| HS Code | 189271 |
| Grade | LLF2019B |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
As an accredited CIPLAS LLF2019B Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CIPLAS LLF2019B Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25-kg bags of CIPLAS LLF2019B Linear Low Density Polyethylene, shrink-wrapped and secured for shipment. |
| Shipping | CIPLAS LLF2019B Linear Low Density Polyethylene is shipped as a non-hazardous solid resin, typically in 25 kg bags or bulk, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Keep away from heat, moisture, sunlight, and ignition sources. Not regulated for transport. |
| Storage | Store CIPLAS LLF2019B Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and strong oxidizers. Keep bags or containers closed, clean, and palletized. Prevent moisture, dust, and static buildup. Avoid temperature extremes, stack securely, and use first-in, first-out stock rotation. Follow manufacturer instructions and local regulations. |
| Shelf Life | Shelf life is 12 months from production when stored in a dry, clean, well-ventilated area away from direct sunlight. |
Agricultural greenhouse covering films and mulch films consume CIPLAS LLF2019B Linear Low Density Polyethylene in direct monolayer blown film extrusion. Incoming resin certification uses melt flow rate measured at 1.9 g/10 min under 190 °C/2.16 kg according to ISO 1133-1:2022 and density verified by ISO 1183-1:2019. The resin is introduced as a dry blend containing 70–80 wt% LLF2019B and 20–30 wt% LDPE of melt flow rate 0.30–0.45 g/10 min; the LDPE fraction raises bubble stability and melt strength when blow-up ratio exceeds 2.0:1. For greenhouse service of 12 months, hindered amine light stabilizer masterbatch is dosed at 4.0–8.0 wt% and an anti-drip/anti-fog masterbatch at 0.8–1.5 wt%; for mulch film, carbon black masterbatch at 2.5–4.0 wt% replaces the anti-drip package. Before extrusion, pellet surface moisture is maintained below 0.05% by weight; if storage relative humidity exceeds 60%, drying for 2–4 h at 70–80 °C is required to limit surface defects. Processing uses a single-screw extruder with L/D 30:1, a barrier or Maddock mixing section, annular die diameter 150–350 mm, die gap 1.8–2.2 mm, and a dual-lip air ring delivering 12–18 m³/min per meter of die circumference. Melt temperature is maintained at 195–220 °C, blow-up ratio at 2.0:1–2.5:1, frost line height at 4–6 die diameters, and winding tension at 10–20 N/m. Bubble failure modes include draw resonance and frost-line oscillation; if frost line position fluctuates more than ±5 cm, cooling air distribution is rebalanced before further adjustment. Film thickness is 150–200 µm for greenhouse covering and 20–60 µm for mulch. Terminal product types include greenhouse covering films, low-tunnel films, silage clamp liners, and soil fumigation films. Compliance for agricultural films follows EN 13206:2017 for thermoplastic films used in agriculture and horticulture; direct food-contact uses require verification under Regulation (EU) No 10/2011 and 21 CFR 177.1520(c) item 1.1 extractives limits for olefin polymers.
