| HS Code | 910065 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Melt Index | 1.0 g/10 min (190°C/2.16 kg) |
| Density | 0.918 g/cm³ |
| Melt Flow Ratio | 27 |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 150 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 12% |
| Gloss | 60% |
| Vicat Softening Point | 93°C |
| Melting Point | 120°C |
| Crystallization Temperature | 105°C |
| Coefficient Of Friction | 0.2 |
| Antiblock | 2000 ppm |
| Slip | 500 ppm |
As an accredited CIPLAS LLW1018F Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CIPLAS LLW1018F Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial use. |
| Container Loading (20′ FCL) | CIPLAS LLW1018F Linear Low Density Polyethylene loaded in 20′ FCL, palletized bags, securely stowed and lashed for safe ocean transport. |
| Shipping | CIPLAS LLW1018F Linear Low Density Polyethylene is shipped as a non-hazardous thermoplastic resin in 25 kg bags, jumbo bags, or bulk trucks/containers. Keep dry, avoid direct sunlight, heat, and moisture. Handle with clean equipment. Protect packages from punctures and contamination. Store in a cool, dry, well-ventilated area. |
| Storage | Store CIPLAS LLW1018F Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed, clean, and clearly labeled. Protect from moisture, dust, and contamination. Store on pallets, stack securely, and follow local regulations and manufacturer guidance. |
| Shelf Life | Indefinite if stored cool, dry, sealed, away from sunlight, heat, and contaminants; no specific expiration for CIPLAS LLW1018F. |
Three-layer blown-film extrusion for agricultural silage cover and greenhouse cladding is one production route where CIPLAS LLW1018F is placed in the core layer at 60–80 wt% between skins of metallocene-catalysed LLDPE or EVA. The grade is a butene-copolymer linear low-density polyethylene with a nominal melt flow rate of 1.0 g/10 min at 190°C under 2.16 kg (ASTM D1238) and a nominal density of 0.918 g/cm³ (ASTM D1505). On a 75 mm single-screw extruder with 30:1 L/D and a barrier screw, the core-layer melt temperature is maintained at 190–210°C. Die gap is set to 2.0–2.4 mm and blow-up ratio is controlled between 2.2:1 and 2.6:1; bubble instability becomes measurable below 2.0:1 because the low melt strength of butene LLDPE produces asymmetric frost-line motion. Frost-line height is held at 600–900 mm above the air ring to stabilize the bubble before the upper nip. Silage cover film at 150–200 µm is specified under EN 13207:2018; dart drop impact under ASTM D1709 method A in commercial trials typically exceeds 800 g at 150 µm. Tensile strength at break is measured under ASTM D882 with crosshead speed 500 mm/min; typical machine-direction values for 150 µm film fall between 28 MPa and 35 MPa. Elmendorf tear is measured under ASTM D1922; transverse-direction tear values are commonly 15–25 N/mm depending on orientation. Haze is measured under ASTM D1003; greenhouse cover film requires less than 25% total haze for 200 µm, which makes the use of 0.2–0.5% HALS stabilizer and 0.1–0.3% slip/antiblock masterbatch necessary. UV stabilization for 12-month outdoor exposure in high-solar-radiation regions is verified under ISO 4892-2 cycle 1 with tensile elongation retention of not less than 50% after 2000 h. Processors must not exceed 220°C melt temperature because oxidation of the film edge at the frost line creates gel particles above 230°C. Output rates on a 75 mm line are typically 160–220 kg/h depending on screw speed and backpressure; screw speed is limited to 90–110 rpm to avoid melt fracture at the die lip. The terminal article is either a 150–200 µm silage wrap or an 80 µm greenhouse film with a minimum 12-month service life, supplied in widths from 6 m to 12 m.
