Dow Bynel 41e762 Anhydride Modified Lldpe

Dow Bynel® 41E762 Anhydride Modified LLDPE

    • Product Name: Dow Bynel® 41E762 Anhydride Modified LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 627813
    Material Type Anhydride Modified Linear Low Density Polyethylene (LLDPE)
    Grafting Agent Maleic Anhydride
    Density 0.931 g/cm³
    Melt Index 190 C 2 16 Kg 2.7 g/10 min
    Melting Point Dsc 124°C
    Vicat Softening Point 88°C
    Tensile Strength At Break 20 MPa
    Elongation At Break 600%
    Flexural Modulus 250 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Thermal Conductivity 0.33 W/m·K
    Processing Temperature 230-260°C
    Adhesion To Evoh Excellent
    Adhesion To Nylon Excellent
    Adhesion To Polyethylene Good

    As an accredited Dow Bynel® 41E762 Anhydride Modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Bynel 41E762 is supplied in 25 kg polyethylene-lined bags, typically stacked on pallets for transport and storage.
    Container Loading (20′ FCL) 20′ FCL dry container loaded with palletized 25 kg bags of Dow Bynel® 41E762 anhydride-modified LLDPE, securely stowed for sea transport.
    Shipping Dow Bynel® 41E762 is shipped as non-hazardous, non-regulated solid pellets in sealed moisture-barrier bags or bulk bags, palletized and stretch-wrapped. Keep dry, clean, and out of direct sunlight. Transport in covered vehicles; avoid excessive heat, moisture, and contamination. No UN number or hazard class required.
    Storage Store Dow Bynel® 41E762 Anhydride Modified LLDPE in a cool, dry, well-ventilated area away from heat, ignition sources, and strong oxidizers. Keep containers tightly closed in original packaging, protected from moisture, direct sunlight, and contamination. Maintain recommended temperature, avoid excessive stacking, and follow SDS. Use first-in, first-out. Store only in labeled, compatible containers, away from acids, bases, and incompatible materials.
    Shelf Life Shelf life is 24 months from manufacture when stored unopened in original packaging below 30°C, dry and protected from moisture.
    Application of Dow Bynel® 41E762 Anhydride Modified LLDPE

    Seven-layer barrier film constructions for protein and dairy packaging run Bynel 41E762 as the reactive tie resin between polyolefin skins and an EVOH core. The resin is introduced through a dedicated satellite extruder with a 24:1 L/D single screw and a compression ratio of 3.0:1, while the barrier layer is melted in a separate 30:1 L/D extruder with a vented barrier screw. The die is a 350 mm seven-layer spiral mandrel assembly with die gap set at 1.8–2.2 mm, a blow-up ratio of 2.0–2.6, and a frost line height maintained between 150 mm and 300 mm below the die lip. Bynel 41E762 has a nominal melt flow rate in the range of 2.5–3.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022, a solid-state density of 0.916 g/cm³ per ISO 1183-1:2019, and a peak melting temperature of 120–122 °C per ISO 11357-3.

    The tie layer thickness is controlled to 10–15 µm per side. Below 8 µm, interfacial contact is discontinuous on blown film lines running above 100 m/min, and the peel resistance drops below the internal specification of 4 N/15 mm measured by ASTM D1876-08. Melt temperatures at the feed block are held at 220–235 °C for the tie resin and 225–245 °C for the EVOH, with interlayer temperature not allowed to fall below 205 °C before the chill roll or nip. The anhydride functionality reacts with ethylene-vinyl alcohol hydroxyl groups at the interface; the reaction rate is strongly dependent on EVOH melt temperature and contact time. Prior to extrusion, EVOH is dried to below 0.10 wt% moisture and Bynel 41E762 is protected from ambient humidity, because anhydride hydrolysis in an open package at relative humidity above 60% for more than 24 h reduces bond strength. The film is evaluated for oxygen transmission rate per ASTM D3985-05 and tensile properties per ASTM D882-18 to verify barrier retention after lamination.

