| HS Code | 193314 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Butene |
| Catalyst | Ziegler-Natta |
| Density | 0.919 g/cm3 |
| Meltflowrate | 1.0 g/10 min at 190°C/2.16 kg |
| Meltflowratio | 28 |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 90 °C |
| Tensilestrengthatyield | 10 MPa |
| Tensilestrengthatbreak | 25 MPa |
| Elongationatbreak | 700% |
| Dartdropimpact | 120 g |
| Elmendorftearstrengthmd | 120 g |
| Elmendorftearstrengthtd | 250 g |
| Haze | 12% |
| Gloss | 60% |
| Coefficientoffriction | 0.2 |
| Blocking | 60 g |
As an accredited CIPLAS LLF1019F2 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CIPLAS LLF1019F2 Linear Low Density Polyethylene is supplied in 25 kg polyethylene-lined paper bags, palletized and shrink-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of CIPLAS LLF1019F2 Linear Low Density Polyethylene, shrink-wrapped for safe ocean transport. |
| Shipping | CIPLAS LLF1019F2 Linear Low Density Polyethylene is shipped as non-hazardous solid pellets in 25 kg bags, jumbo bags, or bulk trucks/railcars. Keep containers closed, dry, and away from direct sunlight, heat, and ignition sources. Handle with standard industrial hygiene; avoid dust generation and environmental release. No UN hazard class required. |
| Storage | Store CIPLAS LLF1019F2 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Maintain stable pallets, avoid excessive stacking, protect from physical damage, and follow good housekeeping and local regulations. Use first-in, first-out stock rotation; avoid prolonged exposure to high temperatures. |
| Shelf Life | Shelf life is typically 24 months when stored unopened in original packaging, in a cool, dry, well-ventilated area away from direct sunlight. |
CIPLAS LLF1019F2 enters heavy-duty sack production as the core-layer workhorse in a three-layer coextruded blown film where the technical problem is maintaining dart impact after blending recycled edge trim. The nominal grade parameters used below are a melt-flow index of 1.9 g/10 min (ISO 1133-1:2022, 190°C, 2.16 kg) and a density of 0.919 g/cm³ (ISO 1183-1:2019). The sealing layer is deliberately diluted with 8–12 wt% LDPE of melt-flow index 4.0 g/10 min to reduce seal initiation temperature to 105–115°C, while the core layer carries 20–25 wt% recycled clean edge trim. A starting layer ratio of 30/40/30 by mass allows the outer layer to contain 4–6 wt% white masterbatch without collapsing core-layer tear resistance.
The outer-layer formulation includes process-aid masterbatch at 0.3–0.5 wt%, not as an antiblock substitute but to control die-lip build-up during 72-hour uninterrupted Windmoeller & Hoelscher or Reifenhauser three-layer runs. Erucamide slip is held below 500 ppm because higher concentrations migrate to the sack surface and reduce flexographic ink adhesion below target values. Natural silica antiblock is added at 1,000–2,000 ppm only to the outer layer. Extrusion is carried out on a 65 mm grooved-feed barrier screw with 30:1 L/D, die gap 1.8–2.2 mm, blow-up ratio 2.5:1–3.0:1, and frost-line height 6–8 die diameters. The melt temperature at the die is capped at 215°C to hold shear-induced gel formation at a lot-average level acceptable for automated sack converting and heat-seal operation.
The terminal 80 µm sack is evaluated under ASTM D1709-16a/A for dart impact and ASTM D1922-15 for Elmendorf tear. Commercial three-layer structures built around C4 LLDPE typically show dart drop in the 120–190 g range and transverse-direction tear above 300 gf/µm when LDPE dilution is kept below 10 wt% in the load-bearing layers. For filled sacks, the critical control point is gauge variation; automated capacitance gauges measure transversely at ±5%, and heavy-duty drop failures on production lines more often trace to gauge bands than to low tensile strength.
