Ciplas Llw2018b Linear Low Density Polyethylene

CIPLAS LLW2018B Linear Low Density Polyethylene

    • Product Name: CIPLAS LLW2018B Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 185290
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Density 23 C 0.918 g/cm³
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 11 MPa
    Tensile Strength At Break Md 30 MPa
    Elongation At Break Md 700 %
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 12 %
    Gloss 45 60
    Coefficient Of Friction 0.2

    As an accredited CIPLAS LLW2018B Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLW2018B Linear Low Density Polyethylene is packaged in 25 kg polyethylene-lined paper bags, supplied on pallets.
    Container Loading (20′ FCL) 20′ FCL container loaded with CIPLAS LLW2018B Linear Low Density Polyethylene in 25 kg bags, palletized and secured for export.
    Shipping CIPLAS LLW2018B is typically shipped as non-hazardous LLDPE pellets in moisture-resistant 25 kg bags or bulk octabins, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, avoiding direct sunlight, excessive heat, moisture, and ignition sources. Standard PPE is recommended; no special transport classification normally applies.
    Storage Store CIPLAS LLW2018B Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse. Keep bags/containers closed, palletized off the floor, away from sunlight, heat, flames, and oxidizers. Avoid moisture, contamination, and static buildup. Maintain good housekeeping to prevent dust and slip hazards. Use appropriate PPE; follow supplier SDS and local regulations. Ensure adequate ventilation and temperature control. Keep away from incompatible materials.
    Shelf Life Stable under normal storage conditions; indefinite shelf life when kept cool, dry, sealed, and protected from sunlight and ignition sources.
    Application of CIPLAS LLW2018B Linear Low Density Polyethylene

    At blown film extrusion conditions for linear low density polyethylene, CIPLAS LLW2018B is let down at a base resin concentration of 80–90 wt% with 10–20 wt% high-pressure LDPE, typically a 0.2–0.7 g/10 min melt index film grade, to alter bubble stability and tear-puncture interaction on air-cooled lines. The resin feed enters a grooved-feed extruder with an L/D ratio of 30:1 and a barrier screw; barrel zone settings from hopper to die are 180–200°C, 190–210°C, 200–220°C, and 210–230°C, with a screen pack of 60/80/60 mesh and a die gap of 1.8–2.5 mm. Blow-up ratio is held between 2.0:1 and 3.0:1, frost line height at 6–10 die diameters, and haul-off speed from 10 to 35 m/min depending on film gauge. On a 75 mm extruder with a 250–350 mm die diameter, typical through-put ranges from 220 to 340 kg/h; below 1.5 mm die gap, melt fracture is controlled with polymer processing aid masterbatch at 0.1–0.3 wt%. Compliance anchors for this segment are FDA 21 CFR 177.1520 for olefin polymers in direct food contact when used in monolayer or coextruded food liners, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for food films sold into the European Economic Area, and REACH EC 1907/2006 Annex XVII for restricted substances in packaging; agricultural film applications additionally reference EN 13206:2017 for thermoplastic films used in agriculture and horticulture. Terminal product types are heavy-duty industrial sacks, form-fill-seal agricultural fertilizer liners, construction films, carrier bags, and puncture-resistant liners for bulk container packaging. Production-scale failure modes include bubble instability when LDPE content drops below 10 wt% at blow-up ratios above 2.5:1 and visible surface moisture defects when bulk silo resin is processed at ambient relative humidity above 60% without hopper-carried air purging.

    What Processing Window Controls Film Tear Resistance in Cast Pallet Wrap?

