Ciplas Llf1019f Linear Low Density Polyethylene

CIPLAS LLF1019F Linear Low Density Polyethylene

    • Product Name: CIPLAS LLF1019F Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 100751
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Type 1-Butene
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Density 0.919 g/cm³
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800 %
    Dart Drop Impact 25 µm Film 120 g
    Elmendorf Tear Strength Md 25 µm Film 200 g
    Elmendorf Tear Strength Td 25 µm Film 400 g
    Haze 25 µm Film 12 %
    Gloss 45 25 µm Film 50

    As an accredited CIPLAS LLF1019F Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLF1019F Linear Low Density Polyethylene is supplied in 25 kg polyethylene-lined bags, palletized for convenient industrial handling and storage.
    Container Loading (20′ FCL) 20′ FCL container loaded with CIPLAS LLF1019F Linear Low Density Polyethylene, 25 kg bags, palletized and securely stowed for transport.
    Shipping CIPLAS LLF1019F Linear Low Density Polyethylene is shipped as non-hazardous resin pellets, typically in 25 kg polyethylene bags on pallets, stretch-wrapped and secured. Transport in clean, dry containers or trucks at ambient temperature. Protect from moisture, direct sunlight, heat, and contamination. No UN hazard class required.
    Storage Store CIPLAS LLF1019F Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible chemicals. Keep original containers or bags closed to prevent moisture, dust, and contamination. Palletize securely; avoid excessive stacking or pressure. Maintain ambient temperature and avoid prolonged exposure above recommended limits. Follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life 2 years from production date when stored in a cool, dry, well-ventilated place, away from direct sunlight and heat sources.
    Application of CIPLAS LLF1019F Linear Low Density Polyethylene

    Heavy-duty construction and demolition containment liners are converted from CIPLAS LLF1019F through a blown-film process in which the critical control point is not barrel temperature but die gap, bubble geometry, and frost-line position. CIPLAS LLF1019F, processed as a butene-based linear low-density polyethylene with a nominal melt flow rate in the 0.9–1.2 g/10 min range under ISO 1133-1:2022 at 190 °C and 2.16 kg, exhibits shear-thinning behaviour that is narrower than that of an LDPE homopolymer; die gaps below 1.8 mm on a 350 mm blown-film die therefore produce sharkskin on the outer bubble surface at outputs above 180 kg/h. The preferred die gap is 2.2–2.5 mm, blow-up ratio is held between 2.5:1 and 3.2:1, and frost-line height is maintained at 6–8 die diameters to stabilize the high-stalk bubble. The addition ratio for this segment is 85–100 wt% LLF1019F, 0–15 wt% LDPE homopolymer, and 1–4 wt% pre-dispersed carbon black or UV-shielding masterbatch; the LDPE fraction increases bubble stability and is not used as a primary viscosity modifier. Compliance is verified against ASTM D4635-16 for polyethylene film intended for general industrial application, ASTM D882-18 for tensile yield and break, ASTM D1709-16a Method A for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D1003-13 for haze after conditioning at 23 ± 2 °C and 50 ± 10% RH for 40 h. Downstream equipment on production-scale lines is documented as a single-screw grooved-feed extruder with L/D 30:1, barrier screw geometry, screen pack 80/120 mesh, and internal bubble cooling with chilled air at 8–12 °C; edge trim is re-pelletized in-line. Terminal finished products include temporary dust-containment sheeting, demolition debris bags, concrete curing film, and hazardous-particle abatement liners in thicknesses from 100 µm to 250 µm. Pre-drying at 70–80 °C for 2 h is required when ambient relative humidity exceeds 60% to remove granule surface moisture; this grade is not to be used for food-contact surfaces unless the full additive formulation is cleared under the relevant jurisdiction.

    Why Does Greenhouse Cover Film Demand a Narrow MFR Shift During Three-Layer Coextrusion?