In adhesive-laminated flexible packaging, the sealant web is a 20–40 µm film in which CIPLAS LLW1018F forms the heat-seal layer against BOPP or BOPET print webs. The critical failure mode is not tensile rupture but interfacial seal fracture after hot-bar or impulse sealing; seal strength is therefore evaluated under ASTM F88/F88M with a 25 µm aluminum foil jaw cover and a dwell time of 0.5 s. For a 40 µm CIPLAS LLW1018F sealant web, a seal initiation temperature of 105°C at 0.3 N/mm² sealing pressure is typical; stable seal strength above 2.5 N/15 mm is reached at 125°C. Hot tack is measured under ASTM F1921 with a 0.2 s seal time and a 0.1 s delay; values above 3.0 N/25 mm are required for vertical form-fill-seal packaging of granular products. The coefficient of friction is measured under ASTM D1894; a target kinetic coefficient of 0.15–0.25 is maintained by adding 500–1,000 ppm erucamide and 1,000–2,000 ppm synthetic silica antiblock. Erucamide migration to the sealant surface is time-dependent; under 23°C storage, at least 48 h is required to approach equilibrium, and faster migration is not achieved by increasing erucamide above 1,000 ppm because surface saturation increases the risk of seal contamination on adjacent print surfaces. Corona treatment of the sealant web before lamination is limited to 38–42 mN/m; exceeding 44 mN/m oxidizes the surface and reduces seal initiation temperature consistency according to ASTM F1921 round-robin reproducibility. Extrusion of the sealant web is performed on a 65 mm blown-film line with die gap 1.8 mm and blow-up ratio 2.5:1; bubble cooling at 15°C ambient air delivers a faster crystallization rate than cast-film processing and preserves low haze. Film haze is controlled below 8% for 30 µm film under ASTM D1003. Published data for this specific CIPLAS grade in BOPET adhesive laminations are limited; the processing window is therefore derived from butene LLDPE grades with equivalent density and melt flow rate and should be validated on the actual line. Terminal products include dry-food pouch sealant webs, flow-wrap lamination films, and overwrap for medical device trays where the sealant layer must not transfer detectable odor.
For 120–180 µm industrial heavy-duty sacks and FIBC inner liners, the high-stalk bubble configuration is selected because it raises transverse-direction tear resistance under ASTM D1922 and lowers gel-induced bubble breaks. A typical structure is 20% LDPE skin, 60% CIPLAS LLW1018F core, and 20% LDPE skin; the LDPE component increases bubble stability during jaw closure and raises melt tension. Extrusion is performed on a 90 mm single-screw extruder with 30:1 L/D, die diameter 300 mm, die gap 2.0 mm, and blow-up ratio 1.8:1–2.4:1. Melt temperature is maintained at 195–215°C; melt pressure before the screen changer is limited to 350 bar to avoid excessive shear heating. Output rates of 250–350 kg/h are controlled by screw speed, with maximum screw speed not exceeding 110 rpm because higher shear rates reduce bubble stability at frost-line heights above 900 mm. Heavy-duty sack film is specified under ASTM D1709 method B; 150 µm three-layer film typically has a dart impact above 1,000 g. Puncture resistance is measured under ASTM D5748; a 150 µm film commonly shows a peak load of 120–160 N. Elmendorf tear values in machine and transverse directions are balanced by adjusting the blow-up ratio; a BUR below 1.8:1 produces transverse-direction tear below 10 N/mm, which is insufficient for filled-sack drop resistance. The film is printed on the outer skin after corona treatment to 38 mN/m; ink adhesion is tested under ASTM D3359 method B with tape peel. Sacks are converted by bottom-seal and side-seal welding; weld strength is measured under ASTM F88 and must exceed 60% of the film tensile strength. A process conflict arises when post-industrial recycled LLDPE trim is incorporated above 15% in the core layer: gel speck area under ASTM D5140 exceeds 100 ppm and reduces dart impact below 800 g. Therefore the recycled fraction is held at 10–15% and pre-dried at 70°C for 4 h when storage humidity exceeds 60% RH. Terminal articles are 50 kg polymer granule sacks, mineral filler sacks, and FIBC inner liners of 150–200 µm.
