| HS Code | 373236 |
| Base Resin | Linear Low Density Polyethylene (LLDPE) |
| Modification | Maleic Anhydride Grafted |
| Density | 0.920 g/cm³ |
| Melt Index | 10 g/10 min (190°C/2.16 kg) |
| Melting Point | 122°C |
| Vicat Softening Point | 96°C |
| Tensile Strength At Break | 16 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 200 MPa |
| Shore D Hardness | 50 |
| Water Absorption | <0.1% |
| Adhesion To Nylon | Excellent |
| Adhesion To Evoh | Excellent |
| Adhesion To Metals | Excellent |
| Processing Temperature | 200-260°C |
As an accredited Dow Bynel® 4140 Anhydride Modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Bynel® 4140 Anhydride Modified LLDPE is supplied in 25 kg (55 lb) polyethylene-lined bags, palletized for industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of Dow Bynel® 4140 Anhydride Modified LLDPE, shrink-wrapped and secured. |
| Shipping | Dow Bynel® 4140 Anhydride Modified LLDPE is typically shipped as solid pellets in 25 kg bags or bulk supersacks. It is not DOT/IMDG/IATA regulated for transport. Protect from moisture, heat, and contamination; keep containers closed. Follow applicable local, national, and international shipping regulations. |
| Storage | Store Dow Bynel® 4140 Anhydride Modified LLDPE in a cool, dry, well-ventilated area away from direct sunlight. Keep original containers or packaging tightly sealed to prevent moisture ingress and contamination. Protect from heat, sparks, flames, oxidizing agents, amines, alcohols, bases, and other reactive materials. Maintain ambient warehouse temperatures and good housekeeping. Follow local regulations and the SDS. |
| Shelf Life | Typically 24 months from date of manufacture when stored in original unopened packaging under cool, dry conditions, away from sunlight. |
In five-layer blown-film coextrusion of a PE/tie/EVOH/tie/PE structure, Bynel 4140 is processed as the discrete adhesive layer between the nonpolar polyethylene skins and the polar ethylene-vinyl alcohol copolymer core. The anhydride functionality reacts with hydroxyl groups on the EVOH chain during melt contact in the die and early air-ring region. Blown-film lines with a 55 mm barrier extruder and a 250 mm die typically run the tie resin at 195 °C to 235 °C, while the EVOH layer is maintained within its supplier-approved 205 °C to 230 °C window. Die lip gaps of 1.4 mm to 2.0 mm and a blow-up ratio of 2.0:1 to 2.5:1 are used. The primary control variable is interfacial melt temperature measured at the adapter exit. Interlayer adhesion is quantified by ASTM F904 or ISO 11339 T-peel on flat film after separation in a tensile tester at 100 mm/min for flexible laminates. A common acceptance criterion is cohesive failure within the polyethylene layer rather than interfacial separation at the tie/EVOH boundary. The tie-layer thickness is held between 5 µm and 8 µm; at less than 4 µm, peel values become line-speed sensitive, and at more than 12 µm, haze increases because of interfacial melt instability. Surface treatment of the finished film with corona discharge at 38 mN/m to 42 mN/m is used only if subsequent printing or lamination requires wetting. Food-contact status is assessed on the finished laminate under 21 CFR 177.1395; the adhesive is not intended for direct food contact. The process limitation is narrow. A residence time above 10 min at 240 °C can produce gel particles from anhydride ring opening and crosslinking. Purging with low-melt-index polyethylene after shutdown prevents carbonized deposits.
Retortable nylon-based multilayer film is processed with a discrete adhesive layer between nylon 6 and a linear low-density polyethylene sealant. Bynel 4140 reacts with terminal amine groups in the nylon phase and co-crystallizes at the interface with the polyethylene sealant. Extruders configured with a 45 mm nylon extruder and a 65 mm tie/sealant extruder feed a three-layer cast die at 240 °C to 265 °C for the nylon stream and 220 °C to 250 °C for the Bynel 4140 stream. The nylon layer must be pre-dried to below 0.10 % moisture using a desiccant dryer at 80 °C for 4 h to 6 h; moisture above this threshold volatilizes at the die lip and creates pinholes. Tie-layer thickness is held between 6 µm and 12 µm. At less than 6 µm, bond strength after retort can drop below the sealant yield point. At more than 12 µm, the film can curl because of differential crystallization. Seal strength is measured per ASTM F88 on 25.4 mm strips; immersion retort conditioning at 121 °C for 30 min is used to simulate terminal sterilization. The relevant failure mode is delamination at the nylon/tie interface, not sealant tearing. A useful on-line indicator is amperage stability on the tie extruder; fluctuations of more than ±5 % at constant screw speed indicate melt-temperature non-uniformity and can precede bond-strength scatter. Bynel 4140 should not be combined with amine-based antifog concentrates in the tie layer because free amines compete with the nylon surface and reduce anhydride grafting efficiency. Film curl becomes severe when the layer ratio exceeds 12 % nylon and quench temperature is below 15 °C. Published data for retort-specific Bynel 4140/nylon 6 peel values after multiple retort cycles is limited; end users typically establish internal specifications on the actual pouch geometry.