    LayerResinThicknessProcess control
    Outer skinHDPE/LLDPE15–20 µmMelt pressure 200–300 bar
    TieBynel 41E76210–15 µmFeedblock temperature 220–235 °C
    BarrierEVOH 38 mol%5–8 µmDew point −40 °C drying
    TieBynel 41E76210–15 µmThickness profile ±1.5 µm
    Inner sealantLLDPE15–20 µmSeal initiation 105–110 °C

    On seven-layer high-barrier films, batch-to-batch variance in tie resin melt flow above ±0.3 g/10 min can shift layer distribution in the spiral mandrel die and require adjustment of satellite extruder speed. Optical gauge profilers with 1 µm resolution are used to confirm tie-layer uniformity. If gel particles greater than 200 µm appear in the finished film, the tie resin residence time has exceeded the recommended limit or the melt temperature has exceeded 250 °C. The film remains suitable for food contact when the structure complies with FDA 21 CFR 177.1520 and EU 10/2011 as applicable to olefin polymers and adhesive layers.

    Does Anhydride-Modified LLDPE Maintain Adhesion to Aluminium Foil After Retort Processing?

    Extrusion lamination of foil-based retort pouches and lidding uses Bynel 41E762 as a bonding web between aluminium foil and a polyolefin sealant film. The adhesive is processed on a tandem extrusion-coating line in which a 120 mm single-screw extruder with an L/D 32:1 feeds a flat die with a deckle width of 1.2–1.6 m. Barrel temperatures are set between 280 °C and 320 °C, the air gap is 120–180 mm, and the chill roll is held at 12–18 °C with a mirror finish. The coating weight is usually 12–20 g/m², equivalent to approximately 13–22 µm at the nominal melt density. The foil grade is typically 8079 or 8011 aluminium at 7–9 µm, and the foil surface must be free of rolling oil above 5 mg/m² because hydrocarbon residues interfere with wetting and with the reaction between maleic anhydride groups and aluminum oxide hydrate.

    Adhesion of the laminate is measured by T-peel per ASTM F904-16 after conditioning at 23 °C and 50% RH for 48 h. Before retort, cohesive failure in the PE sealant web is the expected failure mode when coating weight exceeds 15 g/m². After retort at 121 °C for 30 min, peel strength may decline by 10–20% depending on foil surface hydration and the moisture transmission rate of the outer layer; published specific values for Bynel 41E762 in this exact configuration are limited. The reduced adhesion is associated with water accumulation at the metal-polymer interface and with pH shifts in the retort water above 8.5. For applications requiring long-duration retort cycles, the foil is primer-treated with an epoxy or silane-based adhesion promoter rather than relying solely on the anhydride bond.

    Line speed is limited by neck-in and draw resonance rather than by adhesion. With Bynel 41E762, stable coating is maintained up to 250 m/min when chill roll tension and air gap are held within stated ranges. At melt temperatures above 325 °C, oxidative chain scission generates low-molecular-weight species that migrate to the foil interface and reduce peel strength; at melt temperatures below 280 °C, incomplete foil wetting produces pinholes and tunnel defects. The laminate is also subjected to water vapor transmission rate testing per ASTM F1249-20 and oxygen transmission rate testing per ASTM D3985-05 to rank retort barrier performance.

    Three-layer external corrosion protection for gas and oil pipelines uses a fusion-bonded epoxy primer, a Bynel 41E762 adhesive tie layer, and a high-density polyethylene topcoat. The steel pipe is blast-cleaned to Sa 2.5 per ISO 8501-1 and heated by induction or gas-fired ring to 190–210 °C. Fusion-bonded epoxy powder is applied at 80–150 µm dry film thickness. The adhesive tie layer is then extruded through a flat die onto the rotating pipe while the FBE remains within its gel stage; the window between FBE gel time and full cure is usually 20–40 s at 200 °C. The Bynel 41E762 layer is deposited at 170–300 µm and melt temperature 200–230 °C, and the HDPE topcoat is applied at 2.5–3.5 mm by a crosshead or flat die with pressure rolls. The anhydride groups form carboxylate bridges with amine-cured epoxy hydroxyl functionalities, and the bond is sensitive to the concentration of unreacted epoxy groups at the FBE surface. If the FBE is allowed to cure beyond the gel point before the tie layer contacts the pipe, adhesion to the tie layer drops sharply.

