| HS Code | 428685 |
| Density | 0.918 g/cm³ |
| Melt Index | 8.0 g/10 min |
| Melting Point | 106 °C |
| Vicat Softening Point | 85 °C |
| Tensile Strength At Break | 10.3 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 240 MPa |
| Brittleness Temperature | < -70 °C |
| Shore D Hardness | 45 |
| Water Absorption | < 0.01% |
| Dielectric Constant | 2.3 |
| Dissipation Factor | 0.0002 |
| Volume Resistivity | > 10^16 ohm·cm |
| Thermal Conductivity | 0.33 W/m·K |
| Haze | 6% |
| Gloss | 60% |
As an accredited Dow 722 Linear Low Density Polyethylene (LDPE) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow 722 LLDPE supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for safe industrial handling. |
| Container Loading (20′ FCL) | Dow 722 Linear Low Density Polyethylene (LDPE), 25 kg bags, palletized and shrink-wrapped, loaded in 20′ FCL; approx. 18–20 MT net. |
| Shipping | Dow 722 Linear Low Density Polyethylene (LDPE) is shipped as non-hazardous solid resin pellets in sealed bags, boxes, or octabins on pallets. Transport in clean, dry trucks or containers. Protect from moisture, excessive heat, sunlight, and punctures. No special hazard placards are generally required; follow local transport regulations. |
| Storage | Store Dow 722 Linear Low Density Polyethylene (LDPE) in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers closed, palletized, and protected from moisture, dust, and contamination. Separate from strong oxidizers and incompatible materials. Follow local regulations and the supplier’s SDS. Avoid prolonged high temperatures to prevent melting, degradation, or block formation. |
| Shelf Life | Typically indefinite if stored cool, dry, and sealed in original packaging; no specific expiry under normal warehouse conditions. |
In high-cavitation thin-wall injection moulding lines for dairy and deli packaging, Dow 722 linear low density polyethylene is introduced as the base polymer for 0.4–0.8 mm wall sections. The resin is pre-dried for 1 h at 70 °C only when ambient relative humidity exceeds 60% to minimise surface splay, although the polyolefin backbone does not undergo hydrolytic degradation. A general-purpose screw with 20:1–24:1 L/D and compression ratio 2.5:1–3.0:1 is used on hydraulic accumulator machines with clamp force 250–350 t. Melt temperature measured at the nozzle is held within 190–230 °C while the hot runner manifold is balanced to ±5 °C because a wider deviation creates short shots at the 0.4 mm sidewall flow length. Mould supply water is set at 8–12 °C, giving cavity wall temperatures of 10–30 °C and allowing a cycle time of 4–7 s for 12–20 g shot weights. Injection velocity is set at 80–120 mm/s and hold pressure at 50–70 MPa. The formulation is let down with 2.0–3.0 wt% slip masterbatch carrying 5–10% erucamide active, and 0.05–0.10 wt% phenolic/phosphite antioxidant masterbatch. Compliance for food containers is established under FDA 21 CFR 177.1520, covering olefin polymers in food-contact use, and EU Regulation 10/2011. Under EU testing, overall migration into food simulants must remain below 10 mg/dm². Finished articles include snap-fit dairy tubs, deli containers, and disposable lids. Process failures observed on production lines include warpage of rectangular containers from asymmetric gate freezing, sink marks at rib intersections deeper than 0.15 mm, and gate blush when injection velocity exceeds 140 mm/s.
Table 1 summarises the injection moulding envelope for this grade.
