| HS Code | 924024 |
| Chemicalfamily | Linear low density polyethylene (LLDPE) |
| Modification | Anhydride-modified |
| Form | Pellets |
| Color | Natural |
| Density | 0.92 g/cm³ |
| Meltindex | 3.0 g/10 min at 190°C/2.16 kg |
| Meltingpoint | 122°C |
| Vicatsofteningpoint | 91°C |
| Tensilestrengthatbreak | 18 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 270 MPa |
| Hardness | 50 Shore D |
| Thermalstability | 260°C |
| Waterabsorption | 0.03% |
| Adhesiontonylon | Excellent |
| Adhesiontoevoh | Excellent |
| Adhesiontometal | Excellent |
As an accredited Dow Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Bynel 41E556 comes in 25 kg moisture-resistant bags, palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Dow Bynel 41E556 adhesive resin, 25 kg bags, palletized, shrink-wrapped, and securely stowed for ocean transport. |
| Shipping | Dow Bynel® 41E556 ships as a non-hazardous, non-regulated solid resin in sealed 25 kg bags or bulk containers. It requires no DOT/IMDG/IATA hazard labels. Keep dry, cool, and out of direct sunlight; avoid moisture and prolonged heat. Follow local regulations and the manufacturer’s SDS. |
| Storage | Store Dow Bynel® 41E556 in a cool, dry, well-ventilated area using original, tightly closed containers. Protect from direct sunlight, heat, moisture, and contamination. Keep away from oxidizing agents, acids, and bases. Maintain recommended ambient temperature and avoid prolonged exposure above supplier limits. Use first-in, first-out. Reseal opened packages promptly. Inspect containers regularly for damage or leaks. Follow SDS and local regulations. |
| Shelf Life | Shelf life is 2 years from manufacture when stored in original unopened containers under recommended storage conditions. |
The anhydride-modified LLDPE grade Bynel® 41E556 is specified in coextruded structures where a non-polar polyethylene surface must be melt-bonded to a polar barrier polymer such as ethylene vinyl alcohol copolymer or polyamide. Manufacturer technical data list a melt flow rate of 3.6 g/10 min under ISO 1133-1 at 190°C/2.16 kg and a density of 0.905 g/cm³ under ISO 1183-1. The anhydride graft level is not published, but the resin is qualified by its ability to maintain interlayer adhesion at low tie-layer thickness without excessive die drool or surface haze. Food-contact use of structures containing Bynel® 41E556 must be confirmed against 21 CFR 175.105 for adhesives or 21 CFR 177.1520 for olefin polymers, depending on the classification of the tie layer in the finished article. Migration testing under EU Regulation 10/2011 may be required for fatty and aqueous simulants because the final laminate, not the resin alone, determines overall migration.
In five-layer blown film production, a common structure is LLDPE skin / Bynel® 41E556 tie / EVOH core / Bynel® 41E556 tie / LLDPE skin. Tie layers are typically run at 8–12 µm within a total gauge of 50–80 µm. The tie-layer extruder is frequently a 45 mm single-screw unit with 30:1 L/D and a grooved feed section; barrel settings from 180°C in the feed zone to 225°C at the metering zone are used to prevent unmelted pellets from reaching the die. The critical processing boundary is the EVOH core temperature. If the core layer exceeds 240°C for more than 10 min, gel-like discoloration and streaking appear at the tie-layer interface, and peel delamination under flex-crack testing becomes more likely. Consequently, the die adapter and spiral mandrel distribution are held at 220–225°C to balance tie-layer flow stability against barrier-layer degradation. Adhesion is measured after 24 h conditioning at 23°C and 50% RH using ASTM F904-16, with a jaw separation speed of 200 mm/min. Published peel data for this exact tie/EVOH combination are limited, and converters establish internal control limits through line qualification. Oxygen transmission rate is monitored separately by ASTM D3985-17 at 23°C and 0% RH to confirm the EVOH core has not been degraded by the tie-layer heat history.
