Dow Bynel 4109 Anhydride Modified Lldpe Adhesive Resin

Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 903903
    Polymer Type Anhydride-Modified Linear Low Density Polyethylene (LLDPE)
    Melt Index 190 C 2 16 Kg 5.0 g/10 min
    Density 0.925 g/cm³
    Melting Point 125 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Break 16 MPa
    Elongation At Break 800 %
    Flexural Modulus 200 MPa
    Shore D Hardness 50
    Water Absorption <0.1 %
    Adhesion To Evoh Excellent
    Adhesion To Polyamide Nylon Excellent
    Adhesion To Polyethylene Excellent
    Recommended Processing Temperature 230–260 °C
    Thermal Stability Good

    As an accredited Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Bynel® 4109 adhesive resin is supplied in 25 kg polyethylene-lined multiwall paper bags, palletized and stretch-wrapped; typically 40 bags per pallet.
    Container Loading (20′ FCL) Dow Bynel® 4109 adhesive resin in 25 kg bags, palletized, stretch-wrapped, and secured in a dry 20-foot FCL for ocean transport.
    Shipping Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin is transported as non-hazardous solid pellets in original sealed bags, boxes, or bulk containers. It is not regulated under DOT, IMDG, IATA, or ADR. No UN number, hazard class, or packing group applies. Keep dry and avoid excessive heat.
    Storage Store Dow Bynel® 4109 in a cool, dry, well-ventilated area in tightly closed original containers. Protect from moisture, heat, direct sunlight, sparks, and open flames. Keep away from strong oxidizers. Avoid prolonged storage at elevated temperatures. Maintain good housekeeping and follow the manufacturer’s SDS and local regulations. Use first-in, first-out inventory. Do not store near food, drink, or animal feed.
    Shelf Life Shelf life is 24 months from manufacture when stored unopened in original packaging in a cool, dry place, away from direct sunlight.
    Application of Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin

    Can a Linear-Low-Density Tie Resin Maintain EVOH Barrier Integrity in Seven-Layer Blown Film?

    In a seven-layer blown film structure comprising LLDPE skins, an EVOH core and two adhesive interlayers, Bynel® 4109 is processed as a neat tie resin rather than as a dilution additive; the two tie layers are commonly set at 4% to 7.5% of total film thickness each, placing the combined adhesive fraction at 8% to 15% while the EVOH core occupies 5% to 10%. The resin is metered through satellite single-screw extruders with 25:1 to 30:1 L/D ratios and barrier screws, with melt temperature maintained at 210 °C to 240 °C; a die gap of 2.0–2.4 mm and a blow-up ratio of 2.0:1–2.5:1 are used to limit melt orientation that can reduce interlayer peel force. Bynel® 4109 does not require pre-drying when stored at relative humidity below 60%, but bulk containers opened at relative humidity above 80% should be dried for 4 h at 60 °C to prevent hydrolytic reversion of the anhydride groups. The downgauged film is tested for lamination bond strength by a T-peel method under ISO 11339:2022 after 24 h conditioning at 23 °C and 50% RH. The compliance envelope for food contact is derived from 21 CFR 175.105 for the adhesive component and (EU) No 10/2011 for the finished multilayer article, with overall migration limited to 10 mg/dm² and good manufacturing practice demonstrated under EC No 2023/2006. The finished article is a vacuum or modified-atmosphere barrier bag for fresh red meat, processed cheese, and frozen seafood, where the observed production-scale failure mode is not barrier loss but seal-area delamination when the tie-layer thickness drops below 4% due to feedblock flow imbalance.

    External Three-Layer Polyethylene Pipe Coating Compliance and Tie-Layer Thickness

    For three-layer polyethylene external coating of buried steel line pipe, Bynel® 4109 is extruded as a continuous adhesive stratum between a cured fusion-bonded epoxy primer and a high-density polyethylene topcoat. The qualified layer allocation places the FBE primer at 60–150 µm, the Bynel® 4109 adhesive layer at 200–400 µm, and the HDPE topcoat at 2.5–3.5 mm; the adhesive layer is processed at 100% resin without dilution, because dry-blending into the HDPE topcoat at 5–15 wt% is confined to non-standard repair procedures for which published adhesion data are limited. The pipe is preheated to 180–230 °C after FBE curing, and the adhesive resin is delivered through a side-wrap or crosshead flat die at 210–250 °C. Residence time above 260 °C is limited to less than 10 min to avoid gel formation from anhydride crosslinking. Project specifications under ISO 21809-1:2018, DIN 30670:2012, and CSA Z245.21-18 require peel-strength testing at 23 °C and 60 °C, with commonly applied acceptance thresholds of 20 N/cm and 10 N/cm respectively, although end-user specifications may vary by pipe diameter and service temperature.