| Variable | Control range | Measurement |
|---|---|---|
| Melt temperature | 190–230 °C | Nozzle immersion probe per ISO 1133-1:2022 |
| Mould circuit water | 8–12 °C | Supply-pressure gauge and flow meter |
| Cavity wall temperature | 10–30 °C | Surface thermocouple |
| Injection velocity | 80–120 mm/s | Linear velocity transducer |
| Hold pressure | 50–70 MPa | Hydraulic pressure transducer |
| Clamp force | 250–350 t | Toggle clamp specification |
| Shot weight | 12–20 g | Precision balance |
On single-station shuttle blow moulding machines, Dow 722 is processed through a 24:1 L/D single-screw extruder with a barrier screw and throat cooling. Melt temperature measured at the die head is held between 180–210 °C and the die gap is set to 0.8–1.2 mm. Blow ratio is kept within 2.0:1–3.0:1. Because the high-flow character of this grade reduces screw torque but also lowers melt strength, parison sag becomes the primary processing hazard. Die temperature is reduced in 5 °C increments to below 190 °C when wall thinning exceeds 20% across the bottle shoulder. The formulation contains 2 wt% white color masterbatch and 0.02 wt% antioxidant. No slip agent is added where label adhesion or hot-stamp decoration is required. Food-contact compliance follows EU Regulation 10/2011 and FDA 21 CFR 177.1520. Typical end products are cosmetic squeeze tubes, sample sachets, and pharmaceutical dropper bottles. The material is not recommended for hot-fill above 70 °C because dimensional distortion occurs at the neck finish. It is also excluded from carbonated beverage bottles. Process failure points include pinch-off weld line cracking if the die temperature falls below 175 °C, and environmental stress cracking when the bottle stores aggressive surfactant solutions above 40 °C.
For masterbatch producers, high-flow LLDPE serves as a carrier resin where pigment wetting and strand stability dominate. A 40:1 L/D co-rotating twin-screw extruder is set with barrel temperatures of 180–220 °C and screw speed of 400–700 rpm. Specific mechanical energy is held at 0.18–0.22 kWh/kg. The formulation is dry-blended in a low-speed ribbon blender for 15 min before dosing: 60 wt% titanium dioxide, 20 wt% low molecular weight polyethylene wax, and 20 wt% Dow 722 carrier. Melt temperature at the die plate must not exceed 240 °C to prevent carrier degradation and pigment colour shift. Strand pelletising through a 30 °C water bath and air knife yields 3 mm cylindrical pellets. REACH registration for imported masterbatch requires physico-chemical characterisation of the carrier resin and the final mixture. This carrier is not a direct food-contact grade when loaded with pigments, unless the finished article is evaluated under EU Regulation 10/2011. End product is white masterbatch for film and injection moulding. Failure modes include screw blockage from undispersed pigment when wetting time is insufficient, and strand breakage when melt strength drops below the minimum draw requirement at 220 °C.
High-cavitation cap moulding lines specify Dow 722 for tamper-evident caps when the seal is moulded directly into the crown. A 48–96-cavity hot runner mould with valve gates is installed on a 250 t toggle clamp machine. Cycle time is 8–12 s. Melt temperature is 200–230 °C and core temperature is maintained at 10–20 °C using turbulent water flow. The linerless seal geometry uses a continuous circumferential land of 0.2–0.4 mm height and 0.8–1.0 mm width. Formulation comprises 0.5–1.0 wt% erucamide-free lubricant masterbatch to avoid organoleptic transfer and 0.08 wt% phenolic antioxidant. Compliance for carbonated soft drink and mineral water closures follows EU Regulation 10/2011 with overall migration below 10 mg/dm² under OM2 simulant D, and FDA 21 CFR 177.1520. Finished articles include 30/25 mm mineral water closures and tamper-evident bands. Dimensional shrinkage after demoulding of 0.8–1.2% across the thread diameter must be compensated in the tool steel because closure back-off occurs when interference falls below 0.15 mm. Steam sterilisation above 121 °C is excluded because the resin softens below 95 °C Vicat. Process failure on line includes valve gate stringing when melt temperature exceeds 235 °C, and seal land deformation when pack pressure is not reduced before gate freeze.
Co-extrusion coating lines apply Dow 722 as a polyethylene coating layer onto 200–350 g/m² board stock. A 90 mm single-screw extruder with 30:1 L/D feeds a flat die at 280–310 °C. Line speed ranges from 200–400 m/min. The corona-treated board enters a chill roll at 15–25 °C. To reduce neck-in and improve anchorage, the resin is blended with 10–20 wt% of a branched LDPE grade. Coating weight is controlled between 12–20 g/m². Food-contact compliance for coated board is established under FDA 21 CFR 176.170 for contact with aqueous and fatty foods, and EU Regulation 10/2011 with overall migration below 10 mg/dm². End products include gable-top cartons and aseptic brick packs. Failure modes include pinholes at coating weights below 12 g/m², edge neck-in exceeding 40 mm at high line speed, and odour carry-over if melt temperature exceeds 320 °C due oxidative degradation. Adhesion must be checked on-line by tape pull and boiling-water peel because paperboard moisture at the interface can cause blistering when line speed drops below 180 m/min.
