Dow Aspun 6835a Linear Low Density Polyethylene Lldpe

Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE)

    • Product Name: Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE)
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 927145
    Density 0.935 g/cm³
    Meltindex 35 g/10 min (190°C/2.16 kg)
    Meltingpoint 124 °C
    Crystallizationtemperature 103 °C
    Vicatsofteningpoint 93 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 21.4 MPa
    Elongationatbreak 600 %
    Flexuralmodulus 386 MPa
    Hardnessshored 55
    Thermalconductivity 0.35 W/m·K
    Specificheatcapacity 1.9 J/g·°C
    Dielectricconstant 2.3
    Dissipationfactor 0.0002
    Volumeresistivity 1e16 ohm·cm
    Waterabsorption <0.01 %

    As an accredited Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg multiwall paper bags, palletized and stretch-wrapped for safe handling and storage.
    Container Loading (20′ FCL) Dow ASPUN™ 6835A LLDPE is packed in 25 kg bags and loaded into 20′ FCL containers for efficient bulk transport.
    Shipping Dow ASPUN™ 6835A LLDPE is a non-hazardous polyethylene resin supplied as pellets. It ships in 25 kg bags, 500–1000 kg bulk bags, or bulk trucks/railcars. Standard freight, no placards required. Store dry, cool, ventilated, away from ignition; protect from moisture and UV.
    Storage Store Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE) in a clean, dry, well-ventilated area at ambient temperature. Keep away from direct sunlight, heat, ignition sources, and strong oxidizers. Maintain original packaging closed; place pallets off the floor to prevent moisture and contamination. Use first-in, first-out rotation. Avoid prolonged UV exposure and physical damage. Consult the SDS for detailed storage requirements.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored in original, unopened packaging under cool, dry conditions.
    Application of Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE)

    What Limits Spunbond Line Speed When ASPUN™ 6835A Is Run Through a Reicofil-Type Beam?

    In commercial spunbond operations using a single-screw extruder with an L/D ratio of 30:1 and a positive-displacement gear pump, the melt flow rate of 17 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022 and the density of 0.950 g/cm³ per ISO 1183-1:2019 define the throughput ceiling before filament breakage or web defects appear. The extruder barrel profile is normally set from 90–150°C in the feed zone to 205–230°C in the metering section, with die melt temperature maintained between 220°C and 245°C. Below 220°C, spin pump pressure can exceed 12 MPa on wide beams because the resin has not completed its crystalline melting transition; above 250°C, oxidative chain scission accelerates even with the incorporated stabiliser package, generating gel counts that interrupt filament formation and increase web breaks. Quench air temperature is held at 12–18°C with relative humidity below 80% to keep filament diameter coefficient of variation under 5%. The calender bonding rolls are set 5–15°C below the differential scanning calorimetry melt peak obtained under ISO 11357-3:2018; higher roll temperatures convert the web into a continuous film rather than discrete bond points. At line speeds from 200–350 m/min, a minimum calendered bond area of 12–18% is required to prevent fuzzing during downstream converting. Fabric tensile strength is measured under ISO 9073-3:2023, hydrostatic head under AATCC 127-2018, and basis weight uniformity under ISO 9073-1:1989. The terminal article is typically a 10–15 g/m² hygiene topsheet or medical hood cover where line speed is limited by edge flutter and tear-out at calender nips when filament denier falls below 1.0 dpf.

    Thermal Bonding Window in Bicomponent Sheath-Core Fibres

    When ASPUN™ 6835A is co-extruded as the sheath around a polypropylene core with melt flow rate of 25–35 g/10 min at 230°C/2.16 kg, the cross-sectional sheath ratio is normally held between 30% and 50% to balance bond strength and core dimensional stability. The two melt streams are combined in a spin pack equipped with 25–40 µm absolute-rated filter elements, and the viscosity ratio at the spinneret wall shear rate of 10³–10⁴ s⁻¹ must remain below 2.0; higher ratios produce eccentric sheath distribution or sheath rupture during the draw-down stage. Thermal bonding of the collected web is performed on an engraved calender at roll temperatures of 120–135°C, derived from the onset temperature of the sheath melting endotherm rather than the polypropylene core melt peak. Because the sheath density is 0.950 g/cm³, the bonded fabric shows higher abrasion resistance but lower drape than a conventional 0.930 g/cm³ polyethylene sheath, a trade-off quantified by bending length under ISO 9073-7:1998 and Martindale abrasion cycles under ASTM D4966-22. The finished product is typically a coverstock or acquisition layer with basis weight of 15–30 g/m², and bond-point peel strength is monitored by delamination testing under ISO 9073-4:2021. A process boundary appears at line speeds above 300 m/min where quench air turbulence can shear semi-molten sheaths before bonding, increasing visible core exposure and reducing fabric uniformity.

