Ciplas Llw2018f Linear Low Density Polyethylene

CIPLAS LLW2018F Linear Low Density Polyethylene

    • Product Name: CIPLAS LLW2018F Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 452714
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Density 0.918 g/cm3
    Melting Point 121 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 24 MPa
    Elongation At Break 700 %
    Dart Drop Impact 85 g
    Elmendorf Tear Strength Md 180 g
    Elmendorf Tear Strength Td 400 g
    Haze 12 %
    Gloss 45 55 %
    Coefficient Of Friction 0.2

    As an accredited CIPLAS LLW2018F Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLW2018F Linear Low Density Polyethylene is typically supplied in 25 kg bags, palletized at 1,000 kg.
    Container Loading (20′ FCL) CIPLAS LLW2018F Linear Low Density Polyethylene is securely loaded in 25kg bags into a 20′ FCL container for export.
    Shipping CIPLAS LLW2018F Linear Low Density Polyethylene is typically shipped as solid pellets in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport by truck, rail, or sea in dry, ventilated containers. Store away from moisture, direct sunlight, and heat; follow local regulations for non-hazardous polymer transport.
    Storage Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep containers sealed to prevent moisture/dust contamination. Avoid prolonged UV exposure. Maintain clean, dry floors; stack pallets securely to prevent bag damage. Store in original packaging or lined containers, protected from crushing and punctures. No smoking or open flames; use appropriate handling to control static. Observe local regulations.
    Shelf Life Shelf life: typically 24 months in original unopened packaging, stored cool, dry, and out of direct sunlight under recommended conditions.
    Application of CIPLAS LLW2018F Linear Low Density Polyethylene

    CIPLAS LLW2018F Linear Low Density Polyethylene is evaluated in six conversion-specific downstream application routes: blown-film extrusion for industrial liners and heavy-duty sacks, cast stretch-film extrusion for pallet unitization, extrusion coating for flexible packaging laminates, rotational moulding for storage tanks, flat-die geomembrane extrusion, and agricultural film extrusion. The processing temperatures, addition ratios, and testing thresholds are collated from converter records, equipment technical bulletins, and consensus test methods. Where a value would require product-specific certificate data not in the public domain, the text identifies that limitation rather than substituting an unverified figure. Melt-flow characterisation under ISO 1133-1:2022 and density measurement under ISO 1183-1:2019 typically place the material in the film-extrusion envelope, with melt-flow rate maintained within the 1.8–2.2 g/10 min range during production-lot acceptance testing.

    Conversion routeRegulatory or specification anchorTest methodsOperational boundary
    Blown-film industrial linersFDA 21 CFR 177.1520; Commission Regulation (EU) No 10/2011ASTM D882-18; ASTM D1709-22 Method A; ASTM D3354-21Melt temperature not to exceed 230 °C; residence time below 10 minutes
    Cast stretch filmFDA 21 CFR 177.1520 where food contact is claimed; ASTM D5458-21ASTM D882-18; ASTM D5748-19; ASTM D1922-23Line speeds above 500 m/min require melt-flow rate of 1.8–2.2 g/10 min
    Extrusion coatingFDA 21 CFR 177.1520; Commission Regulation (EU) No 10/2011ASTM F88/F88M-21; ASTM D903-20Not for retortable structures above 121 °C without secondary barrier
    Rotational mouldingFDA 21 CFR 177.1520; NSF/ANSI 61 for potable-water partsASTM D638-22; ASTM D1693-21Oven air temperature not to exceed 330 °C; wall thickness minimum 3 mm
    GeomembraneGRI-GM17 or equivalentASTM D5596-21; ASTM D6392-12; ASTM D6693-20Use LLDPE-specific modulus; do not default to HDPE anchorage values
    Agricultural filmEN 13206:2017ISO 4892-2:2013/A1:2021; ISO 527-3:2018Sulfur-based agrochemical exposure requires non-HALS stabilizer package

    What Governs Bubble Stability in Thin-Gauge Blown Film?

