| HS Code | 610617 |
| Density | 0.920 g/cm3 |
| Melt Index | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 28 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12% |
| Gloss | 60% |
| Coefficient Of Friction | 0.2 |
| Blocking | 100 g |
As an accredited Dow 620I Linear Low Density Polyethylene (LDPE) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow 620I Linear Low Density Polyethylene (LDPE) is supplied in 25 kg moisture-resistant bags, palletized, or 1,000 kg bulk sacks. |
| Container Loading (20′ FCL) | Dow 620I Linear Low Density Polyethylene loaded in 20′ FCL: 25 kg bags, palletized, stretch-wrapped, secured for ocean transport. |
| Shipping | Dow 620I Linear Low Density Polyethylene (LDPE) is a non-hazardous thermoplastic resin. It ships in 25-kg bags, bulk bags, or bulk trucks/railcars, palletized and stretch-wrapped. Transport in cool, dry, covered conditions away from moisture, heat, sunlight, and ignition sources. No dangerous-goods placards or UN number required. |
| Storage | Store Dow 620I LDPE resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original containers or bags sealed and palletized off the floor to prevent moisture and contamination. Avoid strong oxidizers. Protect from ultraviolet light and physical damage. Maintain moderate temperatures and use first-in, first-out inventory. |
| Shelf Life | Shelf Life: Stable under normal storage; typically 24 months if kept cool, dry, sealed, and away from sunlight, heat, and contamination. |
On high-output blown-film lines running 1,200–1,500 kg/h through a 350 mm die, Dow 620I linear low density polyethylene is blended with high-pressure LDPE at 70–85 wt% Dow 620I and 15–30 wt% LDPE to improve bubble stability; the LDPE fraction supplies shear thinning that lowers screen-pack pressure drop and reduces motor load at constant screw speed. The monolayer formulation adds 0.5–1.5 wt% antiblock masterbatch and 0.1–0.3 wt% slip masterbatch based on total polymer mass, with dosing through a gravimetric feeder at the throat of a 30:1 L/D grooved-feed extruder. The die gap is maintained at 1.8–2.2 mm, melt temperature at 190–230°C, and blow-up ratio at 2.5:1–3.2:1; operation outside this window produces stalk resonance and transverse thickness variation exceeding ±8%. Compliance for food-contact liners is verified against FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with mechanical acceptance tested per ASTM D1709-19 Method A for dart impact, ASTM D882-18 for tensile properties, and ASTM D1922-15 for Elmendorf tear. Terminal finished articles from this conversion route include FIBC liners, heavy-duty shipping sacks, industrial bulk liners, and construction sheeting.
| Verification item | Referenced method | Typical production specification |
|---|---|---|
| Dart impact resistance | ASTM D1709-19 Method A | ≥ 700 g at 125 µm |
| Elmendorf tear strength, MD/TD | ASTM D1922-15 | ≥ 350 g MD / 500 g TD |
| Tensile strength at break | ASTM D882-18 | 25–35 MPa |
| Food-contact compliance | FDA 21 CFR 177.1520(c) | Resin certificate of conformity |
Puncture retention in cast pallet stretch film is limited first by chill-roll quenching rate, second by air-gap melt sag, and third by uneven migration of the cling additive to the film surface. On a 3-layer cast line with a feedblock and 900 mm slot die, Dow 620I is placed in the core layer at 55–70 wt% of total film mass, while the skin layers contain 15–25 wt% metallocene LLDPE and 2–8 wt% cling resin; polyisobutylene-based cling masterbatch is dosed at 0.5–2.0 wt% only in the tack layer to prevent blocking on the nontack side. Melt temperature is held at 220–260°C, die-to-chill-roll air gap at 20–40 mm, chill roll temperature at 15–30°C, and line speed at 300–600 m/min; when the air gap exceeds 40 mm, edge neck-in and transverse thickness variation increase, and the cling layer loses uniformity. Compliance for pallet handling films is tested under ASTM D5748-19 for stretch retention, ASTM D1894-14 for coefficient of friction, and ASTM D5458-95 for cling; food contact grades additionally require FDA 21 CFR 177.1520(c). Terminal converted products include pre-stretched hand film, machine film, top sheet film, and pallet hood film.