Cast stretch film produced from LLF2019B uses a formulation in which LLF2019B comprises 88–95 wt%; a metallocene-catalysed LLDPE of density 0.912–0.918 g/cm³ is added at 5–12 wt% to raise dart drop and puncture resistance. Polyisobutylene cling agent of number-average molecular weight 800–1,400 g/mol is incorporated at 1.0–2.5 wt%; a synthetic silica anti-block masterbatch is dosed at 0.3–0.8 wt%. Processing uses an extruder with L/D 30:1 and a barrier screw, melt temperature 240–260 °C, die gap 0.45–0.70 mm, air gap 10–18 mm, chill roll temperature 18–25 °C, and haul-off speed 250–650 m/min. Film thickness ranges from 10 µm to 23 µm for machine-grade film. At haul-off speed above 420 m/min, cling force measured by ASTM D5458-19 on 23 µm film can fall below 3.0 N/25 mm if the polyisobutylene level is below 1.2 wt%, because tackifier migration to the film surface is time- and temperature-dependent. The film is wound with taper tension between 18 and 28 N/m, and wound roll hardness is held at 65–75 Shore A to reduce telescoping without causing blocking. Terminal product types are machine-grade stretch wrap, hand stretch wrap, and pallet overwrap. Compliance for food-contact use as secondary packaging follows Regulation (EU) No 10/2011 and 21 CFR 177.1520(c) item 1.1; mechanical acceptance is assessed by ASTM D5748 puncture resistance and ASTM D882-18 tensile elongation. On a 2.2 m wide cast line at 500 m/min and 20 µm gauge, theoretical output is approximately 1,200 kg/h; die residence time is 1.4–2.0 s. If die lip back pressure is below 80 bar, the melt curtain edges exhibit neck-in above 25 mm per side and require edge trim recapture at 3–5% of web width. Published data for this specific grade in this configuration are limited; validation by capillary rheometry at 230 °C and 1,000 s⁻¹ is required before changing die gap or output.
Extrusion coating of woven polypropylene sacks and metallized polyester laminates uses LLF2019B in a melt blend of 50–80 wt% LLF2019B and 20–50 wt% LDPE of melt flow rate 4–8 g/10 min. The LDPE fraction is added to reduce neck-in and draw resonance at line speeds of 100–220 m/min; without LDPE, neck-in can exceed 35 mm per side at 150 m/min. A processing aid masterbatch is dosed at 0.3–0.7 wt% to delay melt fracture. For aluminium foil and metallized PET substrates, an ethylene acrylic acid or maleic anhydride tie layer is applied at 0.5–1.5 g/m² before the LLDPE coating; paper webs require no primer when surface energy is above 40 mN/m. Melt temperature is maintained at 285–320 °C, die gap at 0.50–0.75 mm, die-to-chill-roll air gap at 100–180 mm, and chill roll temperature at 12–18 °C. Coating weight is 12–25 g/m² on woven sacks. Adhesion to woven polypropylene is checked by 180° peel testing; values below 2.5 N/15 mm indicate insufficient oxidative bonding or substrate corona treatment below 38 mN/m. Terminal product types include fertilizer-grade woven polypropylene sacks, pet food bags, and industrial paper sacks with moisture barrier. Compliance for dry food contact follows Regulation (EU) No 10/2011 and 21 CFR 177.1520(c) item 1.1; REACH Regulation (EC) No 1907/2006 Annex XVII applies to substances in the compounded resin.
Thin-wall lids and overcaps moulded from LLF2019B use a blend of 85–95 wt% LLF2019B and 5–15 wt% HDPE of melt flow rate 20–30 g/10 min to increase flexural modulus and reduce sink marks. A nucleating/clarifying masterbatch may be added at 0.5–1.5 wt%, and a slip masterbatch at 0.2–0.5 wt%. The resin is processed on an injection moulding machine with screw L/D 18:1–22:1, melt temperature 205–235 °C, mould temperature 10–30 °C, injection speed 80–140 mm/s, and holding pressure at 35–55% of peak injection pressure. Clamp force requirement is 4–6 kN/cm² of projected area. Gate freeze time for a 1.0 mm side-gated lid is 0.8–1.4 s; if holding pressure is released before gate freeze, warpage exceeds 0.6 mm on a 70 mm diameter lid. Post-mould dimensional inspection is conducted after 24 h; linear mould shrinkage for unfilled LLDPE is typically 1.4–1.8%. Terminal product types are flexible overcaps, detergent canister lids, and cosmetic jar overcaps. Regulatory requirements include 21 CFR 177.1520(c) item 1.1 for olefin polymers, Regulation (EU) No 10/2011 for plastic food-contact materials, and, where applicable, EU Directive 2001/95/EC general product safety for closures. The material is not recommended for cold-impact closure applications below -20 °C; a high-density polyethylene or impact-copolymer polypropylene is preferred for those conditions.