When a 7 µm to 9 µm aluminium foil is extrusion-laminated to a low-density polyethylene sealant or a biaxially oriented polypropylene print web, Bynel 4140 is deposited as a melt web between the foil and the nonpolar polymer. The process is performed on a tandem extrusion coating line with a 90 mm single-screw extruder, a 300 mm flat die, and a chill roll temperature of 15 °C to 25 °C. A melt temperature of 280 °C to 320 °C at the die is used for the adhesive melt to create sufficient oxidative bonding to the aluminium surface. The air gap between die exit and nip is set at 100 mm to 200 mm; longer air gaps increase oxidation of the adhesive but also increase neck-in. An adhesion promoter or pre-treatment is not required when the foil has been annealed to a wetting tension equivalent to 40 dyn/cm or higher. The failure mode in production is usually not interfacial peel but transfer of aluminium oxide to the polymer side. Adhesion is tested under ISO 11339 or ASTM D1876 T-peel at 100 mm/min after 24 h aging at 23 °C and 50 % relative humidity. Values vary with foil temper and thickness; no universal minimum exists. Processing windows narrow when line speed exceeds 180 m/min because the melt curtain becomes unstable and pinhole formation increases. Bynel 4140 must not be processed at melt temperatures above 330 °C for more than 5 min because thermal degradation produces acetic-acid-like odour and gel specks. If the foil is coated with a nitrocellulose primer, published data for this specific configuration is limited and the printer must validate bond retention after solvent-based ink contact.
Three-layer external polyethylene pipe coating systems use a fusion-bonded epoxy primer, an adhesive polymer layer, and a high-density polyethylene outer sheath. Bynel 4140 is used as the adhesive layer when a linear-low-density backbone is required for low-temperature flexibility. The pipe travels through a side-wrap or cross-head extrusion station at 0.5 m/min to 1.5 m/min, depending on diameter. The adhesive is extruded through a flat die or a slot die at 200 °C to 240 °C onto the epoxy primer while the epoxy is still in the gel window. The epoxy must retain reactive oxirane groups for the anhydride to form ester bonds. Epoxy thickness is verified at 60 µm to 100 µm per ISO 21809-1. Adhesive layer thickness is held at 170 µm to 250 µm for pipe diameters from 219 mm to 610 mm. Peel adhesion is tested per ISO 21809-1 or DIN 30670 at 23 °C ± 2 °C and at 60 °C, with the strip width fixed at 25 mm. A common production acceptance is a peel force of not less than 10 N/mm at 23 °C and not less than 2.5 N/mm at 60 °C, but project specifications vary. The most frequent failure mode is adhesive pull-out from the epoxy primer due to surface contamination with mill scale, rust, or residual phosphate. Shot-blast cleaning to Sa 2.5 per ISO 8501-1 with a surface roughness of 40 µm to 75 µm is mandatory before epoxy application. Processing limitations are severe. The window between epoxy application and adhesive extrusion is governed by gel time, often 20 s to 40 s; if the epoxy over-cures, adhesion falls below specification. Published peel data for Bynel 4140 specifically across all pipe diameters is limited; applicability must be confirmed on the full-scale line rather than laboratory panels.