Agricultural greenhouse cover film produced from CIPLAS LLF1019F2 is normally not run as a monolayer because UV stabilization and anti-fog migration kinetics require layer-specific residence times. In a three-layer 150–200 µm structure, the grade is typically assigned to the middle layer at 35–50 wt%, while the external skin receives the full hindered-amine light stabilizer package. A typical external-layer formulation contains 0.5–0.8 wt% HALS masterbatch, 0.1–0.2 wt% UV absorber, 0.05–0.1 wt% antioxidant, and 0.3–0.5 wt% anti-fog additive based on polyglycerol ester. The inner layer receives 0.4–0.6 wt% anti-fog only, because bulk migration from the middle layer into the inner surface is too slow under greenhouse condensation load.
Film blowing is performed on a 400–600 mm multi-layer die with a die gap of 1.8–2.4 mm and blow-up ratio of 2.0:1–2.6:1. The bubble is run in a low-stalk configuration because C4 LLDPE has lower melt strength than LDPE; the frost line is positioned 6–9 die diameters above the die. Melt temperature is kept between 195°C and 210°C, while the internal bubble cooling volume is set to keep frost-line height within ±10% of the target value. The larger die diameter and narrower blow-up ratio are required to prevent width variation on 12–16 m layflat film when line speed exceeds 60 m/min.
Greenhouse film produced this way is tested under EN 13206:2017 for cover film classification; the relevant properties include light transmission and mechanical retention after accelerated weathering. The haze of a butene-based LLDPE middle layer is higher than hexene or octene equivalents, so the final film spec is typically set below 20% haze for light-sensitive crops. Anti-fog effect is not evaluated by a single standard; commercial producers use a cold-water condensation test at 50°C water bath and 20°C ambient to measure droplet formation over 72 hours. The operational boundary is that this grade does not provide sufficient long-term UV protection by itself; all greenhouse structures require additional film formulation stabilizers or external shading.
On high-output cast stretch lines running above 300 m/min, the limitation of CIPLAS LLF1019F2 is shear heating rather than tensile strength. The grade is introduced at 20–30 wt% into a C8 LLDPE rich blend, or a C6 LLDPE formulation of melt-flow index 2.5–3.5 g/10 min and density 0.912–0.917 g/cm³, to raise puncture resistance and load retention for pallet-wrap duty. Cling additive is not compounded into CIPLAS LLF1019F2; the cling phase is supplied by 1.5–2.5 wt% polyisobutylene or low-molecular-weight tackifier masterbatch added to one outer layer in a three-layer cast line. The core layer remains a two-component blend of CIPLAS LLF1019F2 and metallocene C8 LLDPE at 60/40 by mass.
Cast extrusion is carried out on a 65 mm 33:1 L/D barrier screw with screen pack below 200 mesh, flat die gap 0.7–0.8 mm, air gap 250 mm, and chill roll temperature 18–22°C. Because the melt-flow index of CIPLAS LLF1019F2 is below the typical cast-film window, barrel zone temperatures are reduced by 10–15°C compared with a standard LLDPE cast profile; the die zone is maintained at 210–220°C to balance gauge uniformity against melt fracture. Published data for this specific resin in cast stretch-film blends is limited, so line trials should confirm that the die pressure remains below 350 bar and that motor load stays within the extruder manufacturer’s curve at 300 m/min output.
The final cast pallet-wrap film of 12–35 µm is tested under ISO 527-3:2018 for tensile properties and ASTM D5458-95(2020) for cling. A pre-stretch ratio of 250–300% is typical on high-speed wrappers; mechanical failure at this point is controlled by MD tensile strength and puncture propagation, not by cling. The principal plant-floor failure mode is die-lip build-up after 6–8 hours of continuous running, caused by the lower-melt-index fraction. Scheduled die cleaning is therefore required more frequently than with a pure C8 cast grade.
