Dow Bynel 4105 Anhydride Modified Lldpe Adhesive Resin

Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 230248
    Product Name Dow Bynel® 4105
    Manufacturer Dow
    Product Type Anhydride-Modified LLDPE Adhesive Resin
    Chemistry Anhydride-modified linear low-density polyethylene
    Carrier Resin Linear low-density polyethylene (LLDPE)
    Functional Group Maleic anhydride
    Form Pellets
    Color Natural
    Density 0.921 g/cm³
    Melt Index 190 C 2 16 Kg 2.8 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 92 °C
    Processing Temperature Range 200–260 °C
    Thermal Stability Good at recommended processing temperatures
    Adhesion Substrates Polyethylene, EVOH, polyamide, aluminum
    Food Contact Status Complies with FDA 21 CFR 175.105

    As an accredited Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg multi-wall bags, stacked on pallets; each pallet contains 1,000 kg (40 bags) of Bynel 4105 resin.
    Container Loading (20′ FCL) 20′ FCL loaded with Dow Bynel® 4105 adhesive resin in 25 kg bags, palletized, stretch-wrapped, securely strapped, moisture-protected, evenly distributed.
    Shipping Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin ships as nonhazardous pellets in 25 kg moisture-barrier bags or bulk containers, palletized and stretch-wrapped. It is generally not regulated as dangerous goods. Transport in clean, dry vehicles at moderate temperatures; protect from moisture, heat, and contamination. Store sealed in cool, dry conditions.
    Storage Store Dow Bynel 4105 resin in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers tightly closed and off the floor. Protect from contamination and excessive temperatures. Follow first-in, first-out stock rotation. Consult the Safety Data Sheet (SDS) for detailed handling and storage requirements.
    Shelf Life Shelf life is 24 months from manufacture when stored unopened in original packaging below 30°C, protected from moisture and direct sunlight.
    Application of Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin

    When EVOH Layer Ratios Exceed 5 wt% in Blown Barrier Film, What Governs Interlayer Peel Stability?

    Three-layer coextruded blown film lines running PA6 or EVOH barrier cores with linear low-density polyethylene skin layers frequently deposit the anhydride-modified LLDPE tie resin at the core/skin interface. When EVOH volume fraction in the entire film exceeds 5 wt%, the interlayer peel force obtained after 90° peel testing under ASTM F904-16 may fall below production acceptance thresholds if the tie layer has been calculated as a residual layer rather than as a separate barrier-adjacent mass fraction. Bynel® 4105, with a melt index of 3.2 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and a density of 0.92 g/cm³ under ISO 1183-1:2019, is introduced at 8–15 wt% of total film mass, corresponding to a dry-layer thickness of 5–12 µm in an 80–120 µm structure. Compliance for meat and cheese packaging in export markets is commonly evaluated against 21 CFR 177.1500 for the polyolefin portion and Regulation (EU) No 10/2011 as amended, with end-use migration verification under 21 CFR 174.5 because the anhydride-grafted component must be used within the supplier’s food-contact authorization limits for each film construction. Processing on a three-layer IBC blown film line with barrier screws of L/D 24:1 to 30:1 requires melt temperatures of 220–240 °C at the adapter, a die gap of 1.8–2.5 mm, and a blow-up ratio of 2.2:1–3.0:1; PA6 and EVOH must be pre-dried to <200 ppm moisture to prevent hydrolytic degradation and attendant gel-induced die lip deposits in the tie layer. Terminal products include vacuum pouches for fresh red meat, thermoforming top webs for sliced cheese, and low-oxygen sous-vide bags for cooked protein; terminal peel strength acceptance criteria are typically agreed as pass/fail against a film-specific lower limit, but published data for this specific configuration is limited and plant-scale sampling is required because adhesion values shift with EVOH moisture uptake above 80 % relative humidity in the quarantine warehouse.

    Across multilayer blow moulding lines running high-density polyethylene and polyamide six-layer parisons, delamination at pinch-off welds remains the dominant defect mode when the tie layer is starved below the die gap’s minimum layer-distribution window. Bynel® 4105 is specified at 5–10 vol% of the total container wall, ordinarily a 25–75 µm adhesive stratum within an overall wall thickness of 0.6–1.2 mm; this range prevents the low-melt-strength region that appears when the tie layer falls under 4 vol% in accumulator-head tools. For agrochemical and industrial liquid packaging, the container must be qualified under the applicable UN transport packaging requirements for Packing Group II and III liquids, with oxygen transmission measured under ASTM D3985 and water vapour transmission under ASTM E96/E96M for the complete laminated wall; food-contact declarations are generally not the primary compliance path for solvent-based formulations, but the resin’s polyolefin base may still be evaluated under 21 CFR 177.1500 when the same line is switched to food-compatible barrier bottles. Processing on a six-layer coextrusion blow moulder with an accumulator head of 10–20 kg/h output uses HDPE barrel temperatures of 190–210 °C, Bynel® 4105 at 210–230 °C, and PA6 at 240–260 °C; parison programming is adjusted so that the tie layer thickens at the welding zone because residual heat loss below 200 °C at the pinch-off produces banding and low peel force. Terminal products include 1 L to 5 L HDPE/PA containers for chlorinated solvent cleaning agents, pesticides, and aqueous agricultural adjuvant concentrates; batch-to-batch variance in adhesive performance is monitored by sectioning the bottle wall and performing peel testing after 48 h conditioning at 40 °C.