High-barrier cast film trim scrap containing nylon, EVOH, tie resin, and polyethylene is reprocessed as concentrate into the polyethylene bulk layer in barrier structures. The anhydride functionality in Bynel 4140 reduces interfacial tension between polyamide and polyethylene phases and reacts with residual EVOH hydroxyls. A typical reclaim stream is processed through a twin-screw extruder with 40:1 L/D, vacuum venting at -0.08 MPa, and melt filtration of 80 µm. Bynel 4140 is added at 3 wt% to 5 wt% based on total regrind weight using a gravimetric feeder. Below 2 wt%, the reclaimed pellet still shows phase separation on the film surface; above 7 wt%, the film may lose clarity because the anhydride phase changes the crystallization rate of polyethylene. Tensile properties are measured per ISO 527-3 and dart impact per ISO 7765-1. The processing limitation is reactive volatiles from nylon and EVOH hydrolysis; without vacuum venting, moisture release causes melt pressure fluctuations above 10 bar and visible gels. Bynel 4140 should not be processed in this manner if the regrind contains more than 30 % EVOH because anhydride consumption is excessive and bond performance in the finished barrier layer falls. Published data for Bynel 4140-specific regrind ratios in cast film is limited; pilot evaluations are advised before setting commercial addition thresholds.
Aseptic cartons and flexible aluminium barrier laminates use Bynel 4140 as the melt web between aluminium foil and polyethylene in the sealing layer. The process uses extrusion coating lines at 250 °C to 300 °C with a 100 mm to 150 mm air gap. Adhesion to aluminium is tested per ASTM D1876 after conditioning at 23 °C and 50 % relative humidity for 72 h. Melt temperature and chill roll surface roughness are the primary variables affecting bond strength. A matte chill roll with 0.5 µm to 1.0 µm Ra produces higher peel strength than a polished roll because the polymer conforms to the aluminium oxide morphology. The adhesive layer is typically 12 µm to 20 µm thick. Thicker layers increase cost without proportional adhesion gains. The process window is narrow when the substrate web temperature is below 10 °C; condensation on the foil can create interfacial voids. Bynel 4140 is not compatible with high-acid filling if the aluminium is breached; the laminate must be bench-tested for seal integrity under the intended hydrogen peroxide sterilization conditions. Published data for this specific aseptic structure is limited.
Competitive Dow Bynel® 4140 Anhydride Modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Bynel® 4140 is an anhydride-modified linear low-density polyethylene (LLDPE) supplied as free-flowing pellets for coextrusion, cast film, extrusion coating, and blow molding. The product’s functionality is obtained by covalent grafting of maleic anhydride onto an LLDPE backbone during melt-phase reactive extrusion; this is a structural modification, not a surface treatment. In multi-layer barrier structures, the resin is positioned as an internal tie layer between non-polar polyolefin skins and polar barrier layers such as ethylene-vinyl alcohol copolymer (EVOH) or polyamide. Because the anhydride carbonyl groups interact with amide and hydroxyl functionalities at the interface, the resulting adhesion is characterized by measurable T-peel load transfer under ASTM F904 or ISO 8510-2, whereas unmodified LLDPE typically fails adhesively at the interface. The product is not intended for use as a sealant layer or as an external surface layer.
Unmodified LLDPE has no chemically reactive functionality. In coextruded film, unmodified LLDPE adjacent to polyamide or EVOH typically separates at the interface before cohesive deformation of the tie layer is observed, resulting in low T-peel values under ASTM F904. Bynel 4140 addresses this limitation through maleic anhydride grafting. With polyamide, the anhydride ring can undergo ring-opening at melt temperatures of 210–250°C and react with terminal amine groups on the polyamide surface to form covalent imide or amide linkages. With EVOH, hydrogen bonding and esterification involving the vinyl alcohol hydroxyl groups are dominant. The graft level is proprietary; therefore, stoichiometric calculations for formulators should not rely on a published maleic anhydride mass fraction but on the manufacturer’s coverage factor expressed in g/m² at a given tie-layer thickness.
Interfacial adhesion is also influenced by the acid–base interaction between the carbonyl of the grafted anhydride and polar functional groups in the barrier layer. In polyamide coextrusion, higher amide end-group concentrations generally increase the number of potential reaction sites, but they also increase water absorption in the polyamide layer. Peel strength is therefore not a simple function of anhydride level; it depends on the molecular weight and end-group balance of the polyamide, the ethylene content of the EVOH, and the thermal history of the interface. Converters often evaluate a matrix of three polyamide grades and two EVOH grades under identical layer ratios and test adhesion according to ASTM F904 before selecting the tie layer.
