| HS Code | 963245 |
| Material Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.919 g/cm³ |
| Melt Flow Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Dart Impact Strength | 100 g |
| Elmendorf Tear Strength Md | 120 g |
| Elmendorf Tear Strength Td | 150 g |
| Haze | 12% |
| Gloss 45 | 75% |
| Coefficient Of Friction | 0.15 |
| Bulk Density | 0.55 g/cm³ |
| Processing Temperature | 180-220 °C |
As an accredited CIPLAS LLF1019F1 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CIPLAS LLF1019F1 Linear Low Density Polyethylene is packaged in 25 kg polyethylene-lined woven sacks, palletized and stretch-wrapped for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): CIPLAS LLF1019F1 Linear Low Density Polyethylene, 25 kg palletized bags, approx. 20 MT net, securely loaded. |
| Shipping | CIPLAS LLF1019F1 is a linear low density polyethylene resin, supplied as solid pellets in 25 kg bags or bulk containers. It is not classified as dangerous goods. Store in a cool, dry, well-ventilated area away from ignition sources. Handle with standard PPE to avoid dust and slipping. |
| Storage | Store CIPLAS LLF1019F1 Linear Low Density Polyethylene in original packaging indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed and labeled, protect from moisture and contamination, and avoid dust generation. Use appropriate grounding and PPE. Keep away from incompatible materials. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Two years from manufacture when stored in original unopened packaging, in a cool, dry, well-ventilated area away from direct sunlight. |
On three-layer blown film lines running CIPLAS LLF1019F1 for fresh produce packaging, the resin is typically placed in the outer skin layers at 20 wt% to 40 wt% while a core of lower-cost LLDPE or LDPE carries the remaining mass fraction. Published data for this specific grade configuration is limited; the processing envelope below reflects production-scale equipment data for linear low density polyethylene film resins with nominal melt index 0.9 g/10 min to 1.1 g/10 min under ASTM D1238 at 190 °C and 2.16 kg, and density 0.916 g/cm³ to 0.922 g/cm³ under ASTM D792. Barrel temperature profiles from 180 °C at the feed throat to 220 °C at the adapter are maintained within ±3 °C to limit melt-temperature overshoot, while head pressure is held between 350 bar and 420 bar on a 70 mm screw with 28:1 L/D and a barrier mixing section. Die gaps of 1.6 mm to 2.2 mm are combined with blow-up ratios of 2.0:1 to 2.6:1; frost line height is set at 350 mm to 500 mm above the die face to balance bubble stability and quench rate. Final thickness from 25 µm to 50 µm is controlled by capacitive gauge arrays with a ±2 µm tolerance across a 1,600 mm die.
Antiblock and slip loadings for produce bag stock are restricted to 1,200 ppm to 2,000 ppm silica and 400 ppm to 800 ppm erucamide because higher slip levels degrade heat-seal strength and can produce visible surface bloom under refrigerated display lighting. Form-fill-seal conversion on servo-driven machines runs at 80 m/min to 120 m/min; the seal bar dwell time is set to 0.5 s to 0.8 s at 125 °C to 145 °C, producing a seal strength above 15 N/25 mm when tested according to ASTM F88/F88M. Haze is measured under ASTM D1003 and remains below 12% for the 25 µm monolayer configuration; Elmendorf tear values under ASTM D1922 typically fall between 8.0 N/mm and 15.0 N/mm in the machine direction, and dart impact under ASTM D1709 Method A exceeds 90 g after conditioning at 23 °C and 50% RH for 40 h. Food-contact compliance is covered by FDA 21 CFR 177.1520(c) for olefin polymers, with overall migration below 10 mg/dm² in food simulants under EU Regulation 10/2011; terminal products include vented produce bags, salad film, and translucent store-level rollstock.
Silage wrap production on five-layer cast stretch lines uses CIPLAS LLF1019F1 as the primary core resin at 60 wt% to 80 wt% of the total structure. The cling layer is compounded with 2.5 wt% to 4.0 wt% polyisobutylene or ultra-low-density polyethylene, while the balance in the outer layers is a propylene-based plastomer added at 10 wt% to 20 wt% to increase puncture resistance around coarse stem stubble. Melt temperatures at the feedblock are kept between 235 °C and 245 °C; higher temperatures above 250 °C initiate gel formation from the PIB concentrate and reduce cling force because low-molecular-weight fractions migrate to the chill roll surface. Chill roll temperatures of 18 °C to 24 °C are maintained with closed-loop glycol control, and the cast film is quenched against a primary roll with a 0.5 mm die gap and an air-knife velocity of 6 m/s to 10 m/s to suppress neck-in and edge bead.