    If Aluminium Foil Pinhole Formation Drives Peel Strength Variability in Aseptic Carton Stock

    Extrusion coating lines producing liquid packaging board for aseptic beverage cartons insert an anhydride-modified LLDPE layer between aluminium foil and the heat-sealable polyolefin skin because foil pinholes generated during cold-roll transfer and downstream scoring act as initiation points for delamination when the interlayer peel strength falls below the carton converter’s die-cut threshold. Bynel® 4105 is applied at 8–15 g/m² coat weight, corresponding to a 10–18 µm tie layer in the laminate; the adjacent foil thickness is typically 6.35–9 µm. Compliance for carton stock placed into the European and North American markets is assessed under Regulation (EU) No 1935/2004 through the member-state declaration for food contact materials, 21 CFR 176.170 for paperboard components, and 21 CFR 177.1500 for the polyolefin contact layer; the aseptic structure itself must also pass hydrogen peroxide sterilisation compatibility because the tie resin should not exhibit surface blush or bond decay after exposure to 35 % H2O2 at 65–75 °C. Process conditions on tandem extrusion coating/laminating equipment use a 26:1 L/D extruder with melt temperatures of 230–260 °C, chill roll temperature of 15–20 °C, and line speed of 200–400 m/min; ozone treatment of the melt at 20–40 g/m³ and corona pre-treatment of the foil surface stabilize oxidative polar species that improve adhesion. Terminal products include gable-top milk cartons, brick-shaped aseptic juice packs, and portion packs for dairy and non-dairy liquids; a documented test protocol under ASTM F904-16 is used to separate the foil/adhesive interface and confirm that the failure mode remains cohesive in the tie layer rather than adhesive at the foil boundary.

    On cast-film chill-roll lines producing high-clarity PA/PE structures for refrigerated protein, the anhydride-modified LLDPE layer is constrained by a narrower thermal quench window than blown film because the flat-die air gap and chill roll temperature determine both optical defects and interfacial crystallinity. Bynel® 4105 is specified as 6–12 wt% of the cast web, with a tie-layer thickness of 5–10 µm in structures ranging from 50–150 µm; higher addition fractions above 12 wt% reduce transparency and increase the probability of chill-roll release oscillation. Food-contact compliance is generally supported by 21 CFR 177.1500 for the polyolefin fraction and Regulation (EU) No 10/2011 as amended, with overall migration testing conducted under EN 1186-1:2002 and specific migration limits for any residual maleic anhydride determined by LC-MS/MS; since Bynel® 4105 is used only as an internal tie layer, it is not considered a direct food-contact surface. The cast-film process uses a flat die with a lip gap of 0.3–0.5 mm, an air gap of 10–20 cm, a chill roll temperature of 15–25 °C, and line speeds of 100–300 m/min; PA6 and EVOH melt streams are pre-dried to <0.02 % moisture, and the tie layer converter must purge with low-density polyethylene when melt temperature exceeds 260 °C to avoid gel spots. Terminal products include high-clarity top lidding films for fresh poultry, bottom webs for modified-atmosphere trays, and cold-sealable flowpack laminates for cheese; adhesion acceptance is checked with a 180° peel test after 24 h conditioning at 23 °C/50 % RH, because polyamide crystallinity continues to evolve during the first day after extrusion.

