| HS Code | 166281 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 100 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 12% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.20 |
| Antiblock | 2000 ppm |
| Slip | 1000 ppm |
As an accredited CIPLAS LLW1020B6 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CIPLAS LLW1020B6 Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with CIPLAS LLW1020B6 Linear Low Density Polyethylene in 25 kg bags, palletized and stowed for transport. |
| Shipping | CIPLAS LLW1020B6 Linear Low Density Polyethylene is shipped as non-hazardous resin pellets in sealed 25 kg bags, octabins, or bulk containers. Transport as non-dangerous goods. Store in a cool, dry, ventilated area away from direct sunlight, heat, moisture, and ignition sources. Avoid package damage or contamination. |
| Storage | Store CIPLAS LLW1020B6 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep bags or containers closed, clean, and palletized off the floor to prevent moisture and contamination. Protect from physical damage and excessive dust generation. Use appropriate grounding where required. Follow the manufacturer’s SDS and all local storage regulations. |
| Shelf Life | CIPLAS LLW1020B6 Linear Low Density Polyethylene: typically 24-month shelf life when kept cool, dry, sealed, and out of direct sunlight. |
Production-scale blown film towers running CIPLAS LLW1020B6 linear low density polyethylene as the primary resin in food-contact flexible packaging operate within a defined bubble stability window because the butene-comonomer structure produces lower melt tension than conventional LDPE. The extruder screw is configured with an L/D ratio of 25:1–30:1 and a compression ratio of 2.5:1–3.5:1; barrel temperatures are profiled from 160 °C at the feed throat to 220–240 °C at the die head, and the melt temperature measured at the screen changer or die adapter is held between 190 °C and 230 °C. The annular die gap is set between 1.8 mm and 2.5 mm, and the blow-up ratio is maintained at 2.0:1–3.0:1 to balance machine-direction and transverse-direction tensile properties; a dual-lip air ring with internal bubble cooling holds the frost line height at 150–300 mm for gauges between 25 µm and 150 µm. On older lines without internal bubble cooling, the frost line is raised toward 300 mm to reduce bubble instability, but output rates may fall by 20–30% compared with IBC-equipped towers. Gel formation is controlled by limiting melt residence time below 15 minutes and purging the die at 220 °C during shutdown; iron content from screw wear is kept below 50 ppm because transition-metal residues accelerate thermo-oxidative degradation in the extruder.
Formulation addition ratios for food-contact blown film made from LLW1020B6 are set by the required slip, blocking, and heat-seal response. A typical starting formulation is 70–85 wt% LLW1020B6 let down with 15–30 wt% LDPE having a melt index of 0.25–2.0 g/10 min as measured by ASTM D1238 at 190 °C/2.16 kg; erucamide slip masterbatch is added at 0.3–0.8 wt% to achieve a coefficient of friction of 0.25–0.45 after 24 h migration to the film surface under ASTM D1894; synthetic silica antiblock masterbatch is added at 0.5–1.5 wt%; and a fluoropolymer processing aid is added at 0.02–0.05 wt% to suppress die-lip deposit during extended runs. For frozen food packaging, antioxidant loadings may be increased by 0.02–0.10 wt% to withstand heat-seal temperatures of 120–150 °C on cyclic jaw sealers. All additives must be present in the positive list of EU Regulation (EU) No 10/2011 and comply with the overall migration limit of 10 mg/dm² in EN 1186-1 testing. In the United States, the base resin and additive masterbatch carrier must satisfy FDA 21 CFR 177.1520(c), and the finished structure must meet FDA 21 CFR 176.170(c) if it is intended for fatty foods with a thickness below 100 µm.
