Dow Aspun 6811a Linear Low Density Polyethylene Lldpe

Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE)

    • Product Name: Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE)
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 705345
    Density 0.941 g/cm³
    Meltindex 30 g/10 min (190°C/2.16 kg)
    Meltingpoint 125 °C
    Vicatsofteningpoint 94 °C
    Crystallizationtemperature 108 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 20.7 MPa
    Elongationatbreak 600%
    Flexuralmodulus 448 MPa
    Hardnessshored 50
    Comonomer 1-Octene
    Molecularweightdistribution Narrow

    As an accredited Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ASPUN™ 6811A LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for shipping.
    Container Loading (20′ FCL) Dow ASPUN™ 6811A LLDPE in 25 kg bags, palletized and securely loaded into a 20′ FCL container, maximizing capacity.
    Shipping Dow ASPUN™ 6811A LLDPE ships as solid pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. It is generally non-hazardous under DOT/IMDG/IATA. Store in a dry, cool, ventilated area away from heat, sunlight, moisture, and contamination. Follow the SDS and local transport rules. Handle carefully to prevent package damage.
    Storage Store Dow ASPUN™ 6811A LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed, palletized off the floor, and protected from moisture, dust, and contamination. Avoid prolonged high temperatures to prevent pellet fusion. Follow the SDS, local regulations, and good first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 2 years from manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE)

    When 100% LLDPE Replaces Polypropylene in High-Speed Hygiene Spunbond Lines

    In high-output spunbond conversion for disposable hygiene, ASPUN™ 6811A is gravimetrically fed to a single-beam or multi-beam spunbond line equipped with an extruder having 30:1 L/D and a barrier screw designed for linear low-density polyethylene. The resin has a nominal melt flow rate of 17 g/10 min at 190°C/2.16 kg per ASTM D1238 and a nominal density of 0.941 g/cm³ per ASTM D792; the melt-index-to-density relationship places the material in a viscosity window that supports spinnerette hole counts from 1,000 to 7,000 holes/m on commercial beams. Compliance for skin-contact hygiene output is established under ISO 10993-5 and ISO 10993-10, and batch release includes web mass uniformity per ISO 9073-1 and tensile strength per ISO 9073-3. The formulation addition ratio is either 100% virgin ASPUN™ 6811A or a dry blend of 97 wt% resin and 3 wt% TiO₂ masterbatch, with antistatic additive limited to 0.2–0.6 wt% when static charge disrupts web formation. Downstream processing follows a melt profile of 205°C to 230°C, continuous screen filtration at 40–60 µm, two-sided quench air at 12–18°C, pneumatic draw-jet pressure between 0.5 bar and 2.5 bar, and deposition at line speeds from 250 m/min to 700 m/min. Thermal calender bonding is run at patterned roll temperatures of 118–132°C and nip pressures of 60–90 N/mm, producing a bond area of 14–22%. Terminal products include topsheets, acquisition cores, and coverstock for infant diapers, adult incontinence garments, and feminine hygiene pads at basis weights of 8–25 g/m². The upper processing boundary is 240°C; above this melt temperature, low-molecular-weight fractions form and accumulate as gel deposits in the spin pack, while draw-line break frequency increases sharply.

    Coextruded PE/PP Sheath–Core Bicomponent Fiber and Calender Bonding

    Bicomponent spunbond lines running a PE sheath over a polypropylene core use ASPUN™ 6811A in the sheath stream to lower the thermal bonding activation temperature while retaining a higher-melt-temperature PP core for dimensional stability. Sheath content is held between 25 wt% and 40 wt% of total filament mass, with the core resin selected from PP grades having a melt flow rate of 20–35 g/10 min; the two polymer melts are coextruded through a sheath–core spin pack in which distribution plates maintain layer integrity into each spinnerette capillary. Compliance for medical-grade output uses biological evaluation per ISO 10993-5 and ISO 10993-10, and sterile barrier packaging is validated under ISO 11607-1:2019 and ISO 11607-2:2019 for seal strength and microbial barrier retention. The sheath extruder is operated at a barrel profile of 180–210°C and a melt temperature of 210–225°C, while the PP core melt is run at 230–245°C; the viscosity ratio between the two phases must be maintained within converter-established limits to prevent interfacial distortion and sheath rupture during high-speed drawing. Quench air at 10–16°C stabilizes the composite filament before the web passes to a calender set at 125–135°C, where the PE sheath fuses without melting the PP core. Terminal products include medical gowns, disposable drapes, hygiene backsheet layers, and laminated coverstock for bed linen and protective bedding. The primary operational boundary is the sheath melt temperature: below 205°C, unmelted gel accumulations appear in the spin pack; above 230°C, oxidative chain scission reduces subsequent peel strength measured according to ASTM D903.