    In blown-film conversion of CIPLAS LLW2018F, the primary process conflict is the narrow window between die-lip shear and bubble instability. On three-layer coextrusion lines with annular die gaps of 1.8–2.3 mm, the bubble is run at a blow-up ratio of 2.2:1–2.8:1 and a frost-line height of 600–1000 mm. Melt temperature is held between 190 °C and 220 °C; at temperatures above 230 °C, the low-molecular-weight fraction of the linear-low-density resin contributes to die-lip deposit and gel formation during prolonged runs. Output rates on a 250 mm die are normally 0.80–1.25 kg/h per millimetre of die circumference, and gauge variation of ±5% is achieved with a dual-lip air ring combined with internal bubble cooling. The lack of long-chain branching in LLDPE reduces strain-hardening behaviour compared with LDPE; therefore bubble oscillation is controlled by adjusting frost-line height and internal bubble cooling exhaust rather than by increasing melt temperature alone. Residence time after start-up transition should not exceed 10 minutes.

    Formulation for industrial liners and heavy-duty sacks uses 70–85 wt% CIPLAS LLW2018F in the core and inner skin layers, 10–25 wt% LDPE or HDPE to increase bubble stiffness, 2–4 wt% carbon black or colour masterbatch for UV-stable grades, 0.5–1.5 wt% slip masterbatch, 1–3 wt% antiblock masterbatch, and 200–500 ppm fluoropolymer processing aid where melt fracture is observed. Food-contact monolayer structures must satisfy FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011 with overall migration below 10 mg/dm². Mechanical acceptance tests include ASTM D882-18 for tensile strength and elongation, ASTM D1922-23 for Elmendorf tear, ASTM D1709-22 Method A for dart impact, and ASTM D3354-21 for blocking. Terminal product types include industrial bin liners, compression-stacked heavy-duty shipping sacks, freezer films, and agricultural liners.

    Cast Stretch Film Draw Resonance and Pre-Stretch Ratios

    Cast stretch-film conversion on five-layer lines applies a slot die gap of 0.55–0.90 mm, a die-to-chill-roll air gap of 15–25 mm, air-knife pressure of 20–40 mbar, and chill-roll temperature of 12–20 °C. Lines run at 200–600 m/min; the onset of draw resonance is sensitive to melt-index lot variation and to the balance between air-knife vacuum and chill-roll speed. A melt-flow rate outside 1.8–2.2 g/10 min under ISO 1133-1:2022 shifts the draw resonance threshold downward at line speeds above 500 m/min. Pre-stretch ratios of 200–300% are achieved on power pre-stretch rollers at 70–90 °C, and cling is controlled in the air-side layer without migrating to the machine-roll core.

    Layer distribution uses 60–90 wt% CIPLAS LLW2018F in the core, 10–30 wt% metallocene LLDPE in the skin layers for puncture resistance, 0.5–3.0 wt% polyisobutylene tackifier masterbatch in the cling layer, and 0.3–1.0 wt% slip masterbatch in the release layer. Testing follows ASTM D882-18 for tensile properties, ASTM D5458-21 for cling, ASTM D5748-19 for puncture resistance, and ASTM D1922-23 for tear. Direct food-contact stretch film must comply with FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011. Terminal product types are hand stretch film, machine stretch film, pre-stretched film, and silage stretch film; film thickness ranges from 8 µm to 35 µm depending on pre-stretch ratio and load class.

    When LLW2018F Replaces LDPE in Extrusion Coating

    Replacing LDPE with CIPLAS LLW2018F in extrusion coating lowers seal-initiation temperature and improves hot-tack response but requires higher melt temperature at the die. Coating lines for flexible laminates operate at 280–320 °C melt temperature, die gap 0.60–1.20 mm, air gap 150–250 mm, and line speed 80–200 m/min. The melt curtain is stabilised with ozone treatment or corona at 42–50 dyn/cm to increase adhesion to paperboard, aluminium foil, or polyester film; chill-roll water temperature is held at 15–25 °C. The formulation is 85–100 wt% CIPLAS LLW2018F, 0–15 wt% LDPE to adjust neck-in, 3–5 wt% adhesion promoter masterbatch for aluminium foil substrates, 200–500 ppm process aid, and 0.2–0.8 wt% slip masterbatch. Food-contact compliance is evaluated under FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011; seal strength is tested by ASTM F88/F88M-21 and bond strength by ASTM D903-20. The route is unsuitable for retortable laminates requiring steam sterilisation above 121 °C unless the polyolefin layer is separated from the aggressive medium by a secondary barrier. Terminal components include liquid carton stock, frozen-food film-laminated paperboard, medical device pouches, and sachet laminates.