    Carded air-through bonded nonwovens produced from staple fibre based on this resin are processed with cut lengths of 38–51 mm and crimp frequencies of 8–14 crimps per 25 mm. The staple fibre is blended with a carrier fibre such as polyester at 10–30 wt% addition, and the carded web passes through an air-through oven set at 128–134°C for 2.5–4.0 s; bonding occurs as the LLDPE binder fibre surface melts while the polyester remains mechanically intact. Spin finish is applied at 0.3–0.6 wt% to control static charge and fibre-metal friction during carding. The central process conflict is the narrow window between adequate thermal bonding and web shrinkage: at oven temperatures above 135°C, cross-machine width shrink can exceed 3%, while below 126°C the bonded fabric fails to meet tensile strength for hygiene acquisition layers. Fibre linear density is verified under ISO 1973:2021 before carding, and fabric breaking force is reported per 50 mm width under ISO 9073-3:2023. The terminal product is a high-loft acquisition distribution layer; however, the 0.950 g/cm³ density limits softness compared with lower-density polyethylene grades. When softer tactility is required, blending with 0.930 g/cm³ LLDPE at 20–40 wt% is necessary, followed by a downward air-through oven temperature adjustment of 3–6°C to prevent over-bonding.

    When LLDPE Replaces Polypropylene in the Spunbond Layers of an SMS Isolation Fabric

    Medical isolation gowns constructed as spunbond-meltblown-spunbond laminates more commonly use polypropylene spunbond layers, but substitution with ASPUN™ 6835A-based spunbond changes the barrier and comfort profile. The spunbond layer is laid at 12–18 g/m², and the finished fabric is evaluated under EN 13795-1:2019 for protective clothing used in surgical and isolation environments. Liquid barrier classification is determined by hydrostatic head testing under AATCC 127-2018 and impact penetration testing under AAMI PB70:2012. Because LLDPE has a lower melting point than polypropylene, the spunbond layer can be calendered at 120–130°C, reducing the risk of thermally degrading the meltblown core during lamination. The limitation is that the polyethylene layer must not be autoclaved with steam above 100°C; ethylene oxide at 55°C and 80% RH or gamma irradiation below 50 kGy is preferred, with post-sterilisation tensile retention measured under ISO 9073-3:2023. Bacterial filtration efficiency is not a property of the spunbond layer alone and is tested on the composite under ASTM F2101-19. Dry lint particle generation from the outer layer is assessed under ISO 9073-10:2003 to confirm that film-free bond points do not fibrillate into clinically visible particulate. Published data for this specific resin configuration in full AAMI PB70 barrier testing is limited, so lot-specific validation is required when the meltblown core supplier changes.

    Verification ItemStandard / ClauseTypical Test Condition
    Melt flow rateISO 1133-1:2022190°C / 2.16 kg
    DensityISO 1183-1:201923°C
    DSC melting endothermISO 11357-3:201810°C/min under nitrogen
    Nonwoven tensileISO 9073-3:202350 mm strip, 200 mm/min
    Hydrostatic headAATCC 127-201860 mbar/min ramp
    Air permeabilityISO 9237:1995200 Pa, 20 cm²
    Food-contact olefin polymerFDA 21 CFR 177.1520Conditions of use A–H

    Pleat Retention Depends on Web Stiffness Rather Than Basis Weight Alone

    Support webs for pleated filter cartridges and flat-sheet membrane filters are produced from ASPUN™ 6835A at basis weights of 20–35 g/m² with cross-machine basis weight coefficient of variation held below 4% to prevent non-uniform pleat height. Air permeability is measured under ISO 9237:1995 at 200 Pa, and pore-size distribution is characterised by capillary flow porometry under ASTM F316-03. The 0.950 g/cm³ density provides a stiffer web than lower-density LLDPE, which is advantageous for pleat retention after scoring; pleat height retention is checked after 500 cycles of cyclic compression at 25°C and 50% RH. A key incompatibility appears when the support web is laminated with solvent-based polyurethane adhesives: residual aromatic solvents can swell the polyethylene and reduce tensile modulus by more than 10%, so water-based acrylic adhesives are preferred. The terminal product is a pleatable filter support that withstands backpressure pulses in dust collector elements; burst strength of the composite is tested under ISO 9073-19:2018 or the filter manufacturer’s internal burst method. When web uniformity deteriorates above 250 m/min line speed, pore-size standard deviation increases and the web is downgraded for low-efficiency pre-filter use.