    The finished coating is tested according to ISO 21809-1:2018, with peel adhesion tested at 23 ± 2 °C and 60 ± 2 °C, and cathodic disbondment tested per ASTM G42-11 or ISO 21809-1:2018 Annex. The tie layer must remain bonded during physical shear events caused by soil movement and during long-term hot-wet service. Published data for the specific peel strength of Bynel 41E762 in three-layer polyolefin systems indicates that the tie layer generally fails cohesively in the HDPE topcoat rather than at the FBE interface when the FBE is correctly applied. If pipe surface roughness drops below Rz 50 µm, mechanical interlock is insufficient and the failure mode changes to adhesive separation at the FBE-primer interface.

    ParameterRangeMeasurement/control
    Pipe preheat190–210 °CIR pyrometer
    FBE thickness80–150 µmDry film thickness gauge
    Tie layer thickness170–300 µmCircumferential thickness gauge
    Topcoat thickness2.5–3.5 mmUltrasonic thickness gauge
    Peel adhesionPer ISO 21809-1:2018Calibrated tensile tester

    Processing on a 24:1 L/D single screw is recommended for the tie layer. The screw should have a low-shear mixing section rather than a high-dispersion pineapple mixer because extensive shear heating above 240 °C may cause pre-gelation of anhydride species and gel particles in the tie layer. The pipe line speed is constrained by the FBE gel time; if line speed increases and the FBE is fully cured before tie layer application, the peel adhesion at 60 °C will be below the acceptance criterion specified by the project specification. The tie resin must be protected from moisture before extrusion because the anhydride functionality hydrolyzes in humid conditions and reduces bond strength to the epoxy primer.

    Compatibilization of Recovered Polyethylene-Polyamide Multilayer Scrap

    Regrind from PE/PA film edges and start-up scrap is compounded with Bynel 41E762 at 3–8 wt% in a co-rotating twin-screw extruder with L/D 40:1 and a side feeder for the polyamide-rich fraction. Barrel temperatures are set from 230 °C to 255 °C, screw speed is 350–500 rpm, and melt filtration through a 100 µm screen pack is used to remove gels. The anhydride-modified LLDPE disperses polyamide domains below 5 µm, and the resulting compound is tested by ASTM D638-14 for tensile and ASTM D256-10 for notched Izod. Addition above 8 wt% does not produce additional mechanical recovery and increases melt pressure at the die. This application is limited to post-industrial scrap with known composition; post-consumer mixed film containing PET or PVC is not a suitable feed because the anhydride functionality does not compatibilize those polymers and thermal decomposition products reduce output quality.

    When Extruded onto Paperboard for Aseptic Liquid Packaging

    Aseptic cartons for dairy and juice packaging use a structure of paperboard, aluminium foil, and polyolefin sealant layers. Bynel 41E762 can be melt-extruded between the paperboard substrate and aluminium foil as the bonding web at a coating weight of 12–25 g/m², corresponding to 13–27 µm at melt density. A single-screw extruder with L/D 30:1 and barrel temperatures of 280–315 °C delivers the melt to a flat die with an air gap of 150–250 mm. The chill roll is maintained at 10–18 °C with a mirror finish and a surface roughness below Ra 0.1 µm. Adhesion of the extruded tie to paperboard is evaluated by peel testing per ASTM D1876-08; fiber tear in the paperboard is the required failure mode. Wetting of the cellulosic substrate depends on the paperboard moisture content, which should be maintained between 4% and 9%. Outside that range, curl and poor nip contact produce tunneling. The anhydride groups react with surface hydroxyls on the cellulosic fibers and on the aluminium oxide layer; however, if the foil is stored above 70% RH, hydrated oxide formation may weaken the bond. The final carton is tested for seal integrity by ASTM F88/F88M-21 and for pinholes by ASTM D3078-02.

    Coextrusion Blow Molded Automotive Fuel Tank Tie Layer

    Six-layer HDPE fuel tanks coextruded for low hydrocarbon permeation place Bynel 41E762 between the HDPE outer/recycle layers and the EVOH barrier. The tie layer is typically 150–250 µm thick in a total wall thickness of 8–12 mm. Accumulator-head blow molding machines with clamp forces of 300–600 t and parison programmers run the tie resin at 215–235 °C; EVOH is processed at 220–240 °C and dried to below 0.05 wt% moisture to prevent bubble formation and loss of barrier. Interfacial peel adhesion in the molded tank is measured on cross-sectioned specimens per ASTM D1876-08; the required failure mode is cohesive in HDPE rather than interfacial at the EVOH tie boundary. Fuel permeation is tested under SAE J1737 or EPA 40 CFR 1051 depending on the vehicle class. The main processing risk is cross-layer flow instability in the accumulator head during parison extrusion; melt flow differences between the tie resin and HDPE above 1.0 g/10 min cause waviness in the EVOH layer. Regrind from trimmed tank flash may be incorporated into the outer HDPE layers without reducing tie layer performance if the regrind fraction is kept below 30%.