Compounding of unfilled and talc-filled polypropylene for automotive interior trims uses Dow 722 LLDPE as a discrete impact modifier rather than as the matrix. A 44:1 L/D co-rotating twin-screw compounder is set from 190 °C in the feed zone to 220 °C at the die. The LLDPE is added at 5–15 wt% via a side feeder after the polypropylene melt seal. At 10 wt%, notched Izod impact strength tested per ISO 179-1 improves at -20 °C without significant loss in flexural modulus. Above 20 wt%, the dispersed LLDPE domains become co-continuous, reducing heat deflection temperature and causing surface delamination observed at gate regions. The compound is pelletised into 3 mm granules. Compliance for automotive interior parts includes ISO 3795 for burning behaviour and REACH. End product applications are door panel substrates, glove box assemblies, and lower pillar trims. Failure mode in downstream injection moulding is screw slippage when LLDPE content exceeds 15 wt% because the compound viscosity drops below 0.1 s⁻¹ shear response.
Competitive Dow 722 Linear Low Density Polyethylene (LDPE) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The product identified as Dow 722 Linear Low Density Polyethylene (LDPE) in procurement specifications is technically a branched low density polyethylene, not a linear low density polyethylene. The nominal density is 0.918 g/cm³ under ASTM D792, and the nominal melt index is 8.0 g/10 min under ASTM D1238 at 190°C/2.16 kg. These values place the grade in the high-flow segment of extrusion coating LDPE, where melt drawdown, optical clarity, and low seal initiation are prioritised over puncture toughness. Typical applications include extrusion coating of paperboard, aluminium foil lamination, clear monolayer film, and sealant skins in coextruded films. The product is supplied in pellet form; datasheet values are typical rather than batch specifications, and the batch certificate of analysis takes precedence for conversion set-up.
At 8.0 g/10 min, the melt index is 5–40 times higher than that of conventional blown film LDPE grades with melt indices of 0.2–1.5 g/10 min measured under ISO 1133-1:2022 or ASTM D1238. The fluidity difference alters neck-in, backpressure, melt fracture, and draw resonance. In capillary rheometry, the apparent viscosity of this melt-index class at 190°C and 100 s⁻¹ is significantly lower than that of fractional-melt LDPE, allowing lower extruder drive current and reduced melt pressure on single-screw extruders with L/D ratios of 24:1 to 30:1. The trade-off is lower melt tension; the material cannot sustain the same bubble diameter or air gap as a fractional-melt film resin. At coating die shear rates of 100–1000 s⁻¹, branched LDPE typically shows a power-law index between 0.4 and 0.6, which reduces pressure sensitivity to throughput but increases die swell relative to linear resins. Die swell is controlled by increasing die land length to 10–15 times the die gap. For extrusion coating, the air gap is normally kept below 150 mm to limit neck-in and edge bead. For blown film, blow-up ratios above 2.5:1 often destabilise the bubble when the melt index exceeds 7 g/10 min. These boundaries are based on general LDPE rheology; published Dow 722-specific processing curves remain limited.
In extrusion coating, the material is commonly run on a single-screw extruder with a barrier screw, a screen pack of 60/80/100 mesh, and a coat-hanger die with a 0.6–0.8 mm gap. Melt temperature is usually maintained between 280°C and 320°C; above 330°C, thermal-oxidative degradation produces gel specks and increases fuming. Adhesion to paper and aluminium foil is promoted by melt oxidation and polar additives, and peel strengths are verified with ASTM D1876 or ASTM F88 after substrate lamination. Line speeds of 150–250 m/min are typical for LDPE extrusion coating of paperboard; higher speeds require reduced air gap and increased melt temperature to maintain web flatness. Neck-in is controlled by measuring the difference between die width and coated web width, generally maintained to 25–75 mm per side depending on air gap and melt temperature. The exact temperature profile must be set by measuring backpressure, melt pressure stability, and seal strength, rather than by using fixed zone setpoints.
