Dow Bynel 4104 Anhydride Modified Lldpe Adhesive Resin

Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 773069
    Product Name Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin
    Chemistry Anhydride-modified linear low-density polyethylene (LLDPE)
    Density 0.925 g/cm³
    Melt Index 2.5 g/10 min (190°C/2.16 kg)
    Melting Point 125°C
    Vicat Softening Point 90°C
    Tensile Strength At Break 14 MPa
    Elongation At Break 500%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Water Absorption 0.03%
    Adhesion To Evoh Excellent
    Adhesion To Nylon Excellent
    Adhesion To Polyethylene Excellent
    Processing Temperature 200-260°C
    Thermal Stability Good

    As an accredited Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Bynel 4104 adhesive resin comes in 25 kg (55 lb) polyethylene-lined bags, palletized for industrial shipping.
    Container Loading (20′ FCL) Dow Bynel® 4104: 20′ FCL holds 20 pallets × 40 × 25 kg bags, 20,000 kg net, palletized and shrink-wrapped.
    Shipping Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin is shipped as non-hazardous, non-regulated polymer pellets. Typical packaging includes moisture-barrier bags, boxes, or bulk containers. Transport in cool, dry conditions away from heat, sunlight, and moisture. No special DOT, IMDG, or IATA hazard classification applies; keep containers sealed and follow local regulations.
    Storage Store Dow Bynel® 4104 in a cool, dry, well-ventilated warehouse away from heat, direct sunlight, moisture, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture pickup. Use clean, dry handling equipment. Store indoors, off the ground, in original packaging. Protect from physical damage. Recommended storage temperature is below 30°C (86°F). Follow the SDS.
    Shelf Life Shelf life: 24 months when stored unopened in original packaging, cool, dry, well-ventilated area, away from moisture, heat, and sunlight.
    Application of Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin

    What Prevents Delamination in Five-Layer EVOH Barrier Films During Retort Processing?

    In five-layer blown film lines producing EVOH-containing barrier webs, Bynel 4104 is inserted as the continuous adhesive layer between the EVOH core and LDPE or LLDPE skins. The anhydride groups of the resin react with residual hydroxyl functionality on the EVOH surface during coextrusion, forming interfacial covalent grafts that resist delamination after steam retorting at 121°C for 30 min. Typical tie-layer thickness is 8 µm to 15 µm per adhesive layer, corresponding to 10 wt% to 15 wt% of a total film gauge of 80 µm to 150 µm. Extruder zones are maintained at 180°C to 240°C, with die temperature not exceeding 240°C to limit gel formation. EVOH must be pre-dried to below 0.08% moisture before entering the extruder; otherwise microbubble formation at the tie/EVOH interface reduces peel force in downstream ASTM F904-16 testing. Compliance for food-contact use is assessed under FDA 21 CFR 177.1395 and EU Regulation (EU) No 10/2011. Terminal structures include vacuum pouches, cook-in bags, and modified atmosphere packaging for processed meat. Production-scale blown film lines with 60 mm to 90 mm barrier screws and 30:1 L/D ratios observe that purging with low-viscosity LDPE before shutdown prevents stagnated anhydride resin from forming crosslinked specks in the die gap. Blow-up ratios are held between 2.0 and 2.5, and frost line height is adjusted to 3D to 5D above the die. Adhesion of the tie layer to EVOH is measured after 24 h conditioning by peel testing following ASTM F904-16; failure is required to occur within the PE skin rather than at the tie interface. This configuration is not recommended for retort temperatures above 121°C without revalidation because hydrolytic degradation of EVOH accelerates rapidly above that threshold.