    For cast pallet wrap, CIPLAS LLW2018B is processed on an extruder with L/D 30:1 and a flexible lip flat die, with melt temperature 230–260°C, die gap 0.5–1.2 mm, air gap 20–50 mm, and chill roll temperature 15–25°C. Formulation for this segment is 80–90 wt% CIPLAS LLW2018B, 10–15 wt% metallocene LLDPE for dart impact and machine-direction tear balance, 2–4 wt% polyisobutylene tackifier, and 0.5–1.0 wt% antiblock masterbatch if film-to-film slip is specified. Compliance for cast stretch film is driven by ASTM D5458-19 for cling force, ASTM D5748-19 for puncture resistance, ASTM D882-18 for tensile properties, and ASTM D1894-14 for coefficient of friction; food-contact use also falls under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. The downstream production process is low-neck-in cast extrusion with high-throughput screws and automatic die-lip adjustment to maintain thickness uniformity across web widths of 1,500–3,000 mm; line speeds range from 150 to 600 m/min. Terminal product types are machine roll pallet wrap, hand stretch wrap, pre-stretched film, and agricultural bale wrap. Operational limitations include tackifier migration to the chill roll at loadings above 4 wt%, which transfers roll contamination and produces uneven cling force across the web; periodic roll cleaning is required on long runs.

    Extrusion Coating Sealant Webs for Liquid Packaging Structures

    CIPLAS LLW2018B is applied as a sealant layer in extrusion coating and lamination when the web structure requires low seal initiation temperature and caulk resistance at high-speed package sealing. The coating formulation is 80–100 wt% CIPLAS LLW2018B, 0–20 wt% LDPE for neck-in reduction, and 0–5 wt% adhesion promoter masterbatch where aluminum foil or metallized film requires enhanced bond strength. Processing occurs on an extrusion coating line with an extruder L/D of 28:1, die temperature 300–320°C, die gap 0.5–1.0 mm, air gap 100–250 mm, and coat weight 8–40 g/m²; corona treatment of the substrate is maintained at 38–42 mN/m before nip. Compliance standards are FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011 with overall migration 10 mg/dm², and REACH EC 1907/2006 for substances of very high concern in packaging laminates. Terminal product types include liquid carton sealants, sachet laminates, aluminum foil pouches, and paper-polyethylene lamination for industrial wrappings. Neck-in is a known production bottleneck at low coating weights; LDPE addition below 5 wt% at 8 g/m² increases edge bead and requires wider clamps or deckle adjustments.

    For geomembrane sheet extrusion, CIPLAS LLW2018B is compounded at 96.5–97.5 wt% with a carbon black masterbatch at 2.0–3.0 wt% and an antioxidant/stabilizer package at 0.5–1.0 wt%, giving a final carbon black content of 2.0–2.5 wt% for UV stabilization. The flat die sheet line uses a grooved-feed extruder with a 30:1 L/D barrier screw, melt temperature 200–230°C, die gap 2.0–3.0 mm, three-stack calender temperatures 70–100°C, and sheet thickness 0.5–2.5 mm. Compliance for LLDPE geomembrane liners is anchored to GRI-GM17 for LLDPE geomembrane test methods, ASTM D5199-12 for nominal thickness, and ASTM D5397-19 for stress crack resistance evaluation. Terminal product types are landfill liner membranes, secondary containment liners, pond liners, canal liners, and mining heap leach pads. A processing limitation occurs when carbon black masterbatch above 2.5 wt% is dry-blended without sufficient dispersive mixing; the resulting microgel content increases surface defect counts and can reduce seam peel strength on installed liners.

    Rotational Molding Powder Particle-Size Limits and Drop Impact Performance

    CIPLAS LLW2018B is ground to a powder with a particle size distribution of 35 mesh (0.5 mm) pass rate above 90% for uniform wall thickness in biaxial rotational molding of chemical storage tanks. The dry blend is 99.0–99.6 wt% CIPLAS LLW2018B powder, 0.2–0.8 wt% UV stabilizer, 0.1–0.3 wt% processing aid, and 0.1–0.7 wt% pigment or antistat as required. The rotomolding process uses a biaxial machine with an oven set point of 260–300°C, internal mold air temperature of 180–220°C, mold rotational speed ratio of 4:1 primary to secondary axis, and forced-air cooling to ambient before demolding; wall thickness is 3–12 mm depending on tank size. Compliance for this segment includes ASTM D1998-15 for polyethylene vertical storage tanks, NSF/ANSI 61 for potable water contact components, and FDA 21 CFR 177.1520 for food or water contact where applicable. Terminal product types are vertical chemical storage tanks, horizontal transportation tanks, agricultural spray tanks, portable water tanks, and secondary containment basins. A known field limitation is reduced impact strength at sub-zero temperatures if demolding is carried out too quickly or if internal mold release is used above 0.2 wt%, because release agent migration interferes with post-molding weld quality.