Drip irrigation laterals and micro-tubes can be extruded from LLF2019B in a compound containing 96.5–98.0 wt% LLF2019B and 2.0–3.5 wt% carbon black masterbatch of particle size 20–50 nm; a process aid is added at 0.2–0.5 wt% to reduce melt fracture in narrow annular gaps. The pipe is produced on a single-screw extruder with L/D 24:1–30:1 and a grooved feed section, melt temperature 200–225 °C, die head temperature 215–230 °C, and screw speed 30–80 min⁻¹. Vacuum calibration at -0.02 to -0.06 MPa is used for outside diameter control, and line speed is 15–60 m/min depending on wall thickness 0.50–1.20 mm. Carbon black dispersion is assessed according to ISO 18553:2002; agglomerates larger than 50 µm may initiate stress cracking under cyclic irrigation pressure. Short-term burst pressure and emitter uniformity are evaluated according to ISO 9261:2004; long-term hydrostatic design stress is assessed by pressure testing according to ISO 9080:2012. Terminal product types are integral drip laterals, emitter discharge pipes, and micro-irrigation connecting tubes. The compound is not intended for potable water contact without additional migration testing under Regulation (EU) No 10/2011 and NSF/ANSI 61, which are not automatic for this agricultural resin.
Heavy-duty industrial liners and sacks manufactured from LLF2019B use a three-layer blown film configuration with a layer ratio of 20/60/20; the core layer is 60–80 wt% LLF2019B and 20–40 wt% LDPE, while the skin layers contain 10–20 wt% reprocessed edge trim from the same material and 2–3 wt% of a processing aid/color masterbatch. The extruder setup consists of three single-screw extruders of L/D 25:1–30:1, die diameter 200–450 mm, die gap 1.8–2.4 mm, blow-up ratio 1.8:1–2.2:1, and melt temperature 190–225 °C. Film thickness is 50–150 µm. Heavy-duty bags are subjected to dart drop ASTM D1709-16a method A of 200–500 g and Elmendorf tear ASTM D1922-15 of 10–25 N/mm depending on thickness. Terminal product types include flexible intermediate bulk container inner liners, construction aggregate sacks, and industrial rollstock for hazardous-free bulk packaging. In combustible powder filling applications, antistatic additive migration may be required; surface resistivity is evaluated by ASTM D257-14. The film is not a substitute for a certified UN packaging; if used as an inner liner inside a FIBC certified to UN 13H2, the assembly must be tested under the applicable ADR/RID/IMDG provisions and not the film alone. Compliance for dry food contact follows Regulation (EU) No 10/2011 and 21 CFR 177.1520(c) item 1.1; REACH Regulation (EC) No 1907/2006 Annex XVII applies to substances in the compounded resin.
Competitive CIPLAS LLF2019B Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
CIPLAS LLF2019B Linear Low Density Polyethylene is a butene-copolymer blown-film resin supplied as pellets with a nominal density of 0.918 g/cm³ at 23 °C per ISO 1183-1:2019 and a melt flow index of 2.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. The polymer substance is identified by CAS 9002-88-4 and is positioned for general-purpose film extrusion where gauge uniformity, seal response, and converter economics are weighted over extreme melt strength or high-clarity optics. The base stabilization package includes a phenolic primary antioxidant, a phosphite secondary antioxidant, and a metal-stearate neutralizer; exact additive loadings appear only on the producer’s certificate of analysis and safety data sheet, not in generic technical summaries. Public data for the specific reactor configuration is limited; the grade is understood to be a conventional Ziegler-Natta butene-copolymer resin, and processing behavior should be validated against the current lot certificate. Grade designation LLF2019B distinguishes the product from CIPLAS LDPE and metallocene film resins in the same producer portfolio.
