| HS Code | 821268 |
| Chemicaldescription | Anhydride-modified linear low-density polyethylene (LLDPE) |
| Anhydridetype | Maleic anhydride grafted |
| Form | Pellets |
| Color | Natural |
| Density | 0.925 g/cm³ |
| Meltindex | 2.5 g/10 min (190°C/2.16 kg) |
| Meltingpoint | 123 °C |
| Vicatsofteningpoint | 93 °C |
| Tensilestrengthatbreak | 17.2 MPa |
| Elongationatbreak | 600% |
| Flexuralmodulus | 207 MPa |
| Hardnessshored | 50 |
| Waterabsorption | 0.01% |
| Thermalstability | Good |
| Dielectricconstant | 2.3 |
| Volumeresistivity | 1E16 ohm·cm |
As an accredited Dow Bynel® 41E755 Anhydride Modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Bynel® 41E755 Anhydride Modified LLDPE is supplied in 25 kg polyethylene-lined bags, palletized for industrial shipping. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Dow Bynel® 41E755 Anhydride Modified LLDPE in 25 kg bags, palletized, approximately 18–20 MT per container. |
| Shipping | Dow Bynel 41E755 is shipped as solid pellets in sealed moisture-barrier bags, drums, or octabins. It is typically not classified as dangerous goods for transport. Keep dry, closed, and away from heat or sunlight. Follow the SDS and local regulations. No special DOT/IATA/IMDG labels normally required. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed, labeled, and upright to prevent moisture contamination. Avoid contact with oxidizing agents. Protect from excessive temperatures and humidity. Store at ambient temperature; do not exceed manufacturer's recommended limits. Use first-in, first-out stock rotation. Use appropriate personal protective equipment when handling. |
| Shelf Life | Dow Bynel 41E755: typical shelf life is 24 months from manufacture when stored unopened, cool, dry, and protected from moisture. |
In five-layer and seven-layer cast barrier lines configured with symmetrical polyethylene skins around an ethylene vinyl alcohol core, Bynel 41E755 is introduced as the molten tie stratum between the non-polar LLDPE skin and the polar EVOH layer. The anhydride grafts on the LLDPE backbone undergo a ring-opening reaction at the EVOH interface, forming ester linkages and hydrogen bonds across a boundary that would otherwise fail at peel loads below 0.3 N/15 mm. For a film total thickness of 45–70 µm, the two tie layers together are usually maintained at 8–12 wt% of the structure while the EVOH core remains at 7–10 wt%, preserving the oxygen barrier required for modified atmosphere protein packaging. The tie resin is metered through a 30:1 L/D single-screw extruder with a barrier screw, using a barrel temperature profile from feed to metering of 160–195–220–235°C and a melt connection temperature of 225–245°C. The cast die is controlled across zones at 235–250°C, and the air gap to the chill roll is held between 15–30 mm; the chill roll surface is maintained at 15–25°C to suppress post-extrusion crystallisation and limit curl caused by asymmetrical thermal shrinkage between the EVOH and LLDPE phases. Interlayer adhesion is commonly measured by ASTM D1876-15 on specimens cut in the machine direction after 24 h conditioning at 23°C and 50% RH; many production specifications set a minimum T-peel strength of 2.5 N/15 mm for EVOH-to-tie failure in the film.
Tie layer thickness below 2 µm per side creates a critical peel-strength cliff edge because the available anhydride groups at the EVOH boundary are insufficient to saturate reactive sites. At the opposite extreme, continuous tie layers above 5 µm per side displace barrier resin and become a source of gauge variation on high-speed winders, particularly when chill roll temperature drifts above 28°C. The typical oxygen transmission rate for a 55 µm five-layer cast structure containing 8 wt% EVOH is below 1.0 cm³/(m²·d·atm) at 23°C and 0% RH when measured by ASTM D3985-17, but this value is highly dependent on EVOH grade and total EVOH thickness. Food-contact compliance is evaluated under the intended end-use condition; in the EU the structure is assessed against specific migration limits in EU Regulation (EC) No 10/2011, Annex II, and in the US the adhesive component is generally referenced under FDA 21 CFR 175.105 with the final laminate subject to the applicable food-type simulant extraction.