    At the carding line, crimped ASPUN™ 6811A staple fiber cut to 38 mm or 51 mm is processed through a roller-top card containing worker and stripper wire designed for low-denier polyolefin. The resin is extruded through a rectangular spinnerette, quenched, finished with 0.5–1.2 wt% of a non-yellowing fiber lubricant, drawn over heated godets to a ratio of 1.5:1 to 2.8:1, crimped, and cut. Carded web formulations contain 70–100 wt% ASPUN™ 6811A staple fiber blended with 0–30 wt% polypropylene, polyester, or cellulosic carrier fiber; the LLDPE fiber has a peak melting temperature near 126°C by ISO 11357-3, enabling through-air bonding at 128–135°C while preserving loft. Compliance for carded webs includes mass and tensile evaluation per ISO 9073-1 and ISO 9073-3, fiber composition verification per ISO 1833-1, and skin-contact biological evaluation per ISO 10993-5 and ISO 10993-10 where hygienic claims are made. Terminal products include hygiene acquisition cores, medical absorbent pads, wet wipe substrates, and acoustic insulation mats. The main process limitation is card wire loading: at spin-finish levels above 1.8 wt% or carding-room relative humidity above 65%, the fiber surface becomes tacky and causes cylinder wrap and non-uniform web formation. Published data for web tensile isotropy at ASPUN™ 6811A fractions above 85 wt% in through-air bonded carded webs is limited to converter qualification reports.

    Pleated HVAC and industrial air filtration media employ an ASPUN™ 6811A spunbond scrim as carrier and protective layer, not as the primary meltblown filtration layer. The resin’s melt flow rate of 17 g/10 min is too low for nanofiber meltblown die operation requiring melt flow rates typically above 400 g/10 min, so the scrim is produced separately on a single-beam spunbond line at 15–50 g/m² and laminated to meltblown PP or electrospun media at a nip temperature no greater than 115°C to prevent machine-direction shrinkage. Compliance for finished filter elements follows ISO 16890-1:2016 and ISO 16890-2:2016 for coarse and fine PM efficiency classification, EN 1822-1:2019 for high-efficiency elements where applicable, and ASHRAE 52.2 for MERV reporting. Formulation addition ratios in the scrim remain 100% ASPUN™ 6811A or a dry blend with 0–2 wt% carbon black masterbatch; carbon black addition above 2.5 wt% increases scrim bending resistance and can alter pleat scoring behavior during rotary pleating. Terminal product categories include rectangular HVAC panel filters, pleated vacuum cleaner bags, respirator prefilter wraps, and industrial gas-turbine intake support scrims. The recognized boundary is continuous service temperature: at operating air temperatures above 80°C, free-shrinkage measured per ASTM D2732 becomes sufficient to distort pleat geometry and reduce filter element effectiveness. Published data for this specific ASPUN™ 6811A scrim configuration in high-efficiency filter packs is limited to qualified converter laminating trials.

    Application scenarioGoverning standard / codeTest method or clause focusCertification/regulatory context
    Spunbond hygiene nonwovensISO 10993-5, ISO 10993-10, ISO 9073-1, ISO 9073-3in vitro cytotoxicity; skin sensitization/irritation; mass uniformity; tensile strengthSkin contact medical/hygiene claims
    PE/PP bicomponent spunbondISO 11607-1:2019, ISO 11607-2:2019, ISO 10993-5, ISO 10993-10sterile barrier seal integrity; microbial barrier; biocompatibilityMedical gown/drape and sterile packaging
    Carded thermal-bond stapleISO 9073-1, ISO 9073-3, ISO 1833-1, ISO 10993-5web mass; tensile; fiber composition; cytotoxicityHygiene and medical absorbent claims
    Filtration scrim supportISO 16890-1:2016, ISO 16890-2:2016, EN 1822-1:2019, ASHRAE 52.2fractional PM efficiency; high-efficiency classification; MERVHVAC and industrial air filtration
    High-draft industrial spunbondISO 9073-3, ASTM D4595, ISO 13438tensile strength; wide-width tensile; oxidation resistanceGeotextile/construction wrap
    Automotive needlepunched underlayISO 3795, FMVSS 302, VDA 278:2011, VDA 277horizontal burn; VOC and FOG; total organic emissionsVehicle interior air quality and flammability