Compared with acid copolymer tie resins such as ethylene acrylic acid (EAA) or ethylene methacrylic acid (EMAA), Bynel 4140 uses an anhydride functionality on an LLDPE backbone. Acid copolymers bond through pendant or backbone carboxylic acid groups, which can be more hydrophilic and more moisture-sensitive at the interface. Another contrast is anhydride-modified ethylene-vinyl acetate or ethylene-butyl acrylate tie layers; those resins are generally softer but may have lower temperature resistance because vinyl acetate can release acetic acid at elevated temperatures. Bynel 4140 avoids such vinyl acetate content and can be processed up to 250°C in the manufacturer’s recommended range. The LLDPE backbone also provides lower density than anhydride-modified HDPE tie layers with densities near 0.945–0.955 g/cm³; exact density and Vicat values differ by supplier and are not interchangeable. In contrast to maleic anhydride-modified polypropylene tie layers, Bynel 4140 processes at lower melt temperatures and is generally selected for polyethylene-based structures rather than polypropylene-based retortable structures operating above 130°C.
Published representative values from the manufacturer’s product data sheet are listed in Table 1. These values are lot-dependent and are not release specifications; the certificate of analysis supplied with each lot should be used for acceptance. The melt flow rate is measured at 190°C with a 2.16 kg load in accordance with ASTM D1238 or ISO 1133-1:2022. Differential scanning calorimetry per ASTM D3418 or ISO 11357-3 is run at a heating rate of 10°C/min after an initial heating procedure to erase thermal history.
| Property | Typical Value | Test Method |
|---|---|---|
| Density at 23°C | 0.920 g/cm³ | ASTM D792 / ISO 1183-1 |
| Melt flow rate, 190°C, 2.16 kg | 2.7 g/10 min | ASTM D1238 / ISO 1133-1:2022 |
| Peak melting temperature by DSC | 125°C | ASTM D3418 / ISO 11357-3 |
Because the melt flow rate is 2.7 g/10 min, Bynel 4140 occupies a medium-viscosity processing window. In comparison, some unmodified LLDPE sealants are specified with melt flow rate values above 4 g/10 min for draw-down, while some high-density tie layers are specified below 1.5 g/10 min; these comparisons are grade-dependent and not universal. The target melt temperature range of 210–250°C preserves the balance between interfacial reactivity and thermal degradation; a melt temperature below 210°C may generate high melt pressure and incomplete adhesion, while temperatures above 250°C can accelerate anhydride-related degradation. These boundaries should be verified on the specific coextrusion line.
On a five-layer blown-film line with three extruders feeding outer polyethylene skins, Bynel 4140 tie layers, and an EVOH or polyamide barrier, the tie-layer extruder is commonly a single-screw design with a 30:1 to 35:1 L/D ratio and a barrier screw having a compression ratio between 2.8:1 and 3.2:1. The die temperature is typically set at 220–240°C, while the melt temperature measured at the adapter is kept within the manufacturer’s recommended 210–250°C range. Blown-film dies with a die gap of 0.8–2.0 mm and blow-up ratios of 2.0:1–3.0:1 allow the converter to vary interfacial cooling rate and frost-line position; faster quenching yields smaller spherulites and can improve interfacial contact, but published peel strength data for Bynel 4140 at these exact conditions are limited. Processors commonly screen three to five frost-line heights and measure T-peel adhesion per ASTM F904 before committing to a production run. Conditioning of film samples is performed at 23°C and 50% relative humidity for at least 40 h in accordance with ASTM D618 before testing.
Solventless and solvent-based laminating adhesives are replaced by Bynel 4140 only where coextrusion of a tie layer is possible. A coextruded tie layer removes the need for a secondary adhesive lamination step and solvent-drying ovens, but adds an extruder to the line and increases die complexity. Adhesive lamination can deposit less than 2 g/m² of adhesive, whereas a 5–15 µm coextruded tie layer at a density of 0.920 g/cm³ corresponds to 4.6–13.8 g/m². This mass per unit area difference is derived from ASTM D792 density and should be included in cost-per-square-meter comparisons. Coextrusion also requires the barrier resin and substrate to tolerate the melt temperature of the tie layer; for Bynel 4140 that is 210–250°C. In some structures, the heat load can restrict the use of low-melting sealants or oriented substrates.