    Cathodic disbondment resistance is evaluated on laboratory-coated pipe specimens at a negative potential of 1.5 V to 3.5 V and a temperature fixed by the project specification, frequently 65 °C or 80 °C, for 28 days. The terminal coated article is a buried oil or gas transmission line pipe whose external coating must survive field-bending and trench laying without interfacial fracture. On production-scale lines, the dominant failure mode is not extrusion pressure fluctuation but a thin adhesive layer below 150 µm caused by sagging of the wrap band on large-diameter pipe; this produces peel initiation at holidays where the topcoat is punctured during handling.

    In cast film coextrusion for vacuum-skin packaging, Bynel® 4109 functions as a discrete tie layer between a polyolefin sealant and a polyamide or EVOH barrier core, with the two tie layers together occupying 5% to 10% of total film thickness. The film is produced on a chilled-roll cast line with feedblock distribution and satellite extruders having 30:1 L/D ratios; melt temperature at the tie-layer die is held at 230–250 °C, and the cast roll is maintained at 15–25 °C to quench the web before windup. Interlayer adhesion is monitored by ASTM F904-16 after 48 h at 23 °C and 50% RH. The regulatory base for food contact includes 21 CFR 177.1520 for the polyolefin layers, 21 CFR 175.105 for the adhesive component, and (EU) No 10/2011 for the finished film, with overall migration evaluated under EN 1186-1 using 10% ethanol and 3% acetic acid simulants. The terminal flexible web is converted into vacuum-skin packages and flowpack pouches for fresh pasta, sliced processed meat, and high-moisture cheese. A production-scale limitation is that polyamide regrind containing free amine heat stabilizers can reduce tie-layer bonding when regrind content exceeds 15% in the skin layer, so regrind streams must be segregated and tested by infrared composition analysis.

    When Extrusion Lamination Replaces Solvent-Based Adhesives in Aluminum Foil Barrier Webs

    When the roll-stock converter targets a foil-to-sealant structure without solventborne adhesives, Bynel® 4109 is applied as a melt-extruded bonding web at a coat weight of 15–25 g/m² between 7–9 µm aluminum foil and an LDPE or LLDPE sealant film; the formulation addition ratio is therefore expressed as coat weight, not as a blend percentage, although coextrusion coating trials have used 20–30 wt% Bynel® 4109 in an LDPE carrier to improve foil adhesion at reduced coat weights. The extrusion lamination line typically uses a 32:1 L/D single-screw extruder with a flat die gap of 0.5–0.8 mm, an air gap of 100–150 mm, and melt temperature of 260–290 °C; the elevated melt temperature oxidizes the polyethylene melt sufficiently to form polar species at the foil surface, but residence time above 290 °C must be kept below 5 min to prevent visible gel streaks.

    Lamination bond strength is measured by ASTM F904-16 after 24 h conditioning, with a commonly specified acceptance boundary of 2.0–3.0 N/15 mm for foil-based structures. The regulatory envelope for food packaging includes 21 CFR 177.1390 for the laminate and (EU) No 10/2011 for migration compliance. The terminal article is a dry-beverage powder sachet or a lidding web for flanged dairy cups; this structure is not specified for retort service because LLDPE-based sealants lose dimensional integrity during prolonged exposure above 95 °C.

    Coextruded barrier sheet for HDPE/EVOH/HDPE thermoformed containers relies on Bynel® 4109 as the interlayer between high-density polyethylene skins and an EVOH core, with tie layers combined at 4% to 8% of total sheet thickness and EVOH at 3% to 6%, leaving HDPE skins at 86% to 93%. The sheet is produced on a flat-die coextrusion line with a die gap of 0.8–1.5 mm, a polishing stack temperature of 20–30 °C, and a line speed adjusted to deliver a sheet surface temperature of 130–145 °C entering the thermoformer. The tie resin’s low-shear viscosity is matched to the HDPE grade to avoid interfacial waviness, and layer thickness is verified by cross-section microscopy at 200× magnification against a tolerance of ±0.5% absolute. The food-contact compliance base references 21 CFR 177.1520 for the polyolefin layers and (EU) No 10/2011 for the finished article, with overall migration limited to 10 mg/dm² and sensory testing conducted under DIN 10955 where taste neutrality is required. The finished articles are polyethylene-based thermoformed tubs and trays for chilled spreads, margarine, frozen dough, and modified-atmosphere ready meals. A process limitation occurs when trim regrind exceeds 40% in the outer HDPE layers, because oxidized EVOH in the regrind can initiate interfacial gels at the tie interface.