    What Limits Draw Resonance in High-Draft Spunbond Lines Running 100% LLDPE?

    In high-tenacity spunbond nonwovens for industrial packaging and geotextile reinforcement, ASPUN™ 6811A is processed on a dual-beam high-draw line where the dominant process conflict is draw resonance, a periodic filament diameter oscillation caused by the interaction between spinline extension, quench-air turbulence, and the polymer’s extensional viscosity. The formulation is normally 100% virgin pellets; controlled addition of 5–10 wt% broad-molecular-weight-distribution recycled LLDPE broadens the relaxation spectrum and partially suppresses resonance, but reduces machine-direction tensile strength as measured by ISO 9073-3. Compliance for industrial wrap and construction textile applications derives from ISO 9073-3, wide-width tensile per ASTM D4595, and oxidation resistance per ISO 13438 for long-term outdoor exposure. The process uses extruder barrel profiles of 190–225°C, melt temperature setpoint at 220–228°C, air-gap distance of 30–80 mm, quench air velocity of 0.4–1.0 m/s, and draw-jet pressure up to 3.0 bar; the onset of resonance on a 1.1 m beam appears as a machine-direction mass variation exceeding ±7%. The web is thermally bonded at 120–132°C on a smooth or patterned calender and slit into rolls. Terminal products include pallet wrap reinforcement scrim, construction housewrap, oil-absorbent laminate support, and industrial sack reinforcement. The operational boundary is narrow: melt temperature below 215°C elevates spinline stress and prematurely triggers resonance, while melt temperature above 230°C reduces melt strength enough to increase filament breaks. Published data for this specific high-draft configuration using ASPUN™ 6811A is limited to machine qualification trials; draw-ratio limits are not transferable across beam designs.

    Needle-Punched PE/PET Blends in Automotive Underlayments and Airborne Emission Metrics

    Needle-punched nonwoven underlays and wheel-arch liners use ASPUN™ 6811A staple fiber in blends with recycled polyester to balance acoustic absorption, compression set, and interior air quality. The formulation addition ratio is 50–80 wt% ASPUN™ 6811A fiber and 20–50 wt% recycled PET, with 2–4 wt% of a low-VOC spin finish. The fiber deck is carded, cross-lapped, and needle-punched on a double-pass loom at 250–600 punches/cm², then thermally stabilized at 130–145°C to set the LLDPE fiber without inducing melt flow. Compliance for automotive interior use follows ISO 3795 and FMVSS 302 for horizontal flammability, VDA 278:2011 for VOC and FOG emissions, and VDA 277 for total organic emissions. Terminal products include undercarpet acoustic pads, trunk liners, bulkhead insulators, and wheel-arch liners exposed to moderate thermal load. The limitation of the ASPUN™ 6811A phase is thermal in nature: stabilization above 150°C produces surface melting that increases compression set and reduces acoustic absorption; below 130°C, the LLDPE fiber retains insufficient heat-set geometry and the part may exhibit thickness recovery failure after compression. Published data for ASPUN™ 6811A in full VDA 278 round-robin testing is limited to converter qualification reports, and transfer of emission values across different spin-finish formulations is not advisable.

