Dow Bynel 41e850 Anhydride Modified Lldpe

Dow Bynel® 41E850 Anhydride Modified LLDPE

    • Product Name: Dow Bynel® 41E850 Anhydride Modified LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 390672
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 5.0 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 85 °C
    Tensile Strength At Break 12 MPa
    Elongation At Break 500%
    Flexural Modulus 170 MPa
    Shore D Hardness 45
    Water Absorption <0.1%
    Thermal Conductivity 0.25 W/m·K
    Coefficient Of Friction 0.2
    Brittleness Temperature < -70 °C

    As an accredited Dow Bynel® 41E850 Anhydride Modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Bynel® 41E850 Anhydride Modified LLDPE is typically packaged in 25 kg polyethylene bags, 40 bags per shrink-wrapped pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL container loaded with Dow Bynel® 41E850 Anhydride Modified LLDPE pellets, palletized in 25-kg bags, securely braced for transport.
    Shipping Dow Bynel® 41E850 Anhydride Modified LLDPE is shipped as non-hazardous polymer pellets. It is not regulated for transport and has no UN number. Standard packaging is sealed bags, boxes, or octabins on pallets. Keep dry and avoid heat, moisture, and contamination. Handle according to the SDS. Maintain package integrity.
    Storage Store Dow Bynel® 41E850 indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep original containers tightly closed and palletized off the floor. Avoid strong oxidizing agents, amines, alcohols, and bases. Maintain recommended ambient temperatures, use stock rotation, and protect from physical damage.
    Shelf Life Shelf life is 36 months from date of manufacture when stored in original unopened packaging at temperatures below 30°C (86°F).
    Application of Dow Bynel® 41E850 Anhydride Modified LLDPE

    What Causes Interlayer Delamination in EVOH Barrier Film During Retort Cycling?

    In a five-layer polyolefin/EVOH barrier blown film, Bynel® 41E850 performs as the discrete reactive layer that suppresses delamination between non-polar LLDPE and the moisture-sensitive EVOH core when the laminate is exposed to 121 °C retort steam for 30 min. The structure is usually designated PE/tie/EVOH/tie/PE, with each tie layer specified at 3–8 µm in a total film gauge of 50–100 µm; the combined adhesive layers therefore account for 10–20% of the cross-section. On a 250 mm annular blown-film die with a 1.2–2.0 mm die gap and a blow-up ratio of 2.0–2.5, the tie-layer extruder is operated at 200–240 °C melt temperature, with layer recombination placed close to the die lip to avoid consuming anhydride functionality before it contacts the EVOH surface. The upper thermal limit is set by EVOH degradation: residence times above 240 °C for more than 8–10 min in the die lip region generate lactone-derived gel defects and reduce interfacial peel strength. The tie-layer melt flow rate is checked under ASTM D1238 or ISO 1133-1:2022 at 190 °C with a 2.16 kg weight; for blown-film lines running 10–15 m/min, a range of 2.0–3.5 g/10 min is generally required because higher flow leads to gauge variation in thin layers and lower flow increases backpressure and reduces wetting. Interlayer adhesion is tested by T-peel on 15 mm strips conditioned at 23 °C and 50% RH according to ASTM D1876, with minimum bond values of 2.0 N/15 mm before retort and 1.5 N/15 mm after 30 min at 121 °C commonly specified. Oxygen transmission rate is monitored by ASTM D3985 at 23 °C and 0% RH, because any breach in the tie layer exposes the EVOH to moisture and collapses the oxygen barrier. Regulatory compliance for food-contact use is evaluated under EU Regulation 10/2011 with overall migration below 10 mg/dm² in the appropriate simulant, while the adhesive component is assessed under FDA 21 CFR 175.105 or as part of a laminate under 21 CFR 177.1395.

    Control pointStandard or equipment referenceTypical condition
    Melt flow rateASTM D1238, ISO 1133-1:2022190 °C, 2.16 kg
    Interlayer peelASTM D187623 °C, 50% RH, 15 mm strip
    Laminate bond strengthASTM F90424 h conditioning, 23 °C
    Oxygen transmissionASTM D398523 °C, 0% RH
    Food-contact migrationEU Regulation 10/2011Overall migration 10 mg/dm²