    Blow Molded Barrier Containers and the Tie-Layer Viscosity Window

    In coextrusion blow molding of HDPE/tie/EVOH barrier bottles and jerrycans, Bynel® 4109 is processed as a neat tie layer with a combined tie-layer share of 1.5% to 3.0% of total wall thickness, while the EVOH oxygen barrier occupies 2% to 5% and the HDPE structural layers provide 90% to 96%. The parison is formed through an accumulator head or a continuous shuttle/rotary wheel system; tie-layer extruders are specified at 24:1 L/D with a melt temperature of 210–230 °C, and the head is operated to keep tie resin residence time below 8 min because prolonged hold-up in the accumulator can cause localized anhydride crosslinking at the layer interface. Tie-layer melt flow rate is determined under ISO 1133-1:2022 at 190 °C/2.16 kg, but interlayer adhesion is tested on bottle wall specimens with a 90° peel fixture adapted from ASTM F904-16 after 24 h conditioning. The regulatory base for food and personal-care packaging is 21 CFR 175.105 for the adhesive layer and (EU) No 10/2011 for the finished container, supported by good manufacturing practice under EC No 2023/2006. The finished article types include multilayer HDPE bottles for mayonnaise, ketchup, liquid soap, and cosmetic emulsions, where the critical production-scale failure mode is not barrier loss but delamination at the pinch-off weld when the tie-layer thickness falls below 1.5%.

    Free Quote

    Competitive Dow Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Bynel® 4109 is an anhydride-modified linear low-density polyethylene resin supplied as pellets for melt-phase adhesion in coextruded and extrusion-coated multilayer structures. The product functions as a tie layer between non-polar polyolefin layers and polar substrates such as ethylene-vinyl alcohol copolymer, polyamide, aluminum foil, and ionomer. The anhydride functionality introduces reactive sites onto the LLDPE backbone, enabling bonding to hydroxyl, amide, and metal oxide surfaces during melt contact. Typical physical properties reported in manufacturer technical literature include a melt index of 2.0 g/10 min at 190 °C under 2.16 kg load when measured according to ASTM D1238 or ISO 1133-1, and a density of 0.92 g/cm³ when measured according to ASTM D792 or ISO 1183-1. These values place the resin in the medium-viscosity range used for blown film, cast film, extrusion coating, sheet, and blow molding.

    Typical property ranges reported for Dow Bynel® 4109
    PropertyTypical valueTest method
    Melt index at 190 °C, 2.16 kg2.0 g/10 minASTM D1238, ISO 1133-1
    Density0.92 g/cm³ASTM D792, ISO 1183-1
    Melting peak temperature125 °CASTM D3418, ISO 3146
    Vicat softening point105 °CASTM D1525, ISO 306

    How Bynel® 4109 Compares with Anhydride-Modified HDPE and Ethylene Acid Copolymer Tie Resins

    The LLDPE backbone differentiates Bynel® 4109 from maleic anhydride-grafted high-density polyethylene tie resins in several processing-dependent respects. Maleated HDPE grades typically exhibit higher crystalline content, higher flexural modulus, and a density above 0.94 g/cm³, which can produce stiffer tie layers but reduced dart impact and lower stress crack resistance in flexible packaging. Bynel® 4109, with a density near 0.92 g/cm³, provides a balance of interfacial adhesion and film toughness that is more compatible with LLDPE-rich sealant layers and blown film structures requiring dart impact resistance measured by ASTM D1709 or Elmendorf tear by ASTM D1922. Compared with ethylene acid copolymer tie resins, the anhydride-modified LLDPE does not contain carboxylic acid comonomer in the same form and generally exhibits lower moisture pickup, easier processability without pre-drying in closed packaging, and reduced die drool. Acid copolymers can produce higher adhesion to unprimed aluminum and nylon at elevated temperatures, but their carboxylic acid functionality can increase corrosivity toward processing equipment and may require more aggressive purging. Maleic anhydride-grafted random copolymer polypropylene tie resins are not equivalent substitutes in polyethylene-based structures because their higher melting temperatures and different crystallization rates can disrupt layer uniformity and reduce interfacial contact time at standard LLDPE extrusion temperatures.