    Downstream scenarioASPUN™ 6811A addition ratioProcessing equipment and setpointsPrimary process boundary
    Spunbond hygiene nonwovens100% or 97 wt% resin + 3 wt% TiO₂single-beam spunbond; melt 205–230°C; calender 118–132°Cmelt > 240°C gel formation
    PE/PP bicomponent spunbond25–40 wt% sheathcoextrusion spin pack; sheath melt 210–225°C; core melt 230–245°Csheath < 205°C gel; sheath > 230°C chain scission
    Carded thermal-bond staple70–100 wt%roller-top card; through-air oven 128–135°Cspin finish > 1.8 wt% or RH > 65%
    Filtration scrim support100% or 0–2 wt% carbon blackspunbond; laminator nip ≤ 115°Cservice temp > 80°C
    High-draft industrial spunbond100% ± 5–10 wt% recycled LLDPEdual-beam high-draw; melt 220–228°Cdraw resonance > ±7% mass variation
    Automotive needlepunched underlay50–80 wt% ASPUN + 20–50 wt% rPETdouble-pass needlepunch 250–600 punches/cm²; stabilization 130–145°Cstabilization > 150°C surface melting
    Free Quote

    Competitive Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) is a solution-polymerized LLDPE resin supplied as free-flowing pellets for melt-extruded nonwoven, fiber, and specialty monofilament processes. Supplier technical data list a melt flow rate of 19 g/10 min at 190°C/2.16 kg per ASTM D1238, with the corresponding method designation ISO 1133-1, and a density of 0.930 g/cm³ per ASTM D792, with the corresponding method designation ISO 1183-1. Differential scanning calorimetry per ASTM D3418 on as-extruded fiber generally places the main melting endotherm between 124°C and 128°C, depending on cooling rate and comonomer distribution. The 19 g/10 min melt flow rate places the resin above most general-purpose blown-film LLDPE grades, which often fall between 0.5 and 5 g/10 min, and below many extrusion-coating resins, which can exceed 25 g/10 min. In melt-extruded nonwovens, the product is used in hygiene topsheets, acquisition and distribution layers, medical nonwovens, and lightweight industrial wipes. Fabric bending stiffness is commonly evaluated by WSP 90.5 handle-o-meter testing; basis-weight uniformity is measured per ISO 9073-1. Published data for this specific formulation is limited, and converters should validate final article performance against end-use specifications.

    PropertyMethodTypical Value
    Melt flow rateASTM D1238 / ISO 1133-119 g/10 min
    DensityASTM D792 / ISO 1183-10.930 g/cm³
    Melting endothermASTM D3418124°C to 128°C

    Because the product is a linear low-density polyethylene, its crystalline structure and mechanical response differ from both high-pressure LDPE and isotactic polypropylene. The linear backbone has no long-chain branching, so shear-thinning is less pronounced than in LDPE. Melt pressure at a given throughput therefore remains relatively flat across a wide shear-rate window, but the absence of long-chain branching also reduces melt tension at low strain rates. On production-scale spunbond lines using single-screw extruders with 30:1 to 36:1 L/D and compression ratios from 2.5:1 to 3.5:1, barrel temperatures are commonly profiled from 180°C near the feed throat to 230°C in the metering section, with die melt temperature maintained between 210°C and 240°C. These boundaries are not arbitrary; operation below 200°C can increase die pressure and spinline draw resonance, while operation above 250°C accelerates oxidative chain scission and raises extractables in the finished fabric.

    At the die lip, melt temperature and shear rate set the apparent viscosity. Capillary rheometry per ASTM D3835 is used to map viscosity across the spinline shear-rate window of 100 to 10,000 s-1. The melt flow rate alone does not define this full curve; however, the 19 g/10 min value indicates a lower viscosity at 190°C than that of a 5 g/10 min blown-film LLDPE of the same density.

    What Distinguishes ASPUN™ 6811A from Conventional LLDPE Resins?

    Relative to conventional Ziegler-Natta LLDPE of similar melt flow rate and density, ASPUN™ 6811A exhibits a narrower molecular weight distribution and a more uniform interchain comonomer incorporation. The narrow distribution is the primary source of the product’s down-gauge spinnability. In gel permeation chromatography, this class of solution-polymerized LLDPE often shows a polydispersity below 2.5, whereas conventional Ziegler-Natta LLDPE commonly ranges from 3.5 to 5.0; the supplier does not publish a specific Mw/Mn value for this grade, and polydispersity alone does not replace capillary rheometry data. In comparative spunbond trials at equivalent melt temperature and screw speed, converting lines sometimes record lower die-pressure fluctuations and lower gel-related spinneret blockage than with broad-MWD LLDPE. The exact pressure reduction depends on filter pack design, die type, and screw condition, and published data for this specific configuration is limited.