Moisture-related adhesion loss is detectable when pellets are left uncovered above 60% RH for more than 8 h. Hydrolysis of the anhydride functionality reduces the number of reactive sites available for interaction with EVOH. A desiccant dryer set at 80°C for 4 h is the standard correction. In production lines without a dryer, re-sealed original packaging and immediate use of partially consumed containers are mandatory. Laminated films are subjected to gelbo flex testing according to ASTM F392/F392M-21; delamination after 50 flex cycles is treated as a barrier-integrity failure for retort or hot-fill pouches. The tie layer also influences dart impact resistance measured by ASTM D1709-22; a tie-layer thickness reduction below 6 µm often increases interfacial stress concentration and lowers the dart impact value, although the exact threshold depends on the skin resin and EVOH ethylene content.
At the compounding stage, addition of amine-based slip or antistatic masterbatches into the tie layer is avoided because the anhydride can react with free amine species during extrusion, producing a measurable increase in melt pressure and surface haze. When slip is required, it is placed in the skin layer instead. The same restriction applies to zinc stearate-type lubricants at loadings above 0.1 wt%, which can migrate to the EVOH interface and interfere with adhesion. During shutdown, the tie-layer extruder is purged with low-density polyethylene until melt pressure stabilizes; residual EVOH in the adapter can otherwise crosslink and produce persistent black specks on restart.
Barrier blow molding of HDPE bottles for agricultural chemical or personal care products subjects the tie layer to lower melt pressures than film extrusion but longer parison contact with the die bushing. In a six-layer coextrusion blow molding machine with a 65 mm extruder and 25:1 L/D, the Bynel® 41E556 layer is metered at 2–4% of the total wall thickness. Melt temperature at the die head is held between 210°C and 225°C. The key failure mode is not bubble instability but layer folding and thinning at the pinch-off weld, where the barrier core can approach the surface. When the tie layer is too thin at the weld line, a pinhole defect appears in the finished bottle, detected by ASTM D4991-07(2023) vacuum leak testing. The pinch-off tail is also inspected for interlayer separation; converters may set a maximum allowed separation of 1.5 mm from the weld. Because bottle production often includes post-consumer recyclate in the HDPE skin layers, the tie layer must tolerate minor contaminants such as polyamide residues from closures; the anhydride functionality absorbs these residues by reactive compatibilization. However, the moisture content of the recyclate must be kept below 0.05% by weight to prevent hydrolysis of the tie resin. A desiccant dryer is therefore placed upstream of the extruder when wet regrind is introduced.
Drop impact resistance of the finished bottle is measured by ASTM D2463-15 at 23°C. Though the tie layer is not the main structural component, delamination at the EVOH interface causes premature failure due to stress concentration at the interlayer boundary. Incoming Bynel® 41E556 resin is tested for melt flow rate by ISO 1133-1:2022 and density by ISO 1183-1:2019; significant shifts in melt flow rate indicate contamination with standard LLDPE or LDPE, which dilutes anhydride concentration and lowers peel strength. A minimum tie-layer thickness of 0.15 mm is sometimes specified when the bottle is designed for stack load above 50 kg, but final values are confirmed by top-load compression testing to ASTM D2659-16. Published data for Bynel® 41E556 in blow-molded barrier bottles are scarce; line qualification therefore uses infrared microscopy to confirm continuous tie-layer coverage around the circumference.
Multilayer oxygen-barrier pipes for underfloor heating or fuel line sheathing use a three-layer or five-layer wall composed of PE-RT or HDPE skins, a central EVOH barrier, and anhydride-modified LLDPE tie layers. Bynel® 41E556 is selected when the tie-layer graft must survive longer barrel residence times typical of pipe extruders with 30:1 L/D screws and screen changers. Melt temperature at the entry to the spiral die is normally limited to 225°C. The primary process conflict in this application is the narrow gap between EVOH thermal stability and the low melt temperature necessary to maintain pipe wall thickness control. If the die temperature is dropped below 210°C, the tie layer can exhibit high melt viscosity and cause surface melt fracture at the outer PE skin. If the temperature is raised above 235°C, EVOH degradation generates black specks at the tie-layer interface. Adhesion is evaluated by ISO 17454:2017, in which the multilayer pipe is compressed radially and inspected for separation between the barrier and adhesive layers. Because pipes are often coiled, interlayer adhesion must survive bending strain; testing at -20°C is added for refrigeration lines. The tie layer is also evaluated for peel adhesion after immersion in water at 80°C for 1,000 h, because hot-water pipe standards require long-term hydrostatic strength and no layer separation.