On a 90 mm cast-film line with a 1,200 mm flat die, CIPLAS LLW1018F is processed into 40–70 µm film for frozen vegetable and seafood packaging. The grade is used as a monolayer or skin-layer resin; die gap is set to 0.8 mm and chill roll temperature is held at 15–20°C. Line speed is 150–250 m/min; at speeds above 200 m/min, neck-in must be controlled by adjusting air-knife position and die gap. Water vapour transmission rate is measured under ASTM F1249 at 38°C and 90% RH; a 50 µm film typically displays 1.5–2.0 g/m²·day. Oxygen transmission rate is measured under ASTM D3985; values are relatively high at 4,000–6,000 cm³/m²·day·atm, and therefore the resin is used for frozen foods where oxidative shelf life is limited by low storage temperature rather than gas barrier. Cold-temperature seal strength is measured after sealing at 130°C, 0.3 N/mm², and 0.5 s dwell, followed by conditioning at -18°C for 24 h under ASTM F88; seal strength must not fall below 2.0 N/15 mm. Haze is measured under ASTM D1003; cast film of 40 µm typically shows 2–5% total haze because of rapid chill-roll solidification. Gloss at 60° is measured under ASTM D2457 and lies above 85 for 40 µm film. The specified structure for frozen seafood is 30% LDPE in the skin layers and 70% LLW1018F in the core layer, with 0.4% synthetic silica antiblock to keep blocking below 15 g/cm under ASTM D3354. Terminal products include pillow pouches for IQF vegetables, frozen shrimp bags, and ice cream overwrap where low-temperature flexibility and seal integrity at -18°C are the critical acceptance criteria.
In general-purpose food contact film, CIPLAS LLW1018F can replace LDPE at 60–100% of the polyolefin fraction for bakery goods, produce bags, and dry-food pouch outer webs. The driving change is downgauging: at equal dart impact under ASTM D1709, butene LLDPE film can be reduced in thickness by 15–20% versus LDPE of equivalent melt flow rate. However, the lower 1% secant modulus of LLDPE must be compensated on high-speed vertical form-fill-seal machines because film stiffness below 150 MPa in the machine direction under ASTM D882 causes web wander and poor bag mouth opening. Film structure is 40–70 µm with a 70% LLW1018F core and 15% LDPE in each skin; the LDPE skins raise machine-direction secant modulus and preserve bubble stability. Melt temperature is set at 190–210°C, die gap at 1.8 mm, blow-up ratio at 2.4:1, and frost-line height at 600 mm. Total haze is kept below 10% for 50 µm film under ASTM D1003; slip and antiblock levels are selected to maintain kinetic coefficient of friction between 0.12 and 0.20 under ASTM D1894. Extractables are controlled under FDA 21 CFR 177.1520(c) and EU Commission Regulation 10/2011. The film complies with the overall migration limit of 10 mg/dm² for food simulant B under 10/2011 test conditions OM2 for frozen and refrigerated foods, and with the hexane extractable specification under 21 CFR 177.1520(c) 3.2a for fatty food contact. Low-temperature sealing is performed on the film at 110–130°C with 0.3 s dwell; seal strength under ASTM F88 must exceed 2.0 N/15 mm after cooling. Not all food contact uses are permissible without migration testing: hot-filled liquid products above 70°C or high-fat products above 40°C in direct contact require specific migration tests for the selected slip and antioxidant package because LLW1018F alone does not supply the required data for all food simulants. The compliance matrix for this segment is shown in Table 1. Terminal articles are bread bags, produce rollstock, and dry-food pouch outer webs.