| Control parameter | Standard or reference | Typical condition for five-layer cast film |
|---|---|---|
| Interlayer T-peel strength | ASTM D1876-15 | 300 mm/min crosshead, 25 mm specimen |
| Oxygen transmission rate | ASTM D3985-17 | 23°C, 0% RH, 55 µm film |
| Incoming resin melt flow rate | ISO 1133-1:2022 | 190°C, 2.16 kg |
| EU food-contact migration | EU Regulation (EC) No 10/2011, Annex II | Simulant D1, D2 or D3 depending on food type |
| US adhesive component compliance | FDA 21 CFR 175.105 | Final structure extraction under end-use conditions |
The melt curtain in extrusion lamination converts Bynel 41E755 under high temperature and short contact time, making adhesion development time-dependent and strongly influenced by the oxide layer on the foil. The anhydride groups bond to hydrated aluminium oxide and surface hydroxyl species, but the aluminium foil surface is hygroscopic; storage above 60% RH before lamination produces adsorbed water that expands in the nip and forms a weak boundary layer. In a typical tandem laminator, the resin is plastified through a 90 mm extruder with 30:1 L/D at a melt temperature of 260–285°C, discharged through a slot die with a gap of 0.5–0.8 mm, and drawn through an air gap of 100–200 mm before the laminating nip. The chill roll is maintained at 15–25°C, and the nip pressure is set to 25–40 N/mm across the web width to promote wet-out without crushing the 7–9 µm aluminium foil. T-peel adhesion is measured by ASTM D1876-15; converter specifications for foil-to-LLDPE structures commonly require between 2.5 N/15 mm and 4.0 N/15 mm after 24 h.
At line speeds above 200 m/min, the contact time between the molten web and foil is shortened, and the rate of anhydride ring-opening at the metal surface becomes the limiting step. This is more severe in the presence of aluminium stearate or hydrocarbon processing aids that bloom to the melt surface and occupy oxide sites before the tie resin contacts the foil. Converters often respond by raising melt temperature to 285–300°C, but long residence time above 290°C promotes oxidative chain scission and gel formation, producing visible die-lip build-up and smoke. A more stable response is to restrict the air gap to below 150 mm and to preheat the foil to 35–45°C using a contact roll before the laminating nip. No primer is normally used when Bynel 41E755 is the only adhesive layer; when converters add water-based primers, they create a competing polar surface that can reduce peel strength if not fully dried. Published data for prolonged runs above 250 m/min on this specific grade is limited, so line qualification must be completed on the target laminator. Terminal products include lidding foil for dairy multipacks, aseptic brick sachets, and stand-up pouches where the laminating ply separates the barrier foil from the sealant LLDPE.
In extrusion blow moulding, the accumulator head integrates six melt streams into a parison where HDPE skins, a regrind core, EVOH barrier, and tie layers are arranged symmetrically: HDPE / regrind / tie / EVOH / tie / HDPE. Bynel 41E755 is metered as the tie layer at 1.5–2.5% of total bottle wall thickness per side, while EVOH is held at 3.0–4.5% and the regrind layer is typically allowed to reach 40–50% of the total wall. The die head is zoned at 200–230°C, with the polyethylene layers extruded from barrel profiles of 170–210°C, the tie resin at 210–230°C, and EVOH at 210–225°C. Blow air pressure is maintained at 0.7–1.0 MPa, the mould surface temperature is 8–15°C, and the parison programmer is tuned to prevent layer inversion at the pinch-off where barrier layers can pinch to zero thickness. Adhesion is tested on flat sidewall sections using ASTM D1876-15; a production floor specification of 2.0 N/15 mm or higher is common for EVOH-to-HDPE bonding through the tie layer after 24 h conditioning.
Regrind streams in this structure contain mixed polymer from bottle trim, and each heat history above 220°C reduces the concentration of intact anhydride functionality in the recycled tie fraction. At regrind loadings above 40%, converters frequently observe a non-linear drop in sidewall peel strength because the regrind pushes the active tie layer away from the EVOH interface and introduces oxidised low-molecular-weight species that inhibit ester linkage formation. The failure mode shifts from cohesive in the tie resin to adhesive at the EVOH-tie boundary, and bottle drop impact tested by ASTM D2463-15 can decline when a filled bottle is dropped at -20°C. Published data for this specific grade in high-regrind blow moulded containers is limited; however, production experience indicates that regrind content should be restricted to 35–40% when EVOH adhesion is critical, and scrap streams should be dried to below 0.05% moisture before re-extrusion. End products include household chemical containers, edible oil bottles, and agricultural chemical packages where the EVOH layer keeps odour and oxygen ingress within specification.