    Free Quote

    Competitive Dow Bynel® 41E762 Anhydride Modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Bynel® 41E762 is an anhydride-modified linear low-density polyethylene (LLDPE) tie resin supplied in pellet form for coextruded blown film, cast film, sheet, and extrusion coating. The material is specified by a melt flow rate of 2.7 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1, a density of 0.921 g/cm³ per ISO 1183-1, and a differential scanning calorimetry melting peak of 127 °C per ISO 11357-3. These representative values are drawn from manufacturer literature and are not a substitute for a lot-specific certificate of analysis.

    The product functions by reactive coupling. The pendant anhydride groups on the LLDPE backbone form covalent ester or amide linkages with hydroxyl and amide functionality in ethylene vinyl alcohol (EVOH) and polyamide, while the polyethylene backbone entangles with adjacent polyethylene or polypropylene layers. This mechanism distinguishes the grade from a non-reactive LLDPE tie resin, which relies only on mechanical interlocking and polar attraction. The grade is typically embedded between a polyolefin sealant and a polar barrier substrate such as EVOH, polyamide 6, or polyamide 66 in symmetrical five-layer or seven-layer structures.

    What limits adhesion stability after humid retort or pasteurization?

    Adhesion stability is not a function of the tie resin alone. Interfacial bonding occurs when the tie layer remains molten long enough to wet and react with the polar substrate. On a five-layer blown-film die operating at 230 °C, reactive wetting can occur before solidification. On cast-film lines, however, an overly cold chill roll can quench the interface before complete bond formation. Chill-roll temperatures below 20 °C are associated with lower peel-strength consistency in EVOH-containing structures because the interface freezes before the anhydride reaction front is fully developed.

    After film fabrication, humid retort can hydrolyze unreacted anhydride and reduce bond strength if moisture reaches the interface through the barrier layer. The effect is more severe when the EVOH core thickness falls below 3 µm, because moisture transport through the barrier layer increases. Peel adhesion retention is therefore assessed after retort at 121 °C for 30 min using laminate bond-strength testing per ASTM F904-16 or an equivalent tensile-peel method. Published data for a given laminate configuration should be used for specification purposes; generalized peel-strength claims outside a defined structure are not technically valid.

    Incoming resin quality can be monitored by melt flow rate per ISO 1133-1 and by infrared spectroscopy. Maleic-anhydride-derived carbonyl absorption near 1790 cm⁻¹ and 1860 cm⁻¹ is used to confirm the presence of anhydride functionality. However, quantitative anhydride content requires calibration against a standardized reference material, and FTIR absorbance alone should not replace adhesion testing on the final coextruded structure.

    On production-scale cast-film lines, 41E762 is run as a sub-skin or skin layer with an air gap of 100 mm to 250 mm, a die gap of 0.5 mm to 0.8 mm, and a chill-roll temperature of 20 °C to 35 °C for polyamide-containing structures. Line speeds above 150 m/min may require die melt temperatures toward 245 °C and a low-shear screw design to prevent flow instabilities. Draw resonance is controlled by reducing die-gap width and air gap rather than by increasing tie-layer thickness.

    Extrusion temperature, residence time, and gel formation boundaries

    Molten anhydride-modified LLDPE can form gel specks if local temperature and residence time are excessive. On single-screw extruders with 24:1 to 30:1 L/D, a rear-zone temperature of 180 °C, a mid-zone profile of 210–230 °C, and a die setting of 230–250 °C are typical. The melt temperature should not remain above 260 °C for more than approximately 10 min, because prolonged high-temperature exposure promotes hydrolysis of residual anhydride and subsequent condensation reactions that produce visible gel particles. Stagnant zones in adaptors, screen packs, and die ports should be minimized to avoid local residence-time spikes.