Wrapper pre-stretch ratios are held at 70% to 90%; above 100% draw resonance produces gauge bands that reduce bale integrity after 6 to 8 months of outdoor exposure. Thickness is controlled to 25 µm ±1.5 µm across a 1,500 mm die using capacitance gauges and segmented air-knife adjustment. Cling values under ASTM D5458 are specified between 200 g and 600 g, and machine-direction tear under ASTM D1922 is used as the release criterion with a lower limit of 10 N/mm. Ultraviolet stabilization is added as a 5.0 wt% to 7.0 wt% hindered amine light stabilizer masterbatch, and the film is specified to retain at least 50% of initial tensile at break under ISO 527-3 after 12 months of temperate-zone sunlight. Since silage film does not contact food, FDA 21 CFR compliance is not required, but the PIB concentrate must comply with REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons; terminal products include round bale wrap, square bale covers, and silage pit sealing sheets.
The principal processing conflict in heavy-duty sack and industrial bag production from CIPLAS LLF1019F1 is the trade-off between bubble stability and dart impact. On monolayer blown film lines equipped with a 70 mm to 90 mm screw, 28:1 L/D, and a dual-lip air ring, die gap is widened to 2.0 mm to 2.5 mm and blow-up ratio is constrained to 1.8:1 to 2.0:1 to maintain a stable stalk configuration. A blend of 20 wt% to 30 wt% low-density polyethylene with melt index 0.3 g/10 min is introduced to suppress draw resonance and reduce die-lip melt fracture; however, each 10 wt% increase in LDPE content reduces dart impact by approximately 10% to 15% relative to a 100% LLDPE film at equivalent thickness. The following Table 1 records typical comparative ranges for industrial sack film from 40 µm to 125 µm on a 70 mm monolayer line at 190 °C melt temperature.
| Blend ratio (LLF1019F1 / LDPE) | Dart impact (ASTM D1709A) | MD Elmendorf tear (ASTM D1922) | Seal initiation (ASTM F2029) |
|---|---|---|---|
| 70/30 | 650–800 g | 150–210 gf | 108–112 °C |
| 80/20 | 700–850 g | 160–220 gf | 105–110 °C |
| 90/10 | 750–900 g | 170–230 gf | 103–108 °C |
Sealing is performed on impulse or hot-bar equipment with jaw pressure set to 3.0 bar to 4.5 bar; seal initiation temperature for an 80/20 LLDPE/LDPE blend falls between 105 °C and 110 °C, as measured by ASTM F2029. For sacks intended for chemical or mineral filling, the outer wall is compounded with 2.0 wt% to 3.0 wt% carbon black masterbatch for ultraviolet protection and 0.5 wt% to 1.0 wt% fluoropolymer processing aid to lower apparent viscosity at the die lip. Elmendorf tear under ASTM D1922 should remain above 15 N/mm in the machine direction, and dart impact under ASTM D1709 Method A should exceed 220 g for 100 µm film; if the lot-to-lot melt index drifts by more than ±0.05 g/10 min, frost line height must be adjusted by 25 mm to 50 mm to restore bubble stability. Terminal products include heavy-duty shipping sacks, FIBC liners, and industrial packaging for granular polymers and minerals.
Cast stretch film produced from CIPLAS LLF1019F1 for pallet unitization is driven by machine-direction tear resistance and pre-stretch uniformity rather than dart impact. On wider cast lines with a 1,200 mm to 1,800 mm slot die and a 0.5 mm die gap, melt temperature is maintained at 230 °C to 250 °C and the film is quenched on a matte or gloss chill roll at 20 °C to 28 °C. Output rates of 400 kg/h to 900 kg/h are typical; neck-in is controlled by edge-pinning air nozzles and a vacuum box set to 3 kPa to 5 kPa negative pressure. Cling performance is generated by adding 2.0 wt% to 3.5 wt% of a PIB concentrate or an ultra-low-density ethylene copolymer to the skin layer; this layer constitutes 10 wt% to 15 wt% of the total structure.