In thin-wall injection molding of lids, overcaps, and semi-flexible industrial containers, the central process difficulty is screw-slip-induced throughput loss when high-pressure LDPE is absent. A 25–35 mm diameter, 20:1–24:1 L/D barrier screw with a check ring is specified, and the cylinder zones are profiled from 180°C at the feed throat to 230°C at the nozzle. The formulation is run either at 100% Dow 620I or at 85–95 wt% Dow 620I with 5–15 wt% high-pressure LDPE to increase melt extensibility for thin-wall fill; masterbatch addition is limited to 1–4 wt% to avoid viscosity shifts. Melt temperature is 190–230°C, mold temperature 10–40°C, injection pressure 60–90 MPa, hold pressure 50–70 MPa, and wall thickness 0.8–2.5 mm; the mold is vented at the end of fill to reduce burn marks in fast-cycle tools. Compliance is verified by ASTM D1238-20 for melt flow rate, ISO 294-1:2017 for specimen preparation, and FDA 21 CFR 177.1520(c) for food-contact closures. Terminal products include pail lids, waste container lids, overcaps for drums, and thin-walled industrial packaging.
Rotational molding with linear low density polyethylene differs from high-pressure LDPE because the melt has lower zero-shear viscosity, which produces faster sintering but increases the risk of pinhole formation when the powder bed is nonuniform. Dow 620I is pulverized to 35 mesh minimum particle size with a bulk density of 0.32–0.40 g/cm³, and the mold is charged at a shot weight calculated for a nominal wall thickness of 4–8 mm. The oven temperature is set at 260–320°C, the peak internal air temperature is brought to 180–210°C, and the major-axis rotation ratio is 4:1; forced-air cooling is applied until the mold surface temperature drops to 70°C before demolding. The powder formulation is 100% Dow 620I or 90–95 wt% Dow 620I with 5–10 wt% LDPE, with 0.2–0.8 wt% UV stabilizer package and 0.05–0.2 wt% antioxidant dry-blended before charging; stabilizer loading above 0.8 wt% without coupling agent reduces impact strength. Compliance is anchored to ASTM D1998-21 for polyethylene tanks, ISO 3451-1:2019 for ash content, and FDA 21 CFR 177.1520(c) where potable water contact is specified. Terminal products include diesel storage tanks, agricultural sprayer tanks, water storage containers, and outdoor equipment enclosures.
| Rotational molding variable | Set point envelope | Observed process consequence outside envelope |
|---|---|---|
| Peak internal air temperature | 180–210°C | Below 180°C: incomplete sintering and pinholes; above 210°C: oxidative embrittlement |
| Oven temperature | 260–320°C | Above 320°C: surface discoloration and excessive cycle time |
| Major-axis rotation ratio | 4:1 | Deviation beyond ±0.5 increases wall thickness variation |
During extrusion coating and lamination onto paperboard and aluminium foil, neck-in and draw resonance control the maximum usable line speed, not bubble stability or melt strength alone. A blend of 70–80 wt% Dow 620I and 20–30 wt% high-pressure LDPE runs at melt temperatures of 280–320°C through a slit die with a die gap of 0.7–1.0 mm, an air gap of 100–200 mm, and a chill roll temperature of 10–20°C; increasing LDPE content above 30 wt% reduces neck-in but lowers low-temperature seal performance. Coating weight on liquid packaging board is maintained at 15–25 g/m², and in-line corona treatment at 42–48 mN/m is applied before winding to maintain adhesion in subsequent flexographic printing. Compliance is verified under EU Regulation 10/2011 overall migration limit of 10 mg/dm², FDA 21 CFR 177.1520(c), and ASTM D1709-19 for impact after lamination. Terminal products include liquid packaging sachets, aseptic brick laminates, coated release paper, and aluminium foil lamination for flexible packaging.
Agricultural silage film failures in field storage are driven by puncture from stalk ends, ultraviolet embrittlement, and seal failure at the bale edge. A blown-film structure with nominal thickness 150–250 µm is formulated with 85–95 wt% Dow 620I, 5–15 wt% metallocene LLDPE, 1.5–2.5 wt% carbon black or titanium dioxide sunshield masterbatch, and 0.3–0.8 wt% hindered amine light stabilizer; the LLDPE fraction supplies dart impact and tear resistance in the machine direction, while the mLLDPE addition improves hot-tack at seal initiation. The line uses a die gap of 2.0–2.5 mm, melt temperature 190–220°C, blow-up ratio 2.0:1–2.6:1, and internal bubble cooling to hold the frost line at 4–6 die diameters; raising HALS loading above 0.8 wt% without a compatibilizing agent can reduce interlayer adhesion and cause winding slip on the collapsing frame. Compliance is specified under EN 13206-1 for bale-wrap films and ASTM D2732-14 for unrestricted linear thermal shrinkage; terminal products include round bale wrap, silage clamp sheets, silo bags, and agricultural storage covers.