| Standard or regulation | Cited provision | Relevant limit or test condition |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Paragraph 3.2a | Fatty food contact; hexane extractable limitation for olefin polymers |
| EU Commission Regulation 10/2011 | Article 12 and Annex I | Overall migration limit 10 mg/dm² for food simulant B under OM2 |
| ASTM F88/F88M | Seal strength test method | Minimum 2.0 N/15 mm after cooling |
As a carrier resin for polyolefin film masterbatches, CIPLAS LLW1018F is compounded with pigment, slip, antiblock, or UV additive concentrates. The carrier is dry-blended at 20–40 wt% active ingredient for organic pigment concentrates and 50–70 wt% filler for mineral-based antiblock concentrates. Mixing is carried out on a co-rotating twin-screw extruder with 40:1 L/D, screw diameter 50–75 mm, and specific energy of 0.18–0.25 kWh/kg. Melt temperature is maintained below 210°C; higher temperatures degrade erucamide slip additives and cause uncontrolled migration in the final film. Dispersion quality is tested by an extruder screen pack pressure rise method under EN 13900-5, with a target pressure rise of less than 0.20 bar/g over a 14 µm filter medium for a 5% addition in a blown-film diluent. The carrier resin contributes sufficient viscosity to wet the pigment surface and prevent compacted pigment agglomerates in the hopper; its 1.0 g/10 min melt flow rate under ASTM D1238 is chosen because lower-viscosity carriers reduce torque but also reduce shear stress for dispersion above 40% loading. The finished masterbatch is let down at 2–5% in film-grade LLDPE or LDPE. Terminal articles are concentrated color masterbatches, slip/antiblock masterbatches, and weathering stabilizer masterbatches for agricultural film. No further compounding steps are required before film extrusion, and the masterbatch must be dried at 70°C for 2 h only when exposed to storage humidity above 70% RH to avoid steam-driven porosity in the carrier phase.
Competitive CIPLAS LLW1018F Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
CIPLAS LLW1018F is a linear low density polyethylene film grade supplied under the CIPLAS polyethylene brand. The resin is a butene-comonomer LLDPE with a nominal density of 0.918 g/cm³ and a nominal melt flow rate of 1.0 g/10 min measured at 190°C with a 2.16 kg load. The product is manufactured as natural pellets containing antioxidant and processing stabilizer packages, and it is intended for blown-film extrusion. The LLW1018F nomenclature places the grade in the moderate-melt-viscosity, lower-density region of the LLDPE film spectrum. Because the polymer backbone is linear with controlled short-chain branching, the resin does not possess the high degree of long-chain branching characteristic of autoclave or tubular LDPE. This structural difference changes melt extensibility, shear thinning, and film toughness. The grade is therefore specified when converters require higher dart impact and tear resistance than LDPE of comparable density, but do not require the optical and hot-tack performance of metallocene-catalysed LLDPE. The product is supplied in 25 kg bags or bulk containers and should be handled to avoid contamination by fine particles, which can generate gel defects in thin-gauge film. Published technical data should be confirmed against the current supplier certificate of analysis because lot-to-lot variation exists in comonomer incorporation and additive levels.
The melt flow rate of 1.0 g/10 min is determined under ASTM D1238-20 Procedure A or ISO 1133-1:2022 condition 4. This value is higher than many fractional-melt LDPE film grades, which usually fall between 0.2 g/10 min and 0.8 g/10 min. The higher melt index reduces melt pressure and motor load at ordinary extrusion temperatures but also lowers bubble stability compared with a 0.25 g/10 min LDPE. Density is measured according to ASTM D1505-18 or ISO 1183-1:2019. The 0.918 g/cm³ value indicates a short-chain branch content typical of a butene LLDPE with roughly 5–8 wt% comonomer. This amorphous fraction contributes to impact resistance, but it reduces crystallinity, modulus, and barrier compared with a 0.935 g/cm³ HDPE. For extrusion, the rheology of LLW1018F exhibits less shear thinning than LDPE; in a grooved-feed extruder, the specific energy input may be higher, and screen pack pressure rise can be greater for the same output. The viscosity curve for a 1.0 MI butene LLDPE typically shows a Carreau zero-shear viscosity above 3×10⁴ Pa·s at 190°C, but the exact value depends on molecular weight distribution and should be obtained from capillary rheometry for the specific lot. In processing, the absence of long-chain branching means that strain hardening is lower, and the bubble is more sensitive to gusts and frost-line height changes. These differences are critical when replacing LDPE in existing formulations; a conversion from a high-pressure LDPE to LLW1018F may require increasing die gap, reducing blow-up ratio, or raising extruder temperature to avoid melt fracture.