Under EU No 10/2011 and FDA 21 CFR 177.1520(c), a food-contact film may not be evaluated solely by its nominal resin approval status. The converter must demonstrate that the final film, including all additive masterbatches and processing aids, meets overall and specific migration limits under the intended food simulants. For CIPLAS LLF1019F2, the grade can be used in dry-food packaging film when the total additive package is selected from the positive lists; the relevant US regulation remains FDA 21 CFR 177.1520(c) 2.1 for olefin polymers, and the relevant European legislation is Commission Regulation (EU) No 10/2011 with annexes listing permitted monomers and additives.
| Compliance Reference | Test Condition | Limit or Relevance |
|---|---|---|
| EU No 10/2011 Annex I and II | Overall migration, 10% ethanol and 3% acetic acid | 10 mg/dm² or 60 mg/kg for infant food |
| FDA 21 CFR 177.1520(c) | Olefin polymer extraction, heptane and water | Resin density 0.85–1.00 g/cm³ and specified extractables |
| REACH Annex XIV and Appendix 8 | SVHC screening of additives | 0.1% w/w communication threshold |
| EU No 10/2011 Article 19 | Labelling and declaration of compliance | Migration test report required from converter |
The extrusion process for food-contact film from CIPLAS LLF1019F2 must avoid cross-contamination with non-listed additives from prior production campaigns. A standard cleaning procedure is to purge the extruder with a low-MFI LDPE or a dedicated purging compound for 20–30 minutes before switching to food-grade material. Melt temperature is capped at 220°C because oxidative degradation produces low-molecular-weight carbonyl species that can alter organoleptics and raise migration values. The film structure is often a monolayer at 30–80 µm, but a coextruded barrier structure may be used where the CIPLAS LLF1019F2 layer is the food-contact side at 15–25% of total thickness.
Organoleptic failure is a more common rejection than migration failure on commercial packaging lines. The phenomenon is traced to oxidation of unsaturated sites or siloxane contamination from upstream equipment. For dry snacks and cereal liners, the film is tested for taint by sensory panel after 72 hours at 40°C in a sealed ballot jar. The safe operating boundary is that CIPLAS LLF1019F2 should not be used for retort or steam-sterilized food packaging because sustained exposure above 100°C exceeds the oxidation-induction-time safety margin of typical C4 LLDPE formulations.
Flat-die coating of woven polypropylene sacks with a blend of CIPLAS LLF1019F2 and LDPE creates a moisture barrier at coat weights from 14–20 g/m². The blend ratio is normally 20–30 wt% CIPLAS LLF1019F2 and 70–80 wt% LDPE of melt-flow index 4.0–7.0 g/10 min. The LDPE carrier supplies drawdown and neck-in performance at the flat die, while the LLDPE fraction raises seal strength and puncture resistance at the sack mouth. Adhesion to the woven substrate is not ensured by resin composition alone; it requires a primer or a tie layer of ethylene acrylic acid copolymer at 5–8 wt% in the coating blend unless the woven substrate is corona-treated above 42 mN/m.
Extrusion coating is run on a 90 mm 30:1 L/D extruder with a coat-hanger die of 2,400–3,200 mm width. The die gap is 0.8–1.0 mm, and the air gap is kept at 150–250 mm to balance oxidation and adhesion. Melt temperature in the die zone is held at 285–300°C because LDPE-rich blends require high temperature for drawdown; this limits the LLDPE addition to no more than 30 wt% because higher fractions produce visible gel formation and backpressure fluctuation. The line speed is set to 150–250 m/min. Neck-in is controlled within 30–40 mm per side by adjusting die deckle and air-gap length.
Coated sacks are evaluated under ASTM F88/F88M-23 for seal strength and ISO 1518:2015 for coating adhesion. The failure mode observed on production-scale coaters is not tensile failure of the LLDPE-LDPE blend but stress whitening at the woven-weld seam and microcracking at the sack corners. This occurs when the coat weight falls below 12 g/m² or when the coating blend has been overheated for more than 30 minutes during reel changeover. The operational boundary is that CIPLAS LLF1019F2 cannot be used as a neat coating resin in this process; the flat-die drawdown requirement demands the LDPE diluent.