    Extrusion lamination of aluminium foil to LLDPE in laminated tube production applies Bynel 4104 as the first extrusion coat on the foil web, where the anhydride functionality provides adhesion to the metal oxide surface without solvent-based primers. Coating weight is controlled between 8 g/m² and 16 g/m², which corresponds to roughly 12 µm to 20 µm of adhesive resin at a density of 0.92 g/cm³ to 0.93 g/cm³. Melt temperature at the T-die is set to 260°C to 290°C; below 250°C, oxidation of the LLDPE backbone is insufficient to create robust foil wetting, while above 300°C, odour and gel formation become measurable in the laminate. The foil is preheated to 50°C to 70°C before the nip, and the chill roll is maintained at 15°C to 25°C. Peel adhesion is determined by ASTM D903 with a 25 mm specimen width; acceptable failure mode is cohesive within the PE sealant or foil tear, not clean interfacial separation. Food-contact compliance for the laminate is assessed under FDA 21 CFR 177.1395 and EU Regulation (EU) No 10/2011. Terminal products include toothpaste tubes, cosmetic sachets, and pharmaceutical strip packaging where aluminium foil provides the barrier layer. The process is sensitive to foil splice interruptions; closed-loop coat-weight control is typically required on lines running above 150 m/min to hold variation below 2 g/m².

    Application scenarioTie-layer addition ratioProcess windowPrimary compliance anchor
    EVOH blown film10–15 wt%180–240°C die zoneASTM F904-16
    Aluminium foil extrusion lamination8–16 g/m²260–290°C meltASTM D903
    HDPE/PA blow moulding2–5 wt%210–230°C meltUN 1H1
    Three-layer pipe coating150–350 µm200–230°C steelISO 21809-1:2018
    Multi-layer rotational moulding5–8 wt%280–300°C ovenEPA 40 CFR Part 1060
    Cast MAP film6–10 µm per tie layer220–250°C meltASTM D3985-17

    Accumulator-Head Blow Moulding Sets Tie-Layer Ratios Between HDPE and Polyamide

    Accumulator-head coextrusion blow moulding lines running six-layer HDPE/PA structures specify Bynel 4104 as the adhesion layer between high-density polyethylene skins and the polyamide barrier core. The tie layer occupies 2 wt% to 5 wt% of the total container wall, with nominal thickness of 50 µm to 120 µm per tie layer within a 1.2 mm to 2.0 mm sidewall. Melt temperatures for the tie resin are maintained at 210°C to 230°C; exceeding 240°C in the die head increases the rate of anhydride ring opening and can shift melt viscosity downward, destabilising the parison and producing uneven layer distribution. Polyamide must be dried to 0.06% moisture or lower to prevent hydrolytic degradation at the tie/PA interface. Regrind addition is typically limited to 15% of the total shot weight because recycled mixed HDPE/tie/PA material raises gel particle formation when processed above 220°C. The anhydride functionality of Bynel 4104 is incompatible with free amine-bearing processing aids at melt temperatures above 220°C; amine migration from unstabilised polyamide regrind can generate premature crosslinking and interfacial haze in the container wall. Compliance for transport of hazardous agrochemicals is evaluated under UN 1H1 certification and ADR/RID packing requirements. Drop impact resistance is measured by ASTM D2463-15 at -18°C. Terminal products include fluorinated barrier bottles for solvent-based pesticides, herbicide formulations, and industrial cleaning chemicals.

    On a three-layer polyolefin pipe coating line, the steel substrate is first blast-cleaned to Sa 2½ and heated to 200°C to 230°C before fusion-bonded epoxy is applied at 80 µm to 120 µm. Bynel 4104 is then extruded through a flat die or spiral crosshead as the intermediate tie layer at a thickness of 150 µm to 350 µm, followed immediately by the HDPE outer topcoat at 2.5 mm to 3.5 mm. The anhydride-modified LLDPE tie layer provides adhesion to both the partially cured FBE primer and the non-polar HDPE topcoat; interfacial shear strength after water immersion is evaluated by ASTM D4541 pull-off testing. The three-layer system is qualified under ISO 21809-1:2018, and cathodic disbondment is measured according to ASTM G42-11 at 23°C for 28 days. Addition ratio of the tie layer represents approximately 5%–10% of total coating thickness. Line speed is controlled between 1.0 m/min and 2.5 m/min depending on pipe diameter. Operational boundaries are critical: preheating above 230°C can oxidise the Bynel 4104 surface and reduce adhesion, while preheating below 200°C leaves the FBE undercured and weakens the tie layer bonding. Terminal products include buried natural gas transmission pipelines, oil flowlines, and aqueous slurry transport pipe. Continuous service above 60°C requires additional qualification because long-term oxidative embrittlement of the LLDPE backbone accelerates at elevated soil temperatures.