    Against high-pressure LDPE, the linear structure raises the melting point and tensile modulus but reduces melt extensibility in the absence of long-chain branching. LDPE-based spunbond recipes may draw more readily at low shear, but the resulting nonwoven generally has lower tensile strength than an LLDPE of equivalent density. Against isotactic polypropylene, ASPUN™ 6811A has a lower melting point and lower flexural modulus, yielding softer handle and lower thermal resistance. Continuous service at elevated temperatures should be supported by fabric aging per ASTM D6284 or equivalent; no universal upper service temperature is assigned to the resin alone.

    Within the broader LLDPE nonwoven product range, the 19 g/10 min melt flow rate is an intermediate-to-high flow index. Lower-flow LLDPE fiber grades may produce higher fiber tenacity at low line speeds but require higher melt temperatures and may be less suited to the highest-throughput spunbond lines. Higher-flow grades may reduce spinning pressure but can sacrifice fiber tensile strength and increase shot or fly formation.

    High-Speed Spunbond Lines Require a Defined Rheological and Thermal Window

    In high-speed spunbonding, filament attenuation is governed by quench air velocity, spinline length, and the polymer relaxation time. The melt flow rate of 19 g/10 min permits rapid flow through spinneret capillaries at die pressures in the range of 7 to 14 MPa, as measured at the melt pump outlet on commercial lines. Spinneret hole diameters are typically 0.3 to 0.6 mm with capillary L/D between 3:1 and 5:1. Drawing ratios in spunbonding commonly range from 200:1 to 500:1 for fine-denier products; the exact drawing ratio is set by take-up speed and spinneret throughput. The resin’s narrow molecular weight distribution shortens the terminal relaxation time and permits stable spinlines in this drawing window.

    Because the resin has a relatively high melt flow rate, it is often used for fine-denier spunbond nonwovens. Filament diameter is controlled by the ratio of polymer mass flow to spinline velocity. For a 0.4 mm spinneret hole and a drawing ratio of 300:1, the final filament diameter can be estimated from polymer density and mass throughput per hole; the predicted value falls within the 15 to 25 μm range used for soft hygiene fabrics. This calculation is based on conservation of mass and assumes uniform quench and minimal die swell; actual fiber diameters are measured by scanning electron microscopy on fabric samples.

    Quench air is typically supplied at 12 to 20°C with velocity adjusted to filament denier and spinneret width. Thermal bonding after web formation requires roll temperatures below the melting endotherm. Calender bonding roll surface temperatures for LLDPE spunbond are often set between 80°C and 110°C depending on line speed and roll pattern. Bond strength is evaluated on the fabric by ASTM D5035 or ISO 9073-3. If the roll temperature is set too close to the 124°C to 128°C melting range, fiber skin melting can cause roll wrap and web defects. If set too low, bond points remain weak and the web loses tensile strength. Fabric basis-weight uniformity is measured per ISO 9073-1; well-adjusted lines hold coefficient of variation below ±5%. This is an observed line-specific range and not a resin guarantee.

    Slot-die geometry and melt filtration configuration have a greater influence on pressure stability than resin bulk melt-flow rate alone. A typical 1.5 m spunbond line uses a breaker plate with 20/40/60 mesh Dutch-weave screen packs ahead of the screen changer; pressure drop across a clean pack is commonly 5 to 12 MPa depending on throughput and melt temperature. Because gel particles in LLDPE can block fine screens and create pressure hysteresis, processors often stage filtration from 150 μm to 80 μm to maintain uninterrupted operation. The reduced gel load of this solution-polymerized product relative to older Ziegler-Natta LLDPE can lower screen-changing frequency, but startup transients and stagnant melt regions can still generate oxidized material if purging is inadequate. Screen-change intervals should be established on the basis of die pressure rise per hour, not on an assumed resin cleanliness level.

    Filtration also affects melt residence time distribution. A fine screen pack increases the pressure drop but narrows the residence-time distribution by removing stagnant curves. In a 1.5 m line running at 200 kg/h, a 10 MPa pressure drop through the screen pack is a practical threshold; beyond this, processors often use a larger screen changer or coarser upstream screens to avoid pump cavitation. Published data for this specific configuration is limited.