On flat-die coextrusion lines producing HDPE/EVOH barrier sheet for thermoformed food trays, the molten web exits the die into a vertical three-roll stack where Bynel 41E755 must maintain interfacial adhesion during both the machine-direction draw and the subsequent solid-phase stretching in the thermoform tool. The sheet is typically built as HDPE / regrind / tie / EVOH / tie / HDPE, with total thickness between 0.8 mm and 2.5 mm. The HDPE skins carry the structural load, the regrind core is held at 40–50% of the structure, each tie layer is maintained at 2–3% of total thickness, and the EVOH barrier is kept at 3–6%. Extruder barrel temperatures for the HDPE layers are set from 180°C to 210°C, the tie resin is processed at 220–235°C, and the EVOH is fed through a separate screw with melt temperature 220–230°C; the feedblock and sheet die are zoned at 230–240°C to prevent viscosity stratification at the layer boundaries. The three-roll stack runs with top roll temperatures of 80–95°C, centre roll temperatures of 90–105°C, and bottom roll temperatures of 70–85°C to control sheet crystallinity and reduce curl before the puller.
The draw ratio in the thermoforming cavity creates the main failure risk. On deep-draw trays with a depth-to-opening ratio above 0.5, the tie layer can thin from its original 2.5–3.0 µm to below 1.0 µm at the corners, at which point the EVOH-to-tie peel strength drops below the minimum acceptable level and the part shows ring-shaped delamination after impact. Forming shops compensate by lowering surface heating temperatures to 130–140°C and using plug-assisted vacuum forming with mould temperatures of 15–25°C, but if the sheet is too cold the EVOH layer fractures before it draws into the cavity. Adhesion on the flat sheet is measured by ASTM D1876-15; after thermoforming, the corner section is tested by hand peel or by a modified peel fixture because the curvature prevents a standard 25 mm wide specimen. Scrap from sheet edge trim is ground and returned to the regrind layer, but repeated exposure of the tie resin to temperatures above 220°C reduces interfacial bond strength; converters usually limit regrind insertion to 40% and monitor sidewall peel strength at the start of each shift. End products include barrier trays for fresh pasta, cook-chill ready meals, and MAP red meat packaging, where the EVOH layer limits oxygen ingress and the tie resin prevents tray delamination during refrigerated distribution.
A cast film converter that substitutes polyamide 6 for EVOH in a five-layer structure retains Bynel 41E755 as the tie layer because the anhydride grafts react with terminal amine and amide groups in the polyamide, producing a robust interphase without the moisture-limited oxygen barrier sensitivity of EVOH. The structure is typically LLDPE skin / tie / polyamide 6 / tie / LLDPE skin, with total film thickness between 65–90 µm and tie layers each held at 3–5 µm. The nylon layer must be pre-dried to below 0.08% moisture content before entering the extruder; otherwise rapid hydrolysis at melt temperature creates bubbles and microvoids in the barrier layer and reduces interlayer adhesion. The tie resin is extruded at 230–250°C, the polyamide at 240–260°C, and the die is kept at 245–250°C, with a chill roll temperature of 15–20°C. Adhesion measured by ASTM D1876-15 on the polyamide-to-LLDPE interface is usually specified above 2.0 N/15 mm after 24 h at 23°C and 50% RH; failure normally occurs in the tie layer rather than at the interface when the interphase is fully reacted.
The replacement of EVOH with polyamide shifts the primary end-use advantage toward aroma and puncture resistance rather than oxygen barrier under dry conditions. Deep-draw vacuum skin packaging lines can run this film on automatic thermoforming machines with forming temperatures of 95–115°C, where the PA6 layer provides the required draw depth and oil resistance for processed meat and cheese. If a converter selects polyamide 66 instead of polyamide 6, the processing threshold rises to 270–285°C, which is above the practical continuous-processing stability window of the LLDPE-based tie resin; at that point residence time must be shortened and die-lip purging intervals must be increased. Published data for prolonged runs of Bynel 41E755 with PA66 is limited, so production trials with the exact die configuration and reclaim flow are required before commercial commitment. The finished laminate is assessed for food-contact compliance under EU Regulation (EC) No 10/2011, Annex II and FDA 21 CFR 175.105, with the final structure subject to the same migration limits as the EVOH-containing counterpart.
