| HS Code | 476991 |
| Product Name | Dow Bynel 4125 Anhydride-Modified LLDPE Adhesive Resin |
| Chemical Family | Anhydride-Modified Linear Low Density Polyethylene |
| Polymer Type | LLDPE |
| Anhydride Modification | Maleic Anhydride Grafted |
| Density | 0.92 g/cm³ |
| Melt Index | 2.5 g/10 min at 190°C/2.16 kg |
| Melting Point | 122°C |
| Vicat Softening Point | 95°C |
| Tensile Strength At Break | 18 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Hardness | Shore D 50 |
| Water Absorption | <0.01% |
| Thermal Stability | Good |
| Processing Temperature | 200°C to 260°C |
| Adhesion Substrates | EVOH, nylon, PE, foil |
| Form | Pellets |
| Color | Natural |
| Odor | Slight |
| Bulk Density | 0.56 g/cm³ |
| Fda Compliance | 21 CFR 175.105 and 21 CFR 177.1520 |
| Moisture Content | <0.1% |
As an accredited Dow Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin is packaged in 25 kg moisture-resistant bags, typically 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | Dow Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin: 20′ FCL, palletized bags, shrink-wrapped, strapped, dry container, secure stowage. |
| Shipping | Dow Bynel 4125 Anhydride-Modified LLDPE Adhesive Resin is typically shipped as pellets in sealed 25-kg polyethylene bags or bulk containers, palletized and stretch-wrapped. Transport in clean, dry vehicles at ambient temperature, avoiding moisture, heat, and direct sunlight. Generally non-hazardous and not regulated for DOT, IMDG, or IATA transport. |
| Storage | Store in a cool, dry, well-ventilated area away from heat, ignition sources, and direct sunlight. Keep containers tightly closed, elevated off floors, and protected from moisture, dust, and contamination. Avoid prolonged storage above 40°C (104°F). Use first-in, first-out stock rotation. Maintain clean, dry handling conditions and good housekeeping. Consult the SDS for additional requirements. |
| Shelf Life | Dow Bynel® 4125 shelf life: typically 24 months from manufacture if stored unopened in original packaging, cool, dry, protected from moisture. |
Coextrusion lines producing 3-layer and 5-layer barrier films for case-ready meat packaging and frozen food lidding operate Bynel 4125 as the full tie-resin layer at 3–5 μm per adhesive layer. In a 75 μm PA6/tie/LLDPE sealant film, the tie layer represents 4–6.7 wt% of total film mass; in a 90 μm four-layer or five-layer EVOH structure, two tie layers account for 6.7–11.1 wt%. The resin is processed as a neat layer, not as a dry blend, with melt temperature at the die maintained between 210 °C and 225 °C. Barrel profiles from feed to die are set at 180 °C/195 °C/205 °C/215 °C/220 °C on extruders with L/D of 24:1–30:1. The anhydride functionality reacts with amine end groups in polyamide and hydroxyl groups in EVOH within the coextrusion die and air gap; if melt temperature falls below 205 °C, interfacial clarity degrades and peel adhesion measured by ASTM D1876-01 becomes unstable, while operation above 230 °C induces EVOH acetic acid odour and gel speck formation. Edge-trim regrind from the barrier film can be reintroduced into the polyethylene sealant layer at 10–20 wt% without destroying the adhesive layer, but regrind in the tie layer above 15 wt% tends to lower die pressure and shift melt output variability. Compliance for food-contact construction is anchored to FDA 21 CFR 175.105 for adhesive components, EU Regulation (EU) No 10/2011 as amended for plastic materials in contact with food, and China GB 9685-2016 for adhesive formulations; overall migration is determined according to EN 1186-1:2002, and oxygen transmission of the finished film is measured by ASTM D3985 at 23 °C/0% RH while water vapour transmission is measured by ASTM F1249 at 38 °C/90% RH. Terminal products include vacuum pouches for fresh red meat, modified-atmosphere lidding webs for case-ready poultry trays, single-serve coffee bean bags, and laminated stand-up pouches for wet pet food.