The LLF prefix identifies the grade as a linear low-density film resin. The numeric block 2019 indexes the nominal density between 0.916 g/cm³ and 0.920 g/cm³, while the B suffix denotes a butene comonomer. Short-chain branching from 1-butene lowers crystallinity relative to HDPE and produces a melting peak typically between 120 °C and 125 °C under ISO 11357-3:2018. The molecular weight distribution is moderately broad, consistent with a conventional Ziegler-Natta catalyst system, and this breadth contributes to shear thinning and bubble stability. Published reactor details for this specific grade are not fully disclosed in the public datasheet; therefore, hydrogen offgas ratio and comonomer distribution data are not reported here.
Table 1 summarizes the release and film-validation envelope. The film values are typical for a 25 µm blown film produced at a 2.5:1 blow-up ratio, 210 °C melt temperature, and 1.8 mm die gap; production lots are governed by the certificate of analysis rather than by this table.
| Property | Normative method | Representative value |
|---|---|---|
| Density at 23 °C | ISO 1183-1:2019 | 0.918 g/cm³ |
| Melt flow index 190 °C/2.16 kg | ISO 1133-1:2022 | 2.0 g/10 min |
| Tensile strength at yield, MD | ISO 527-3:2018 | 10–11 MPa |
| Tensile strength at yield, TD | ISO 527-3:2018 | 9–10 MPa |
| Elongation at break, MD | ISO 527-3:2018 | 650% |
| Elongation at break, TD | ISO 527-3:2018 | 750% |
| Dart drop impact, F50 | ASTM D1709-16a Method A | 90–110 g |
| Elmendorf tear, MD/TD | ASTM D1922-15 | 100/120 g |
| Haze | ASTM D1003-21 | 12–15% |
| Gloss, 45° | ASTM D2457-21 | 65–70 |
The film data in Table 1 should not be read as a guarantee for any specific film structure because gauge, cooling rate, and masterbatch dilution shift tensile and optical responses.
On production-scale blown-film lines with 45–65 mm grooved-feed extruders at L/D 24:1–30:1, LLF2019B is processed between 185 °C and 215 °C. A barrier screw with a Maddock mixing section is preferred; the temperature profile is set flat to slightly rising from feed to metering zone. Feed-zone temperature is typically kept at 70–90 °C, the compression zone at 160–190 °C, and the metering zone at 200–215 °C. Screw speed on 65 mm lines normally falls between 70 min⁻¹ and 110 min⁻¹, producing 90–120 kg/h at 25 µm gauge on a 1.8 m die circumference. Head pressure typically ranges from 20 MPa to 35 MPa depending on die gap, screen-pack condition, and melt temperature.
Die gap should be set at 1.4–2.0 mm for a blow-up ratio of 2.0:1–2.5:1. Frost line height is controlled between 2.5 and 4.0 die diameters. A lower frost line produces quench-related TD gauge bands, while a higher frost line induces bubble flutter and lowers dart impact. Specific output above 1.2 kg/h per mm of die circumference can exceed melt relaxation capacity and produce shark-skin melt fracture; the onset is shifted by polymer processing aid to apparent wall shear rates in the 150–250 s⁻¹ range. Moisture adsorption is not significant below 60% RH, but exposure to condensing humidity requires 80 °C pre-drying for 2 h in a desiccant hopper before extrusion. Melt temperatures above 220 °C should be avoided because oxidative chain scission raises gel formation and reduces Elmendorf tear.
Field observations on 65 mm monolayer lines show that die pressure fluctuation remains below ±1.5 MPa when screw speed is below 90 min⁻¹ and 100 mesh screen packs are used. A pressure differential across the breaker plate above 8 MPa correlates with screen-pack blinding from oxidized fines and requires a screen change to avoid bubble pump instability. These values are equipment-dependent and should be treated as troubleshooting references rather than product specifications.