Competitive Dow Bynel® 41E755 Anhydride Modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Bynel® 41E755 is an anhydride-modified linear low-density polyethylene supplied as a pelletized adhesive resin. In coextruded barrier packaging, the grade is placed between polyethylene-based skin layers and polar core layers such as ethylene-vinyl alcohol copolymer or polyamide. The LLDPE backbone provides density and melting characteristics similar to conventional liner-grade LLDPE, while the grafted anhydride functionality supplies carbonyl reactivity at the interface. The resin is intended for cast film, blown film, and extrusion coating processes rather than injection molding. It is not an adhesion promoter masterbatch; it is metered directly into the coextrusion feedblock or die as a discrete tie layer.
Table 1 lists representative physical property data from the product datasheet. These values are lot-release indicators and should not be used as design specification limits for a finished laminate without confirming the current certificate of analysis for the specific batch.
| Property | Test standard | Nominal value |
|---|---|---|
| Melt mass-flow rate, 190°C/2.16 kg | ISO 1133-1 | 2.0 g/10 min |
| Density, 23°C | ISO 1183-1 | 0.930 g/cm³ |
| DSC melting peak | ISO 11357-3 | 126°C |
| Vicat softening temperature, A50 | ISO 306 | 107°C |
When processed as a discrete tie layer on a three-layer cast film line, the resin is usually assigned to the satellite extruder feeding the tie layer. A flat barrel temperature profile of 200°C to 230°C and an adapter/die zone of 230°C to 250°C are appropriate when the screw is a barrier design with an L/D ratio of 24:1 to 30:1. Back pressure should remain above 70 bar to maintain stable melt-pump suction; lower back pressure can produce screw surging and tie-layer thickness oscillation at line speeds above 150 m/min. The addition of a gear pump between the extruder and die is recommended when the tie-layer target thickness is below 0.2 mil (5 µm).
The development of peel strength is governed by melt temperature at first contact, contact time before quenching, and thermal history of the barrier layer. In a five-layer blown film line producing PE/tie/EVOH/tie/PE tubing, the tie resin contacts EVOH inside the die and remains in contact through the air gap until the bubble reaches the frost line. If melt temperature is below 220°C, poor wetting can produce a weak boundary layer even though anhydride functionality is present. If die temperature exceeds 250°C, the anhydride group can undergo thermal decomposition or premature reaction, reducing available bonding sites at the interface. The practical upper processing limit for this grade is therefore 250°C for short residence times; prolonged hold-up should be avoided. Published data for this specific configuration is limited, especially for line speeds above 250 m/min.
Adhesion should be measured on the finished coextruded structure rather than on compression-molded plaques. A 180° T-peel test at a crosshead speed of 200 mm/min according to ISO 11339 or ASTM F88 is commonly used. When the tie layer is thinner than 0.1 mil, the failure mode often changes from interfacial delamination to cohesive failure of the polyethylene skin, making direct comparison of peel strengths unreliable.
In five-layer blown film structures containing PA6/EVOH/PA6 core layers, the tie resin is exposed to two different polar interfaces. Polyamide grades containing migratory slip or antiblock additives can reduce adhesion, so the polyamide should be specified without such additives where maximum peel strength is required. EVOH containing 32 mol% ethylene has a higher hydroxyl density than 44 mol% ethylene grades, and the anhydride functionality on Bynel 41E755 interacts more strongly with the higher hydroxyl density. Final peel strength also depends on the viscosity ratio between the tie layer and EVOH at die temperature; excessive mismatch can cause interfacial waviness. A cone-and-plate rheometer measurement at 230°C and 1–100 s⁻¹ is used to compare viscosity curves of candidate tie and barrier resins before production trials.
Because the product is a neat LLDPE-based resin, it should not be fed through a low-shear general-purpose screw designed for easily plasticating LDPE. A three-zone screw with a compression ratio of 2.5:1 to 3.5:1 and a barrier flight in the transition section is suitable for film-grade LLDPE. The metering section should be 30% to 40% of screw length to provide sufficient micro-mixing without excessive shear heat. If a Maddock mixer is installed, its clearance should be maintained at 0.25 mm to 0.4 mm; tighter clearances can raise melt temperature by 5°C to 10°C and initiate gel formation. The die lip should be cleaned with brass tools; steel tools can score chrome plating and create local stagnation zones that degrade the resin.
Intermittent operation is more damaging to this grade than continuous operation. During startup and shutdown, the tie-layer extruder should be purged with unmodified LLDPE of similar melt index, and the temperature should be reduced to 170°C when the line is idle for more than 30 minutes. This reduces oxidized material in the feedblock and prevents brown specks during the next run.