In architectural wall-cladding panels and signage boards, Bynel 4125 is converted into a cast tie film at 30–60 μm thickness, corresponding to 27.3–54.6 g/m² of adhesive mass at a solid density of 0.91 g/cm³ per ISO 1183-1:2019. The tie film is placed between the aluminium skin and a PE-HD or PE-LD core on a flatbed lamination press, with lamination temperature held at 150–180 °C, specific pressure 0.5–1.5 MPa, and dwell time 15–30 min. Roll laminators operating at 2–5 m/min require preheating of the aluminium coil to 100–130 °C; insufficient skin temperature produces peel failure at the tie film/aluminium interface because the anhydride groups cannot convert carbonyl oxygen coordination into a sufficiently polar interaction. Production-scale failure data shows that aluminium surfaces contaminated with drawing oil or silane-based corrosion inhibitors reduce peel strength under ASTM D1781-08 climbing drum testing even when the film thickness is doubled; the failure mode shifts from cohesive failure within the PE core to adhesive failure at the metal oxide interface. Compliance for the building panel is evaluated under EN 13501-1:2018 for reaction to fire, and the resin portion is covered by REACH 1907/2006/EC and RoHS 2011/65/EU for heavy metals. Terminal products include exterior architectural cladding panels, sign board substrates, garage door face sheets, and interior automotive body panels.
In PE-HD/wood-flour composite decking compounds, Bynel 4125 is metered as a coupling agent at 1.5–3.0 wt% of total compound mass, with the ratio calculated on the dry wood fraction after moisture is determined by ASTM D4442-20. The resin is fed into the main throat of a counter-rotating twin-screw extruder with L/D 36:1–44:1, while the wood flour is side-stuffed at 60–70% of barrel length to avoid premature scorching; barrel temperatures from feed to die are typically 160 °C/165 °C/170 °C/178 °C/182 °C, and melt pressure in the die zone is held at 3–6 MPa. If wood moisture exceeds 1.0 wt%, the water vapour released during venting hydrolyses the anhydride ring and esterification with hydroxyl groups on cellulose and lignin becomes incomplete; this is observed on production lines as increased porosity, lower melt strength, and higher 24-hour water absorption measured by ASTM D7031-11. Flexural properties are tested by ISO 178:2019, impact by ISO 179-1, and weathering by ISO 4892-2:2013. Compliance for exterior building products is covered by REACH 1907/2006/EC, RoHS 2011/65/EU, and ASTM D7031-11 as the product standard; where recycled polyethylene is used, the resin must remain below the total heavy metal limits under EC 1907/2006/EC Annex XVII. Terminal products include hollow-core decking boards, railing profiles, exterior wall cladding strips, and automotive interior trim substrates.
The matrix below consolidates the compliance and test anchors applied by converters to Bynel 4125 in the first three process zones.
| Application zone | Addition form and ratio | Key compliance or test standard | Converter-held evaluation endpoint |
|---|---|---|---|
| Barrier film tie layer | Neat resin layer at 3–5 μm | FDA 21 CFR 175.105; EU 10/2011; ASTM D1876-01 | Interfacial peel stability and migration under EN 1186-1:2002 |
| Aluminum composite panel tie film | Neat cast film at 30–60 μm | EN 13501-1:2018; REACH 1907/2006/EC; ASTM D1781-08 | Cohesive failure in PE core, no oil-induced adhesive failure |
| Wood-plastic composite coupling | 1.5–3.0 wt% of total compound | ASTM D7031-11; ISO 178:2019; ISO 179-1 | Flexural modulus and 24-hour water absorption |
Agricultural chemical and solvent-containing product containers constructed with a six-layer wall use Bynel 4125 as the two tie layers at 35–45 μm per layer, combined 70–90 μm in a 1.8 mm nominal wall, equal to 3.9–5.0% of total wall thickness. The structure is PE/tie/PA6/tie/regrind/PE, and the PA6 layer is pre-dried to 0.08 wt% moisture by ISO 15512:2019 before coextrusion; undried PA6 causes moisture-foamed barrier layers and interfacial delamination when the bottle is drop-tested. The blow molding line uses a 6-layer accumulator head, blow air pressure 0.6–1.0 MPa, and mold cooling water at 10–25 °C. Melt temperatures for the tie resins are kept at 215–230 °C, while PA6 is processed at 235–245 °C; the difference must be controlled because prolonged residence at high temperature reduces anhydride functionality and shifts the tie layer's MFR under ISO 1133-1:2022 beyond ±0.3 g/10 min. Compliance for dangerous goods packaging is determined by the UN Model Regulations for 3H1 non-removable-head plastics jerricans, national equivalents such as US DOT 49 CFR 178.508, and transport testing for stack pressure and drop impact. Environmental stress crack resistance of the high-density polyethylene outer layer is tested by ASTM D1693-15, and peel adhesion between PA6 and PE is assessed by ASTM D1876-01 on a flat plaque. Terminal products include 5 L agricultural chemical jugs, 10 L solvent containers, fuel cans, and jerry can inserts for hydrocarbons.
