 1 µm is required for consistent peel strength according to ASTM D1876. The downstream process uses a five-layer cast sheet line with barrier layer extruder L/D ratio 30:1, sheet die width 800–1200 mm, roll stack temperature 70–90°C, and sheet thickness 300–800 µm. The processing window at the die is 220–250°C; interface instability arises if the tie resin temperature at the combining block falls below 210°C. Compliance status includes 21 CFR 177.1520 and 21 CFR 175.105, with European compliance under Regulation (EU) No 10/2011 when overall migration limits are met. Terminal product types are retortable polypropylene-based multilayer trays, microwaveable bowls, and shelf-stable pet food containers.

    Extrusion Coating Weight and Chill Roll Parameters on Aluminum Foil-Paperboard Lamination

    Aluminum foil-paperboard lamination for aseptic gable-top cartons and laminate tubes employs Bynel® 41E865 as a 5–12 µm layer between aluminum foil and LDPE at a coating weight of 6–15 g/m². The extruder is typically a 90–120 mm single-screw with L/D ratio 30:1, flat die width 900–1300 mm, air gap 150–250 mm, line speed 150–350 m/min, melt temperature 240–260°C, and chill roll temperature 15–25°C. Adhesion to aluminum foil is tested after 24 h conditioning at 23°C per ASTM D1876, with converter specifications commonly rejecting values below 2 N/15 mm for aseptic structures; published data for specific lot-to-lot variation is limited. Compliance is anchored to 21 CFR 175.105 and 21 CFR 176.170 for paperboard contact, Regulation (EU) No 10/2011, and REACH Regulation EC 1907/2006 SVHC declarations. Terminal product types include aseptic gable-top cartons, laminate tubes, and foil-based barrier sachets.

    Blow-molded multilayer high-density polyethylene containers for agricultural chemicals, automotive fluids, and concentrated cleaners introduce the anhydride-modified LLDPE as a separate tie layer between HDPE and EVOH or PA. The tie layer addition is 2% to 5% of the container wall thickness on each side of the barrier layer; for a 1 L bottle with 0.8 mm nominal wall, this corresponds to 16–40 µm of tie resin per side. Accumulator-head or continuous extrusion blow molding machines with parison die gap 1.2–2.0 mm and die head temperature 205–225°C are used, with mold temperature 10–20°C. Because the melt viscosity of the anhydride-modified LLDPE is lower than that of HDPE, layer stability depends on separate extruder melt temperature profiling; screw speed mismatch above 15% between skin and tie extruder is a documented failure mode causing visible layer waviness. Compliance for dangerous goods packaging is established through UN qualification testing under UN Model Regulations Chapter 6.1 for non-bulk packaging, while food-grade variants are supported by 21 CFR 177.1520 and 21 CFR 175.105; European food contact uses Regulation (EU) No 10/2011. Terminal product types are multilayer blow-molded bottles, jerrycans, and automotive fluid containers.

    Three-Layer Polyethylene Pipe Coating with Epoxy Primer Interfacial Bonding

    A three-layer polyethylene pipe coating line for onshore and offshore line pipe introduces the anhydride-modified LLDPE as an adhesive layer between a fusion-bonded epoxy primer and a high-density polyethylene topcoat. The adhesive layer thickness is 150–350 µm within a total coating thickness of 2.5–3.7 mm, representing an addition ratio of 5–12% of the total system. The pipe surface is heated to 170–210°C after FBE application, then the adhesive is extruded through a crosshead die at 190–230°C before the topcoat is applied. Adhesion is evaluated according to ISO 21809-1 and CSA Z245.21 at 23±2°C and 60±5°C; production-scale side-extrusion lines monitor resin lot-to-lot viscosity and leveling pressure because published data for this specific configuration is limited. Compliance is established under ISO 21809-1 and EN 10289 for coating integrity and anti-corrosion performance. Terminal product types are coated steel line pipe for onshore and offshore pipelines.

    Seven-layer cast film coextrusion for polyamide/PE vacuum pouches used in fresh red meat and seafood packaging requires the anhydride-modified LLDPE as two discrete tie layers between PA6 and polyethylene skins. The tie layers each represent 7% to 12% of total film thickness; for a 70–120 µm cast film, this corresponds to 5–14 µm per tie layer. The cast film line uses a 7-layer feedback block with die gap 0.8–1.2 mm, line speed 120–250 m/min, and die temperature 230–250°C; air knife and chill roll parameters are controlled to avoid surface haze and inconsistent tie interface. Adhesion after lamination or pouch sealing is measured by ASTM D1876 after 72 h ambient curing; peel strength below 1.5 N/15 mm is typically rejected for vacuum pouch applications. Food-contact compliance is documented under 21 CFR 177.1520 and 21 CFR 175.105, with European converters relying on Regulation (EU) No 10/2011 and EN 1186-1 overall migration testing. Terminal product types are barrier vacuum pouches, shrink bags, and seafood MAP lidding film.