Recycled PE layers frequently contain trace polyamide from multi-layer film regrind. The anhydride functionality in Bynel® 41E556 can react with terminal amine groups of polyamide, reducing interfacial flaws; however, the resulting graft copolymer increases melt viscosity. Extruder torque and melt pressure are therefore monitored continuously, and a pressure rise of more than 15% at constant screw speed indicates contamination above the compatibilization capacity of the tie layer. Backpressure values are line-specific because die resistance and output rate vary, but a 65 mm pipe extruder running at 200 kg/h commonly operates with a pressure of 80–140 bar. No additional amine-based heat stabilizers are compounded into the tie layer; they are preferentially placed in the PE skin to prevent premature reaction with the anhydride grafts. Published long-term adhesion data for Bynel® 41E556 in PE-RT/EVOH pipe systems are limited, so certification requires testing on the actual coextrusion line with the specific EVOH grade and recyclate content.
Extrusion coating of aluminium foil or polyester film with a tie layer is used when a heat-sealable LLDPE skin must be bonded to a barrier substrate in a single pass. On a coating line equipped with a 90 mm single-screw extruder, flat die, and electrostatic edge pinning, Bynel® 41E556 is extruded at a melt temperature of 250–270°C to achieve sufficient wetting of the polar substrate. The melt curtain is set to a width slightly narrower than the substrate to minimize edge beading. Coating thickness is typically 8–15 µm for the tie layer and 15–20 µm for the heat-seal LLDPE layer. The critical failure mode is neck-in exceeding 75 mm on a 1,200 mm die, which causes profile thinning and intermittent adhesion loss at the substrate edges. Lowering the melt temperature below 240°C reduces neck-in but also delays the ring-opening of the anhydride at the interfacial boundary, lowering adhesion in the green laminate. Adhesion after lamination is tested by ASTM F904-16; values below 3 N/15 mm after 24 h aging typically indicate insufficient melt temperature or substrate surface contamination. Corona treatment of the substrate to a wetting tension of 42–48 dyn/cm is required before coating when polyester film is used. Aluminium foil requires no corona treatment but must be free of rolling oil residues above 10 mg/m². The line speed is usually adjusted between 150 m/min and 300 m/min, with higher speeds demanding tighter air gap control to avoid oxidative degradation of the graft.
The coated substrate is immediately nipped to a chill roll held at 15–20°C; higher chill roll temperatures cause blocking in roll form because the anhydride-modified surface remains tacky. When processing high-slip LLDPE over the tie layer, the slip additive migrates into the tie layer and lowers adhesion after 7 days aging; accelerated storage testing at 40°C for 14 days according to ASTM F1927-20 is used to detect this loss. Published data for Bynel® 41E556 in foil coating structures are limited, but the resin is qualified by checking melt flow stability across 3 h continuous runs at 260°C; a flow-rate drift greater than 0.5 g/10 min suggests oxidative chain scission or graft loss.