    Adhesion to aluminium foil in high-speed extrusion coating is governed less by bulk rheology than by the oxidation state of the foil surface, the residence time of the melt curtain in the air gap, and the chill-roll quench profile. When Bynel® 41E850 is placed between LLDPE and aluminium foil in a lidding film or sachet structure, the slot die melt temperature is held at 260–320 °C, the extruder L/D ratio is set to 30:1–36:1, and the die gap is narrowed to 0.5–0.8 mm. The air gap is maintained at 150–250 mm because oxidative melt exposure increases polar bonding to the foil oxide; excessively long air gaps, however, reduce neck-in control and produce edge bead. At line speeds above 300 m/min, the contact time on the chill roll is reduced to less than 0.1 s, and the rapid quench freezes residual stress at the foil-polymer interface unless the chill roll surface is kept between 10 °C and 20 °C and the foil is preheated by infrared heaters to 30–50 °C. Foil surface preparation involves corona discharge at a minimum 38 mN/m wetting tension for thin foil, with atmospheric plasma used when foil temper exceeds 35 µm. Bond strength is measured after 24 h conditioning at 23 °C and 50% RH by ASTM F904 T-peel; industrial specifications frequently require a minimum sealant-to-foil bond of 4.0 N/15 mm for lidding applications, although published data for this specific anhydride-modified LLDPE grade across all foil tempers is limited and line trials are required. For food-contact lidding, the laminate falls under EU Regulation 10/2011 and FDA 21 CFR 177.1395, while the adhesive itself is generally covered by FDA 21 CFR 175.105.

    Three-Layer Polyethylene Pipe Coating Compatibility Windows

    In three-layer polyethylene pipe coating, Bynel® 41E850 is extruded as the intermediate adhesive layer between a fusion-bonded epoxy primer and a high-density polyethylene outer sheath on steel pipe diameters from 219 mm to 1219 mm. The tie-layer thickness is commonly set between 150 µm and 300 µm, which is significantly thicker than flexible packaging tie layers because the coating must survive soil stress, cathodic disbondment, and directional drilling loads. The decisive process variable is not thickness alone but the peak metal temperature at the point where the tie layer contacts the fusion-bonded epoxy primer. Pipe preheat is controlled between 160 °C and 200 °C so that the epoxy is only partially cured and still presents reactive amine and hydroxyl sites; if the pipe surface falls below 140 °C, the anhydride groups cannot interdiffuse with the epoxy network, and peel adhesion tested at 23 °C under ISO 21809-1 can fall below the 15 N/cm acceptance threshold. Above 220 °C, the epoxy primer becomes brittle and may emit volatiles that cause blistering in the overlayer. The tie-layer extruder is usually a 90–120 mm single-screw machine with an L/D of 30:1 and a barrier screw, operated with a zone profile from 180 °C to 240 °C. The melt is introduced through a slot die and pulled around the rotating pipe, with an air ring positioned after adhesive application to keep the melt film smooth before the HDPE outer layer is applied.

    Cathodic disbondment resistance is tested by ASTM G8 at 23 °C with a 1.5 V applied potential for 28 days, and a maximum disbondment radial distance of 12 mm is a typical acceptance value for buried pipelines, although the relevant construction standard controls the exact requirement in each project. Complete coating impact resistance is evaluated by ISO 21809-1 with a 5 kg drop weight at −30 °C depending on service class. Because Bynel® 41E850 is an LLDPE-based material, it contributes greater low-temperature flexibility than LDPE-based tie resins, but its higher melt viscosity narrows the operating window on small-diameter pipe lines running above 5 m/min. The adhesive layer in pipeline service is generally not a food-contact material, but REACH registration and, where applicable, RoHS 2011/65/EU compliance apply for industrial products supplied in the EU.

    Wood-flour-filled LLDPE decking and railing profiles are compounded on counter-rotating twin-screw extruders with L/D ratios of 28:1 to 36:1, where the anhydride-modified LLDPE is fed through the main throat to avoid pre-reaction with surface moisture on the wood. The addition level of Bynel® 41E850 is normally 1–3 wt% of the total compound when wood flour loading is 40–60 wt%. The anhydride groups react with accessible hydroxyl sites on cellulose and hemicellulose during the first 15–25 s of processing at melt temperatures between 160 °C and 190 °C; this residence window is critical because heating above 190 °C releases acetic acid from acetylated hemicellulose and lowers molecular weight. Vent port vacuum is set to at least −0.08 MPa to remove water vapour and volatiles before the pressure build-up section. The coupled compound is extruded through a profiled die at 2–5 m/min, and the hot profile is water-cooled to below 70 °C before flying-cut sawing. Mechanical testing is performed by ISO 527-2 for tensile strength and flexural modulus, with industrial data for anhydride-modified polyolefin coupling agents generally showing a 15–35% increase in tensile strength at 2 wt% addition compared with uncoupled formulations at equal filler loading. Water absorption after 24 h immersion is measured by ISO 62, and weight gain is typically reduced by 20–40% at the same addition level; published data for Bynel® 41E850 in the specific combination of filler species and screw configuration used on an individual line is limited, so laboratory twin-screw trials with actual wood flour moisture are necessary. The end product is a deck board, railing, or outdoor furniture profile that must meet ASTM D7032 for wood-plastic composite deck boards in North America, and REACH documentation applies for EU construction products.