    Coextruded HDPE/EVOH Sheet Split-Edge Defects in Contact-Heated Thermoforming

    Coextruded high-density polyethylene sheets containing an ethylene vinyl alcohol core require the adhesive layer to maintain peel force after plug-assist thermoforming elongates the tie layer by 300–600 % in corner regions. Bynel® 4105 is metered at 8–15 wt% of the sheet mass, producing a 50–150 µm tie layer in sheet from 800–2500 µm; thermoforming plants that reduce the tie layer below 50 µm report delamination at trimmed edges and plug-assist contact scars when the material is stretched at core temperatures of 120–160 °C. Compliance for retail packaged fresh food trays is assessed under 21 CFR 177.1500 and Regulation (EU) No 10/2011 as amended; oxygen transmission of the finished tub is measured under ASTM D3985 at 23 °C/50 % RH and water vapour transmission under ASTM F1249. The five-layer sheet is extruded through a coat-hanger flat die with melt temperatures of 220–240 °C, polished roll temperatures of 60–90 °C, and line speeds of 5–20 m/min; sheet thickness is controlled by a beta gauge, and the EVOH core must be pre-dried to <0.02 % moisture to prevent foaming at the die exit. Terminal products include thermoformed MAP trays for fresh pasta, ham packs, and ready-meal containers; qualified processors monitor tie-layer thickness by sectioning the thermoformed corner and performing peel testing after retort or pasteurization simulation because heating above 90 °C can lower peel force in high-moisture tray bottoms.

    Within five-layer coextruded tube-sleeve lines for toothpaste and cosmetic emulsions, the polyamide or EVOH barrier core is exposed to high moisture on the product side during tube filling, making interfacial adhesion after hot-air welding the governing quality variable. Bynel® 4105 is incorporated at 6–10 wt% of the sleeve wall, typically 25–40 µm in a 250–400 µm five-layer tube body; converters frequently set the tie fraction at the upper limit when the barrier core is a high-viscosity EVOH grade because low melt-strength EVOH grades produce layer-thickness variation at the weld. Cosmetic and oral-care packaging is generally qualified under Regulation (EC) No 1223/2009 for product compatibility, with packaging migration addressed by the supplier declaration for food-grade materials under Regulation (EU) No 10/2011 and 21 CFR 177.1500 when the same tube is used for toothpaste; pharmaceutical creams may require additional testing under Ph. Eur. 3.1.3 for polyolefins and USP <661.1> for plastic packaging components. The sleeve process runs a five-layer extruder with a mandrel die at melt temperatures of 210–240 °C, a cooling water temperature of 8–15 °C, and a haul-off speed of 5–30 m/min; shoulder welding then uses hot air at 220–250 °C and a welding pressure of 0.3–0.6 MPa, after which the tube is annealed for 24 h at 40 °C to stabilize frozen-in orientation. Terminal products include collapsible tubes for fluoride toothpaste, barrier tubes for hair colorants, and laminate tubes for topical ointment bases; batch release testing includes a 90° peel test across the side seam and a burst-pressure test under internal hydraulic pressure of 0.5–0.8 MPa to detect weak tie-layer splice zones.

    Free Quote

    Competitive Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Bynel® 4105 is an anhydride-modified linear low-density polyethylene (LLDPE) adhesive resin supplied in pellet form for coextrusion tie-layer service. The product is produced by grafting maleic anhydride onto an LLDPE backbone, creating a polyolefin melt stream that carries reactive anhydride groups at the polymer–substrate interface. The graft concentration is not disclosed on public technical data sheets; quality control is instead expressed through melt flow rate, density, and thermal transitions.

    PropertyTest MethodTypical Value
    Melt Flow RateASTM D1238 / ISO 1133-13.5 g/10 min at 190 °C, 2.16 kg
    DensityASTM D792 / ISO 1183-10.91 g/cm³
    Melting PointASTM D3418 / ISO 11357-3121 °C
    Vicat Softening TemperatureASTM D1525 / ISO 306103 °C
    Anhydride Graft ConcentrationNot publishedProprietary

    These typical values identify the grade as a low-viscosity LLDPE-based tie resin. The melt flow rate of 3.5 g/10 min at 190 °C under 2.16 kg load permits thin-gauge coating at moderate extruder head pressures. The density of 0.91 g/cm³ and melt point of 121 °C place the resin in the linear low-density polyethylene class; the low melting point supports adhesion development at lower melt temperatures than HDPE-based tie resins.

    What Limits Adhesion Latitude in Coextruded Barrier Structures?

    Adhesion is controlled by two coupled mechanisms: interdiffusion of molten tie-layer chains into the substrate surface and reaction of pendant anhydride groups with nucleophilic sites in the polar layer. In polyamide 6, terminal amine concentration is typically 40–60 meq/kg; anhydride groups form amic acid and imide linkages at the interface. In EVOH grades containing 32–44 mol% ethylene, hydroxyl groups participate in esterification and hydrogen bonding. The reaction conversion is not a simple function of anhydride content; it depends on melt temperature, contact time, interfacial pressure, and cooling rate.

    T-peel adhesion values measured under ASTM D1876 or flexible package bond strength under ASTM F904 therefore include both interfacial chemistry and bulk deformation of the tie layer. Thin tie layers below 5 µm often fail cohesively because the stress concentrates in the LLDPE matrix, not because the substrate surface lacks functional groups. Thicker layers above 15 µm increase peel force but add resin cost and may reduce barrier-layer thickness in the final structure. The practical adhesion latitude is set by layer thickness control on the die, not by graft concentration alone.