The following test matrix is used during application qualification to separate resin variability from line-induced defects.
| Application Zone | Primary Method | Qualification Objective |
|---|---|---|
| Flexible barrier film | ASTM F904-16 | No interlayer separation after 24 h ambient conditioning |
| Barrier bottle | ASTM D4991-07(2023) | No pinhole leakage under specified vacuum |
| Barrier pipe | ISO 17454:2017 | No layer separation under radial compression at test temperature |
| Extrusion coating | ASTM F1927-20 | No adhesion loss after 40°C/14 days storage |
| Compounded blend | ISO 527-2:2012 | Tensile elongation after 48 h conditioning at 23°C/50% RH |
Although Bynel® 41E556 is sold as a tie-layer resin, it is also used as a reactive compatibilizer in polyolefin-rich recycled streams containing small amounts of PA6 or PA66. In a co-rotating twin-screw extruder with 40:1 L/D, barrel temperatures from 220°C to 240°C, and screw speed of 400–600 rpm, the anhydride groups react with terminal amines of polyamide to form a graft copolymer at the phase boundary. The resulting morphology reduces dispersed-phase size and increases tensile elongation of the blend. The loading of Bynel® 41E556 is typically 3–5 wt%; below 2 wt% the interface is not fully saturated, and above 6 wt% unreacted anhydride can promote moisture sensitivity in the final molded part. Processing data show that blend viscosity rises as reaction progresses; the measured melt flow rate drops by 20–35% relative to the uncompatibilized blend when the grafting reaction is complete. Vacuum devolatilization is applied in the last barrel section to remove moisture and low-molecular-weight reaction by-products. The compounded pellets are tested for tensile properties according to ISO 527-2:2012 and impact strength according to ISO 179-1:2010. Published data for Bynel® 41E556 in PA-rich waste streams are limited, so pilot trials are required to determine the optimum loading.
Feeding sequence matters. Polyamide and Bynel® 41E556 are introduced in the main feed, while the polyolefin is side-fed after the first mixing zone to limit peak torque. If all components are premixed, the initial torque spike can exceed the extruder gearbox rating by 10–20%. In injection molding trials, the resulting compound is run at a clamp force of 800–1,200 kN for test plaques; molded parts are conditioned at 23°C and 50% RH for 48 h before testing. Moisture absorption above 0.2% in the pellets must be avoided because the anhydride-grafted polymer is hygroscopic; a closed-loop conveying system with dried air at -40°C dew point is recommended. Amine-based stabilizers are excluded from the compounding formulation, since they compete with the polyamide terminal groups for reaction with the anhydride, resulting in lower interfacial adhesion and inconsistent viscosity.
Coextruded barrier sheet for thermoformed trays and cups is produced on a flat die with a feedblock or multi-manifold distribution system. A five-layer sheet with PP or HDPE skins, Bynel® 41E556 tie layers, and an EVOH core is used when the finished package must survive retort, hot-fill, or aggressive food contact. The tie layer is run at 10–15% of total sheet thickness to maintain coverage during plug-assisted stretching. In a typical sheet line with a 120 mm main extruder and 35 mm tie-layer extruders, melt temperatures are held at 215–230°C at the feedblock. The primary failure mode is layer thickness variation during thermoforming; corners of deep-draw trays can be thinned below 50% of the original sheet gauge, causing localized adhesion loss and oxygen ingress. Sheet samples are tested for oxygen transmission by ASTM D3985-17 and for interlayer adhesion by ASTM F904-16 before and after thermoforming. The EVOH layer must remain continuous; cross-sectional microscopy is used to confirm tie-layer coverage at the tray corners.
Plug-assist thermoforming is performed at sheet surface temperatures between 130°C and 150°C for HDPE-based structures. If the sheet is overheated above 160°C, the tie layer can soften excessively and permit EVOH delamination under forming vacuum. If the sheet is too cold, the tie layer cannot accommodate the stretching of the skin layers, and microcracks form at the interface. The finished tray is tested for leak integrity according to ASTM D4991-07(2023) and for impact resistance at 4°C to simulate refrigerated distribution. Because Bynel® 41E556 is based on LLDPE, its low-temperature flexibility supports adhesion retention at -20°C; however, published data for deep-draw tray structures containing this exact grade are limited, and forming trials should establish the safe window for each EVOH grade and skin resin combination.