Primary end uses include unprinted and reverse-printed industrial films: garment bags, thin produce bags on draw tape lines, carrier bags, liners, and general overwrap. In agricultural mulch and greenhouse film, LLF2019B is typically blended with 10–20 wt% low-density polyethylene to increase bubble stability and reduce melt fracture at wide blow-up ratios; the exact blend ratio is set by the required dart impact, UV stabilizer loading, and converter line. Food-contact status is not an absolute resin property; the finished film, including masterbatch, ink, and adhesive components, must satisfy the applicable migration limits. The base olefin polymer may be used under FDA 21 CFR 177.1520(c) as an olefin polymer and under EU Regulation (EU) No 10/2011 when the overall migration limit of 10 mg/dm² is not exceeded. In cast film trials on a 30 mm laboratory line, seal initiation on 25 µm film is typically observed between 105 °C and 115 °C at 0.5 N/mm² seal bar pressure and 0.5 s dwell; this range is not a specification because seal-bar geometry, film gauge, and additive migration alter the response.
Applications requiring dart drop impact above 150 g on 25 µm film or puncture energy above 2.5 J under ASTM D5748-95 may exceed the practical ceiling of a 2.0 g/10 min butene-copolymer LLDPE. Under ASTM D1709-16a Method A, LLF2019B commonly falls between 90 g and 110 g. Hexene- and octene-copolymer grades of equivalent density and MI often reach 200–400 g because longer comonomer chains increase tie-molecule density and crack propagation resistance. The processing advantage of LLF2019B is lower extruder torque, reduced melt pressure, and a broader bubble stability window at thin gauge than many metallocene products. In coextruded film structures, LLF2019B is therefore placed in core layers or non-seal skins when outer layers deliver the specified optics, stiffness, or seal performance.
Against autoclave LDPE, LLF2019B exhibits higher tensile strength at break and significantly higher Elmendorf tear at equivalent gauge; LDPE retains higher melt strength for heavy-gauge shrink and thick-sheet extrusion. Against C6 and C8 Ziegler LLDPE grades, LLF2019B typically shows lower dart impact, lower puncture resistance, and slightly lower clarity but a better price-to-processability balance on conventional monolayer lines. Against metallocene LLDPE, LLF2019B has broader molecular weight distribution, lower extruder head pressure, and lower tendency for melt fracture; the metallocene product generally gives higher dart impact, lower haze, and lower hexane extractables under FDA 21 CFR 177.1520 protocols. The selection boundary is therefore application-specific: LLF2019B is used when converter runnability and cost per unit area dominate; C8 and metallocene LLDPE are selected when toughness or optical specifications cannot be relaxed.
The base resin is not a food-contact certificate by itself. Compliance is established on the finished article after accounting for slip, antiblock, colorant, and printing components.
| Framework | Reference | Condition |
|---|---|---|
| US food-contact resin status | FDA 21 CFR 177.1520(c) | Olefin polymer status subject to finished-article extraction limits; specific additive package must be confirmed. |
| EU food-contact framework | EU Regulation (EU) No 10/2011 | Finished article requires overall migration ≤ 10 mg/dm² and specific migration compliance for additives. |
| REACH registration | EC 1907/2006 | Polymer substance registration status depends on imported formulation; candidate-list SVHC screening is required for pigment and additive masterbatches. |
| RoHS | Directive 2011/65/EU | Base polyolefin not within restricted categories; lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE thresholds apply only to finished electrical/electronic articles. |
LLF2019B is not designed for high-clarity shrink film requiring haze below 5% on 25 µm gauge, nor for retort or hot-fill packaging where continuous service exceeds 110 °C. The melting peak is below 125 °C, and sustained exposure above 110 °C may cause creep, seal weakening, and additive migration. Heavy oxidized recycle streams above 20 wt% should be avoided because acid functionality deactivates the neutralizer package and raises gel count. The product is not recommended for injection molding or rotomolding; it should be processed only on film extrusion lines.