When CIPLAS LLF1019F2 is processed as a thick-sheet geomembrane bubble of 0.5–1.5 mm, the failure mode shifts from melt fracture to gauge-band formation caused by low melt strength at low blow-up ratios. A monofilament or multi-layer bubble is run at blow-up ratio 1.5:1–2.0:1, die gap 2.0–2.5 mm, and layflat width 3–5 m. The extruder is a 90 mm 30:1 L/D grooved-feed machine with melt temperature from 195°C to 210°C. Internal bubble cooling is mandatory above 0.8 mm thickness because high throughput and low BUR concentrate heat in the bubble stem and create thickness bands outside ±8%.
The compound for temporary containment liner or secondary containment is based on 96–97 wt% CIPLAS LLF1019F2, 2.5–3.0 wt% carbon black masterbatch, and 0.2–0.4 wt% processing stabilizer. The carbon black concentration is verified by ASTM D1603-18 to lie between 2.0% and 2.5% by mass. A separate antioxidant package is required for outdoor exposure; HALS is not normally used in the buried portion but is added at 0.3–0.6 wt% for exposed surfaces. Weld seams are made by wedge welding at 220–260°C with a rolling speed of 0.8–1.5 m/min, and the peel-test performance is checked according to ISO 13937-2:2021 for tear and ASTM D6392-12(2021) for geomembrane seam strength.
The main process control parameter is not thickness alone but bubble stability at the low draw ratios demanded by thick film. C4 LLDPE produces thinner neck lines than HDPE and can oscillate when the frost line is disturbed by ambient air currents. The use of an external cage above the collapsing frame reduces width variation but cannot eliminate the fundamental melt-strength limit. This grade is therefore specified for temporary liners, secondary containment, and pond liners rather than primary landfill base liner duty where the stress-cracking requirement under ASTM D5397-19 favors high-density resin. Bubbles thicker than 1.5 mm require a different melt-flow index or a HDPE-rich blend to prevent bubble flapping and output loss after 48 hours of continuous production.
Competitive CIPLAS LLF1019F2 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
CIPLAS LLF1019F2 Linear Low Density Polyethylene is specified by film converters as a linear low-density polyethylene resin for blown and cast film structures in which downgauging, puncture resistance, and heat-seal strength are critical. Public technical data for this exact commercial grade are limited; the following description therefore combines the product identifier with property windows reported for LLDPE film resins of comparable density and melt-flow range. The suffix F2 in the grade designation does not independently identify comonomer type, slip/antiblock loading, or antioxidant formulation, and converters should obtain the manufacturer’s certificate of analysis before product qualification. Resin density is measured by ISO 1183-1:2019 or ASTM D792, and melt mass-flow rate is measured by ISO 1133-1:2022 or ASTM D1238 at 190°C/2.16 kg. The resin is not classed as hygroscopic, but condensation on pellet surfaces can generate bubble defects in film. If visual moisture is present after storage above 70% relative humidity, pre-drying at 70–80°C for 2–4 h may be applied before extrusion; storage above 40°C or prolonged ultraviolet exposure can accelerate antioxidant depletion and shift extrusion pressure.
The principal distinction between LLF1019F2-class resin and high-pressure low-density polyethylene appears in short-chain branching architecture and molecular weight distribution. High-pressure LDPE contains long-chain branching, which stabilizes the bubble at high blow-up ratios but limits dart impact and Elmendorf tear at equal gauge. LLDPE film resins in the 0.918–0.922 g/cm³ density window typically produce dart drop values under ASTM D1709 Method A that are 30–50% higher than a 0.923 g/cm³ LDPE control at 25 µm, and tensile strength at break under ISO 527-3:2018 is commonly 20–40% greater. Relative to metallocene LLDPE, a conventional LLF1019F2-type resin may exhibit broader comonomer distribution and lower melt strength, producing higher back pressure and lower optical clarity at equivalent density. Metallocene LLDPE typically provides better organoleptics and lower seal initiation, but requires tighter die-gap control and more aggressive cooling to maintain bubble stability. Against high-density polyethylene film, the lower density and alpha-olefin content of LLF1019F2 yield lower tensile modulus and higher puncture elongation, while HDPE provides superior stiffness and water-vapor barrier in mono-layer and multi-layer structures.