    Rotational moulding with CIPLAS LLW2018F is performed on biaxial shuttle or carousel machines with oven air temperature 280–320 °C, mould internal air temperature 200–220 °C, and rotation ratio 4:1 to 8:1. The pellet is ground to 35 mesh, and the fraction below 140 mesh is limited to 10 wt% to avoid trapped airborne fines that create surface pinholes. Wall thickness is normally 3–12 mm; heating time up to 20 minutes is followed by cooling with forced air and then water mist. The formulation is 94–98 wt% CIPLAS LLW2018F, 2–4 wt% UV stabilizer masterbatch, 1–3 wt% pigment masterbatch, and 0.1–0.5 wt% antioxidant concentrate where the part is intended for long outdoor exposure. Compliance for food-contact and potable-water tanks falls under FDA 21 CFR 177.1520 and NSF/ANSI 61; tensile values are measured by ASTM D638-22 and environmental stress cracking resistance by ASTM D1693-21. Terminal parts include agricultural storage tanks, water tanks, kayaks, and playground components. Temperature overshoot above 330 °C should be avoided because oxidative chain scission increases brittleness at the inner surface; wall-thickness transitions below 3 mm also produce incomplete filling of mould corners and reduce part stiffness at demoulding.

    Flat-die sheet extrusion for geomembrane applications uses a single- or twin-screw extruder with die width 2.4–7.0 m and a calender stack temperature of 80–95 °C to stabilise sheet gauge. CIPLAS LLW2018F is formulated at 96–98 wt% with carbon black masterbatch at 2–4 wt%; carbon black primary particle size is specified at 20–30 nm and dispersion is verified by ASTM D5596-21. Sheet thickness ranges from 1.0–2.5 mm, and panel welding is carried out with hot-wedge or hot-air welders at 200–230 °C. Seam peel and shear adhesion are tested by ASTM D6392-12, tensile properties by ASTM D6693-20, tear by ASTM D1004-21, and oxidative induction time by ASTM D3895-19. Published data for this specific grade under GRI-GM17 is limited; therefore converter qualification must correlate the LLDPE sheet modulus with the anchoring design rather than using default HDPE parameters. Terminal product types include landfill closure liners, pond liners, canal liners, root barriers, and temporary flood barriers.

    Agricultural greenhouse and silage films based on CIPLAS LLW2018F are converted on three-layer blown-film lines with die diameter 200–400 mm, die gap 1.6–2.4 mm, blow-up ratio 2.5:1–3.2:1, and melt temperature 190–220 °C. The polymer is used at 70–90 wt% in the core and air-side layers; metallocene LLDPE at 10–20 wt% improves dart impact and tear propagation; UV stabilizer masterbatch is added at 5–10 wt% for multi-season greenhouse service; anti-fog masterbatch is added at 1–2 wt% where condensation control is required. Compliance is assessed under EN 13206:2017 for thermoplastic films used in agriculture and horticulture, and accelerated weathering is carried out according to ISO 4892-2:2013/A1:2021 with retention of tensile elongation measured by ISO 527-3:2018. Terminal products include greenhouse cover films, low-tunnel films, silage bags, and mulch films. Films exposed to sulfur-based agrochemicals require a stabilizer package that is not solely hindered amine light stabilizer, because sulfur vapours deactivate HALS and reduce multi-season weathering resistance.

    Free Quote

    Competitive CIPLAS LLW2018F Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Data for CIPLAS LLW2018F Linear Low Density Polyethylene are evaluated here in relation to blown film conversion, sealant-web performance, and specification compliance. The grade is positioned as a film resin with a nominal density of 0.918 g/cm³ and a nominal melt flow rate of 2.0 g/10 min measured at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. These values correspond to a medium-molecular-weight linear low density polyethylene with a short-chain branching distribution typical of butene- or hexene-based Ziegler-Natta copolymers. Because the manufacturer issues lot-specific certificates of analysis, the nominal values in this document represent the commercial grade family rather than a substitute for certified release data. The resin is intended primarily for monolayer and coextruded blown film where a combination of tear resistance, sealability, and moderate optical clarity is required. The following table lists class-typical property ranges for this density and melt-flow-rate designation.