    Where three-layer blown film lines combine LLDPE sealant skins with EVOH or polyamide core layers, the tie resin is extruded through separate satellite extruders into the feedblock or multi-manifold die. The recommended melt temperature window for Bynel® 4109 in blown film is typically 210 °C to 240 °C, with adapter and die temperatures maintained within 10 °C of the melt stream to avoid thermal stratification. Single-screw extruders with 24:1 to 30:1 L/D and moderate compression ratios from 2.5:1 to 3.5:1 are generally suitable. Excessively low melt temperature produces incomplete wetting of the polar substrate and low peel strength; excessively high melt temperature above 280 °C can accelerate anhydride decomposition, crosslinking, and gel formation on die lips. The process window is therefore governed by two competing failure modes: cold interface starvation at the lower limit and thermally induced gel formation at the upper limit.

    Extrusion coating operations using Bynel® 4109 onto corona-treated aluminum foil or metallized film require higher melt temperatures than blown film because draw-down and web speed demand lower melt viscosity. Typical melt temperatures in extrusion coating range from 260 °C to 290 °C, depending on line speed, die gap, and coating thickness. The anhydride groups react with aluminum oxide and can promote adhesion to foil, but residence time at these temperatures must be controlled. Extended stagnation in the die manifold can produce oxidized gel particles that appear as coating specks. Processors often observe that adhesion to foil increases with air gap and melt temperature up to a threshold, beyond which degradation products interfere with interfacial bonding. Peel adhesion after lamination is typically evaluated by T-peel using ASTM F904, with failure mode being more informative than the absolute load; cohesive failure in the LLDPE layer indicates an effectively bonded tie layer, while adhesive failure at the foil interface indicates inadequate melt temperature, insufficient corona treatment, or surface contamination.

    When Extrusion Coating Replaces Solvent-Based Lamination on Aluminum Foil

    In structures where solvent-based adhesive lamination is replaced by extrusion coating with Bynel® 4109, the tie layer must perform both adhesive and thermal barrier functions. The anhydride-modified LLDPE is often extruded between aluminum foil and heat-sealable LLDPE or LDPE layers. Unlike dry lamination, where adhesive penetration is limited and solvent retention can be a concern, extrusion coating creates a continuous melt-phase interface. The absence of solvent aligns with regulatory and environmental requirements under EU Regulation 10/2011 and reduces volatile organic compound release. The attainable adhesion depends on foil surface energy and the presence of residual rolling oils. Off-line corona treatment of foil to a wetting tension of at least 46 mN/m is common, although exact thresholds are substrate-specific. The bond strength in extrusion-coated foil laminates is measured by ASTM F904, and heat seal performance of the final structure is characterized by ASTM F88 or ASTM F2029. When the coating line speed exceeds the capability of the extruder to maintain a uniform melt curtain, edge neck-in and gauge variation can produce localized adhesion defects. Published data for this specific configuration is limited, and pilot-scale qualification is required because adhesion is highly dependent on die geometry, air gap, and substrate conditioning.

    In coextruded polyamide/EVOH barrier films, Bynel® 4109 is positioned between the non-polar polyethylene layers and the polar barrier core. Polyamide surfaces contain amide groups that can interact with the anhydride functionality, while EVOH surfaces contain hydroxyl groups. Adhesion to EVOH is sensitive to the ethylene content of the EVOH grade and the moisture content of the film at the time of testing. EVOH with higher ethylene content may yield different peel behavior than grades with lower ethylene content because the surface concentration of hydroxyl groups and the layer modulus change. Peel strength in these structures is commonly measured by ASTM F904, but the test result is influenced by layer gauge, delamination angle, and conditioning. When the structure is conditioned at 23 °C and 50% relative humidity, moisture migration into the EVOH layer can lower interfacial shear strength. Barrier films intended for retort or hot-fill use often show reduced tie-layer adhesion after elevated temperature exposure if the EVOH layer absorbs moisture. The resin is therefore selected for its ability to maintain interfacial contact under moisture challenge, but the actual adhesion must be validated in the end-use laminate.