On a 65 mm grooved-feed single-screw extruder with a 25:1 L/D barrel and a 250 mm spiral mandrel die, LLF1019F2 is processed at melt temperatures of 190–230°C at the adapter and 200–230°C at the die. Blow-up ratio is maintained between 2.0:1 and 3.0:1, with frost-line height set at 4–8 die diameters. The die gap for 20–120 µm film is typically 1.5–2.5 mm; operation below 1.2 mm can raise die pressure above 450 bar and generate shear heating that initiates gel formation. Melt pressure at the breaker plate should be monitored continuously; sustained pressure above 350 bar on this extruder class indicates screen blockage or out-of-spec melt-flow resin. Published data for this specific configuration is limited, so these values are initial settings derived from comparable film-grade LLDPE equipment bulletins and should be adjusted through instrumented trial runs.
Die-lip build-up in LLF1019F2 processing is controlled by periodic purging with a high-melt-flow LDPE or a commercial purging compound. On lines running above 220°C, die-lip build-up can appear within 8–12 h and is removed with brass scrapers before gauge uniformity is affected. Screen packs of 60/80/100 mesh are used to trap contaminants during regrind use; regrind levels up to 20% by weight are usually tolerated without measurable loss of dart impact, provided the regrind is free of printed film and adhesive labels. Higher regrind levels reduce bubble stability and should be validated under ASTM D1709 and ASTM D882 on the final film.
Mechanical anisotropy in LLF1019F2 film is controlled by blow-up ratio and frost-line residence time. At a 2.5:1 blow-up ratio and 20 µm thickness, films based on LLDPE of 0.920 g/cm³ density typically show machine-direction tensile strength of 30–45 MPa and transverse-direction tensile strength of 25–38 MPa under ASTM D882 at 500 mm/min crosshead speed. Elongation at break usually falls between 600% and 900% in both directions. Elmendorf tear resistance measured under ISO 6383-2:2022 is normally lower in the machine direction: 150–350 g MD versus 350–700 g TD for a 25 µm film. Dart drop impact by ASTM D1709 Method A frequently lies between 100 g and 200 g at 25 µm, although exact values for LLF1019F2 must be verified on production film. Puncture resistance measured under ASTM D5748 is influenced by comonomer distribution and gauge; the class typically yields probe puncture energies of 0.8–1.5 J at 25 µm. These ranges derive from publicly reported LLDPE film datasets and do not replace the manufacturer’s grade-specific data.
| Property | Test Method | Typical Window for LLDPE Film Grade Class |
|---|---|---|
| Density | ISO 1183-1:2019, ASTM D792 | 0.918–0.922 g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022, ASTM D1238 at 190°C/2.16 kg | 0.9–1.1 g/10 min |
| DSC peak melting temperature | ISO 11357-3:2018, ASTM D3418 | 120–125°C |
| Tensile strength at break, MD | ASTM D882, 25 µm film | 30–45 MPa |
| Tensile strength at break, TD | ASTM D882, 25 µm film | 25–38 MPa |
| Elongation at break, MD/TD | ASTM D882 | 600–900% |
| Elmendorf tear, MD/TD | ISO 6383-2:2022, 25 µm | 150–350 g/350–700 g |
| Dart drop impact F50 | ASTM D1709 Method A | 100–200 g |
| Haze | ASTM D1003 | 10–20% |
| Heat seal initiation temperature | ASTM F88, 0.2 N/mm seal strength | 95–115°C |
Table values are not certified LLF1019F2 specifications; they are typical windows for film-grade LLDPE of matched density and melt-flow class.