    PropertyTest methodNominal value
    DensityISO 1183-10.918 g/cm³
    Melt flow rateISO 1133-1:20222.0 g/10 min
    Melting temperature, DSC peakISO 11357-3121–124 °C
    Vicat softening temperature, A50ISO 30699–102 °C
    Tensile stress at yield, machine directionISO 527-310–12 MPa
    Tensile strain at break, machine directionISO 527-3550–650%
    Dart drop impact, F50, 25 µm filmISO 7765-1100–130 g
    Haze, 25 µm filmISO 1478210–16%
    Gloss, 45°ASTM D245740–60
    Coefficient of friction, film-to-filmISO 82950.10–0.30 with slip package

    High-stalk bubble stability, screw plasticating requirements, and die-gap selection

    Processing of CIPLAS LLW2018F on high-stalk blown film lines requires control of melt strength, frost-line height, and internal bubble air pressure. The linear backbone of the resin produces lower extensional viscosity than autoclave LDPE of equivalent melt index, which reduces neck-in resistance and can destabilize the bubble when the frost-line height is set above 6 die diameters. Extruder configurations of 24:1 to 30:1 L/D with barrier screws and Maddock mixing sections are suitable; screen packs of 60/100/60 mesh are commonly installed to increase back pressure and homogenize melt temperature. Barrel zone temperatures from 160 °C to 200 °C, adapter and die temperatures from 190 °C to 220 °C, and melt temperatures not exceeding 240 °C reduce the risk of gel formation and oxidative chain scission.

    Die-gap selection for this grade class should be in the range of 1.2–2.5 mm, with blow-up ratios between 2.0:1 and 3.5:1. Higher blow-up ratios improve transverse direction tear resistance but reduce bubble stability if the air ring has only a single lip. On lines with dual-lip air rings and internal bubble cooling, the frost-line height can be raised to 6–8 die diameters without losing bubble symmetry. Output rates are limited by draw resonance and melt fracture when the die shear rate exceeds approximately 150–200 s⁻¹ for unmodified LLDPE. If the resin is run as a 100% LLDPE layer on an older low-stalk line, output may be reduced by 10–20% compared with a 70/30 wt% LLDPE/LDPE blend. The addition of 10–30 wt% autoclave LDPE raises bubble stability and permits thinner gauge drawdown but lowers dart impact and hot-tack strength relative to the neat LLDPE.

    Moisture absorption is low for polyethylene, but re-exposure to high humidity can create surface defects on film. At relative humidity above 60% for more than 24 h, pre-drying in a desiccant or hot-air hopper at 60–80 °C for 2–4 h is applied before extrusion. Failure to control feed-section moisture leads to specks, gels, and intermittent bubble pinholes that are unrelated to resin chemistry.

    What separates LLW2018F from autoclave LDPE and metallocene-catalyzed LLDPE on blown film lines?

    The primary difference between CIPLAS LLW2018F and autoclave LDPE is molecular architecture. Autoclave LDPE contains long-chain branching that raises melt strength, reduces draw resonance, and improves optical clarity on conventional blown film lines, but it exhibits lower dart impact and lower tensile elongation than linear low density polyethylene at equivalent film gauge. On a 25 µm monolayer film, representative LLDPE dart drop impact values are typically 2–3 times higher than those of LDPE with the same melt flow rate, while machine-direction tensile strain at break is approximately 1.5–2 times higher. This difference is attributed to the linear short-chain branched structure and the higher molecular weight between long-chain branches in LLDPE. The trade-off is that LLW2018F requires more careful control of bubble geometry and may show higher haze unless the frost-line height and blow-up ratio are optimized.

    Compared with metallocene-catalyzed LLDPE, conventional Ziegler-Natta LLW2018F has a broader molecular weight distribution and a less uniform comonomer distribution. Metallocene grades typically produce higher dart drop impact, lower seal initiation temperature, and better hot-tack strength at equivalent density, but they generate higher extruder drive power and higher melt pressure due to narrower molecular weight distribution and higher shear viscosity. On a single-screw extruder of 45 mm diameter and 24:1 L/D, replacing conventional LLW2018F with metallocene LLDPE of the same density and melt flow rate can raise extruder amperage by 10–20% and reduce output unless the screw is designed with a more aggressive barrier profile. LLW2018F is selected when processability and lower extrusion torque are weighted more heavily than ultimate optical and seal-performance targets.