    When Multi-Layer Rotational Moulding Requires Fuel Vapour Barrier Adhesion to Polyethylene

    Rotational moulding of multi-layer fuel tanks introduces Bynel 4104 as a ground adhesive powder between the outer high-density polyethylene skin and the inner polyamide or EVOH barrier layer. The adhesive powder is dry-blended at 5 wt% to 8 wt% of the total shot weight and applied as a separate drop-in layer after the outer skin has sintered. Oven temperatures are held at 280°C to 300°C, and the cycle time for the adhesive layer is 8 min to 12 min at peak internal air temperature of 180°C to 200°C. Grinding to 35 mesh is required to achieve uniform powder flow and consistent layer thickness; coarse particles above 500 µm produce localised adhesion voids that increase permeation. Compliance for fuel vapour permeation is assessed under EPA 40 CFR Part 1060, and oxygen transmission of the composite wall is measured by ASTM D3985-17 at 23°C and 0% RH. Published data for this specific multi-layer rotational moulding configuration is limited, but the adhesion mechanism is analogous to coextrusion bonding of the same resin. Terminal products include portable diesel fuel tanks, marine fuel cells, and small engine fuel canisters.

    Coextruded Cast Film for Modified Atmosphere Packaging of Fresh Poultry

    A seven-layer cast coextrusion line running modified atmosphere packaging film places Bynel 4104 as three separate tie layers between LLDPE sealant, polyamide, and EVOH barrier cores. Each tie layer is controlled between 6 µm and 10 µm, comprising 8 wt% to 12 wt% of the total 60 µm to 100 µm film. Melt temperature is maintained at 220°C to 250°C, and the chill roll is run at 18°C to 24°C to prevent post-extrusion crystallinity loss in the LLDPE sealant. EVOH layers must be encapsulated between the adhesive resin to protect the moisture-sensitive barrier from humidity; when the film is exposed to 85% RH at 23°C, oxygen transmission rises sharply if the EVOH layer is not properly shielded. Barrier performance is verified by ASTM D3985-17 for oxygen transmission rate and ASTM F1249-20 for water vapour transmission rate. Food-contact compliance is assessed under FDA 21 CFR 177.1395 and EU Regulation (EU) No 10/2011. Terminal products include lidding film for fresh poultry trays, flowpack wrappers for processed cheese, and MAP bags for fresh meat exposed to high-humidity retail display.

    Free Quote

    Competitive Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Among the tie-layer resins used for coextruded high-barrier films, Dow Bynel® 4104 is an anhydride-modified linear low-density polyethylene adhesive resin supplied in pellet form. The product is designed for discrete adhesive layers in structures where polyolefin skins, particularly LLDPE and LDPE, must be joined to polyamide, ethylene-vinyl alcohol copolymer, or metal foil. The base polymer is a linear low-density polyethylene with a nominal density of 0.92 g/cm³; maleic anhydride is grafted onto the backbone to create reactive carbonyl sites without introducing the vinyl acetate comonomer found in EVA-based tie resins. The low-density ethylene backbone permits co-crystallization with LLDPE and LDPE skins, while the anhydride functionality can react with terminal amines in polyamide, hydroxyl groups in EVOH, or metal oxides on foil. Melt rheology is controlled by a melt mass-flow rate in the range 1.0–1.5 g/10 min at 190 °C and 2.16 kg, as determined by ASTM D1238 or ISO 1133-1. This low-flow condition favors blown-film bubble stability and retention of melt integrity in thin tie layers. On three-layer blown-film lines equipped with tie-layer screw diameters from 25 mm to 45 mm, the resin is normally processed at melt temperatures of 210–250 °C; line operators report that die-lip deposit formation remains lower than with high-melt-flow maleated EVA grades when the adapter temperature is held below 240 °C. The primary use is as a discrete tie layer in packaging laminates, barrier shrink bags, and multilayer sheet, but the grade is also used in extrusion coating of aluminium foil where a low-moisture-transmission adhesive layer is required. Dow Bynel® 4104 is not a general-purpose LLDPE; it is intended for bonding layers rather than as a structural skin.