| Compliance requirement | Standard/regulation | Test method | Typical boundary |
|---|---|---|---|
| Overall migration in food simulant | EU 10/2011, Art 12 | EN 1186-1 | 10 mg/dm² |
| Olefin polymer base resin | FDA 21 CFR 177.1520(c) | Extraction and density | Base resin specification |
| Melt index | ISO 1133-1:2022 / ASTM D1238-20 | 190 °C/2.16 kg | 0.8–1.2 g/10 min |
| Dart impact, 50 µm film | ASTM D1709-16a Method A | Falling dart | 90–150 g |
Downstream conversion includes surface corona treatment at 38–42 mN/m for flexographic or rotogravure printing, followed by vertical form-fill-seal pouch forming or bag making. Terminal product types include frozen vegetable films, bakery films, fresh produce bags, carrier bags, and industrial liners; the same LLW1020B6-based film is often coextruded in three layers where the skin layers carry slip and antiblock additives and the core layer carries 20–30% recycled or off-spec LLW1020B6 trim, subject to migration compliance verification. Tensile properties are tested according to ISO 527-3, tear resistance according to ASTM D1922, dart drop impact according to ASTM D1709 Method A, and haze according to ASTM D1003; the haze of a 50 µm monolayer film after addition of antiblock typically shifts from 8–12% to 12–20%, which defines the transparency ceiling for retail display packaging.
Cast pallet stretch film lines running LLW1020B6 in the core or back layer face draw resonance and cling uniformity limits governed by melt temperature, die-to-chill-roll air gap, and chill roll temperature. Slot die gap is 0.5–1.0 mm; melt temperature at the feedblock is held at 245–275 °C to reduce viscosity; the air gap is closed to 20–50 mm for thin films and extended to 50–100 mm when higher adhesion to the chill roll is required. The primary chill roll is polished and maintained at 15–25 °C; the secondary chill roll is set at 10–20 °C for gauge uniformity. Line speeds for 15–23 µm films are operated between 300 m/min and 600 m/min; above 450 m/min, edge-necking and draw resonance increase unless LLW1020B6 is let down with 10–20 wt% LDPE or a metallocene LLDPE with higher melt strength. A vacuum box positioned at the die-to-chill-roll gap applies 2–5 kPa suction to pin the web and reduce air entrapment; without it, transverse gauge variation can exceed ±8%.
For a three-layer A/B/C cast stretch film, LLW1020B6 is commonly placed in the core layer at 60–80 wt% of the total structure; the back layer uses 10–20 wt% metallocene LLDPE to increase elongation at break above 400% in ISO 527-3; the cling layer uses 5–10 wt% of an ethylene-vinyl acetate or ultra-low density polyethylene carrier compounded with polyisobutylene tackifier at 0.5–2.0 wt% of the total cling layer. Slip and antiblock additives are confined to the back layer at 0.3–0.8 wt% to maintain unwind performance without reducing front-layer cling. The tackifier must satisfy EU Regulation (EU) No 10/2011 if the pallet wrap is used in food-contact environments; outside such environments, the overall migration limit of 10 mg/dm² does not automatically apply, but downstream logistics specifications may still require REACH registration of tackifier components. ASTM D5458-95 is used for peel cling, with typical values of 50–150 g/cm depending on tackifier loading; ASTM D5748-19 provides puncture resistance under probe puncture, and ASTM D882-18 gives tensile strength at break. Predraw ratios on powered prestretch units are from 150% to 300%; above 250% LLW1020B6-dominant films show increased puncture propagation in pallet corners at gauges below 17 µm.
Terminal product types are machine-grade pallet wrap, hand-grade stretch film, agricultural bale wrap, and furniture transport film. Machine wrap produced with LLW1020B6 in the core layer shows cling-layer transfer of 0.1–0.5 wt% tackifier onto the pallet after 30 days at 40 °C, which must be validated for downstream label adhesion. For refrigerated storage at −18 °C, impact resistance is measured by ASTM D3420 Method B because the film must resist pallet corner release under cyclic compression. Processors report die-lip buildup and smoke generation when melt temperature exceeds 275 °C or when tackifier is added to the core layer by mistake; maximum melt residence time is kept below 12 minutes. Published data for LLW1020B6-specific cast film performance in tropical warehouse conditions are limited, so line trials with a chill roll water temperature of 20–25 °C and winder tension tapering from 120 N to 60 N are used to establish curl-free rolls.