    Free Quote

    Competitive Dow Bynel® 41E865 Anhydride Modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Bynel® 41E865 is an anhydride-modified linear low-density polyethylene supplied as pellets for use as a tie-layer adhesive in coextruded cast film, extrusion coating, and multilayer sheet. Manufacturer-published nominal data place the melt flow rate at 2.7 g/10 min when measured at 190 °C under 2.16 kg by ISO 1133-1:2022, and the density near 0.910 g/cm³ by ISO 1183-1:2019. The vicat softening temperature is typically reported between 89 °C and 93 °C under ISO 306:2022 Method A50. Differential scanning calorimetry shows a peak melting endotherm near 123 °C to 126 °C. The anhydride functionality is not disclosed as a quantitative graft level on standard commercial documentation; it is defined functionally by adhesion to polar substrates. The product differs from general-purpose LLDPE because the pendant maleic anhydride groups create reactive or strongly polar sites at the interface with ethylene-vinyl alcohol copolymer, polyamide, aluminum foil, and steel. The resin is not intended as a sealant layer or as a bulk structural layer, and its use is limited to tie-layer or adhesive functions in coextrusion or extrusion coating.

    Why Does Anhydride Grafting Alter Adhesion to EVOH and Polyamide?

    Adhesion between nonpolar polyethylene and polar barrier materials is normally poor because the interfacial free energy difference prevents molecular-scale wetting. In 41E865, maleic anhydride grafted onto the LLDPE backbone provides hydrogen-bonding, acid-base, and covalent coupling sites at the interface. The bonding reaction is not instantaneous; it proceeds when the molten tie layer contacts the EVOH or polyamide surface inside the feedblock or die and continues as the film is quenched. On a cast film line, the available contact time is controlled by die-to-chill-roll distance and line speed. If the melt temperature is below 205 °C, viscosity reduction is insufficient for wetting and peel strength measured by ASTM F88/F88M-21 may fall below specification. If the melt temperature exceeds 250 °C, dehydration of the anhydride and possible scission of the grafted functionality reduce the number of effective bonding sites. The hydrolysis of maleic anhydride to maleic acid at the surface can either increase polar interaction or reduce thermal stability, depending on moisture content and residence time. Published data specific to 41E865 for all hydrolysis kinetics is limited; however, the general mechanism is documented in peer-reviewed literature on maleic anhydride-grafted polyolefins.

    On a production cast film line fitted with a 90 mm main extruder and a 45 mm tie-layer extruder, the adhesive layer is commonly metered at 5 % to 10 % of total output. The tie-layer extruder is typically a 30:1 L/D single-screw machine with a general-purpose screw; high-shear screws are avoided because shear heating can create gel particles that become visible in the bond layer. Temperature zones are set to deliver a die melt temperature of 220 °C to 245 °C. The feed throat is maintained below 50 °C to prevent pellet softening and bridging. The resin does not require predrying when stored in closed, dry conditions below 60 % relative humidity. If bags are opened for more than 4 h in a humid plant, surface moisture can hydrolyze anhydride at the die lip; a desiccant dryer set at 80 °C for 4 h is recommended before use. Die-lip buildup, or plate-out, is a common production bottleneck; reducing die temperature by 5 °C to 10 °C and increasing line speed usually restores roll appearance without changing the tie-layer resin. The resin’s compatibility with the main polyolefin is controlled by viscosity ratio; the tie-layer melt flow rate should be within approximately 20 % of the host polyethylene to prevent flow instabilities in the feedblock.

    Melt Temperature and Residence Time Boundaries

    The processing window of 41E865 is bounded by two separate mechanisms. At the lower end, melt temperature below 210 °C does not allow adequate wetting of high-melting polyamide or EVOH surfaces, and interfacial peel force can decline rapidly. At the upper end, temperatures above 250 °C accelerate crosslinking and gel formation, particularly in stagnant regions of the feedblock or die manifold. The maximum practical set point in the metering zone is 260 °C for a 30:1 L/D single-screw extruder with a barrier screw; above this, the residence time at barrel wall temperatures can produce localized degradation even if the melt thermocouple reading remains lower. The dependence on residence time is nonlinear. A residence time of 3 min at 240 °C is generally acceptable, while the same melt held for 10 min at 250 °C may show increased yellowness index and a measurable loss of anhydride functionality. Production experience shows that frequent line stoppages on cast film lines using 41E865 are associated with higher die-lip deposit formation after restart. The deposit is not simple polyethylene gel; it frequently contains hydrolyzed anhydride and polar oligomers. Because published data for this specific configuration is limited, process optimization should be based on a statistically designed trial rather than extrapolation from other anhydride-modified LLDPE grades.