    In three-layer agricultural blown-film lines, LLF1019F is placed in the core and the skin layers because its butene-branch distribution raises dart impact without the EVA-related acid migration observed on some greenhouse structures. The MFR shift is critical because a change from 1.0 g/10 min to 1.4 g/10 min at the die lowers head pressure by roughly 10–15% but simultaneously reduces bubble stability at a 2.8:1 blow-up ratio; published data for this specific configuration is limited, so the production window is confirmed by in-line melt-pressure and film-thickness scanning rather than by single-point rheology alone. Compliance under EN 13206:2017 for covering thermoplastic films used in agriculture and horticulture requires demonstration of tensile elongation at break and light transmission after accelerated weathering, with test methods referenced to ISO 527-3:2018 and ISO 4892-2:2013. The formulation addition ratio in the core layer is 65–75 wt% LLF1019F, 15–25 wt% LDPE, and 5–10 wt% process-stabilizer masterbatch; the external skin contains 70–80 wt% LLF1019F, 20–30 wt% LDPE, hindered amine light stabilizer at 0.3–0.8 phr, and UV absorber at 0.2–0.5 phr. The downstream process uses a 250–400 mm die with 1.5–2.0 mm die gap, internal bubble cooling, and a frost-line temperature maintained within ± 3 °C to prevent gauge bands; corona treatment is applied to 38–42 mN/m for later anti-drip or thermal coating. Terminal finished products include multi-season greenhouse covers, low-tunnel films, and anti-drip sheeting in thicknesses of 120–200 µm.

    Layer formulation distribution for three-layer agricultural film
    LayerLLF1019F loadingLDPE loadingAdditive loadingPrimary function
    External skin70–80 wt%20–30 wt%HALS 0.3–0.8 phr; UV absorber 0.2–0.5 phrUV shielding and slow degradation
    Core65–75 wt%15–25 wt%Process stabilizer masterbatch 5–10 wt%Impact and tear resistance
    Internal skin65–75 wt%25–35 wt%Anti-drip masterbatch 1–2 phrCondensate control

    Heavy-Duty Sack Film: Seal-Through-Fill Thresholds and Gusset Integrity

    The conversion of LLF1019F into heavy-duty sack film begins with a single-layer or coextruded blown-film line, where gusset integrity and seal-through-fill performance matter more than drawdown speed. Form-fill-seal sack lines running cement, mineral fillers, resin pellets, and dry pet food at fill speeds above 25 sacks/min require puncture and tear reserve at bottom-seal and valve-seal geometries. The formulation addition ratio is 85–90 wt% LLF1019F, 10–15 wt% LDPE, 2–4 wt% anti-block masterbatch based on diatomaceous earth or synthetic silica, and 0.5–1.0 wt% slip masterbatch. Downstream conversion uses gusseted blown film with a die gap of 1.8–2.2 mm, blow-up ratio of 2.8:1–3.5:1, and surface treatment to 38–42 mN/m for flexographic or rotogravure printing. Seal integrity is validated by ASTM F88/F88M-21 for seal strength, ISO 7765-1:1988 for impact resistance, and ASTM D882-18 for tensile properties; packaging waste compliance is checked against EU Directive 94/62/EC, with the sum of lead, cadmium, mercury, and hexavalent chromium below 100 ppm by weight. Terminal finished products include gusseted valve sacks for cement and fine powders, open-mouth sacks for resin pellets, and pinch-bottom sacks for pet food and feedstuffs in thicknesses from 80 µm to 150 µm. An operational boundary is that anti-block additions above 4 wt% increase haze and reduce seal strength, while post-industrial recycled film containing more than 0.5 wt% polypropylene contamination creates gel specks on the seal bar.

    Extrusion lamination of reverse-printed barrier webs with LLF1019F as the sealant layer shifts the critical control point from optical clarity to hot-tack and seal-through-contamination performance. The polymer is applied at 80–100 wt% LLF1019F with 0–20 wt% LDPE to adjust draw-down, and 1–2 wt% anti-block masterbatch only where the lamination is destined for high-speed vertical form-fill-seal lines. Air gap is set between 150 mm and 250 mm on 2.5–3.5 m wide tandem extrusion-lamination lines; melt temperature at the die is held between 280 °C and 320 °C, and line speed is governed by adhesion to the reverse-printed web rather than by polymer output. Terminal finished articles include dry-food pouches, stand-up pouch sealant plies, lidding webs for membrane-sealed cups, and non-retort snack wrappers. For food-contact use, the formulation must comply with FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011, including overall migration below 10 mg/dm² under the assigned food simulant; non-food industrial laminations are governed by ASTM F1249-20 for water-vapour transmission rate. The product alone provides no oxygen barrier and is not suitable for retort or high-acid fills unless a barrier layer is present and migration testing is completed on the finished structure.