Machine-direction tensile elongation under ASTM D882 is specified above 500%, while transverse-direction elongation should remain above 700% because hand-wrapper force spikes can exceed 45 N per layer without film break. The film is pre-stretched at ratios of 150% to 250% on powered wrapper carriages; at ratios above 250%, edge tear propagation becomes the dominant failure mode and machine-direction tear resistance under ASTM D1922 is used as the release test with a minimum of 12 N/mm. Tensiometer measurements of cling force under ASTM D5458 are held between 300 g and 800 g for machine wrap, while hand wrap specifications call for 150 g to 300 g to avoid manual unwind difficulty. Since pallet wrap is an industrial product, food-contact compliance under FDA 21 CFR 177.1520 is required only where the film is used in food distribution but not direct contact; terminal products include machine pallet wrap, hand stretch film, and bundling film for beverage and logistic operations.
Coextruded barrier structures using CIPLAS LLF1019F1 as the sealant layer require a low and stable seal initiation temperature to avoid damaging the EVOH or nylon barrier layer during heat sealing. In a five-layer blown film line, the sealant layer comprises 20 wt% to 30 wt% of the total structure, a tie resin is placed at 8 wt% to 12 wt%, and the barrier layer is 5 wt% to 10 wt% EVOH with 38 mol% ethylene and 1.6 g/10 min melt index. Die gap is set at 1.6 mm to 2.0 mm and blow-up ratio at 2.0:1 to 2.5:1; the die temperature is held at 220 °C to 230 °C because EVOH degradation accelerates above 240 °C and produces brown specks and pinholes in the finished laminate.
Slip and antiblock loadings in the sealant layer are limited to 1,000 ppm erucamide and 1,500 ppm silica to balance coefficient of friction with seal strength. Heat-seal testing according to ASTM F2029 shows seal initiation between 103 °C and 108 °C for an 80 mL/min nitrogen purge, which is low enough to avoid barrier-layer retraction at seal jaw temperatures below 125 °C. The seal strength tested under ASTM F88/F88M exceeds 20 N/25 mm at 130 °C with a 0.5 s dwell and 2.0 bar jaw pressure. Food-contact compliance follows FDA 21 CFR 177.1520(c) for the polyolefin sealant layer and EU Regulation 10/2011 with overall migration below 10 mg/dm² in 10% ethanol, 3% acetic acid, and olive oil simulants; the compliance matrix in Table 2 summarizes the required test designations. Terminal products include vacuum pouches for processed meat, cheese block overwrap, and stand-up pouches for dry food.
| Requirement | Standard / regulation | Test condition | Limit |
|---|---|---|---|
| Olefin food-contact | FDA 21 CFR 177.1520(c) | Integral tray / film | n/a |
| Overall migration | EU 10/2011 | 10% ethanol, 3% acetic acid, olive oil | ≤10 mg/dm² |
| Seal strength | ASTM F88/F88M | 130 °C, 0.5 s, 2.0 bar | ≥20 N/25 mm |
| Seal initiation | ASTM F2029 | 80 mL/min N2 purge | 103–108 °C |
| Haze | ASTM D1003 | 25 µm film | ≤12% |
In continuously welded bottom-seal trash bag conversion from CIPLAS LLF1019F1, the resin is normally processed in a high-output single-layer blown film line with a 90 mm grooved-feed extruder and 30:1 L/D. Melt temperature is kept between 180 °C and 200 °C, die gap is 2.0 mm, and blow-up ratio is set at 2.5:1 to 3.0:1 to provide balanced machine-direction and transverse-direction tear properties. Carbon black masterbatch at 1.0 wt% to 2.0 wt% is used for opacity and ultraviolet resistance in outdoor waste bags; erucamide slip is limited to 300 ppm to 600 ppm because higher slip reduces heat-seal strength on rotating hot-bar sealers at 60 m/min to 90 m/min. Film thickness from 20 µm to 80 µm is measured by beta gauge, and the finished bags are sampled for Elmendorf tear under ASTM D1922 with a minimum of 10 N/mm in the machine direction and dart impact under ASTM D1709 Method A with a minimum of 140 g for 50 µm film. Because this is a well-established conversion practice, the dominant production risk is not formulation but gauge profiling across the bubble; operators adjust the air ring pressure by 5% increments when the transverse gauge variation exceeds ±4%. Terminal products include bin liners, heavy-duty refuse sacks, and industrial waste containment bags.
Competitive CIPLAS LLF1019F1 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
CIPLAS LLF1019F1 Linear Low Density Polyethylene is a film-grade ethylene-alpha-olefin copolymer produced with the linear backbone architecture characteristic of LLDPE. The short-chain branching distribution, rather than the long-chain branching found in high-pressure low density polyethylene, governs melt rheology and solid-state properties. The grade is positioned for blown film extrusion and selected cast film operations in which downgauging, puncture resistance, and seal integrity are necessary performance attributes. Because the producer has not published a complete grade-specific data sheet in public repositories, the controlling specification for CIPLAS LLF1019F1 is the lot-level certificate of analysis. Incoming inspection should verify melt mass-flow rate by ISO 1133-1:2022 and density by ISO 1183-1. The resin class commonly associated with this grade designation falls in the nominal density range of 0.918–0.922 g/cm³ and the nominal melt flow rate range of 0.8–1.2 g/10 min at 190 °C/2.16 kg, but supplier documentation remains the only valid source for acceptance testing.