In form-fill-seal packaging, LLF1019F2-class film is assessed by heat-seal strength and hot-tack methods. Under ASTM F88 with a dwell time of 0.5 s and jaw pressure of 2.0 bar, seal strength above 0.2 N/mm is typically reached at 100–115°C for films from LLDPE of this density class. Hot-tack strength measured under ASTM F1921 at 0.5 s dwell and 0.2 N/mm peel is commonly retained to 120–130°C before seal failure occurs. The window narrows at packaging speeds above 30 packages/min because contact time decreases and the seal interface cools below the crystallization temperature before load transfer. Slip and antiblock masterbatches reduce static coefficient of friction under ASTM D1894 to 0.1–0.3, but they can broaden seal initiation by 3–7°C depending on additive concentration and particle size. Converters should validate production seal windows using a temperature gradient method and not apply static laboratory values directly to vertical form-fill-seal machines.
In cast extrusion, LLF1019F2 can be processed at melt temperatures of 220–260°C through a flat die with a die gap of 0.5–1.0 mm and chill-roll temperatures of 15–25°C. The lower melt temperature at the chill roll limits transverse orientation; cast film therefore exhibits lower machine-direction tear resistance and higher elongation at break than blown film of the same gauge. Draw resonance is suppressed by maintaining an air gap below 10 cm and a film speed between 30 m/min and 100 m/min for typical line configurations. In lamination and sealant webs, the resin is selected for low-temperature sealing response, but contact with high-melt-temperature substrates can produce localized thinning unless melt temperature is reduced to the lower end of the recommended range. Published data for this specific configuration is limited; cast line operators typically start from the supplier’s extrusion recommendations and adjust using melt pressure and chill-roll torque measurements.
Compliance statements for LLF1019F2 require manufacturer documentation. Olefin polymers of this class are generally evaluated for indirect food contact under FDA 21 CFR 177.1520, but the final article must meet extractives limitations and additive restrictions in subpart B. In the European Economic Area, LLDPE film resins are commonly assessed under Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for food simulants; grade-specific migration testing is required because additive packages alter the result. REACH registration under EC 1907/2006 applies at substance level, and the RoHS Directive 2011/65/EU restricts lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE to 0.1% by weight in homogeneous materials. A certificate of analysis should list residual heavy metal concentrations and any SVHC content above 0.1% w/w. Processors should not rely solely on resin class to demonstrate final product compliance.
Storage-induced processing defects in LLF1019F2 are most often caused by condensation, pellet bridging, or ultraviolet exposure. The resin should be stored in sealed containers at 10–40°C and 40–70% relative humidity. Although polyethylene is non-hygroscopic, sudden transfer from cold storage to a warm production hall can generate surface moisture that produces bubble voids in film; conditioning to ambient temperature for 24 h before opening is recommended. Outdoor storage under ultraviolet radiation accelerates antioxidant consumption and photo-oxidation, which can raise the yellowness index measured under ASTM D6290 and shift extrusion pressure. The resin should not be blended with oxo-degradable pro-oxidant masterbatches unless the degradation schedule has been validated by ASTM D5510 or equivalent. Contact with amine-based additives and un-neutralized acidic convey residues can generate yellow discoloration at processing temperatures above 220°C, and such additives should be avoided unless specifically validated.
In heavy-duty sacks, agricultural silage, and industrial liner constructions, LLF1019F2 is selected for the balance of dart impact and seal performance. A 25 µm mono-layer film evaluated under ASTM D1709 can often be down-gauged by 10–20% relative to a high-pressure LDPE of equivalent stiffness, provided the bubble is operated at the upper end of the blow-up ratio window and the frost-line height is adjusted to preserve transverse orientation. In multi-layer lines, the resin is placed in core or seal layers where low-temperature seal response improves closure without increasing overall film density. Tensile, tear, and seal strength are validated by ISO 527-3:2018, ISO 6383-2:2022, and ASTM F88; burst strength for liners may be measured under ASTM D4266. Processors should qualify each structure at production speed because static specimen data do not capture the time-dependent seal and impact behavior observed on continuous converting lines.