    Twin-screw compounding of colour masterbatch for polyolefin nonwoven lines uses ASPUN™ 6835A as a carrier at 30–50 wt% of the total formulation, with pigments or carbon black dispersed at 40–60 wt% in a 40:1 L/D co-rotating twin-screw extruder at melt temperatures of 200–220°C. The narrow molecular weight distribution and 17 g/10 min melt flow rate enable wetting of pigment agglomerates without excessive viscosity rise, but high-surface-area carbon black loadings above 50 wt% can increase torque beyond 85% of motor load and require screw speed reduction from 600 rpm to 400 rpm. The finished masterbatch is pelletised into 3.0–4.0 mm cylindrical granules and let down at 2–6 wt% on spunbond lines. Fibre colour strength and filter pressure rise are monitored respectively by spectrophotometry under ISO 11664-4:2008 and by a 20 µm screen pack pressure test; pressure increase above 1.5 MPa after 60 min indicates insufficient pigment dispersion and should trigger reformulation. Because the carrier density is 0.950 g/cm³, the masterbatch has a slightly higher bulk density than LDPE-based carriers, which reduces feeding variability in gravimetric hoppers by 5–8%; however, the same density reduces compatibility with very soft 0.915 g/cm³ spunbond layers if let-down exceeds 8 wt%, producing localised stiff spots. No additional food-contact claim can be transferred from the resin to the finished coloured article without independent evaluation under the relevant article-specific regulation.

    Free Quote

    Competitive Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ASPUN™ 6835A is a linear low-density polyethylene resin supplied for continuous filament, staple fibre, and nonwoven web processes. The manufacturer’s published nominal melt mass-flow rate is 17 g/10 min at 190°C under a 2.16 kg load determined in accordance with ASTM D1238 or ISO 1133-1:2022, and the nominal density is 0.950 g/cm³ determined in accordance with ASTM D792 or ISO 1183-1:2019. The 0.950 g/cm³ density places the grade at the upper end of the linear low-density polyethylene density band and above conventional butene-LLDPE film resins that typically range from 0.918 g/cm³ to 0.922 g/cm³. That density elevation increases crystallinity, reduces softness relative to lower-density polyethylene, and raises the tensile yield stress of the consolidated fibre web.

    The product designation ASPUN™ 6835A is not a film-extrusion resin and should not be assessed against film-resin specifications such as dart impact or Elmendorf tear. The resin is formulated for high-shear, short-residence-time fibre spinning, where a fractional-melt-index film resin would generate excessive spin-pack pressure and poor filament count. Published data for the molecular weight distribution of ASPUN™ 6835A is limited, but the 17 g/10 min melt flow rate indicates a lower average molecular weight than typical cast-film LLDPE grades, which generally exhibit melt flow rates of 0.5 g/10 min to 2.0 g/10 min under the same test condition.

    ParameterDow ASPUN™ 6835A nominalConventional butene LLDPE film resinPolypropylene homopolymer spunbond resin
    Melt mass-flow rate17 g/10 min at 190°C/2.16 kg per ASTM D12380.5–2.0 g/10 min at 190°C/2.16 kg per ASTM D123825–40 g/10 min at 230°C/2.16 kg per ASTM D1238
    Density0.950 g/cm³ per ASTM D7920.918–0.922 g/cm³ per ASTM D7920.900–0.910 g/cm³ per ASTM D792
    Typical melt processing range210–240°CFilm extrusion: 190–230°C230–250°C
    Primary process fitSpunbond, staple fibre, bicomponent sheathCast film, blown film, laminationSpunbond, meltblown, monocomponent fibre

    Processors using Reicofil-style spunbond beams typically select extruder screw geometries with L/D ratios of 30:1 to 36:1 and barrier screw sections for high-flow polyolefins. The 17 g/10 min melt flow rate reduces spin-pack pressure relative to fractional-melt-index LLDPE film grades, allowing lower melt temperatures in the range of 210°C to 240°C. Higher melt temperatures above 250°C increase thermo-oxidative chain scission, broaden molecular weight distribution, and can increase odour and smoke in the bonding area. A nitrogen blanket is not required for neat polyethylene; pellet surface condensation from outdoor silo storage should be avoided because it can generate melt-pressure fluctuations at the spin pump.