Density and melt flow rate are controlled parameters for film-grade LLDPE because they determine the gauge at which a blown film line can maintain bubble stability and the temperature window for heat sealing. Density according to ISO 1183-1 or ASTM D1505 reflects comonomer content; a higher comonomer fraction reduces density and generally lowers seal initiation temperature while reducing stiffness. Melt mass-flow rate according to ISO 1133-1:2022 or ASTM D1238 indicates average molecular weight. For similar film applications, the lower MFR edge of the range provides higher melt strength and better bubble stability, while the higher MFR edge improves drawdown in thin-gauge cast film. The producer’s certificate of analysis should report the comonomer type, such as butene, hexene, or octene, although published data for this specific configuration is limited. Additional parameters such as melting peak by ISO 11357-3, volatile content by ASTM D1509, and slip/antiblock additive levels by producer methods may be specified for high-speed packaging lines.
| Property | Test method | Representative class range | Processing relevance |
|---|---|---|---|
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238 | 0.8–1.2 g/10 min | Bubble stability and drawdown |
| Density | ISO 1183-1 / ASTM D1505 | 0.918–0.922 g/cm³ | Stiffness, optics, seal initiation |
| Melting peak temperature | ISO 11357-3 | 119–126 °C | Extruder barrel profile setting |
| Tensile stress at break in film | ISO 527-3 | 25–45 MPa | Load-bearing capacity |
| Elongation at break in film | ISO 527-3 | >400% | Impact absorption and stretching |
| Dart impact on 25 µm film | ASTM D1709 | 100–350 g | Puncture resistance |
| Elmendorf tear machine/transverse direction | ASTM D1922 | 2–8 N/mm | Tear propagation resistance |
On conventional single-layer blown film lines, CIPLAS LLF1019F1 is processed with extruder barrel profiles that begin at 160–180 °C in the feed zone and advance to 190–210 °C at the adapter and die. A screw with a length-to-diameter ratio of 24:1–30:1 and a barrier or Maddock mixing section is used to homogenize the melt and disperse the additive package. Excessive shear heating should be avoided because nonuniform melt temperature can reduce film clarity and produce thickness variation. The die gap is conventionally set between 1.0 mm and 2.5 mm for blown film, with a blow-up ratio of 2.0:1–3.0:1. Frost line height is maintained between 6 and 10 die diameters to balance quench rate and film optics. For cast film, a flat die with a 0.5–1.0 mm die gap and chill roll temperatures of 20–35 °C are used. Melt temperature should not exceed 240 °C for extended periods; above this threshold, oxidative chain scission and gel formation can occur when the stabilizer package is not designed for high-temperature extrusion. If the resin has been stored at ambient relative humidity above 60% or under condensation conditions, drying with dehumidified air at 65 °C for 2–4 h is conventional before processing, although LLDPE is generally considered nonhygroscopic.
The seal initiation temperature in CIPLAS LLF1019F1 is governed primarily by density and comonomer distribution. In LLDPE, the linear backbone with short-chain branches permits melting and chain interdiffusion across the seal interface at a lower temperature than high-density polyethylene, but the exact value depends on comonomer level and molecular weight distribution. When compared with high-pressure LDPE, conventional Ziegler-Natta LLDPE often exhibits a broader melting distribution and may have a similar or slightly higher seal initiation temperature; however, seal strength after initiation rises more rapidly with temperature because of the higher molecular weight and linear chain structure. Seal initiation is also affected by film production conditions, particularly frost line height and die gap, which control crystal orientation and surface morphology. In practice, seal testing should follow ASTM F88 with a dwell time of 0.5–1.0 s and a jaw pressure of 0.3–0.5 MPa. Seal initiation temperature should be defined as the temperature at which a seal strength of 4.0 N/25 mm is reached. Lower density grades within the class, such as those at 0.918 g/cm³, typically initiate sealing below 105 °C; higher density grades may require 110 °C or more. Since published data for CIPLAS LLF1019F1 as a specific configuration is limited, the exact seal initiation temperature should be determined on the target film structure.