Across liquid packaging lines where extrusion coating replaces solventborne adhesive lamination, LLW1020B6 is processed through a slot die directly onto paperboard, aluminium foil, or biaxially oriented polypropylene at melt temperatures of 290–320 °C, a die opening of 0.7–1.0 mm, and an air gap of 200–250 mm; the elevated melt temperature is required to oxidize the web surface slightly and develop adhesion to polar substrates. The substrate is preheated to 35–60 °C, and the chill roll temperature is maintained between 15 °C and 25 °C with a matte or gloss finish depending on sealing performance. Line speed is 100–300 m/min for 15–40 g/m² coating weights; above 200 m/min edge tear and draw-down instability increase unless LLW1020B6 is blended with 10–40 wt% LDPE having a melt index of 4–8 g/10 min to lower neck-in. Neck-in on a 1,200 mm die is typically 30–60 mm per side, and edge bead trimming is required. Adhesion to aluminium foil is measured by peel strength using a 90° peel test at 50 mm/min; values below 1.0 N/15 mm indicate insufficient surface oxidation and require reducing the air gap to 150 mm or raising melt temperature to 310–320 °C.
Where adhesion to foil or metallised film is specified, a maleic anhydride grafted polyethylene tie layer is included at 5–15 wt% or a separate extruder applies a 3–5 g/m² tie layer, while LLW1020B6 remains in the bulk coating layer at 60–90 wt%. Antioxidant masterbatch at 0.05–0.10 wt% and antiblock at 0.2–0.5 wt% are used when the coated web is wound before lamination. For aseptic liquid packaging, the coating must meet FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, and the finished laminate must pass hydrogen peroxide sterilisation at 30–35% concentration at 70–80 °C without delamination. Barrier properties are governed primarily by the aluminium foil layer, not by the LLW1020B6 coating, so water vapour transmission rate is not assigned to the polyethylene layer; published data for LLW1020B6 in this multi-layer configuration are limited, requiring pilot coating trials. Terminal product types include aseptic brick cartons, paper cups, sachet laminates, medical packaging pouches, and lidstock for dairy products.
Rotational moulding powder requirements and oven cycle limits for LLW1020B6 differ from those of medium-density or high-density rotomoulding grades because butene-comonomer LLDPE yields lower zero-shear viscosity but also lower tensile modulus. The pellet form is dry ground to a powder passing 35 mesh (500 µm) with a bulk density of 0.45–0.52 g/cm³ measured by ASTM D1895; high fines content below 200 mesh increases static charging and is kept below 10% of the powder fraction. The dry blend consists of 97–99 wt% LLW1020B6 powder, 0.2–0.5 wt% hindered amine light stabilizer masterbatch, 0.05–0.15 wt% primary antioxidant, and 0.05–0.20 wt% internal mold release; for outdoor agricultural service, UV absorber is added at 0.1–0.3 wt% with carbon black or titanium dioxide dispersion at 1–3 wt%. Oven temperature is set to 260–300 °C, with residence time of 12–25 min depending on wall thickness between 3 mm and 10 mm; main spindle rotation ratio is 4:1 and minor axis ratio is 1:4 to maintain uniform wall thickness. Peak internal air temperature should reach 180–200 °C before cooling begins, because premature removal causes weld-line porosity at the parting line.
Compliance is anchored to ASTM D1998-15 for polyethylene upright storage tanks and ASTM D1693-15 Condition B for environmental stress crack resistance in 100% Igepal CO-630 at 50 °C; butene-based LLW1020B6 may show F50 values below 100 h in aggressive surfactant environments, so the resin is suitable for non-stressed tanks and bins rather than primary chemical containment. Food-contact bins comply with FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; outdoor tanks intended for potable water require additional extractables testing under local plumbing regulations. Published data for LLW1020B6 rotomoulded ESCR in Igepal are limited, so part-specific data must be generated for any regulated application. Terminal product types include agricultural chemical storage tanks up to 5,000 L with wall thickness 6–10 mm, water storage cisterns, material handling bins, hoppers, and playground components.
When LLW1020B6 is compounded into thin-wall injection moulding feedstock for non-appearance parts, the melt temperature is set at 180–230 °C and the mold temperature at 15–30 °C, with injection pressure of 70–120 MPa and holding pressure of 40–70 MPa. The screw uses an L/D ratio of 20:1–25:1 and a compression ratio of 2.0:1–2.5:1; because LLW1020B6 has higher melt viscosity than high-flow HDPE, spiral flow length at 1,000 bar injection pressure and 220 °C is typically 25–35% shorter, so gate size and runner diameter are increased by 20–30% relative to HDPE. The blend ratio is 60–80 wt% LLW1020B6 with 20–40 wt% HDPE to raise flexural modulus and reduce sink marks; color masterbatch is added at 2–4 wt%; and antistatic additive at 0.5–1.5 wt% is used for closures in dry food service. Shrinkage after 24 h is measured by ASTM D955-21 and ranges from 1.5% to 2.5%, with post-mold shrinkage of 0.3–0.7% after 7 days, so mold design compensation is essential. Compliance is limited to FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 for dry food lids; published data for LLW1020B6-specific injection shrinkage cards are limited, and mold trials are required to establish cavity pressure curves. Terminal product types include flexible lids for dry food containers, overcaps for non-carbonated beverage cups, and thin-wall bins for material handling.