    Compliance checklist for LLF1019F lamination sealant web
    ReferenceRequirementTest condition or methodAcceptance criterion
    FDA 21 CFR 177.1520(c)Olefin polymer clearanceUse conditions E–GComplies with applicable food types
    EU Regulation (EU) No 10/2011Overall migrationFood simulants A/B/C/D1, 10 days at 40 °C≤ 10 mg/dm²
    ASTM F1249-20Water vapour transmission rate38 °C, 90% RHAs specified by package structure

    When Pallet Hood Film Replaces Polyester Strapping in High-Stack Warehousing

    The primary process deviation in pallet-hood film production is the intentional rise in blow-up ratio to 3.5:1–4.5:1, above the packaging-film optimum, to redistribute orientation toward the transverse direction and raise dart impact. LLF1019F is compounded at 75–85 wt% with 15–25 wt% LDPE and 1–3 wt% anti-block masterbatch; slip is kept below 0.5 wt% because excessive surface slip reduces pallet stabilization after heat shrinking. The downstream process uses a high-stalk bubble with internal cooling, gusseted tubular film cut to pre-determined layflat widths, and impulse or continuous heat sealing to form hoods. Compliance references include ASTM D4649-20 for selection and use of stretch wrap materials, ASTM D5748-95 for protrusion puncture resistance, ASTM D5458-95 for cling, and ASTM D2732-20 for unrestrained linear thermal shrinkage. Terminal products are pallet hoods, top covers, and anti-slip unitization films for high-stack warehouse storage in thicknesses 80–150 µm. The operational boundary is that film below 80 µm exhibits corner-protrusion failure when tested under ASTM D5748-95 at 23 °C; published data for this specific configuration is limited, so each pallet geometry and shrink-tunnel profile should be trial-validated before full-scale rollout.

    Free Quote

    Competitive CIPLAS LLF1019F Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    CIPLAS LLF1019F Linear Low Density Polyethylene is a pelletized polyolefin resin positioned for blown film extrusion and, in thinner constructions, cast film conversion. The grade identifier contains a film suffix, which in standard LLDPE nomenclature denotes a film-grade product rather than a rotational molding or injection molding material. Because the manufacturer’s certificate of analysis controls lot-to-lot density, melt flow rate, comonomer type, and additive loading, processors should not consider the present class-level discussion a substitute for the lot-specific specification sheet. Published data for this specific configuration is limited; the following sections therefore distinguish product-specific requirements from the broader Ziegler-Natta or metallocene LLDPE film class when the supplier’s published data is unavailable.

    Specification and acceptance testing for a LLF1019F-grade film resin typically includes density, melt flow rate, tensile properties, optical properties, and impact resistance. Density is determined by ASTM D1505 density-gradient column or ISO 1183; melt flow rate is determined by ASTM D1238 at 190 °C with 2.16 kg. Film tensile properties are measured on specimens prepared under controlled blown film conditions, typically 25 mm width and 50 mm gauge length, using ASTM D882 at a crosshead speed of 500 mm/min. Elmendorf tear is reported for machine direction and transverse direction under ASTM D1922; dart impact is reported under ASTM D1709 Method A using a 38 mm diameter dart and 660 mm drop height. Optical haze and gloss are tested under ASTM D1003 Procedure A and ASTM D2457 at 60°. The Vicat softening point, when required for thermal resistance, is measured under ASTM D1525 with a 10 N load and 120 °C/h heating rate; melting peak temperature is measured by differential scanning calorimetry under ASTM D3418 or ISO 11357-3 at 10 °C/min. None of these values should be converted from one specimen geometry to another without recognizing that orientation, thickness, and cooling rate alter the result.

    Why Does Melt Index and Melt Temperature Control Set the Practical Extrusion Window?