Competitive Dow 620I Linear Low Density Polyethylene (LDPE) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow 620I is a low density polyethylene extrusion coating resin produced by high-pressure ethylene polymerization. The product is supplied in pellet form for conversion on cast film and extrusion coating lines. Under ASTM D1238 at 190°C/2.16 kg, the resin typically yields a melt index of 7.7 g/10 min; solid-state density is measured at 0.918 g/cm³ per ASTM D792. These values place the grade in the intermediate-melt-index range for paperboard and flexible packaging coating. The relatively high melt index lowers pumping pressure and increases throughput on narrow-die coaters, while the density corresponds to a sealant with moderate crystallinity. The material is often referenced in packaging specifications under FDA 21 CFR 177.1520(c)(2.2) and EU Regulation (EU) No 10/2011 for olefin polymers in food contact. It is not a linear low density polyethylene; the “linear” qualifier should be treated as a procurement misnomer rather than a molecular architecture description. Typical production-scale equipment experience indicates that this grade has lower neck-in than butene-LLDPE at equivalent coating weight, but higher neck-in than specialised low-neck-in LDPE grades.
The distinction is consequential because LDPE and linear low density polyethylene differ in branching topology. Dow 620I is a high-pressure LDPE with long-chain branching introduced during free-radical polymerization; no alpha-olefin comonomer is used to control density. In contrast, LLDPE grades are copolymers of ethylene with 1-butene, 1-hexene, or 1-octene and possess short-chain branches along an essentially linear backbone. Under ASTM D1238 or ISO 1133-1:2022, both may share similar melt index values, but extensional rheology differs: long-chain branched LDPE exhibits strain hardening, which sustains a stable web at high draw-down. Converter records on monolayer extrusion coaters commonly show lower neck-in for Dow 620I relative to linear resins at equivalent melt index. The use of the phrase “linear low density polyethylene” in a purchasing specification should be corrected to LDPE to avoid supply-chain misclassification.
On production-scale extrusion coating lines, melt temperature is typically set between 288°C and 316°C, with the die zone maintained 5°C to 10°C above the adapter to avoid edge tearing. A single-screw extruder with a length-to-diameter ratio of 24:1 to 30:1 and barrier screw geometry is adequate; high-shear mixing is not required because the resin does not contain the high melt viscosity fractions of broad molecular weight LLDPE. Operators report that high die pressure, typically 80 bar to 120 bar, is required to maintain uniform flow across a coat-hanger die with a 0.5 mm lip gap. The web width reduction, or neck-in, observed at a 300 m/min line speed with a 20 g/m² coating weight on kraft paper is narrower than with butene-LLDPE but wider than with some autoclave LDPE grades designed for low neck-in. The data for this specific configuration is limited to line-specific records; start-up should always include a neck-in mapping run at two line speeds.Unlike linear polyethylenes, Dow 620I demonstrates strain-hardening in extensional flow. In extrusion coating, this property is quantified by comparing draw-down speed at which the molten curtain begins to resonate or “draw resonance” appears. A resin with stronger strain-hardening can be drawn to lower coating weights without web break. On a laboratory-scale take-off system with a 25 mm extruder and a 150 mm flat die, a draw-down speed of 180 m/min to 220 m/min is attainable before draw resonance at a melt temperature of 300°C, but line-specific data should be generated because die gap and air gap strongly influence the threshold. The melt relaxation spectrum is broader than that of a linear resin with the same ASTM D1238 value; this broad spectrum contributes to both die swell and coating thickness uniformity. The storage modulus at 0.1 rad/s and 190°C is used in quality-control rheology to detect lot-to-lot variation in long-chain branching, although published data for this specific configuration is limited.
Field data from monolayer coating lines identify two recurrent failure modes when switching from LLDPE to Dow 620I. The first is edge pinning loss at high air gap, where the molten curtain snaps away from the substrate edge and begins to oscillate. Corrective action includes reducing the air gap from 200 mm to 150 mm and increasing the edge pinning air pressure by 10%. The second is chill roll mottling caused by insufficient oxidation of the melt surface, which reduces adhesion to aluminium foil. Increasing the melt temperature to 315°C and raising the chill roll gloss band temperature to 15°C to 20°C often restores adhesion; adhesion must be checked by tape peel per ASTM D3359 or a peel test at 180° per ASTM F904. Decreased adhesion to low-density paperboard is observed when the substrate moisture content exceeds 8%, so reel moisture should be verified before start-up. These operating ranges are drawn from converter logs and should be confirmed on the actual line.Seal initiation temperature for Dow 620I is typically reported in the range 90°C to 105°C, depending on seal pressure, dwell time, and film gauge. In a standard heat seal test per ASTM F2029 or ASTM F88/F88M, the resin produces a seal strength that rises rapidly once the interface reaches 95°C. Hot-tack testing per ASTM F1921 is used to qualify the resin for vertical and horizontal form-fill-seal equipment, where failure occurs if the still-molten seal cannot hold product pressure. The long-chain branching in Dow 620I provides melt elasticity that resists peel-opening force during the cooling phase; on rotary pouch machines running at 80 cycles/min, the hot-tack window is generally wide enough for drop-in replacement of LDPE with a melt index of 7.7 g/10 min, but it is not equivalent to high-performance plastomer sealants used for cold-seal packaging. Converters should map the seal initiation curve for their specific dwell time, because published data for this specific configuration is limited.