Competitive Dow Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Bynel® 41E556 is an anhydride-modified linear low-density polyethylene adhesive resin supplied for coextruded tie-layer service in packaging and industrial laminate structures. The material is defined by a melt index of 2.5 g/10 min measured at 190 °C under a 2.16 kg piston load according to ASTM D1238, and by a solid-state density of 0.920 g/cm³ according to ASTM D792. The polymer backbone is a linear low-density polyethylene; the adhesive character originates from anhydride groups appended to the polyolefin chain. These reactive sites permit the resin to form covalent and hydrogen-bonded interactions with amide end groups in polyamide 6, polyamide 66, and polyamide 6/66 copolymers, with hydroxyl groups in ethylene-vinyl alcohol copolymer, and with oxide and metal hydroxide species on aluminum, steel, and copper after melt contact. In coextrusion practice, Bynel 41E556 is inserted as a discrete tie layer between non-polar polyethylene skins and polar barrier cores. Typical structures are three-layer films of LLDPE/tie/EVOH or LLDPE/tie/polyamide, five-layer films containing two tie layers, and multi-material sheet or blow-molded containers in which the adhesive layer is used at 3–15 % of the total thickness. The resin is also used in extrusion coating and lamination of aluminum foil, steel sheet coating, and pipe coating, where bonding to metal is developed during the brief molten contact time in the nip or coating die.
Thermal characterization of the grade is described by a Vicat softening point of 106 °C measured under ASTM D1525 and a differential scanning calorimetry melting peak near 126 °C under ASTM D3418. The crystallization peak is reported near 107 °C. These values are consistent with an ethylene-octene or ethylene-butene LLDPE backbone, although the exact comonomer is not disclosed in the public datasheet. More important for converting is the upper-temperature boundary: anhydride-grafted polyolefins can undergo thermal decomposition of the graft when held above 280 °C for extended periods. The result is a loss of adhesive functionality and the possible formation of oxidized gel particles in the melt stream. In production and purge cycles, the melt temperature is therefore controlled in the 210–250 °C band, and startup after a stop is kept as short as feasible. Unlike unmodified LLDPE, the presence of polar functionality means that moisture in the feed stream can affect consistency only after exposure of regrind to humid storage; virgin pellets do not require pre-drying under normal warehousing conditions, but hopper condensation should be prevented in high-humidity plants.
Standard LLDPE provides no reactive functional group for bonding to polyamide or EVOH. Interfacial strength between unmodified LLDPE and a polar barrier layer is controlled by interdiffusion and mechanical interlocking, which can be sufficient in thick stiff substrates but becomes variable in thin flexible packaging. The anhydride functionality on Bynel 41E556 changes the adhesion mechanism: maleic anhydride ring-opening reacts with terminal amines in polyamides and with alcohol functions in EVOH during melt contact, producing ester-amide or amide-acid covalent bonds. These bonds are formed at the die or in the feedblock, but only if the temperature at the interface remains above the melting point of the tie layer and below the decomposition point of the graft. In practical line terms, this means the tie layer must not be starved as a solid skin along the die wall; adequate residence time and compression are required to bring reactive groups into contact with the barrier polymer before quenching.
The modification also changes the surface energy of the resin. The polar anhydride groups reduce interfacial tension against polyamide and EVOH, producing more uniform layer distribution and lowering the tendency toward interfacial waviness in thin films. However, the base polymer remains polyolefinic; it absorbs much less moisture than nylon or EVOH and does not develop the same degree of hygrothermal expansion. This is a design advantage in multi-layer packaging because the tie layer acts as a stress-decoupling phase between high-moisture-barrier and low-moisture-barrier layers during retort or hot-fill cycles. On the other hand, the addition of anhydride can reduce thermal oxidative stability relative to the base LLDPE, and it can slightly increase the affinity for basic contaminants from ink or corona surfaces; process hygiene must be maintained to avoid displacing interfacial adhesion.