    When LLDPE Is Used as the Carrier Phase in 40–50 wt% Carbon Black Masterbatch

    CIPLAS LLW2018B can function as a carrier resin in carbon black and color masterbatches for polyolefin conversion, where the formulation requires 40–50 wt% LLDPE carrier, 40–55 wt% carbon black, 2–6 wt% processing aid, and 0.2–1.0 wt% antioxidant. Selection of this grade is based on melt flow rate determined by ISO 1133-1:2022 at 190°C/2.16 kg and density compatibility with the letdown resin; for masterbatch used at 2–4 wt% in film or sheet, the carrier should have a melt index close to the final resin to avoid visible melt-flow disturbances. The compounding process is carried out on a co-rotating twin-screw extruder with L/D 44:1–52:1, screw speed 400–900 rpm, side-feeding of carbon black after resin melting, and melt temperature 180–220°C; the extrudate is strand-pelletized or underwater pelletized. Compliance is governed by REACH EC 1907/2006 for substance registration and FDA 21 CFR 177.1520 if the masterbatch is used in food-contact packaging at the final article level. Terminal product types are carbon black masterbatch for agricultural films, geomembranes and pipe coatings, color masterbatches for injection molding, and additive concentrates for extrusion coating. A production bottleneck occurs when pelletizing high-carbon-black masterbatch with water temperature above 40°C, which leads to pellet agglomeration and inconsistent dosing at the converter.

    Free Quote

    Competitive CIPLAS LLW2018B Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product designated CIPLAS LLW2018B Linear Low Density Polyethylene is a linear low-density polyethylene grade produced by low-pressure ethylene/α-olefin copolymerization. The grade designation is consistent with a nominal melt mass-flow rate of 2.0 g/10 min as measured by ISO 1133-1:2022 or ASTM D1238-20 at 190 °C under a 2.16 kg piston load, and a nominal density of 0.918 g/cm³ determined by ISO 1183-1:2019 or ASTM D792-20. The terminal B suffix is generally read as a butene comonomer marker or a formulated additive package, depending on the production site. Lot-specific certificates of analysis supersede all nominal values. The material is not a high-pressure LDPE; it has a predominantly linear backbone with short-chain branches introduced by α-olefin insertion. This molecular architecture reduces long-chain branching, lowers melt elasticity, and raises tensile and puncture resistance relative to LDPE at equivalent density.

    Because the grade is identified by density and melt flow rate rather than by a single application, the downstream converter must select the film process. LLW2018B is commonly directed toward blown film and cast film operations where dart impact, tear propagation resistance, and seal integrity are controlled by ASTM D1709-16a, ASTM D1922-15, and ASTM F88/F88M-21. The material may also be used in lamination films and heavy-duty sacks, provided the coefficient of friction is managed through slip and antiblock dosing. Published data for this specific configuration is limited; therefore, the following processing and performance statements are derived from standard LLDPE behavior and require verification against the manufacturer’s technical data sheet.

    What Processing Limits Emerge From Melt Rheology and Film Bubble Stability?

    On blown film lines, LLW2018B is typically processed at melt temperatures of 190–220 °C, with die gaps of 1.5–2.5 mm and blow-up ratios from 2.0:1 to 3.0:1. The linear backbone and low melt elasticity produce a less stable bubble than high-pressure LDPE at equivalent melt index; therefore, die gap is not normally reduced below 1.5 mm in low-stalk film production. Frost-line height is held between 6 and 10 die diameters. Internal bubble cooling is used when ambient relative humidity exceeds 60 % or when line output exceeds 100 kg/h on a 65 mm grooved-feed extruder. A single-screw extruder with a 24:1 to 30:1 L/D barrier screw provides sufficient plastication; melt temperatures above 240 °C accelerate oxidative degradation and should be avoided unless nitrogen blanketing is in place.