    Pre-drying is not normally required for this LLDPE-based tie resin. If bags are exposed to high humidity or surface condensation, surface moisture can be removed with a desiccant dryer at 80 °C for 2–4 h. Amine-containing purge compounds are incompatible with the anhydride functionality and may leave a higher-viscosity residue at the die lip. A neutral LLDPE or LDPE purge should be used for startup and shutdown.

    In blown-film coextrusion, the grade is processed at a blow-up ratio of 2.0:1 to 2.5:1 and a frost-line height of 4–8 die diameters. Higher blow-up ratios increase transverse orientation and can reduce peel strength in that direction; this is a laminate orientation effect rather than a resin defect. In symmetrical five-layer PE/tie/PA/tie/PE or PE/tie/EVOH/tie/PE structures, tie layers typically occupy 6–10 % of total film thickness. EVOH must be completely encapsulated because edge trim containing exposed EVOH can absorb moisture and produce surface roughness or gel in regrind streams.

    When a grooved-feed extruder with L/D below 24 runs 41E762

    Short grooved-feed extruders may generate insufficient melting if the rear temperature is kept too low. With 20:1 to 24:1 L/D equipment, the rear-zone setpoint should be raised to 190 °C, and the adapter and die zones should be moved toward 240 °C to complete melting. Screw speed should be limited on such machines because high output from a short barrel can produce unmelted material at the die and reduce adhesion consistency.

    Die-lip buildup is more common on low-shear lines because of local oxidation at the metal surface. Maintaining the die lip 5–10 °C above the melt temperature and avoiding excessive lip opening reduces die-lip deposit formation. If optical gel detection identifies particles larger than 100 µm, residence time should be reduced, screen-pack area increased, and stagnant adapter sections removed or modified.

    Controlling the property ceilings against EVA- and HDPE-based tie layers

    Compared with anhydride-modified LDPE, the LLDPE backbone of Bynel® 41E762 provides higher tensile elongation and dart-impact resistance in film. The tradeoff is lower melt strength and wider neck-in during high-draw extrusion coating. Compared with anhydride-modified HDPE, this grade has a lower melting peak of 127 °C and lower modulus, which improves low-temperature flexibility but limits continuous service at higher temperatures. Compared with EVA-based tie layers, the anhydride chemistry creates covalent interfacial bonds rather than relying on hydrogen bonding; this difference is most apparent after humid aging, repeated flexing, or contact with aggressive liquid products.

    Non-reactive LLDPE tie resins may fail to bond to EVOH and polyamide under retort conditions because no covalent interfacial layer is formed. The anhydride modification in 41E762 does not make the resin a sealant; it is intended to be buried beneath a polyethylene or polypropylene sealant layer. The grade is also not designed for injection molding or blow molding applications where high melt stability under low-shear, long-residence-time conditions is required.

    In food-contact packaging, the regulatory status of the final structure is governed by the complete composition and end-use conditions. The polyethylene backbone is evaluated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 as applicable. However, the anhydride-modified layer must meet the specific migration limit for maleic anhydride or be separated from food by a functional barrier. REACH and RoHS documentation should be confirmed for each lot before use in restricted applications.

    Compliance checklist for Bynel® 41E762 in packaging structures
    Regulation or standardRelevant provisionTypical assessment
    FDA 21 CFR 177.1520Olefin polymers for food contactApplicable to the LLDPE backbone when final structure and end-use conditions comply; supplier confirmation required
    EU Regulation (EU) No 10/2011Plastic materials and articles intended for food contactOverall migration limit 10 mg/dm²; specific migration of maleic anhydride and additives is structure-dependent
    REACH Regulation (EC) No 1907/2006SVHC communication under Article 33No SVHC above 0.1 % w/w in supplier safety data sheet; verify lot-specific documentation
    RoHS Directive 2011/65/EU Annex IILead, mercury, cadmium, hexavalent chromium, PBB, PBDENot primarily intended for electrical and electronic equipment; no intentionally added RoHS-restricted substances

    Lot-to-lot variability should be controlled through incoming melt-flow-rate testing per ISO 1133-1 and through periodic confirmation of anhydride functionality by infrared spectroscopy. The performance of the final laminate is best evaluated on the production line using the actual substrate combination, tie-layer thickness, and thermal history, because no single resin property predicts adhesion in every coextruded structure.

    Top