    Compared with high density polyethylene, LLW2018F has lower density, lower tensile modulus, lower melting temperature, and lower stiffness. Its use is driven by sealant-layer performance and impact toughness rather than load-bearing rigidity. In coextruded structures, LLW2018F is commonly placed in the sealant web or the bulk core layers, while HDPE or MDPE supplies stiffness and moisture-barrier performance. The difference in melting point is approximately 10–15 °C, which is sufficient to allow selective seal initiation in coextruded films without melting the HDPE layer.

    In cast film and lamination applications, the same grade class can serve as a sealant layer but requires different additive management. Cast film conversion of an 0.918 g/cm³ LLDPE with 2.0 g/10 min melt flow rate typically uses lower melt temperatures of 200–230 °C and smaller die gaps of 0.4–0.8 mm to reduce neck-in. The absence of a stabilizing bubble means that draw resonance is not the limiting factor; instead, the main failure mode is edge tear. For lamination webs, slip and antiblock packages are adjusted to maintain a coefficient of friction below 0.30 at 23 °C and 50% relative humidity. Published data for this specific CIPLAS configuration in cast film is limited, so the processing window should be confirmed with a line trial before commercial purchase.

    When seal-initiation temperature and hot-tack force limit form-fill-seal line speed

    Flexible packaging lines running vertical form-fill-seal or horizontal form-fill-seal equipment impose a sealing window that must match the resin’s melting and crystallization behavior. For LLW2018F used as a sealant web, the practical seal-initiation temperature is typically 90–105 °C at a sealing pressure of 0.5–1.0 N/mm² and a dwell time of 0.5 s. Hot-tack force, measured according to ASTM F1921, reaches a usable range of 1.5–3.0 N/25 mm between 110 °C and 130 °C. These values are lower than metallocene LLDPE sealants but higher than LDPE of equivalent melt index. The difference is operationally significant: on a packaging line running at 45–60 cycles/min, a sealant web with high hot-tack force prevents seal opening when the filled bag is released before the seal has solidified.

    Multilayer structures using LLW2018F in the sealant web are produced on coextrusion lines with layer ratio control. A typical structure may have a sealant layer thickness of 10–15 µm, a core layer of 20–40 µm, and a skin layer of 10–15 µm. The sealant layer is formulated with slip and antiblock additives to reduce blocking. Without an antiblock package, film-to-film blocking at 40 °C can prevent package opening on automatic bagging equipment. A silica antiblock concentration of 2000–5000 ppm and an erucamide slip concentration of 500–1000 ppm are common starting points, but the exact package depends on film gauge, winding tension, and storage temperature.

    For frozen food packaging, LLW2018F retains impact toughness at temperatures down to −30 °C, which is an advantage over LDPE sealants that embrittle more readily. For heavy-duty sacks and industrial liners, the resin can be blended with reclaimed LLDPE from post-industrial trim at 10–30 wt% without losing dart impact below the minimum required value of 80 g for 100 µm film. The specific value must be verified because regrind quality and contamination level influence the result.

    Regulatory cross-reference and storage boundaries for direct food contact applications

    Compliance statements for CIPLAS LLW2018F must be obtained from the manufacturer for the production lot in question, because polymer regulatory status depends on catalyst residues, comonomer type, and additive formulation. The applicable reference framework for the resin class is provided in the table below.

    Standard or regulationDesignationApplicability boundary
    EU food contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²; verify specific migration limits for short-chain comonomer-derived species
    US food contact21 CFR 177.1520(c)Applicable to olefin polymers for food-contact articles; conditions of use must match packaging line exposure
    REACHEC 1907/2006Substance registration is required for EU sale; confirm registration number with supplier
    RoHSDirective 2011/65/EUPolyethylene is not a characteristic RoHS substance; additive package must meet lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE limits
    Halogen contentIEC 61249-2-21Non-halogenated polyolefin base resin, but additive package must be confirmed if used in electronics packaging

    Storage should be in a dry, closed warehouse at temperatures below 50 °C and away from direct sunlight. Extended storage above 12 months from the manufacture date may shift slip-agent migration and affect coefficient of friction. The resin should not be exposed to oxidizing acids, strong chlorinating agents, or prolonged service above 60 °C without thermo-oxidative stabilization because the resulting chain scission reduces melt viscosity and film toughness. When regrind is fed back into the process, the maximum recommended regrind level is 30 wt% for critical sealant layers and up to 50 wt% for non-critical industrial film unless lot-specific testing demonstrates acceptable retained dart impact and seal strength.

    Top