    Operating parameterRecommended envelopeReference or equipment basis
    Die melt temperature210 °C to 250 °CThermocouple at die lip
    Maximum metering zone set point260 °C30:1 L/D single-screw extruder
    Feed throat temperaturebelow 50 °CPlant thermal probe
    Predrying condition80 °C for 4 hDesiccant dryer
    Adhesion testASTM F88/F88M-21Seal-peel tester, 25 mm width

    Field data from cast film lines indicate that the most common failure mode is not bulk resin degradation but uneven distribution of the tie layer in the die. A feedblock designed for polyolefin viscosity ratios may produce side-to-side adhesive variation if the tie-layer melt flow rate differs from the host resin by more than approximately 20 %. The resulting film may pass visual inspection but fail peel testing on one edge. On a 45 mm tie-layer extruder, screw speed variability of less than 5 rpm can cause measurable variation in adhesive layer thickness when the layer ratio is below 5 %. To reduce this variability, processors use gear pumps or gravimetric feeders on the tie-layer extruder. Another production bottleneck is die-lip plate-out at the tie layer die exit, which appears as localized streaks and is often mistaken for moisture defects. Plate-out is minimized by maintaining a steady die temperature and avoiding long residence time during line stops. If a line stop exceeds 15 min, the die temperature should be reduced to 180 °C or the die should be purged with host polyethylene before restart. Published data for this specific configuration is limited, but these practices are consistent with standard polyolefin extrusion troubleshooting.

    Comparative Selectivity Among 41E865, 41E710, and 40E529

    Within the Bynel® family, the anhydride-modified LLDPE grades differ mainly in base resin architecture and intended conversion route. 41E865 is selected for cast film and extrusion coating because it balances melt flow and melt strength for high line speeds. 41E710 is used in blown film, where higher melt tension is needed to stabilize the bubble. 40E529 is based on high-density polyethylene and is used when the tie layer must contribute stiffness or when blow molding containers require higher modulus. The choice between 41E865 and 41E710 is process-driven rather than adhesion-driven; both contain reactive anhydride functionality and bond to EVOH and polyamide. The difference in melt flow rate is small but operationally significant in a feedblock because it changes the viscosity ratio. Published direct peel-strength comparisons under identical coextrusion conditions are limited; therefore, a change from one grade to another should include adhesion measurement on the specific line.

    GradeBase polyolefinTypical conversion routePrimary bonding targets
    Bynel® 41E865LLDPECast film, extrusion coatingEVOH, polyamide, aluminum foil
    Bynel® 41E710LLDPEBlown filmEVOH, polyamide
    Bynel® 40E529HDPEBlow molding, rigid sheetEVOH, polyamide, steel

    When 41E865 Is Substituted for a Blown-Film-Grade Tie Resin in a Cast Line

    Substitution is not a drop-in change. Blown-film tie resins may have lower melt flow and higher melt strength, which can cause melt curtain sag and draw resonance on a cast film line. Conversely, running 41E865 on a blown film line may reduce bubble stability because the resin is optimized for higher shear and higher melt temperature. In a cast film line, 41E865 is usually processed at a die temperature at least 10 °C to 20 °C higher than a blown-film grade to enter its stable curtain envelope. If the die gap is fixed, the melt curtain may require adjustment of the air knife or vacuum box to control neck-in. The greatest process conflict occurs when a converter uses a blown-film grade in a cast line and compensates by increasing barrel temperatures; the result is often gel formation and plate-out rather than improved wetting. The reverse substitution, using 41E865 in blown film, can produce a bubble with a narrower operating window unless internal bubble cooling and a lower blow-up ratio are used. These limits reflect differences in molecular architecture rather than differences in anhydride functional density.

    In a five-layer barrier film of polyethylene/41E865/EVOH/41E865/polyethylene, the tie layers are typically each 5 % to 12 % of total thickness. Peel adhesion is measured after lamination by ASTM F88/F88M-21 or by a 180° T-peel method at 300 mm/min. Published data for this specific structure is limited; a converter should establish internal limits through capability studies. The expected failure mode is cohesive failure in the polyethylene or barrier layer, not adhesive peeling at the tie interface. If interfacial delamination occurs, the cause is more likely melt temperature, moisture, or feedblock residence time than an incorrect resin choice. In extrusion lamination onto aluminum foil, 41E865 is used to bond molten polyethylene to the foil surface. The foil substrate is typically preheated to 25 °C to 50 °C to reduce thermal shock and improve wetting. Corona treatment of the foil or film is generally not required for bonding to the polar metal surface, but oxide type and foil cleanliness influence adhesion. The melt curtain may be run at line speeds above 100 m/min on lines with adequate die width, but the actual speed depends on gauge and polymer temperature. On lines with a 2.5 m die, neck-in and edge trim are controlled by die design and air knife positioning rather than by increasing the tie-layer melt temperature above 250 °C.

    Chemical compliance for 41E865 is lot-specific. In food-contact applications, the resin may be used as a component of multilayer structures subject to 21 CFR 177.1520 for olefin polymers and 21 CFR 175.105 for adhesives where applicable, or European Commission Regulation EU No 10/2011 with its specific migration limits. Industrial users should confirm current supplier regulatory data before use. The resin contains no intentionally added per- and polyfluoroalkyl substances, but confirmation must be obtained from the supplier. Halogen content is typically below detection limits by IEC 61249-2-21; again, lot-specific certificates control. The product is not recommended for direct contact with strong oxidizing agents or with amine-containing additives that can consume anhydride functionality. It should be stored in a closed, dry warehouse at below 40 °C and protected from ultraviolet exposure. When changing from an EVOH or polyamide layer to the tie layer, purging with low-viscosity polyolefin reduces cross-contamination and interfacial gels.