Radiant floor heating pipe with a PE-RT/EVOH barrier layer uses Bynel 4125 as the two adhesive layers at 0.08–0.15 mm each in a 16 × 2.0 mm five-layer pipe, corresponding to 8–15% of the 2.0 mm wall. The EVOH oxygen barrier layer is typically 0.10 mm. The coextrusion line runs a 5-layer spiral mandrel pipe die with vacuum calibration tanks, line speed 15–35 m/min, and melt temperatures of 210–225 °C for the tie resin. The critical production risk is interfacial degradation at the tie/EVOH boundary when the melt temperature exceeds 230 °C; this produces gel-like deposits on the calibration sleeve and an oxygen diffusion rate that fails the barrier pipe evaluation under DIN 4726:2017. Compliance is anchored to ISO 22391-2:2009 for PE-RT pipe, DIN 4726:2017 for oxygen barrier performance, and ISO 17455-1:2008 for oxygen permeability measurement. Terminal products include floor heating loops, ceiling cooling panels, snow melt systems, and potable water distribution piping.
Medium-voltage armored cables with a polyethylene sheath over steel tape use Bynel 4125 as an extruded adhesive tie layer at 0.15–0.30 mm thickness between the PE jacket and the metal tape. The cable line uses a pressure extrusion tooling setup with a 25:1 L/D single-screw extruder, melt temperature 210–230 °C, and steel tape preheated to 50–80 °C by induction or hot air before entering the coating die. If the steel tape is below 45 °C, condensate from ambient humidity creates a weak boundary layer and the peel strength measured by ASTM D1876-01 on flat laminated specimens falls below the batch release value required for cable bending. The resin's adhesion mechanism to the metal oxide surface requires the tape to be free of drawing lubricants and not passivated with chromate; production lots with residual drawing lubricant exhibit intermittent jacket peeling at bending radii below 6× cable diameter in cold bend tests per IEC 60811-506:2012. Because published data for Bynel 4125 in armored cable jacket configuration is limited, converter trials are required to establish the oil contamination threshold and minimum peel strength value for each cable design. Compliance for power cables is assessed under IEC 60502-1:2021 for rated voltages 1–36 kV, and jacket mechanical properties are tested by IEC 60811-501:2012; the resin is covered by REACH 1907/2006/EC. Terminal products include buried medium-voltage distribution cables, mining trailing cables, and submarine cable armor jackets.
Competitive Dow Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Bynel® 4125 is an anhydride-modified linear low-density polyethylene (LLDPE) adhesive resin supplied in pellet form. The material carries maleic anhydride functionality on a semi-crystalline LLDPE backbone, producing a tie-layer resin for coextruded multilayer films, sheet, extrusion coating, and blow-moulded structures. Published typical values include a melt mass-flow rate of 1.0–1.2 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022, and a density of 0.921–0.923 g/cm³ under ISO 1183-1:2019. The differential scanning calorimetry melting peak is reported in the 124–126°C range under ISO 3146 or ASTM D3418-15. These values are typical catalog data and not contractual specification limits; lot-specific certificate-of-analysis data govern acceptance. The grade is used to bond non-polar polyethylene layers to polar barrier polymers such as polyamide 6, polyamide 66, ethylene vinyl alcohol copolymer (EVOH), and to aluminium foil in selected laminate constructions. Because the anhydride is grafted along the polymer chain rather than applied as a discrete surface coating, adhesive performance is retained through melt processing and is not dependent solely on mechanical interlocking. The product is also used as a functional adhesive in polyethylene/polyamide and polyethylene/EVOH coextrusions where conventional LLDPE would delaminate under package flexing or retort conditions.