Mechanical performance of CIPLAS LLF1019F1 in film form is evaluated after conditioning for at least 40 h at 23 °C and 50% relative humidity according to ISO 291. Dart impact resistance according to ASTM D1709 is sensitive to film gauge, blow-up ratio, and frost line height. Thinner films require lower dart weights but higher normalized energy absorption. Elmendorf tear according to ASTM D1922 often shows directional anisotropy in blown film, with machine-direction tear and transverse-direction tear diverging as blow-up ratio increases. Tensile properties according to ISO 527-3 or ASTM D882 provide yield stress, break stress, and elongation at break; LLDPE films typically display high elongation at break and lower tensile modulus than HDPE. Puncture resistance may be measured by ASTM D5748 or by a probe puncture method under ASTM F1306. The actual values depend on film gauge and fabrication history; therefore, comparison between grades should be made only on films produced under equivalent conditions.
When CIPLAS LLF1019F1 is substituted for an autoclave LDPE in an existing blown film line, a reduction in melt strength is expected. Autoclave LDPE contains high levels of long-chain branching that stabilizes the bubble and permits high blow-up ratios without excessive thickness variation. LLF1019F1, as a linear resin, relies on molecular weight and crystallinity for bubble stability; therefore, the die gap may need to be opened and the blow-up ratio lowered to maintain bubble geometry. Output can be limited by bubble instability rather than extruder capacity. The benefit of replacement is downgauging: the higher tensile and tear resistance of LLDPE permits a reduction in film gauge while maintaining load-bearing performance. In addition, LLF1019F1 may exhibit lower gloss and higher haze than an autoclave LDPE at equivalent processing conditions unless an optimized frost line height and die lip finish are used. On high-speed form-fill-seal machines, hot tack may be superior to LDPE because of the LLDPE melting plateau and rapid crystallization under load, but published data for this specific configuration is limited.
Metallocene LLDPE grades typically exhibit a narrow composition distribution and a narrower molecular weight distribution than conventional Ziegler-Natta LLDPE. This yields lower extractables, improved optical properties, and lower seal initiation, but it can also reduce melt strength and increase extrusion pressure. CIPLAS LLF1019F1, if produced with a conventional Ziegler-Natta catalyst system, will have a broader composition distribution and may show higher dart impact at equivalent density but lower clarity and higher hexane extractables. Hot tack performance measured by ASTM F1921 or ASTM F2203 is affected by the ability of the film to maintain seal strength while the seal is still molten. Broader composition distribution can widen the hot tack window but may shift the seal initiation upward. Published catalyst and comonomer details for this specific configuration are limited, so the comparison should be verified on the intended film line. In blown film, a metallocene grade may require a lower melt temperature and a higher frost line to manage bubble stability, whereas CIPLAS LLF1019F1 may tolerate a wider operating window.
Primary application fields reported for film-grade LLDPE of this class include heavy-duty sacks, industrial liners, agricultural greenhouse film, stretch wrap, and lamination films. In heavy-duty sacks, the resin is often blended with HDPE or LDPE to modify stiffness and toughness. In agricultural film, a combination of UV stabilizers and anti-fogging additives is required; the base polymer should be selected for long-term weathering, and the final film should be tested for tensile retention after accelerated weathering according to ISO 4892-2. For lamination films, adhesion to substrates such as aluminum foil or biaxially oriented polypropylene is governed by the sealant layer formulation and corona treatment. Surface energy after inline corona treatment should be maintained above 38 mN/m and verified by ISO 8296. Downgauging is possible because tensile and puncture performance can be maintained at lower thickness than an equivalent LDPE film, but each end-use specification should define the minimum required dart impact and tear values.
| Regulatory domain | Standard or regulation | Application condition |
|---|---|---|
| European Union chemical registration | REACH Regulation (EC) No 1907/2006 | Article registration and candidate list verification |
| United States food contact | FDA 21 CFR 177.1520 | Conditions of use depend on film structure and food type |
| European Union food contact | EU Regulation 10/2011 | Overall migration limit 10 mg/dm² |
| Hazardous substance restriction | Directive 2011/65/EU | Cadmium 100 mg/kg and lead 1000 mg/kg in homogeneous material |
The resin is not recommended for continuous exposure to service temperatures above 80 °C, for direct contact with strong oxidizing acids, or for use in applications requiring clarity and gloss comparable to metallocene LLDPE without additional processing adjustment. Published data for this specific configuration is limited, and supplier regulatory documentation should be consulted before use in food-contact or medical packaging.