The following typical values are used for process design and incoming inspection; they are not sales specifications and may vary within normal manufacturing tolerance.
| Property | Test method | Published typical value |
|---|---|---|
| Melt index | ASTM D1238 at 190 °C / 2.16 kg | 2.5 g/10 min |
| Density | ASTM D792 | 0.920 g/cm³ |
| Vicat softening point | ASTM D1525 | 106 °C |
| Melting peak | ASTM D3418 | 126 °C |
| Crystallization peak | ASTM D3418 | 107 °C |
A single melt-index value is insufficient for die design because the resin, like all LLDPE grades, is non-Newtonian. Capillary rheometry according to ASTM D3835 should be used to generate shear viscosity data at 190 °C and at the planned processing temperature. The melt-viscosity curve of the tie resin should overlap as closely as possible with the polyamide or EVOH grade in the shear-rate range of 100–1000 s⁻¹ to minimize interfacial instability. Published shear-viscosity data for this specific grade are limited; converters generally generate their own flow curves before specifying an extrusion screw or feedblock.
In a three-layer or five-layer cast film line, the adhesive layer is normally run at 10–25 % of the total film thickness, with the exact percentage set by the required adhesion and by the barrier-core thickness. The EVOH layer must be dried to a moisture content below 0.10 % before entering the feed throat; moisture from undried EVOH can hydrolyze the anhydride at the interface and reduce peel adhesion even when the tie resin itself is dry. Polyamide cores are typically dried to below 0.15 % residual moisture. The tie layer is not hygroscopic in pellet form, but trim containing unshielded EVOH or polyamide is not acceptable for direct reintroduction into a tie-layer feedstream because polar fines can create unmelted inclusions.
The extruder profile for the tie resin in cast film is usually set from 170 °C at the feed section to 210–230 °C at the metering section and die. The adapter and die lip temperatures are held at 220–230 °C for EVA-free LLDPE skin layers. If the die temperature drops below 210 °C, viscosity mismatch with typical EVOH may generate wavy interfaces and local tie-layer thinning; if it exceeds 250 °C, the graft may degrade and produce gel streaks. The die gap is commonly set at 0.5–1.0 mm for cast film. Interfacial adhesion is quantified by a T-peel test based on ASTM D1876 after 24 h conditioning at 23 °C and 50 % relative humidity. However, published universal adhesion values for this grade against all barrier films are not available; each manufacturer establishes internal acceptance limits on its own coex line because results depend on layer thickness, chill roll temperature, and film orientation.
In flat-die coextrusion, the feedblock is the primary location where the tie resin and barrier polymer meet. Interfacial reaction begins in the feedblock and continues through the die; therefore, feedblock residence time should be kept below 60 s at 230 °C to avoid over-reaction, which can increase the viscosity of the interfacial layer and create optical defects. The recommended tie-layer thickness is normally 5–15 µm in films below 100 µm total thickness. Thinner tie layers may give intermittent adhesion because any barrier-layer surface unevenness can cause local tie-layer rupture. Thicker tie layers add cost and reduce barrier contribution without proportional gain in peel force. When the tie layer is thickened beyond 20 µm, the additional mass may also reduce film clarity and increase curl due to differential shrinkage between the LLDPE backbone and the polar barrier layer.
The major processing conflict is the combination of low tie-layer thickness with high line speed. At line speeds above 300 m/min, wall shear stress in the die can cause unstable layer interfaces, especially when the tie resin viscosity is more than 30 % higher or lower than that of the adjacent barrier layer at the same shear rate. This is not a defect unique to 41E556, but it is a limiting condition for all LLDPE-based tie resins. A production line equipped with a 75 mm single-screw tie-layer extruder and a 30:1 L/D screw typically operates with a melt temperature rise of 15–30 °C above the barrel set point due to viscous dissipation. The actual melt temperature should therefore be measured in the adapter with an immersion thermocouple rather than estimated from the set point.
For blown film lines, the tie resin is run at 210–230 °C with a die gap of 1.5–2.5 mm and a blow-up ratio of 2.0–2.8. These settings are within standard LLDPE ranges, but excessive shear in spiral mandrel dies can overheat the anhydride graft; screw speeds and backpressure should therefore be monitored against the melt-temperature rise. The use of processed regrind containing nylon or EVOH is limited to the non-barrier skin layers, not to the tie layer, because contamination can cause gel flecks and loss of interfacial clarity.