    When Physical Property Demands Require Blend Rationalization

    Blends of ASPUN™ 6811A with LDPE or lower-MFR LLDPE are sometimes used to adjust fabric drape, elongation, and tear resistance. Adding up to 20 wt% LDPE reduces melt viscosity and increases melt extensibility, but reduces tensile strength as measured by ASTM D5035. Blends with mLLDPE of density 0.918 g/cm³ increase softness while decreasing modulus; the property balance depends on the density difference and the crystallization half-time. Blends with isotactic polypropylene are not thermodynamically miscible and require compatibilization; without a compatibilizer, such blends exhibit coarse phase separation and loss of fabric uniformity. Processors evaluating these blends should generate stress-strain data on actual nonwoven fabric rather than on pressed plaques because fiber diameter and bond pattern dominate fabric tensile response.

    Blend ratios below 10 wt% may not produce statistically significant changes in handle-o-meter values; ratios above 30 wt% can shift the melting range enough to alter thermal bonding. The effect on melting is measurable by ASTM D3418 and on fiber tensile strength by ISO 9073-3.

    Another formulation variable is the addition of slip or antistatic masterbatches. Because the base resin has controlled molecular architecture, additive migration to the fiber surface follows the solubility parameter and molecular weight of the additive. High-molecular-weight slip additives migrate more slowly and can require post-extrusion storage before coefficient-of-friction targets are reached. Surface resistivity is measured per ASTM D257; antistatic additive loading is dictated by final fabric basis weight and end-use requirement. Overloading low-molecular-weight slip agents can increase surface bloom and interfere with ultrasonic bonding, so additive masterbatch levels are typically limited to 1 to 3 wt% in the melt.

    Compliance Matrix for Hygiene and Food-Contact Applications

    The resin is often evaluated against olefin polymer food-contact and medical nonwoven requirements. The matrix below lists provisions that converters commonly verify. Inclusion of a standard does not automatically mean the resin or fabricated article complies; final article compliance requires migration testing under the intended food type and temperature condition.

    ProvisionScopeTypical Test or Status
    FDA 21 CFR 177.1520Olefin polymers for food contactSupplier compliance letter with end-use conditions
    EU 10/2011Plastic food-contact materials and articlesOverall migration per EN 1186; specific migration limits
    REACH EC 1907/2006Registration and SVHC screeningNo SVHCs above 0.1 wt% in article if supplied as compliant
    CONEG / TPCHHeavy metals in packagingSum of lead, cadmium, mercury, and hexavalent chromium below 100 ppm by weight

    Compliance declarations for food contact are not automatically transferable from resin to finished article. For polyethylene, FDA 21 CFR 177.1520 applies to olefin polymers and permits use subject to extractives limits and end-use restrictions. In the European Union, plastic food-contact articles must meet overall migration limits of 10 mg/dm² of surface area under EU 10/2011, with specific migration limits for additives and monomers. The resin supplier may provide a compliance letter, but the final laminate, print, adhesive, or coating can alter the overall migration result.

    For medical nonwovens, cytotoxicity and irritation testing is conducted under ISO 10993-5 and ISO 10993-10, but these tests apply to the final device rather than to the resin alone. The processor must control formulation, thermal history, and any surface finishes because these factors alter the extractable profile. No claim is made that ASPUN™ 6811A is intrinsically biocompatible.

    In a production-scale hygiene nonwoven line, the resin is delivered by vacuum conveying and fed through a hopper magnet and metering screw. Because the polymer is not hygroscopic, pre-drying is generally unnecessary unless cold pellets are moved into a warm, humid building and surface condensation forms. The extruder screw is configured with a shallow metering section to limit frictional heat, and the gear pump is set to maintain die pressure between 7 and 14 MPa. Screen packs are staged from 150 μm to 80 μm to protect spinneret holes from gel and agglomerates. Start-up purging with a lower-MFR LLDPE or purging compound is used after shutdown to displace aged melt from the system. The line throughput is matched to fabric basis weight; no universal throughput limit is assigned to the resin because the narrow molecular weight distribution allows higher flow per hole than broad-MWD grades, but quench air and web formation remain the limiting factors.

    Top