During melt coextrusion, the anhydride groups on the LLDPE chain are available for interfacial reaction with the amine end groups of polyamide and the hydroxyl groups of EVOH. In polyamide systems, primary amine terminal groups react with grafted maleic anhydride to form amide or imide structures. In EVOH systems, esterification or strong hydrogen bonding can occur with the vinyl alcohol hydroxyl pendant groups. The result is a covalent or strongly associated interphase rather than simple wetting. Adhesion is therefore sensitive to barrier-resin end-group concentration, molecular weight, melt contact time, and the temperature of the coextruded melt stream. In film qualification work, peel strength is usually measured after conditioning at 23°C and 50% relative humidity using a tensile tester operated under ASTM D1876-08 or ASTM F904-16. Published data for every combination of layer gauge, barrier-resin grade, and line configuration is limited, and adhesion values from one coextrusion line should not be extrapolated to another without pilot confirmation. On blown-film lines, corona or flame treatment of the barrier layer can raise polar surface energy, but the anhydride reaction remains the dominant adhesion mechanism for this grade. The LLDPE backbone is non-polar and does not create the same acid-induced corrosion in downstream metal surfaces as some acid-copolymer tie resins. Trace moisture can hydrolyse a portion of the anhydride to diacid, which may then participate further in hydrogen bonding at the interphase.
On production-scale cast film lines, Bynel® 4125 is processed on barrier-screw single-screw extruders with L/D ratios from 24:1 to 30:1. A typical three-layer coextrusion line may set the tie-layer extruder feed throat below 60°C to prevent pellet bridging, while downstream barrel zones are ramped from 180°C to 240°C. Melt temperatures at the flat die are commonly held between 230°C and 250°C. The exact barrel profile depends on extruder diameter, screw speed, backpressure, and throughput; no fixed profile applies to every machine. Pre-drying is not normally required for the LLDPE carrier, but surface condensation can cause bubble defects in blown film if pellets are stored in unheated areas at relative humidity above 60%. A dry-air hopper set at 60–70°C for 2–4 hours can be used if pellet surface moisture is visible or if the ambient dew point approaches the pellet storage temperature. The melt should not be held above 280°C for extended periods because anhydride functionality can undergo thermal breakdown, reducing adhesion and potentially forming gel particles. When the tie layer is starved below 5–10% of total throughput in a five-layer film, melt-flow instability and uneven gauge distribution may occur. These operating ranges reflect general anhydride-modified polyolefin tie-resin practice; published data for this specific grade on every line geometry is limited.
| Property | Typical value | Test method |
|---|---|---|
| Melt mass-flow rate | 1.0–1.2 g/10 min | ISO 1133-1:2022 |
| Density | 0.921–0.923 g/cm³ | ISO 1183-1:2019 |
| DSC melting peak | 124–126°C | ISO 3146 / ASTM D3418-15 |
| Vicat softening temperature, 10 N load | 101–103°C | ISO 306:2013 |
These values are measured on neat resin under standardized laboratory conditions and do not directly predict bond performance in a finished package. The Vicat softening temperature should not be used as a maximum service temperature for a multilayer structure; continuous service temperature depends on barrier-layer properties, layer geometry, mechanical load, and packaging conditions. Post-crystallization or shrinkage in the LLDPE backbone can occur after thermal bonding, and dimensional stability should be measured on the final structure, not inferred from density or thermal data alone. The melt-flow rate of this grade is lower than that of typical extrusion-coating LDPE tie resins, which favours higher melt strength in cast and blown film but reduces ease of flow through narrow die gaps. In injection-moulded or high-speed thin-gauge applications, the grade is not a direct substitute for high-flow tie resins with MFR above 10 g/10 min.