Slip and antiblock concentrates are let down at 2–5% by mass when low coefficient of friction is required for high-speed form-fill-seal lines. Erucamide-based slip migrates to the film surface and reduces kinetic coefficient of friction; the effect is time- and temperature-dependent, and the coefficient is measured under ASTM D1894. Silica-based antiblock at 1000–5000 ppm is used to prevent blocking, but each 1000 ppm increase in antiblock raises haze and lowers gloss. Final loading should be optimised against optical and frictional specifications. Off-spec film and edge trim can be recycled into the same layer at 10–20% by mass without substantially shifting density or melt index, provided the reclaim is not contaminated with hygroscopic polymers or ink solvents.
At 0.918 g/cm³, Dow 722 has relatively low crystallinity after melt processing, which supports high clarity and low haze. Film haze is measured by ASTM D1003; gloss is measured with ASTM D2457 at 45°. Rapid quenching on chilled rolls or high-velocity air rings lowers spherulite size and improves optical properties; thick sections or slow cooling increase haze. Heat seal initiation is measured by ASTM F2029 and reported as seal strength per ASTM F88. LDPE sealant layers typically develop measurable seal strength around 95–105°C at a 0.5-second dwell and 2.5–3.0 bar jaw pressure; LLDPE sealants often require 5–10°C more for equivalent seal strength. These values are typical polyolefin ranges rather than guarantees for any specific Dow 722 lot. Barrier properties are controlled primarily by density; the 0.918 g/cm³ resin transmits water vapour more than an HDPE of 0.960 g/cm³ but less than many polar copolymers. Exact water vapour transmission should be measured on the final film under ASTM F1249 because thickness, orientation, and lamination all shift the result.
Dow 722 is not a drop-in replacement for LLDPE in puncture-dominated or frozen-food packaging. LLDPE made with 1-butene, 1-hexene, or 1-octene comonomer generally has higher dart impact, tensile toughness, and slow crack growth resistance at similar density because the linear backbone and short-chain branches allow greater tie-molecule formation. A high-melt-index branched LDPE can show dart impact values under ASTM D1709 that are two to three times lower than those of an LLDPE sealant of comparable thickness. Conversely, LDPE provides lower seal initiation, better melt drawdown, and often lower haze in thin sealant skins. The standard compromise is a coextruded film in which Dow 722 forms the sealant surface at 10–20% of total thickness, while an LLDPE core supplies puncture and dart impact resistance. On a three-layer blown film line, a thin Dow 722 outer layer may be run at 1–2% of total gauge when high clarity is required, but the LLDPE core dominates mechanical response. Comparative data for Dow 722 against specific LLDPE sealants should be generated on the target line; published data for this specific configuration is limited.
Differences from other polyethylenes become more pronounced when the final application requires stiffness or barrier. High-density polyethylene provides higher modulus and lower water vapour transmission but less environmental stress crack resistance and poorer clarity in thick sections. Fractional-melt LDPE provides higher melt strength and better bubble stability but requires higher melt temperature and reduces line throughput in extrusion coating. LLDPE improves puncture and tear strength under ASTM D1922 and ASTM D1709 but typically raises seal initiation. The selection of Dow 722 is therefore tied to applications where high line speed, low seal initiation, and optical clarity outweigh mechanical toughness; the grade is not intended for geomembranes, heavy-duty sacks, or frozen-food packages where slow crack growth is the controlling failure mode.
Food-contact status is structure- and condition-specific, not resin-specific. Unfilled LDPE grades can generally be evaluated under 21 CFR 177.1520 and EU 10/2011, but migration of additives, reactor residues, and printing inks must be assessed on the final package. Dow 722 does not require pre-drying for typical ambient storage below 60% relative humidity; however, condensation on pellets should be avoided because surface moisture can create surface defects in extrusion coating. Purging with a compatible LDPE or commercial purge compound is required after processing PVC, nylon, or adhesive tie resins; residual chlorine or amine species can discolour or destabilise the melt. The grade should not be stored in direct sunlight or in contact with aromatic hydrocarbon solvents, which swell polyolefin surfaces and can shift surface friction.
| Regulation or standard | Scope | Verification required |
|---|---|---|
| 21 CFR 177.1520 | Olefin polymers in food contact | End-use extraction or migration testing for food type and temperature |
| EU 10/2011 | Plastics in food contact | Overall migration and specific migration limit compliance |
| REACH | Registration and SVHC declarations | Confirm full registration and absence of restricted substances |
| RoHS 2011/65/EU | Heavy metals and flame retardants | Supplier declaration required even if unfilled LDPE is outside typical scope |