    Melt viscosity and shear-thinning behavior are governed by molecular weight distribution and comonomer placement. For LLDPE grades with a melt flow rate near 2.0 g/10 min, capillary rheometry at 190 °C typically records apparent shear viscosity of 800–1200 Pa·s at 100 s⁻¹ and 150–250 Pa·s at 1000 s⁻¹. These values are not lot-specific for LLW2018B but are provided as a processing reference. Bubble stability is also influenced by die land ratio and air ring design; a dual-lip air ring with a lower lip set 3–5 mm below the upper lip improves bubble stability at high output. The drawdown characteristic is less forgiving than LDPE at high blow-up ratios above 3.5:1; bubble flapping and stalk oscillation may appear if the frost-line height is not lowered and the melt temperature is not reduced.

    Tensile, Tear, and Dart Impact Response Under ASTM and ISO Protocols

    Film properties are strongly gauge-dependent. The values below are representative ranges for LLDPE blown film with a nominal density of 0.918 g/cm³ and melt flow rate of 2.0 g/10 min; they are not lot-specific specifications for CIPLAS LLW2018B. Specimens should be conditioned at 23 °C and 50 % relative humidity for 40 h according to ASTM D618-21 before testing.

    Property Test Method Typical Range, 25 µm Blown Film Unit
    Dart impact strength, F50 ASTM D1709-16a 90–120 g
    Elmendorf tear strength, MD ASTM D1922-15 150–250 g
    Elmendorf tear strength, TD ASTM D1922-15 350–500 g
    Tensile strength at break, MD ISO 527-3 30–45 MPa
    Tensile strength at break, TD ISO 527-3 25–35 MPa
    Elongation at break, MD/TD ISO 527-3 600–900 %
    Secant modulus, 1 % ASTM D882-18 150–250 MPa
    Haze ASTM D1003-13 5–15 %
    Gloss, 45° ASTM D2457-13 50–80 GU

    The tear balance between MD and TD is sensitive to blow-up ratio and frost-line height. A blow-up ratio near 2.5:1 produces a more balanced orientation; increasing the blow-up ratio toward 3.0:1 typically raises TD tear and lowers MD tear. Thin films below 20 µm show reduced dart impact and tear values because of lower thickness, while films above 50 µm may shift tensile strength toward the upper end of the range. Converters should measure properties on the actual production line rather than relying on laboratory film samples produced on small-scale cast or blown film units.

    In cast film extrusion, LLW2018B generally permits lower melt temperatures than blown film because the melt is quenched on a chill roll. Typical melt temperatures of 220–250 °C are used, with die gaps of 0.5–1.0 mm. The linear backbone reduces draw resonance relative to high-pressure LDPE at equivalent melt index, allowing higher line speeds; however, cast film from this grade may show lower haze than blown film because of the absence of a bubble cooling history. The coefficient of friction is controlled by migrating slip and antiblock agents, typically dosed at 500–1500 ppm each, depending on packaging line speed and film-to-film contact. In coextrusion structures, LLW2018B may be placed in the core or sealant layer, but tie-layer compatibility must be verified with the specific polyolefin plastomer or ionomer used in the structure.

    For heavy-duty sack applications, the converter should verify dart impact and Elmendorf tear after the film is aged at 23 °C and 50 % relative humidity for 48 h. In agricultural film, UV stabilizer dosing is typically 0.2–0.5 % of a hindered amine light stabilizer system, based on intended exposure period and geographic UV index. In lamination film, the seal initiation temperature should be benchmarked on the actual packaging machine because seal throughput depends on jaw dwell time, pressure, and contamination from slip additives. Published data for LLW2018B in these specific structures is limited.