    When ATH Loading Exceeds 60 wt% in LLDPE Jacketing Compounds

    Halogen-free flame-retardant cable jackets filled with 60–65 wt% alumina trihydrate or magnesium dihydroxide create a two-phase system in which the polar filler particles agglomerate unless an anhydride-functionalised LLDPE coupling agent is introduced. In compounding lines using co-rotating twin-screw extruders with L/D ratios of 40:1 to 44:1, the coupling agent is added at 2–5 wt% of total compound, usually by melt side-feeding after the first kneading block, to avoid excessive torque and early filler surface passivation. The barrel temperature profile is kept between 140 °C and 170 °C, because alumina trihydrate begins to dehydrate above 180 °C and the released water vapour can hydrolyse the anhydride before it can form filler-matrix bonds. A vacuum devolatilisation port at −0.09 MPa is placed before the second kneading block to strip released moisture. The finished jacket compound is evaluated by IEC 60811-501 for tensile strength and elongation at break after ageing 168 h at 110 °C. With coupling agent addition, elongation at break for a 60 wt% ATH-filled LLDPE compound can be maintained above 150% before ageing, whereas uncoupled compounds often fall below 120%; these are class-level industrial ranges, and published data for Bynel® 41E850 in a specific co-rotating screw configuration is limited. Flame retardancy is tested by IEC 60332-1-2 single vertical flame propagation, and smoke density by IEC 61034-2 for low-smoke halogen-free specifications. The final product is a cable jacket for building wire, control cable, or automotive cable where the jacket must survive installation at temperatures down to −25 °C and must comply with RoHS 2011/65/EU and REACH for the EU market.

    For Polyamide-Based Barrier Cast Films, a Reactive Tie Layer Must Bridge Amide-End Group Polarity

    In cast coextrusion of LLDPE/tie/PA/tie/LLDPE films for vacuum skin packaging and lidding, the polyamide layer supplies puncture resistance and oxygen performance, but the amide end groups and internal hydrogen bonding make direct adhesion to LLDPE poor. Bynel® 41E850 is metered into the two tie channels at a combined thickness of 8–15% of total film thickness, typically 2–5 µm per side for a 40–70 µm film. The cast film die is set to 0.3–0.6 mm die gap, and the tie-layer melt temperature is held between 220 °C and 250 °C to promote imide or amide reaction products at the polyamide interface. Chilling roll temperature is controlled at 15–25 °C because rapid quench improves film clarity and reduces post-crystallisation haze. Interlayer adhesion is tested by ASTM D1876 at 23 °C and 50% RH, with converters often requiring 3.0 N/15 mm bond strength after 48 h conditioning. Adhesion falls when polyamide layer thickness exceeds 15 µm due to higher crystallinity and reduced surface amine availability; corona treatment of the polyamide layer before tie-layer contact improves wetting but cannot replace the anhydride functionality. The terminal package is a lidding film containing a polyamide barrier layer, where the structure may be used under EU Regulation 10/2011 and FDA 21 CFR 177.1395 if the food contact layer is LLDPE.

    Free Quote

    Competitive Dow Bynel® 41E850 Anhydride Modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Bynel® 41E850 is an anhydride-modified linear low-density polyethylene (LLDPE) supplied in pellet form for use as a tie-layer resin in coextruded and laminated structures. The base polyethylene is grafted with maleic anhydride, producing pendant succinic anhydride groups that can react with nucleophilic end groups on polyamide, ethylene vinyl alcohol (EVOH), ionomer, and aluminium foil surfaces. In multilayer flexible packaging and rigid container sheet, the resin is placed between a non-polar polyethylene layer and a polar barrier layer to prevent delamination during converting and end-use. The grade is designed for thin-gauge adhesive layers, typically 5–15 µm in cast film and blown film structures. Because the anhydride functionality is located on the polymer chain rather than in an external additive package, the interfacial bond forms during the molten contact window and remains stable through subsequent orientation or thermoforming steps.

    How Does Anhydride Grafting Alter Melt Rheology and Substrate Wetting?