    When a 17 g/10 min Melt Index Resin Is Run on High-Speed Spunbond Equipment

    Melt-pressure stability at the metering pump is a critical control parameter because the high flow rate responds rapidly to screw-speed changes. Control systems with active melt-pump pressure regulation are preferred. The resin’s lower elongational viscosity reduces orientation freezing and permits higher filament counts without excessive spin-pack pressure. In monocomponent spunbond, the resin is processed through spinnerets with capillary diameters typically below 0.8 mm, and the resulting filaments are attenuated in slot or multi-orifice aerodynamic jets. Melt-filtration screens in the range of 200–250 µm are common to remove gel particles and agglomerated additive residues; finer filtration may be used but increases residence time and pressure drop.

    The resin is suitable for monocomponent and sheath-core bicomponent structures. In bicomponent spinning with a polyester or polypropylene core, the ASPUN™ polyethylene sheath provides a lower-temperature bonding surface and a softer hand. The polyethylene sheath also reduces thermal degradation of temperature-sensitive core polymers during calender bonding. When the sheath content falls below 20 wt%, bond-point strength can decline because the bonding surface lacks sufficient polyethylene continuity to wet the calender embossing roll evenly. At sheath contents above 50 wt%, the fabric hand becomes increasingly dominated by polyethylene behaviour, including higher flexural modulus than polypropylene-rich nonwovens.

    What Separates ASPUN 6835A from Cast-Film and Blow-Moulding LLDPE Grades?

    Film-grade LLDPE resins are designed for bubble stability, melt strength, and high draw-down in blown film. Their lower melt flow rates and broader molecular weight distributions contribute to film toughness but create high head pressure and uneven filament coalescence in spunbond. ASPUN™ 6835A is processed at a higher melt flow rate, allowing the spin pump to maintain output without excessive melt temperature. The higher density also raises crystallisation rate, which reduces tackiness of filaments exiting the quench zone and allows more stable web formation at high line speed.

    The melt strength of ASPUN™ 6835A is lower than fractional-melt-index film resin. This limits its use in vertical-web processes where gravitational sag must be controlled by quench air. However, in spunbond the lower melt strength is acceptable because filament attenuation is completed in the jet, not by a melt-phase draw. Compared with high-density polyethylene blow-moulding grades at 0.958–0.965 g/cm³, ASPUN™ 6835A yields lower flexural modulus and lower fabric stiffness, which is relevant for hygiene and medical nonwovens where drape is specified by bending-length methods such as ISO 9073-7.

    Compared with polypropylene homopolymer grades used in spunbond, the polyethylene chemistry provides different thermal behaviour and radiation stability. Polypropylene at 230°C to 250°C has higher melt strength and lower density, but it embrittles after gamma irradiation at typical sterilisation doses of 25 kGy unless stabilised. Polyethylene generally retains a higher fraction of post-irradiation tensile strength, although published data for this specific fabric configuration is limited. These differences are quantified on final fabrics by tensile strength per ASTM D5035-11, tear resistance per ASTM D5733-99, and stiffness per ISO 9073-7.

    Thermal Crystallization and Fabric Property Boundaries

    The density of 0.950 g/cm³ increases crystallisation exotherm and can shorten optimal quench-air quenching length relative to lower-density LLDPE. Cooling-air temperature is typically maintained between 12°C and 20°C, depending on ambient humidity and filament denier. Thermal calender bonding for LLDPE-rich webs is normally set between 120°C and 135°C; above 140°C the web can fuse into film-like areas and lose loft. Bond-point geometry and roll pressure determine tear strength and drape, and these parameters must be re-established when switching from polypropylene because the polyethylene softening region is narrower.

    Because of the elevated density, fabrics made from ASPUN™ 6835A are stiffer than ULDPE or lower-density LLDPE nonwoven grades. Design of composites should account for a flexural modulus increase relative to 0.918 g/cm³ LLDPE. The resin has lower melt strength than fractional-melt-index LLDPE, so vertical web sag during high-speed take-up may require higher quench flow. The resin should not be dry-blended with unneutralised acid-containing pigments or certain amine-based antistatic additives because these can discolour the polymer or interfere with phenolic stabiliser systems. Fluoropolymer polymer processing additives are used at 200–500 ppm to delay die build-up in high-speed fibre extrusion; polyolefin waxes and erucamide slip additives alter surface friction and may affect thermal bond strength.

    Regulatory Standards and Testing Requirements for Converted Articles

    If the converted nonwoven is intended for food-contact packaging, the finished article must be evaluated under FDA 21 CFR 177.1520 for olefin polymers or EU Regulation (EU) No 10/2011 as applicable; compliance of the raw resin does not automatically extend to the converted article. Medical article evaluation may require ISO 10993-5 and ISO 10993-10. The manufacturer’s product stewardship certificate for ASPUN™ 6835A should be consulted for current food-contact, REACH, and RoHS status; published data for this specific configuration is limited in public literature.

    Top