Moisture uptake by the pellet surface is another operational boundary. The resin should be stored at 50°C or below in sealed packaging. At ambient relative humidity above 60%, pellets can adsorb enough surface moisture to create bubbles or pinholes in the tie layer during extrusion. Pre-drying in a desiccant dryer at 80°C for 2 h is a conservative measure when packaging has been opened for more than 24 h in humid conditions.
The anhydride functionality is diluted when the tie layer is mixed with unmodified polyethylene regrind. If the regrind fraction exceeds 20% by weight of the tie layer, peel adhesion to EVOH can decline because the concentration of available anhydride groups at the interface is reduced. The decline is not linear with dilution; surface excess concentration of functional groups depends on melt diffusion and interfacial segregation rather than bulk composition alone. For critical barrier applications, the tie layer should be run as a 100% virgin stream. If edge trim must be re-used, it should be partitioned into the bulk PE skin layer rather than the tie layer. Incorporation of polyamide regrind into the tie layer is not recommended because free amine groups in the polyamide can react with the anhydride group, increasing melt viscosity and generating gel particles.
The incompatibility with primary amine-containing additives also applies to slip concentrates and antistatic concentrates that may contain amide waxes or amine-based antistats. Such additives should be kept out of the tie-layer extruder. If antistatic performance is required in the final structure, it should be placed in the PE skin layer or applied as an external coating after film formation.
Table 2 summarizes the functional placement of Bynel 41E755 relative to other tie-resin classes. The LLDPE backbone is the principal difference from maleic anhydride grafted LDPE grades, which may have lower dart drop resistance and tear strength at equivalent melt flow. Because the LLDPE backbone contains short-chain branches but no long-chain branching, it provides different extensional viscosity and bubble stability in blown film. On a blown film line with a 300 mm die and a blow-up ratio of 2.5:1, the tie layer must support the bubble during expansion; LLDPE-based resins often require a slightly higher frost line or smaller die gap than LDPE-based tie resins to prevent unstable bubble deformation. The anhydride modification does not eliminate the characteristic LLDPE melt behavior.
| Resin class | Functional group | Melt flow rate at 190°C/2.16 kg | Thermal processing ceiling | Primary limitation |
|---|---|---|---|---|
| Anhydride-modified LLDPE, Bynel 41E755 | Anhydride graft | 2.0 g/10 min | 250°C short residence | Hydrolysis sensitivity in humid storage |
| Unmodified LLDPE | None | 1–2 g/10 min | 260°C | No adhesion to EVOH or polyamide |
| EVA tie resin | Acetate | 5–20 g/10 min | 220°C | Acetic acid evolution above ceiling |
| Acid copolymer tie resin | Acid/ester | 5–10 g/10 min | 230°C | Corrosive to steel at high temperature |
Compared with ethylene-vinyl acetate tie resins, this grade has higher thermal stability because it does not liberate acetic acid at processing temperatures. EVA-based tie resins containing 18% to 28% vinyl acetate begin to degrade above 220°C, producing acetic acid and causing corrosion of downstream equipment and odor in the final film. The anhydride-modified LLDPE can tolerate short excursions to 250°C, but it is not fully resistant to oxidation. Oxidative degradation accelerates at high screw speeds above 150 rpm on a 45 mm extruder; the actual limit depends on screw design and back pressure.
Compared with acid copolymer tie resins, the anhydride-modified grade is not intended for direct adhesion to aluminum foil or metalized substrates. Acid copolymer and ionomer adhesives provide ionic bonding to metal oxides, a mechanism that is not present in this product. For foil-containing retortable structures, a different adhesive system or an external primer should be used. Bynel 41E755 is designed primarily for polyolefin-to-EVOH or polyolefin-to-polyamide adhesion in flexible packaging, not for rigid barrier containers.
Food-contact compliance for the neat resin should be verified through supplier regulatory documentation. Many anhydride-modified polyolefin tie layers of this class are manufactured to meet FDA 21 CFR 175.105 for adhesives when used in compliance with stated limitations. The anhydride modification does not automatically confer direct food-contact status under 21 CFR 177.1520 for polyolefins, so the tie layer must be separated from food by a functional barrier unless migration testing under Regulation (EU) 10/2011 demonstrates compliance. Heavy metals restricted under RoHS Directive 2011/65/EU are not intentionally added to the resin, but end-product certification must be based on the finished laminated or compounded article.