    Manufacturer-published nominal data for Bynel 41E850 indicate a melt flow rate of 3.0 g/10 min when measured at 190 °C with a 2.16 kg load in accordance with ISO 1133-1. The nominal density is 0.91 g/cm³ under ISO 1183-1, and the main melting endotherm is near 124 °C under ISO 11357-3. The grafted anhydride raises melt polarity relative to unmodified LLDPE; this improves wetting of polar substrates but also increases sensitivity to hydrolysis and oxidative crosslinking. In laboratory rheometry, the resin exhibits pseudoplastic behavior typical of linear low-density polyethylene, with shear thinning apparent above 100 s⁻¹. At coextrusion melt temperatures of 220 °C to 240 °C, the resin maintains sufficient flow for layer distribution in spiral mandrel dies and flat dies. Prolonged residence above 260 °C is not recommended because chain extension and gel formation can interfere with die lip uniformity. Because the anhydride content is the primary reactive species, dilution through blending with unmodified PE should be limited to avoid reducing peel adhesion below specification. Published data for specific dry-blend ratios is limited and must be confirmed by ASTM F904 peel testing.

    PropertyTest methodNominal value
    Melt flow rateISO 1133-13.0 g/10 min at 190 °C/2.16 kg
    DensityISO 1183-10.91 g/cm³
    Main melting endothermISO 11357-3124 °C

    On five-layer blown film coextrusion lines with polyamide or EVOH barrier cores, Bynel 41E850 is frequently run as the adhesive layer between the barrier core and polyethylene skin layers. Die diameters above 250 mm with spiral mandrel distribution are common; stable bubble geometry is maintained by dual-lip air rings and internal bubble cooling. At output rates above 250 kg/h, melt pressure variation in the adhesive layer extruder should be held below ±0.5 MPa to prevent thickness non-uniformity. A layer thickness variation greater than ±0.5 µm around the bubble circumference has been associated with intermittent delamination after pouch filling and heat sealing. Frost line height is typically maintained between 300 mm and 600 mm when the blow-up ratio is 2.0:1 to 2.5:1. Blow-up ratios above 2.5:1 can reduce bubble stability. Adjusting air ring pressure and cooling air temperature is preferred over increasing melt temperature, which accelerates anhydride degradation.

    Failure Signatures in Cast Film Tie-Layer Thickness Oscillation

    Cast film operations running three-layer polyamide or EVOH structures have shown that tie-layer thickness oscillation is closely tied to adhesive-layer extruder stability. Single-screw extruders with 24:1 L/D and barrier mixing sections are generally suitable, but screw speeds above 80 min⁻¹ on 45 mm barrels can produce surging when solids-conveying zones are optimized for unmodified polyethylene. Thickness variation across the web is measurable by transverse peel testing under ASTM F904; peel readings taken every 100 mm may vary from 4.0 N/15 mm at center to 1.5 N/15 mm near the edge when die lip deposition is present. The deposit is typically oxidized anhydride-rich material formed at the lip exit above 250 °C. Reducing die lip temperature, purging hoppers with nitrogen, and using die-lip configurations with shorter land lengths can delay deposit formation. These corrective actions should be verified by peel retention after 48 h of continuous operation rather than by visual inspection alone.

    In extrusion coating of aluminium foil for retort pouch structures, the anhydride groups on Bynel 41E850 are expected to interact with the hydrated aluminium oxide surface. Peel strength measured by ASTM F904 after conditioning at 25 °C generally exceeds 3.0 N/15 mm when coating thickness is above 15 µm and die melt temperature is 230 °C. Thicknesses below 15 µm may reduce peel values and create pinholes due to incomplete wetting. Corona treatment of the foil at 2.0–3.0 kW·min/m² can improve reproducibility; overtreatment above 4.0 kW·min/m² may create excessive oxide species that weaken the interfacial boundary. Paperboard backings should be conditioned to 5–7 % equilibrium moisture content to prevent steam eruption through the molten polymer. Published data for adhesion on chemically primed aluminium surfaces is limited, and converter trials are required for retort-specific structures.

    When Pellitized Regrind Ratios Exceed 20 Percent in Barrier Structures

    Regrind addition to multilayer barrier films containing Bynel 41E850 requires monitoring of gel count, viscosity shift, and interfacial adhesion. At regrind levels above 20 % of total structure, the adhesive layer may be diluted by commingled barrier and skin polymers, reducing the effective anhydride concentration at the tie-layer interface. This is observable as downward drift in peel adhesion under ISO 11339 T-peel testing after 7 days of film production. If the regrind stream contains nylon or EVOH, moisture and amine or hydroxyl reactions may generate microgels that appear as localized lumps in the melt. Extruder screen packs with 250 µm mesh or finer can be used to remove coarse gels, but pressure rise across the screen pack should not exceed 1.0 MPa because high shear can crosslink the grafted phase. When regrind ratios exceed 30 %, placement of regrind in the polyethylene skin layer rather than the adhesive layer is preferred.