    Specification intervals and release methods

    Because lot-to-lot variation in graft level and molecular weight affects downstream adhesion, the resin is controlled by both melt-flow and density measurements. The table below lists representative property intervals used for incoming qualification when the product is released for tie-layer applications. Values should be confirmed against the current lot certificate; published data for adhesion performance in any specific structure remain dependent on substrate surface preparation, tie-layer thickness, and extrusion temperature.

    Property Unit Test method Representative release interval
    Melt mass-flow rate at 190 °C/2.16 kg g/10 min ASTM D1238 / ISO 1133-1 1.0–1.5
    Density at 23 °C g/cm³ ASTM D1505 / ISO 1183-1 0.918–0.924
    Vicat softening point °C ASTM D1525 / ISO 306 90–100
    Melting peak temperature, DSC second heat °C ASTM D3418 / ISO 11357-3 118–126

    The melt-flow range distinguishes Bynel® 4104 from its higher-flow counterpart Bynel® 4105, which is selected for cast film or extrusion coating where lower shear viscosity is required. The density and melting peak are consistent with ethylene-based copolymers in the 0.915–0.925 g/cm³ range. The absence of a high-pressure LDPE fraction means that melt strength is supplied by the LLDPE backbone rather than by long-chain branching; therefore, bubble stability in blown film depends on correct extruder temperature profiling and die-gap selection. In coextrusion, the higher melt strength of Bynel® 4104 allows tie-layer thickness reductions from 20 μm to 5 μm in some structures without immediate interfacial fracture, but adhesion per unit area is not linear with thickness. Published equipment trials on three-layer blown film lines with a 300 mm die report that reducing tie-layer thickness below 4 μm can generate interfacial void growth during bubble oscillation; this is an operational boundary for barrier film rather than a resin defect.

    How does anhydride grafting alter adhesion to nylon, EVOH, and aluminium?

    Maleic anhydride grafted onto an LLDPE backbone introduces highly electrophilic succinic anhydride rings. At processing temperatures of 200–250 °C, these rings can open and react with primary amines in polyamide 6 or polyamide 66 to form amide or imide linkages at the interface. With EVOH, the reaction forms ester bonds with pendant hydroxyl groups; with untreated aluminium foil, the adhesion mechanism is primarily an acid–base interaction with the oxide layer, but the anhydride ring may also react with hydrated alumina surfaces. In all three cases, interfacial adhesion increases with the surface concentration of reactive species, not simply with the total maleic anhydride content. Over-grafting can reduce LLDPE backbone crystallinity and lower cohesive strength, producing a weak boundary layer within the tie layer. The optimum graft level is therefore a compromise between interfacial bonding and cohesive integrity. In peel tests performed according to ASTM F88 on sealed pouches or ASTM D1876 on T-peel laminates, adhesion to EVOH is strongly structure-dependent; measured values are not transferable across layer thicknesses or seal-bar conditions. Published data for this specific configuration is limited, particularly for thin-gauge oriented films.

    When bonding to polyamide, melt temperature at the interface must exceed the polyamide melting point sufficiently to promote molecular interdiffusion. A tie-layer melt temperature of 230 °C at the die is typical for polyamide 6 structures; temperatures near 210 °C are used for EVOH to reduce thermal degradation of the barrier layer. Because anhydride functionality is hydrolytically active, humid storage of precompounded resin can reduce adhesion to EVOH and aluminium. The LLDPE backbone retains low water absorption, but surface hydration of the anhydride groups can alter reaction efficiency. Unlike EVA-based tie resins, no acetic acid is released during processing; therefore, no corrosion of downstream metal parts is associated with the polymer itself.