In steel pipe coating, the adhesive is applied by flat-die or crosshead annular extrusion over a blast-cleaned steel surface, with surface preparation typically controlled to ISO 8501-1 cleanliness of Sa 2.5. The pipe surface temperature is maintained above 150 °C to promote wetting and adhesion before quenching. Adhesion strength in this configuration is not governed solely by the resin chemistry; surface profile, oxide condition, and preheating influence the measured peel force. Therefore, plant trials on the actual line speed and pipe diameter are required to establish acceptance data.
Bynel 41E556 is distinguished from anhydride-grafted LDPE by its linear low-density backbone. At equivalent thickness, LLDPE-based adhesive films generally show higher tensile elongation and higher dart impact and Elmendorf tear resistance than LDPE-based films under ASTM D882, ASTM D1709, and ASTM D1922; the trade-off is reduced melt strength during drawdown and a wider neck-in in extrusion coating. The melt index of 2.5 g/10 min is sufficiently low to retain bubble stability in blown film, yet high enough to permit adequate flow in cast film and coating dies. In comparison with acid copolymer tie resins, Bynel 41E556 does not introduce carboxylic acid functionality into the melt; this can reduce corrosion of unplated carbon steel screw and die surfaces and can lower moisture uptake in the finished tie layer. Acid copolymer tie resins may offer better adhesion to some metallic surfaces and may be processable at lower melt temperature, but they are also more polar and may require more careful purging and drying. The selection between anhydride-grafted LLDPE and acid copolymer is therefore made on the basis of barrier-layer type, process temperature, required sealant properties, and equipment metallurgy rather than on a single adhesion value.
Within the Bynel anhydride-modified polyolefin family, grades are differentiated by melt index, base density, and functional graft level. A lower melt index improves melt strength for blown film and pipe coating; a higher melt index improves penetration into nonwovens or metal surfaces at low coating weights. Bynel 41E556, at 2.5 g/10 min, occupies the middle range and is therefore specified for both cast and blown coexistence. Processors that require more drawdown in extrusion coating or lamination may need to compare it with higher-melt-index products; however, published direct substitution data for these configurations are limited and must be generated on the target line.
Food-contact compliance for Bynel 41E556 is typically reviewed against FDA 21 CFR 175.105, which covers adhesives used in packaging. In the European Union, relevant compliance is assessed under Regulation (EU) No 10/2011 for plastic materials and articles intended to come into contact with food, together with applicable national provisions. For industrial uses, the converter should confirm that the finished article meets REACH and RoHS requirements at the article level. The resin should be stored in closed, contaminant-free containers at temperatures below 40 °C. Storage near volatile amines, strong bases, or oxidizing agents should be avoided because such materials can react with the anhydride functionality. Equipment purging after use is best performed with unmodified LLDPE or LDPE; barrier polymers such as PA and EVOH are not acceptable purging materials for the tie layer because their high melting points and polar character can retain material in dead spots and cause degradation during subsequent startups.
On an extrusion lamination line applying Bynel 41E556 between aluminum foil and a heat-sealable LLDPE sealant, the melt temperature is normally held at 220–250 °C, the die-to-nip air gap at 150–250 mm, and the chill roll at 15–25 °C. The anhydride functionality contributes to bonding against the oxide layer of the foil, but the dominant variables are contact time, temperature, and nip pressure. Peel-strength measurement is conducted by ASTM D1876 after 24 h conditioning at 23 °C and 50 % relative humidity. Because foil temper, coating weight, sealant type, and line speed all change the result, an internal acceptance range is established on the production line rather than transferred from a single published value. In five-layer barrier films where the tie layer contacts both EVOH and polyamide in different zones, the same resin may be used on both sides only if the converter verifies that the two interfaces achieve the required peel force after sterilization or humid aging; otherwise, the tie-layer pair is split between two grades with different melt indices or functional levels.