Where a monolayer LLDPE geomembrane is specified for a low-to-moderate chemical containment application, LLW1020B6 is converted on a flat-die sheet line with a die width of 2.0–4.0 m and a polished three-roll stack. Melt temperature is maintained at 200–230 °C, die gap at 2.0–3.0 mm, and roll-stack temperature at 60–80 °C; sheet thickness is controlled from 0.75 mm to 2.50 mm with transverse gauge variation below ±5% by automatic die bolt adjustment. The formulation includes 75–90 wt% LLW1020B6, 10–25 wt% HDPE to raise tensile yield and environmental stress crack resistance, 2–3 wt% carbon black masterbatch for UV protection, 0.1–0.3 wt% hindered amine light stabilizer, and 0.05–0.15 wt% antioxidant. Carbon black dispersion is assessed by ASTM D5596; a rating of A-1 or A-2 is required in GRI-GM13, and poor dispersion accelerates oxidative degradation by creating localized stress concentrations.
| Property | Method | Typical acceptance criterion |
|---|---|---|
| Thickness | ASTM D5199 | Minimum average ≥ specified thickness |
| Density | ASTM D1505 | 0.920–0.940 g/cm³ for LLDPE-rich sheet |
| Tensile yield strength | ASTM D6693 | ≥16 kN/m after HDPE blending |
| Oxidative induction time | ASTM D3895 | ≥100 min at 200 °C |
| Carbon black dispersion | ASTM D5596 | Category A-1 or A-2 |
Test methods for geomembrane acceptance are anchored to ASTM D5199 for thickness, ASTM D1505 for density, ASTM D6693 for tensile properties, ASTM D1004 for tear resistance, ASTM D4833 for puncture, ASTM D5397 for single point notched constant tensile load, and ASTM D3895 for oxidative induction time at 200 °C and 35 kPa oxygen. GRI-GM13 requires OIT above 100 min for HDPE/LLDPE geomembranes, but butene-comonomer LLW1020B6-rich sheet may fall below this limit, so the HDPE fraction is adjusted toward the upper end of 10–25 wt% for primary landfill lining. Wedge welding is carried out at 400–450 °C with a speed of 1.5–2.5 m/min, and the welded seam shear strength must exceed 80% of parent sheet yield strength per ASTM D6392. Published data for LLW1020B6 in GRI-GM13 conformance are limited; users typically blend with HDPE to meet GM13. Terminal product types include landfill cap liners, pond liners, secondary containment, and canal liners.
Competitive CIPLAS LLW1020B6 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
CIPLAS LLW1020B6 is a linear low-density polyethylene resin whose model designation places it within the low-pressure ethylene copolymer family used principally for thin-gauge film extrusion. The grade is evaluated for blown-film and cast-film conversion where puncture resistance, elongation, seal initiation, and melt flow consistency are specified alongside density and additive package. Because grade-specific published data for CIPLAS LLW1020B6 is limited, this technical introduction separates class-typical linear low-density polyethylene behavior from values that require lot-level verification against the manufacturer’s certificate of analysis.
Linear low-density polyethylene resins of this class are typified by density values from 0.915 g/cm³ to 0.935 g/cm³ when measured by ISO 1183-1:2019 or ASTM D1505. Melt flow rate for film grades is generally determined at 190 °C under 2.16 kg load in accordance with ASTM D1238 or ISO 1133-1:2022; film-extrusion grades commonly fall between 0.5 g/10 min and 2.0 g/10 min. Tensile specifications for blown film may require yield strength from 10 MPa to 20 MPa and elongation at break above 600% per ASTM D638 or ISO 527-3. Dart impact values for 25 µm linear low-density polyethylene film often range from 150 g to 400 g under ASTM D1709. These ranges are class-typical and do not constitute the specification for CIPLAS LLW1020B6; the exact comonomer type, whether 1-butene, 1-hexene, or 1-octene, is not identified by the model designation alone.