    During three-layer coextrusion on a single-screw line with a 45 mm tie-layer extruder and a 24:1 L/D metering screw, the feed section is maintained at 170–190 °C, the transition zone at 190–210 °C, the metering zone at 210–230 °C, and the adapter and die at 230–250 °C. Screw speed for the tie layer is often kept in the 15–40 rpm range to maintain short residence time and avoid excessive shear heating from the low-melt-flow resin. Back pressure under these conditions typically remains below 35 MPa; if screen-pack pressure rise exceeds 10 MPa over baseline, gel contamination from degraded anhydride crosslinking should be suspected. Field experience indicates that purging with a low-melt-flow LDPE after each production run reduces die-lip deposit accumulation when switching from polyamide to EVOH. The resin should not be mixed with polyamide or EVOH in the tie-layer hopper because pre-reaction can generate high-viscosity interface networks that cause pressure fluctuations. In cast film and sheet processes, the same melt-temperature limits apply, but line speed can be increased because melt strength is less critical; edge trim containing coextruded nylon and Bynel® 4104 should be segregated for recycling because mixed-stream reprocessing can degrade nylon at LLDPE processing temperatures.

    When LLDPE-based anhydride tie resins replace EVA or acid copolymers

    When a converter replaces an EVA-based tie resin with Bynel® 4104 in a polyolefin/EVOH/polyolefin structure, the main technical advantages are higher thermal stability and the elimination of vinyl acetate degradation products. EVA tie resins begin to release acetic acid above 200 °C, which limits extrusion melt temperature and can cause odor or adhesion to processing equipment. Bynel® 4104 does not contain vinyl acetate and can be processed at temperatures up to 250 °C without generating acidic volatiles. The trade-off is lower adhesion to difficult surfaces without surface treatment. EVA and ethylene-acrylic acid copolymers can wet polar substrates more readily; Bynel® 4104 may require corona treatment of aluminium foil or EVOH at 42–48 dyn/cm to reach equivalent bond strength. In lamination of LLDPE to polyester or polyamide, a coextruded tie-layer thickness of 10 μm is often used; if thickness is reduced to 5 μm, adhesion to untreated polyester is typically lower than with EVA-based tie resins at the same thickness.

    Compared with anhydride-modified HDPE grades, Bynel® 4104 offers lower flexural modulus and better compatibility with LLDPE skins; it is therefore preferred for flexible packaging and films requiring low-temperature sealability. Compared with acid copolymer or ionomer tie resins, Bynel® 4104 is less corrosive to steel equipment because it does not carry free acid groups. However, it is not a substitute for ionomer resins in high-clarity, high-puncture multilayer applications where ionic crosslinking contributes to toughness. The difference in thermal stability also appears in extrusion coating: EVA-based tie layers often require a lower die temperature to avoid chemical degradation, while Bynel® 4104 can tolerate a broader die-temperature window across the width of the die without measurable viscosity loss.

    Food-contact use of Bynel® 4104 may fall under 21 CFR 175.105 for adhesives and 21 CFR 177.1520 for olefin polymers, subject to end-use migration limits and temperature conditions. For European Union applications, the grade is typically evaluated against Commission Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food; the finished article must be tested for overall migration according to EN 1186 or specific migration of maleic anhydride according to EN 13130. The resin should not be blended with amine-based processing aids or polyamide regrind in the tie-layer extruder because primary amines can react prematurely with the anhydride groups and create high-molecular-weight gel networks. The anhydride functionality is also sensitive to alkaline disinfectants in wet packaging areas; prolonged exposure to pH above 9 may reduce bond strength to aluminium foil. The material has low water absorption; therefore, predrying is not normally required for sealed bags, but if the resin has been opened in an environment with relative humidity above 60%, drying at 70–80 °C for 4–6 h can correct surface hydration. These drying parameters should be validated for each facility because desiccant dryer efficiency and tray depth affect moisture removal. The product is not recommended as a standalone sealant layer; it should be coextruded between non-polar and polar layers to avoid seal-initiation artifacts caused by high anhydride surface concentration.