A property cliff edge exists in dart impact as density increases. For butene LLDPE blown film, published trends indicate that a density increase from 0.918 g/cm³ to 0.924 g/cm³ may reduce dart impact by 25–35% while increasing tensile modulus by 15–25%. This sensitivity means that shifts in comonomer feed during polymerization or addition of high-density scrap can alter the film balance unexpectedly. Converters blending LLW1018F with HDPE for stiffness must evaluate the nonlinear impact on toughness; at 10 wt% HDPE addition, dart impact may decline more than predicted from simple linear mixing. A similar nonlinearity appears in haze: additions of LDPE above 10 wt% can increase haze disproportionately due to surface roughness and optically distinct domains. These interactions are derived from published polymer-blend behaviour; specific data for LLW1018F blends should be generated on the production line.
On a production-scale monolayer blown-film line equipped with a 65 mm grooved-feed extruder with 30:1 L/D, a 200 mm spiral mandrel die, and 1.6 mm die gap, the grade is run at barrel temperatures from 160°C to 210°C, with die zones at 220°C. Blow-up ratio is maintained at 2.0:1 to 2.5:1. Frost-line height is kept between 3 and 5 die diameters. Under these settings, melt pressure is typically 18–22 MPa and melt temperature is 215–225°C at screw speeds of 80–100 min⁻¹. Bubble stability remains acceptable if the ambient airflow is low and the die lip is clean. Die-lip build-up can occur when the film is run at high output for extended periods; this is a known characteristic of butene LLDPE and can be mitigated by periodic purging with HDPE or by using low-molecular-weight polyethylene purge compounds. For three-layer coextrusion, LLW1018F can be used as a skin layer or core layer. When combined with ethylene-vinyl alcohol or polyamide barrier layers, tie-layer selection must be confirmed by adhesion tests because published data for this specific coextrusion configuration is limited. Corona treatment should be applied immediately before printing or lamination. The required surface energy for solvent-based lamination is 38–42 mN/m; unprimed film typically tests at 30–32 mN/m. These operational figures are representative of this product category and must be re-evaluated on the specific line.
The following table lists supplier-published typical values for LLW1018F film produced at 25 µm gauge with a blow-up ratio of 2.2:1 and a 1.6 mm die gap. The values are not shipment specifications; a lot-specific certificate of analysis should be requested for production release.
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Melt flow rate | ASTM D1238-20 / ISO 1133-1:2022 | g/10 min | 1.0 |
| Density | ASTM D1505-18 / ISO 1183-1:2019 | g/cm³ | 0.918 |
| Melting point | ASTM D3418-21 | °C | 122 |
| Vicat softening point | ASTM D1525-17 | °C | 95 |
| Tensile strength at yield MD/TD | ASTM D882-18 / ISO 527-3:2018 | MPa | 11/10 |
| Tensile strength at break MD/TD | ASTM D882-18 / ISO 527-3:2018 | MPa | 38/30 |
| Elongation at break MD/TD | ASTM D882-18 / ISO 527-3:2018 | % | 800/900 |
| Dart drop impact F50 | ASTM D1709A-16 / ISO 7765-1:2004 | g | 110 |
| Elmendorf tear MD/TD | ASTM D1922-15 | gf | 300/450 |
| Haze | ASTM D1003-21 | % | 8 |
| Gloss at 60° | ASTM D2457-19 | GU | 55 |
The tensile values are gauge-dependent and orientation-dependent. At 25 µm thickness, the machine-direction orientation generated by the bubble is reflected in higher machine-direction yield stress and lower machine-direction elongation compared with transverse direction. Dart impact under ASTM D1709A-16 measures the mass at which 50% of test specimens fail; a value of 110 g at 25 µm is typical for a butene LLDPE of this density and melt index, whereas a metallocene LLDPE of similar density may reach 150–200 g. Haze and gloss are strongly influenced by die gap, frost-line height, and cooling air temperature; the values in the table therefore represent a defined laboratory film line, not all production films. For applications where optical properties are critical, the converter should run designed experiments rather than relying solely on nominal values.