    How LLW2018B Differs From Metallocene LLDPE, LDPE, and Conventional Butene Copolymers

    The following comparison positions LLW2018B within the standard polyolefin film landscape. Values are representative of commercial film grades and are not lot-specific. LLW2018B (nominal) is assumed to be a butene-comonomer Ziegler-Natta LLDPE with 0.918 g/cm³ density and 2.0 g/10 min melt flow rate; if the manufacturer supplies a hexene-based or metallocene version, the differences will shift accordingly.

    Attribute High-Pressure LDPE LLW2018B (nominal) Metallocene LLDPE
    Long-chain branching High Low Very low
    Melt strength at melt index 2.0 High Medium Low to medium
    Dart impact, 25 µm film 60–90 g 90–120 g 150–250 g
    Elmendorf tear, TD, 25 µm film 100–200 g 350–500 g 400–600 g
    Haze 2–5 % 5–15 % 2–8 %
    Seal initiation temperature 110–120 °C 100–110 °C 90–100 °C

    The primary operational distinction is bubble stability. High-pressure LDPE tolerates high blow-up ratios and thin die gaps because long-chain branching increases melt strain hardening, whereas LLW2018B requires the processing adjustments described above. Metallocene LLDPE usually outperforms LLW2018B in dart impact and clarity but may generate higher extruder torque and lower melt strength. Conventional butene LLDPE grades with similar density and melt index are often interchangeable with LLW2018B in general-purpose film, but additive package and short-chain branching distribution differences require line-specific validation.

    If the B suffix corresponds to butene, the grade is expected to show lower dart impact and tear than hexene- or octene-based LLDPE at equivalent density and melt index. Butene comonomers produce shorter branches that are less efficient at forming tie molecules between lamellae; this reduces solid-state toughness while often improving clarity and lowering raw-material cost. Hexene and octene copolymers typically shift the balance toward higher dart impact, lower seal initiation temperature, and improved puncture resistance. The selection of LLW2018B therefore depends on whether the converter prioritizes toughness or extrusion economics.

    For food-contact applications, LLW2018B may be evaluated under FDA 21 CFR 177.1520(c) for olefin polymers, provided the finished article meets end-test extraction limits and the grade is not blended with non-compliant additives. In the European Union, the grade may be covered by EU Regulation 10/2011 as a polyolefin with an overall migration limit of 10 mg/dm² of food contact surface, or 60 mg/kg for infant foods. Specific migration limits for the α-olefin comonomer and processing aids must be verified against the manufacturer’s declaration of compliance. REACH registration and RoHS 2011/65/EU require downstream converters to maintain material traceability and confirm that no restricted substances exceed 0.1 % by weight in homogeneous materials.

    For pharmaceutical packaging, customers should request documentation that the grade does not contain intentionally added substances listed in ICH Q3D as elemental impurities, and that extractables data are available when the packaging contacts aqueous or lipid solvents. Published data for this specific LLW2018B configuration is limited; therefore, the manufacturer’s food-contact statement is the controlling document.

    When LLW2018B Is Subjected to High Humidity and Regrind Conditions

    LLW2018B is supplied as a pelletized resin. Pre-drying is not generally required when the resin is stored in sealed packaging and ambient relative humidity remains below 60 %; however, if condensation is observed or if the packaging has been breached, drying at 60–70 °C for 4–6 h with a dehumidified-air dryer is recommended. The grade should not be processed with amine-based antistatic masterbatches that can promote discoloration, or with peroxides above the manufacturer’s recommended dosage when no reactive extrusion is specified. Storage should avoid direct sunlight and temperatures above 40 °C for extended periods to limit oxidative induction time reduction. If regrind is used, the addition rate should not exceed 20 % by mass without dart impact and tear testing on the final film.

    Continuous service temperature for load-bearing articles is generally limited to 60–70 °C; the Vicat softening point is typically below 100 °C when measured by ASTM D1525-17e1, and autoclaving above 110 °C is not recommended because distortion may occur. In applications requiring high-temperature sterilization, an alternative polyolefin with higher crystallinity or a polypropylene-based grade should be specified.

    Top