Compared with extrudable tie-layer grades based on maleic anhydride-grafted HDPE or PP, Bynel 4140 is chosen for polyethylene-rich structures where low sealing initiation temperature and film impact resistance are required. Film impact resistance is often measured by ASTM D1709 or ASTM D3420, but values depend strongly on total gauge and layer distribution. Replacing a laminating adhesive with Bynel 4140 can also alter oxygen barrier performance because the tie layer becomes part of the total wall thickness. In a five-layer film, a 10 µm EVOH layer with two 10 µm tie layers may show different gas barrier than an adhesive laminate with a 2 g/m² adhesive layer because the coextruded tie layers are thicker and alter the effective oxygen transmission path. Oxygen transmission is measured according to ASTM D3985 at 23°C and 0% relative humidity or 90% relative humidity, depending on the application. Under retort conditions of 121°C or higher, an anhydride-modified HDPE or PP tie layer may be more dimensionally stable, because the LLDPE matrix of Bynel 4140 softens at a peak melting point of 125°C. Published standardized retention data for Bynel 4140 in all retortable configurations are limited; therefore, pilot-line testing is required, with adhesion measured after hydrothermal challenge by ASTM F904 or ISO 8510-2.
Although the LLDPE backbone is not hygroscopic like polyamide, the maleic anhydride grafts can hydrolyze to diacid structures if pellets are exposed to high-humidity air before entering the extruder. At ambient relative humidity above 60%, surface moisture can be carried into the melt; some processors dry Bynel 4140 in desiccant dryers at 80°C for 2–4 h using a dew-point setpoint of −40°C. In the melt, residual water may reduce the concentration of reactive anhydride rings at the tie-layer surface and contribute to interfacial haze measured by ASTM D1003 in transparent barrier structures. Hydrolysis is not typically the dominant failure mode in a dry indoor environment.
Dwell time is a further critical parameter. Because the maleic anhydride graft can participate in chain extension or crosslinking reactions at elevated temperature, the resin should not remain stagnant in transfer pipes, screen changers, or the die for extended periods. Processors using continuous blown-film lines typically purge the tie-layer extruder with low-melt-index polyethylene if the line is stopped for more than 30–60 min; published guidelines for Bynel 4140 specifically should be confirmed with the manufacturer. Screen-pack configuration for tie-layer extruders is typically a breaker plate followed by a screen pack of 60/100/60 mesh; finer screens below 120 mesh can increase shear heating and are generally unnecessary for pelletized resin. A pressure drop across the screen pack above 70 bar can indicate significant contamination or gel accumulation. During start-up after a shutdown, the first 5–10 kg of extrudate should be discarded until the melt is clear and free of oxidized gel. These operational limits reduce the probability of black specks and gel streaks at the die lip.
For regulatory compliance, Bynel 4140 must be evaluated in the final article, not as an isolated resin. Table 2 summarizes the frameworks commonly referenced for barrier packaging and industrial applications. The base LLDPE may be covered by FDA 21 CFR §177.1520 for olefin polymers, but the grafted anhydride tie-layer function and the final multi-material structure require additional confirmation. Under EU food-contact legislation, Commission Regulation (EU) No 10/2011 establishes specific migration limits for authorized monomers and additives; compliance is determined by migration testing under the intended time-temperature conditions. In the United States, FDA 21 CFR §175.105 may also apply to adhesives used in food contact, depending on construction and end use. REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU documentation must be obtained from the supplier for the specific grade and production site.
| Regulatory framework | Relevant standard or code | Verification requirement |
|---|---|---|
| U.S. food contact | FDA 21 CFR §177.1520 / §175.105 | Confirm final article compliance with the manufacturer’s food contact statement and end-use conditions |
| EU food contact | Commission Regulation (EU) No 10/2011 | Migration testing under intended time-temperature profile |
| Chemical sustainability | REACH Regulation (EC) No 1907/2006 | Supplier safety data sheet and SVHC declarations for the production site |
| Electrical/electronic applications | RoHS Directive 2011/65/EU | Supplier certificate where applicable |
On a three-layer coextrusion blow molding machine producing polyamide-barrier HDPE containers, Bynel 4140 is used as the tie layer at 5–10% of total wall thickness. The tie-layer extruder temperature profile is set from 190°C at the feed throat to 230°C at the die head to maintain anhydride reactivity without excessive thermal degradation. Clamp force and parison programming are adjusted to avoid thin spots at pinch-off regions where tie-layer coverage may be lost; a minimum pinched-wall thickness of 1.0 mm is monitored in some containers, but acceptable values depend on container design. Peel strength is difficult to measure on blow molded walls, so section thickness measurement, oxygen transmission by ASTM D3985, and drop impact by ASTM D2463 are used as indirect indicators of tie-layer continuity. Published data for this specific application is limited; converters validate each container geometry by barrier testing and drop testing before release to production.