Heavy-duty sack film from LLW1018F is typically coextruded in three layers with outer layers containing 10–20 wt% HDPE to improve creep resistance and stiffness. Lamination sealant layers using LLW1018F benefit from the lower seal initiation temperature relative to HDPE seal layers. Typical seal strength on 25 µm film reaches 3–4 N/15 mm after flat-jaw sealing at 140–160°C for 0.5 s, but users should verify seal strength under actual packaging line dwell times because seal temperature and pressure vary with jaw configuration. For agricultural film, addition of carbon black masterbatch at 2–5 wt% provides ultraviolet protection; unstabilized natural film is not recommended for extended outdoor exposure.
LLW1018F is differentiated from metallocene-catalysed linear low density polyethylene primarily by molecular weight distribution and catalyst system. Metallocene LLDPE typically has a narrower molecular weight distribution, which lowers seal initiation temperature, reduces extractables, and improves optical clarity. However, the narrower distribution also reduces shear thinning and can increase extruder backpressure or melt fracture at equivalent output. In film testing at 25 µm, a C6- or C8-metallocene LLDPE can show dart impact values 30–50% higher and haze values 40–60% lower than a conventional butene LLDPE of the same density. LLW1018F therefore occupies a position between high-pressure LDPE and metallocene LLDPE: it provides significant toughness improvement over LDPE without the higher cost and tighter processing behaviour of metallocene grades.
Against a higher-α-olefin Ziegler-Natta LLDPE with hexene or octene comonomer, the butene grade of LLW1018F generally shows lower puncture resistance, lower tear propagation, and lower hot-tack strength at similar density and melt index. The property differences are not universal; they depend on molecular weight distribution, comonomer distribution, and film processing conditions. A converter evaluating replacement should compare dart impact, Elmendorf tear, and seal strength at the intended film gauge rather than relying on density and melt index alone. Compared with HDPE of density 0.952 g/cm³, LLW1018F has lower tensile modulus, lower temperature resistance, and higher permeability to oxygen and water vapour, but significantly higher strain at break and better stress-crack resistance under flexural loads. This makes it unsuitable for rigid containers but suitable for flexible films that must survive drop loading at low temperatures.
For applications governed by food-contact regulations, the base resin is an olefin polymer that falls within the scope of 21 CFR 177.1520 for polyethylene in the United States, and compliance with EU Regulation 10/2011 is assessed on the finished article by migration testing. The unpigmented natural grade is not UV-stabilized; outdoor exposure without adequate carbon black or hindered-amine light stabilizer will cause chain scission and embrittlement. Storage should be in dry, shaded conditions; although LLW1018F does not normally require predrying, bags opened at relative humidity above 60% may require drying at 60–70°C for 2 hours to avoid moisture-related bubble defects. Avoid melt temperatures above 240°C because prolonged residence time can generate oxidative gels and discoloration. The grade should not be dry-blended with copper-containing pigments or free-halogen flame-retardant packages without specific thermal stability testing. For exact compliance statements, the current supplier product stewardship bulletin and lot-specific certificate of analysis are the controlling documents.