    Accumulator-head blow molded containers with polyamide barrier layers use Bynel 41E850 as the adhesive layer in agricultural chemical and detergent packaging. Pressure fluctuation in the accumulator head below 0.5 MPa during parison extrusion assists uniform layer distribution; higher fluctuation creates weld-line splitting and unequal wall thickness. Because anhydride grafting broadens molecular weight distribution relative to metallocene LLDPE, parison swell is managed by die gap adjustment rather than by melt temperature alone. Sidewall sections can be peeled after notching to assess interlayer adhesion. ASTM F88 seal-strength testing may also be applied to welded sections if the adhesive layer participates in seal joints. Processing temperatures near 220 °C are typical for the tie layer, while barrel zones above 240 °C should be limited to reduce resin degradation during accumulator hold times.

    Thermoformed barrier sheet for modified atmosphere packaging uses Bynel 41E850 in the coextruded sheet structure. Sheet with a polyamide or EVOH core and polyethylene skins is coextruded through a flat die with a width above 800 mm. Die gap setting is typically 0.5–1.0 mm above final sheet gauge to accommodate draw-down. During plug-assisted forming at 1.5–2.0 draw ratios, adhesive layers below 10 % of total sheet thickness may thin disproportionately at corners, causing localized delamination. Preheating at 100 °C to 120 °C with uniform core-layer temperature is necessary. Uneven heating can delaminate the tie layer before the polymer reaches forming temperature. Peel testing under ISO 11339 after 1 h at forming temperature is used to verify adhesion retention in formed corners.

    Why Is Pre-Drying Critical for Anhydride-Modified LLDPE?

    Moisture content in the anhydride-grafted resin is a primary processing variable. At ambient relative humidity above 60 %, pellet surface moisture and absorbed water can hydrolyze anhydride groups to dicarboxylic acid, reducing reactive adhesion and generating volatile species during extrusion. Pre-drying in desiccant dryers at 70–80 °C for 4 h is commonly specified to bring residual moisture below 100 ppm. Drying air dew point should be below -40 °C. Pellets held in open gaylords overnight may show a 5–15 % reduction in peel adhesion due to surface moisture. Resin exposed to rain or high condensate should not be dried and used without first confirming melt flow stability and adhesion by ASTM F904.

    Comparative Position Within the Bynel Adhesive Resin Portfolio

    For tie-layer selection, Bynel 41E850 occupies the low-density, moderate-melt-flow segment of the Bynel anhydride-modified polyethylene range. Compared with anhydride-modified EVA grades, it has lower density and lower moisture absorption. However, EVA-based tie resins may offer better low-temperature wetting on polar substrates at melt temperatures below 200 °C due to higher amorphous content. Compared with acid-copolymer tie resins, the anhydride grade is less likely to release acidic volatiles at 240 °C and is more reactive toward EVOH hydroxyl groups. Acid-copolymer grades may provide simpler adhesion to aluminium foil in some extrusion coating structures. Compared with higher-density maleated polyethylene grades, Bynel 41E850 is more suited to flexible packaging where film softness is required. It is less suited to rigid hot-fill containers where higher Vicat softening point is needed.

    Resin chemistryMelt flow indexDensityAdhesion targetProcess limitation
    Bynel 41E850 anhydride LLDPE3.0 g/10 min0.91 g/cm³PA, EVOH, foilMoisture sensitivity; upper melt limit 260 °C
    Anhydride-modified EVA2.0–6.0 g/10 min0.93–0.95 g/cm³PA, EVOH, aluminiumAcetic acid volatiles above 220 °C; lower thermal stability
    Acid copolymer tie resin2.5–5.0 g/10 min0.93–0.94 g/cm³Aluminium foil, polyolefinThin-layer pH sensitivity; lower reactivity with EVOH hydroxyls

    Regulatory Compliance Matrix and Storage Boundaries

    Regulatory compliance documentation for Bynel 41E850 references FDA 21 CFR 175.105 for adhesives used in food packaging and EU 10/2011 for plastic materials intended to contact food. Specific migration limits for maleic anhydride and derived oligomers must be evaluated in the final multilayer structure because conversion conditions and adjacent layers influence migration into food simulants. The grade is not recommended for direct contact with primary-amine-containing additives because premature imide or amide formation can consume anhydride functionality before the tie-layer interface is formed. Storage in unopened original packaging at temperatures below 40 °C and low humidity reduces pre-drying burden. Opened packaging should be sealed and used within 24 h when plant relative humidity exceeds 60 %.