When tie layers are diluted with neat LLDPE to reduce cost, adhesion to EVOH and polyamide is not linear with dilution because the reactive species are confined to the Bynel® 4125 fraction. At 30 wt% tie-layer content, the effective anhydride concentration at the interface may be insufficient to saturate the available reactive groups in the barrier layer, and the probability of forming an adequate interphase drops. Coextruders commonly limit LLDPE let-down to 20–30 wt% to preserve bond robustness, but quantitative adhesion loss is highly system-specific. Published data for this particular dilution series across all layer gauges and barrier resins is limited; pilot validation is required. In cast film, the rapid quench reduces time for interfacial reaction compared with air-cooled blown film, so cast structures may require a higher tie-layer thickness or lower line speed to achieve equivalent adhesion. Operators sometimes raise the tie-layer melt temperature by 10–15°C to compensate for reduced contact time. Such adjustment should be validated by peel testing under ASTM D1876-08 before production release, and the failure mode and location should be recorded because adhesive transfer to the barrier or sealant layer can falsely elevate reported peel values.
Adhesion of maleic anhydride grafted polyolefins to polyamide depends on the concentration and accessibility of amine end groups. For polyamide 6, amine end-group concentration may range from approximately 30 mmol/kg to 80 mmol/kg depending on molecular weight and polymerization conditions. Polyamide 66 can exhibit lower available amine end groups, and the interfacial imide formation may be reduced if acid end groups dominate. In EVOH, ethylene content controls hydroxyl density; a grade with 32 mol% ethylene has a higher hydroxyl concentration than a grade with 44 mol% ethylene, and the adhesion response of Bynel® 4125 differs accordingly. If adhesion is measured on a finished laminate, specimen width, peel angle, and jaw separation rate follow ASTM D1876-08; for flexible packaging laminates, ASTM F904-16 may be applied. When the structure contains a printed or metallised surface, measured peel force may reflect ink or metal transfer rather than the true polymer interphase, so the failure location must be reported. In some polyamide 66 structures, surface crystallinity can reduce the number of accessible chain ends even when bulk amine content is adequate; higher die temperature and longer contact length can partially offset this effect. Conversely, excessive melt temperature can degrade the polyamide layer and create gels that interfere with the interphase. Melt-temperature control within a ±5°C window is therefore applied on some multilayer lines, with verification against a calibrated melt probe. Published data for this exact grade across all polyamide end-group levels is limited; qualification on the actual barrier-resin lot is required.
Differences from ethylene acrylic acid (EAA) copolymers are significant. EAA acid copolymers rely on carboxyl groups for adhesion and can bond well to aluminium foil, but acidity can cause corrosion of downstream equipment and may affect taste in sensitive packages. Bynel® 4125 carries anhydride functionality on an LLDPE backbone, giving a non-corrosive melt and a more polyolefin-like balance of thermal stability and surface friction. Compared with maleic anhydride grafted HDPE tie resins, Bynel® 4125 has lower crystallinity and lower density; HDPE-based tie resins often have densities above 0.940 g/cm³, while this grade is near 0.922 g/cm³. The lower density is accompanied by lower flexural modulus and higher elongation, making Bynel® 4125 more suitable for flexible film and less suitable for rigid blow-moulded containers where HDPE provides greater top-load strength. Compared with EVA- or EMA-based tie resins, Bynel® 4125 has a higher melting point and may require higher extrusion temperatures; it also generally offers better thermal performance in hot-fill or pasteurization environments, but published data for this specific grade under all retort conditions is limited and must be validated. In blown film, the LLDPE backbone improves bubble stability relative to LDPE-based tie resins, while in cast film it provides higher tear resistance. The anhydride modification level is proprietary and not stated on the typical data sheet; therefore differences relative to other Bynel® grades are best assessed by comparative coextrusion trials rather than by bulk property inspection alone.
For food-contact applications, Bynel® 4125 is supplied with a product stewardship bulletin addressing regional compliance. In the United States, olefin polymer components may be assessed under FDA 21 CFR 177.1520. In the European Union, multilayer packaging materials are evaluated under Regulation (EU) No 10/2011, with migration limits expressed in mg/kg food simulant under standardized testing such as EN 1186 and EN 13130. The anhydride-modified layer is not automatically cleared in every jurisdiction; final packaging approval depends on the migration of the grafted substance and its reaction products. No claim for direct food contact should be made without the lot-specific certificate and the supplier’s regulatory letter. For non-food packaging, the resin may be used without those constraints, but local waste management and recycling codes apply. The grade is not a universally drop-in replacement for all anhydride-modified polyolefins; substitution requires revalidation of adhesion, sealing, and regulatory status in the finished structure.