    Blow molding of barrier containers uses Bynel® 4109 as the adhesive layer in three-layer or five-layer parison structures containing polyamide or EVOH barrier layers. The parison is extruded at melt temperatures typically between 210 °C and 240 °C, with the tie resin melt stream controlled separately from the barrier layer to avoid excessive shear heating. Intermittent extrusion presses often use accumulator heads where residence time can vary across the parison. Because anhydride-modified polyolefins can undergo slow crosslinking at elevated temperature, prolonged hold time in the accumulator can generate gel specks or cause layer instability. Purging with low-melt-index polyethylene between runs is common to prevent crosslinked material from adhering to head surfaces. Burst strength and drop impact of the molded container are measured by ASTM D2463 or ASTM D5276, while barrier performance is validated by oxygen transmission rate using ASTM D3985 or ASTM F1927. The tie layer is not normally the limiting variable in oxygen barrier performance, but adhesion loss at the barrier interface can create voids that reduce burst resistance and delamination resistance.

    Moisture Uptake, Regrind Limits, and Food-Contact Standard Citations

    Bynel® 4109 is generally less hygroscopic than acid copolymer tie resins, but surface moisture pickup can occur when pellets are stored outside moisture-proof packaging. If pellets are exposed to relative humidity above 60% for extended periods, drying with desiccant air at 80 °C for 4 h is commonly used to remove surface moisture before processing. Moisture at the pellet surface can hydrolyze anhydride functionality during extrusion, reducing the concentration of reactive groups available for bonding to EVOH, polyamide, or metal oxide surfaces. The resin should not be dried at temperatures above 90 °C without adequate airflow, because pellet agglomeration can occur in the hopper. Regrind use is process-dependent; levels up to 20% by weight are used in some non-critical cast film applications, while high-clarity or retort structures typically require lower regrind levels to limit gel content and optical defects. The incorporation of regrind containing mixed barrier and tie-layer fractions can alter adhesion and haze, and published data for regrind thresholds in high-clarity coextrusions is limited.

    For food-contact applications, Dow provides compliance documentation referencing FDA 21 CFR 175.105 for adhesive components in multilayer food-packaging structures, subject to end-use conditions and any applicable limitations on layer thickness or food type. Regional compliance must be verified against current regulatory lists, including EU Regulation 10/2011 for plastic materials and articles intended to come into contact with food. The product is not intended for direct food contact as a monolayer surface; its function is as an internal adhesive layer. Processors should retain supplier compliance certificates and confirm that the final migrated level of any adhesive component remains within the applicable specific migration limit. For non-food industrial laminates, no food-contact standard applies, but material handling and volatile emissions are governed by workplace exposure limits and applicable regional health and safety regulations.

    Addition of certain nitrogen-containing additives, including primary and secondary amines, should be avoided in formulations containing Bynel® 4109. Amine-based processing aids or slip concentrates can react with anhydride groups before the tie layer contacts the polar substrate, reducing the number of available bonding sites. Near the die, the resulting reaction products can increase die lip deposit formation. In coextrusion with polyamide resins containing high residual caprolactam or amine end groups, interfacial chemistry can vary with the specific polyamide grade and its polymerization catalyst. Processors should also avoid prolonged contact with copper-based stabilizer packages in wire and cable constructions where the tie resin is not exposed to the metallic conductor but may contact trace copper ions in the melt; published data for this interaction is limited. The operational boundary therefore includes not only melt temperature and residence time but also the additive environment of adjacent layers.

    For structures requiring low-temperature seal initiation, Bynel® 4109 is generally used adjacent to an LLDPE sealant layer rather than as the direct sealant layer. The presence of the anhydride functionality does not primarily govern seal initiation temperature, but the LLDPE backbone provides a lower seal initiation range than HDPE-based tie resins under ASTM F88 or ASTM F2029 testing. The heat seal strength of a finished laminate is influenced by seal bar temperature, dwell time, and pressure. Typical seal testing is performed at temperatures from 110 °C to 150 °C, depending on the sealant resin and film gauge. When Bynel® 4109 is used in the sealant layer itself, the presence of the anhydride functionality can alter the seal strength curve and the seal through contamination tolerance; qualification by heat seal testing is therefore required before commercialization.

    Top