Processing stability is controlled by melt viscosity, shear response, and oxidative degradation. On a single-screw blown-film extruder with screw diameter between 45 mm and 75 mm and length-to-diameter ratio from 24:1 to 30:1, adapter melt temperature is typically maintained between 190 °C and 240 °C. Below 180 °C, incomplete melting and excessive die pressure are observed; above 250 °C, oxidative chain scission produces gel particles and low-molecular-weight volatiles. Gel accumulation at the screen pack raises backpressure and shortens continuous run time.
The die gap for linear low-density polyethylene blown film is generally set between 1.5 mm and 2.5 mm, wider than the 0.8 mm to 1.2 mm gap often used for branched low-density polyethylene. This wider gap reduces shear stress at the die lip and limits sharkskin melt fracture. If die pressure remains unstable, fluoropolymer processing aid is introduced at 500 ppm to 1000 ppm through masterbatch addition; the additive migrates to the die steel surface and reduces the shear stress required for slip.
Blow-up ratio is commonly limited to 2:1 to 3:1 for linear low-density ethylene copolymers because lower melt strength relative to branched LDPE reduces bubble stability at higher inflation ratios. Frost-line height is adjusted so that film web temperature at the collapsing frame is 35 °C to 55 °C. A lower frost line increases quench rate and reduces crystallinity, improving clarity but increasing blocking unless antiblock is present. Pre-drying is not mandatory when packaging is intact and pellet surface condensation is avoided. If bags have been opened under high humidity, pellets may be conditioned in a hopper dryer at 40 °C to 60 °C for 30 min to 60 min; hopper temperatures above 70 °C are not recommended because pellet surface tack can reduce feed consistency.
Published production-scale comparisons for general-purpose LLDPE film extrusion indicate that screw motor load can be 10% to 25% higher than branched LDPE at identical screw speed and die diameter. The effect is most pronounced at apparent shear rates from 100 s-1 to 500 s-1, where linear low-density resins display less shear thinning. For CIPLAS LLW1020B6 specifically, published data for this configuration is limited, and actual motor load should be verified during a production trial.
Where distinction from other ethylene polymers is required, the controlling variable is not density alone but branch structure along the ethylene backbone. Autoclave low-density polyethylene carries long-chain branches that increase melt strength and extensional hardening; linear low-density polyethylene carries short-chain branches that disrupt crystallinity and improve toughness. High-density polyethylene has lower branch content and therefore higher crystallinity, which raises modulus but reduces film tear resistance and optical quality.
| Property | Test Method | LLDPE Class | LDPE Class | HDPE Class |
|---|---|---|---|---|
| Density | ASTM D1505, ISO 1183-1:2019 | 0.915–0.935 g/cm³ | 0.912–0.925 g/cm³ | 0.941–0.965 g/cm³ |
| Melt flow rate | ASTM D1238 190 °C/2.16 kg | 0.5–2.0 g/10 min | 0.3–2.0 g/10 min | 0.05–1.0 g/10 min |
| Tensile yield strength | ASTM D638 | 10–20 MPa | 6–12 MPa | 20–30 MPa |
| Elongation at break | ASTM D638 | 600–900% | 200–600% | 100–600% |
| Dart impact, 25 µm film | ASTM D1709 | 150–400 g | 50–150 g | 20–100 g |
| Haze | ASTM D1003 | 4–15% | 3–8% | 20–50% |
The tabulated values are class-typical ranges from resin-selection literature for compression-molded or blown-film test specimens; they are not lot-specific specifications for CIPLAS LLW1020B6. They demonstrate the engineering trade-off: linear low-density resin classes provide higher dart impact and elongation than branched LDPE at equivalent melt flow rate, while high-density polyethylene offers higher yield strength but lower optical clarity.
Extruder selection for linear low-density film grades frequently involves a grooved-feed single-screw configuration with screw diameter from 45 mm to 90 mm and 24:1 to 30:1 L/D. Grooved-feed zones improve solids conveying but raise feed-section barrel pressure; therefore, barrel temperatures in the first two zones are often set 10 °C to 20 °C lower than the metering zone to avoid bridging. Barrier screws or Maddock mixing sections are preferred because they reduce solid-bed breakup and improve melt homogeneity.