    EVA-based tie resins with 9–18 wt% vinyl acetate undergo deacetylation above 230 °C, generating acetic acid and creating odour, corrosion, and interfacial voids. Bynel® 4105 contains no vinyl acetate side group; its thermal ceiling is set by LLDPE backbone degradation. This difference permits coextrusion with polyamide at 240 °C without the volatile acetic acid release observed with EVA tie resins. Compared with acid copolymer tie resins, anhydride-modified LLDPE is less moisture-sensitive and has a non-acidic backbone, but acid copolymers may develop adhesion to aluminium foil at lower melt temperatures because the carboxylic acid functionality is present along the entire chain rather than only at grafted sites.

    When Bynel® 4105 Replaces EVA-Based Tie Layers in Cast Film and Sheet

    Coextrusion with EVOH or polyamide is carried out on conventional polyolefin equipment. The tie-layer extruder is typically a single-screw machine with a 24:1 to 30:1 L/D ratio and a barrier screw with a Maddock mixing section; melt pressure variation should be held below ±1.5 MPa to avoid visible layer-thickness oscillation on production-scale cast lines. A flat temperature profile of 210–240 °C is recommended for the Bynel® 4105 melt stream, with the die held at 220–240 °C. The resin does not require pre-drying when stored below 60% relative humidity; surface condensation must be removed before processing.

    On three-layer blown-film lines, the addition of Bynel® 4105 as a tie layer does not normally destabilize the bubble if the die gap is maintained at 1.8–2.5 mm and the blow-up ratio is kept between 2.0:1 and 3.0:1. Lower melt strength relative to LDPE can reduce bubble stability at high haul-off tension; this is managed by reducing the collapsing frame height or increasing the frost line height. Batch-to-batch variation in melt flow rate should be monitored because a drift of ±0.5 g/10 min at the same extruder speed can alter tie-layer thickness by more than 10% in low-output lines.

    The melt temperature must not exceed 260 °C. At temperatures above 260 °C, prolonged residence time beyond 10 minutes can deplete anhydride functionality through thermal decomposition and generate gel particles. The anhydride groups react with primary amine additives; therefore, amine-containing slip or antiblock masterbatches must not be added directly to the tie layer. If amine additives are present in an adjacent polyamide layer, they remain separated by the tie layer and do not consume Bynel® 4105 functionality until melt contact occurs at the interface.

    In five-layer barrier films used for vacuum packaging of processed meat, Bynel® 4105 is typically placed between a polyethylene sealant skin and an EVOH or polyamide core. A common film architecture is LLDPE/Bynel® 4105/EVOH/Bynel® 4105/LLDPE. The EVOH layer is dried to 0.08% moisture or lower before extrusion; the tie-layer thickness is maintained between 5 µm and 12 µm per side. Peel adhesion after film conversion is assessed by ASTM F904; failure in the sealant layer rather than at the tie interface is the standard acceptance criterion.

    In coextruded blow-molded containers for food, Bynel® 4105 serves as the tie between high-density polyethylene and EVOH. The container wall may contain 2.0–3.0 wt% tie layer. Drop impact resistance is evaluated by ASTM D2463; delamination at pinch-off weld lines indicates inadequate interfacial temperature or insufficient tie-layer thickness. The LLDPE backbone reduces weld-line stiffness relative to HDPE-based tie resins, which mitigates stress concentration during impact at -20 °C.

    Storage of opened bags in high humidity can hydrate the anhydride functionality. If pellets are exposed to relative humidity above 60% for more than 8 h, surface moisture is best removed by drying at 80 °C for 4 h in a desiccant dryer. Regrind of Bynel® 4105 from edge trim can be incorporated back into the tie layer at up to 20 wt% if it has not been contaminated with EVOH or polyamide dust; cross-contamination of tie-layer regrind with barrier resin reduces the available anhydride surface and should be controlled by dedicated grinding and conveying.

    Compared to unmodified LLDPE, the anhydride functionality of Bynel® 4105 changes melt rheology only slightly; the low-shear viscosity is similar to standard LLDPE with the same melt flow rate. The presence of grafted anhydride may, however, raise the melt elasticity and reduce melt fracture. In coextrusion, the melt flow ratio between the tie layer and the adjacent polymer should not exceed 3:1; otherwise, interfacial instability can occur. When Bynel® 4105 is coextruded with a 0.5 g/10 min HDPE layer, the melt flow ratio is 7:1, and die-lip adjustment is required to maintain layer uniformity.

    Top