Because the resin is used as food contact sealant, the compliance matrix includes FDA 21 CFR 177.1520(c)(2.2), which permits olefin polymers produced by high-pressure polymerization of ethylene for food contact use. The resin is also subject to EU Regulation (EU) No 10/2011 Annex I Table 1. Overall migration limits must be verified under EN 1186 based on the actual surface-to-volume ratio of the package. The product is not suitable for direct retort or autoclaving at 121°C for more than 30 min unless the package design includes an additional high-temperature barrier layer. Pellets should be stored in dry conditions and remaining bags should be sealed; predrying is not routinely required at relative humidity below 60%, but wet pellets from condensation must be dried at 70°C for 2 h to 4 h before extrusion to prevent surface defects.| Standard or Regulation | Scope | Method / Clause | Condition |
|---|---|---|---|
| FDA 21 CFR 177.1520(c)(2.2) | Olefin polymer food contact | Extraction limits in 21 CFR 177.1520(d) | Food-simulant extraction based on use temperature |
| EU Regulation (EU) No 10/2011 | Plastic materials and articles | Annex I Table 1 positive list | Overall migration 10 mg/dm² or 60 mg/kg |
| EN 1186 | Overall migration test | Aqueous, acidic, alcoholic, fatty simulants | Specific migration limits as applicable |
| ASTM D1238 | Melt mass-flow rate | 190°C/2.16 kg | 7.7 g/10 min |
| ASTM D792 | Density | Method A or B | 0.918 g/cm³ |
| ASTM F1921 | Hot-tack strength | Seal temperature range | 90–105°C |
Substitution of a butene-LLDPE sealant web with Dow 620I requires re-tensioning of the film and re-mapping of the heat-seal temperature because LDPE seal initiation is generally lower than LLDPE and the hot-tack plateau is shorter. In horizontal form-fill-seal systems running polyethylene-to-polyethylene seals at 30 m/min, the LLDPE film may tolerate a 10°C overshoot; Dow 620I may exhibit seal-through or edge thinning at temperatures above 120°C, depending on dwell time. Conversely, the LDPE grade provides better draw-down on the filling tube and reduces film drag due to lower coefficient of friction. The change should be qualified on the actual machine, using seal strength tests per ASTM F88/F88M and leak tests per ASTM F2096 on filled packages. LLDPE offers superior dart impact and tear resistance; Dow 620I should not be used as a direct replacement where the specification requires ASTM D1709 dart impact above 300 g for a 50 µm film, because typical LDPE values are lower. Published data for this specific configuration is limited.
Within the Dow LDPE coatings family, grades with melt index below 4.0 g/10 min are typically selected for low neck-in paperboard coating, while Dow 620I at 7.7 g/10 min is used where higher line speed and lower screw amperage are valued. Grades above 12 g/10 min are used for curtain coating or thin-wipe coatings where melt strength is less critical. The molecular architecture of Dow 620I provides an extrusion coating balance of draw-down and heat-seal integrity, but the resin is not formulated for rotational molding, blown film, or geomembrane applications where high environmental stress-crack resistance under ASTM D1693 is required. In any application where the final article must comply with REACH or RoHS Directive 2011/65/EU, the converter is responsible for verifying that downstream additives, inks, and adhesives do not alter the migration or hazardous substance profile. Published data for specific configurations of Dow 620I in high-temperature hot-fill packaging is limited. The Vicat softening point per ASTM D1525 is approximately 91°C, which restricts use in hot-fill packaging above 80°C unless the package is constructed with a higher-temperature outer layer. If the downstream application involves contact with fatty foods, specific migration of polymer additives must be re-evaluated under EU Regulation (EU) No 10/2011 Annex III using food simulant D2 or olive oil substitutes; the resin alone does not confer compliance for printed or laminated structures. The processing window should be confirmed on the converted line because differences in die gap, air gap, draw ratio, and chill roll temperature produce measurable shifts in adhesion, seal initiation, and coating weight uniformity.