If CIPLAS LLW1020B6 is processed on a high-output line above 150 kg/h, a melt pump may be installed after the extruder to stabilize output against die pressure fluctuations. Melt pump suction pressure is kept between 5 MPa and 12 MPa to prevent cavitation, while discharge pressure at the die is adjusted depending on die diameter and gap, commonly from 15 MPa to 35 MPa. Published data for this specific grade in high-output gear-pump configurations is limited.
Filtration is typically performed with screen packs from 40 mesh to 200 mesh, often using layered sequences to reduce gel transfer into the film. Continuous screen changers are specified for long campaigns because gel accumulation can increase pressure at rates of 0.5 MPa/h to 2 MPa/h under oxidation-prone conditions. Batch-to-batch variation in antioxidant loading can shift this rate; incoming lots of CIPLAS LLW1020B6 should be evaluated for oxidation induction time by ASTM D3895 where long-run stability is critical.
The apparent shear rate at the die lip is calculated from volumetric output and die gap. For a 300 mm diameter blow-up die operating at 80 kg/h with 1.8 mm gap, the apparent shear rate is approximately 250 s-1. Under these conditions, melt fracture defects are controlled by maintaining melt temperature above 200 °C and adjusting the external air ring to stabilize the bubble. If sharkskin persists, fluoropolymer processing aid concentration is increased in 100 ppm increments until the film surface clears.
In regulatory evaluations, the starting point is the base resin compliance statement for the supplied lot and not the nominal polymer class. Polyethylene homopolymers and copolymers intended for food-contact use in the United States are evaluated under 21 CFR 177.1520. Finished articles sold in the European Union are subject to EU 10/2011, which applies an overall migration limit of 10 mg/dm² for food simulants. The product may also require documentation under REACH 1907/2006 and RoHS 2011/65/EU when supplied into regulated industrial markets. Conformity cannot be inferred from resin type because antioxidant, antiblock, slip, and processing aid packages can alter migration and restricted-substance status.
| Regulatory Instrument | Scope | Core Limit or Test | Required Confirmation for CIPLAS LLW1020B6 |
|---|---|---|---|
| 21 CFR 177.1520 | US FDA food-contact olefin polymers | Base resin recognition and extractives testing | Supplier food-contact statement for the exact grade |
| EU 10/2011 | Plastics in food contact | Overall migration 10 mg/dm² | Migration test on finished film or container |
| REACH 1907/2006 | EU chemical safety | SVHC concentration 0.1 wt% | Safety data sheet and SVHC disclosure |
| RoHS 2011/65/EU | Electrical and electronic equipment | Lead 1000 ppm, cadmium 100 ppm, mercury 1000 ppm, hexavalent chromium 1000 ppm | Homogeneous material test or supplier certificate |
The compliance matrix applies to the finished article and the specific lot. A statement that a resin belongs to the linear low-density polyethylene class is insufficient for food-contact or electrical-equipment documentation.
When the grade is compared with metallocene linear low-density polyethylene, the differences become measurable in dynamic rheology and film optics rather than in density alone. Ziegler-Natta and hybrid-catalyst linear low-density resins typically exhibit broader molecular weight distribution than metallocene-catalyzed grades of equivalent melt index. The practical consequence is that conventional LLDPE processes with lower melt pressure and less severe melt fracture, but may show lower dart impact and higher haze. A typical metallocene film formulation may show dart impact improvements of 30% to 70% for the same gauge and density band; however, published data for CIPLAS LLW1020B6 in direct comparison with metallocene grades is limited. Film-to-film evaluation under identical extrusion conditions is therefore required for final resin selection.
Operational boundaries for linear low-density ethylene copolymers include continuous service temperature under load generally not exceeding 60 °C to 70 °C without loss of creep resistance. Contact with strong oxidizing acids, chlorinated solvents, or high-aromatic hydrocarbon streams at elevated temperature causes softening, swelling, or environmental stress-cracking. In outdoor film applications, ultraviolet stabilization with hindered amine light stabilizers and adequate carbon black loading is required for multi-season service; unmodified natural resin will undergo rapid embrittlement under ASTM G154 weathering conditions. The specific weathering life of CIPLAS LLW1020B6 has not been published in this document.