    In blown film conversion, the practical extrusion window is governed by the pairing of melt flow rate and melt temperature. For LLDPE film grades in the class represented by CIPLAS LLF1019F, a melt index range of 0.8–2.0 g/10 min under ASTM D1238 at 190 °C with 2.16 kg is typical for the broader film class, although the lot-specific value may be narrower. On a production extruder—commonly a grooved-feed single-screw unit with L/D between 24:1 and 30:1 and a barrier screw—the melt temperature is maintained between 180 °C and 220 °C. Below 180 °C, melt pressure increases and the risk of sharkskin melt fracture on the die lip becomes significant; above 240 °C, oxidative degradation can produce gels and off-odor. The permissible thermal window on a given die can be as narrow as 5–10 °C when running a high-shear spiral mandrel die with a die gap of 1.8–2.5 mm. Blow-up ratio is normally held at 2.0–3.0, and the frost line is positioned to produce a stable neck without excessive stalk resonance. These parameters are not cosmetic; they determine bubble contact angle at the air ring, gauge uniformity, and the orientation balance that controls Elmendorf tear under ASTM D1922.

    Density, Comonomer Type, and Tear-Resistance Hierarchy in LLF1019F-Class Resins

    The nominal density class for a film-grade LLDPE of this type is typically between 0.915 g/cm³ and 0.925 g/cm³ when measured according to ASTM D1505. Density is not a single-value quality parameter; it correlates with crystallinity and therefore with stiffness, tensile yield stress, and permeability. A butene-based LLDPE at 0.918 g/cm³ generally exhibits lower dart impact under ASTM D1709 Method A than a hexene- or octene-based copolymer at the same density and melt index, because the longer comonomer branches more effectively generate tie chains between lamellae. The result is a tear-resistance hierarchy: octene > hexene > butene, with lower seal initiation temperature in the more linear copolymers. The suffix F in LLF1019F does not independently disclose the comonomer type; the manufacturer’s specification or lot certificate is required to establish whether the grade is butene- or hexene-based.

    Representative published ranges for the broader Ziegler-Natta LLDPE film class, LDPE autoclave film class, and metallocene hexene LLDPE are shown in the following matrix. These are not lot-specific CIPLAS LLF1019F values.

    PropertyZiegler-Natta LLDPE film classLDPE autoclave film classmLLDPE hexene film classTest method
    Density0.915–0.925 g/cm³0.917–0.930 g/cm³0.912–0.920 g/cm³ASTM D1505 / ISO 1183
    Melt index0.8–2.0 g/10 min0.2–2.0 g/10 min0.5–2.0 g/10 minASTM D1238 / ISO 1133-1
    Dart impact100–250 g50–120 g>300 gASTM D1709 Method A
    Elmendorf tear MD150–400 g50–150 g250–500 gASTM D1922
    Haze5–15%3–8%2–5%ASTM D1003
    Seal initiation temperature95–110 °C105–120 °C85–100 °CASTM F1921

    Line conversion from an LDPE autoclave grade to a Ziegler-Natta LLDPE film resin of the LLF1019F class is not a drop-in substitution. The LLDPE melt typically has lower melt strength and higher shear viscosity at equivalent ASTM D1238 melt index, which increases extruder motor load and can require a die gap increase from 1.0–1.2 mm to 1.8–2.5 mm. Bubble stability is often recovered by blending 10–30 wt% LDPE or by using a dual-lip air ring with higher internal air pressure. The benefit appears in downgauged structures: an LLDPE-rich film at 25 µm can provide dart impact comparable to or better than an LDPE film at 50 µm under ASTM D1709, but the quantitative result depends on comonomer type, frost line height, and orientation. Converters should not attribute haze or gloss differences solely to resin; surface roughness from die lip deposits and air ring turbulence can shift ASTM D1003 haze by several percentage points without any change in the resin.

    For heavy-duty sack, industrial liner, and agricultural silage film applications, the film-grade LLDPE class represented by CIPLAS LLF1019F is used in thicknesses determined by puncture and tear requirements. Heavy-duty sack applications exploit the impact strength and Elmendorf tear resistance of LLDPE-rich films at 80–150 µm thickness. Industrial liners often use 50–100 µm LLDPE or LLDPE/LDPE blends where puncture resistance is required. Agricultural silage film uses a 25–70 µm structure and requires UV stabilization; the selection of hindered amine light stabilizers must be verified with the film producer because outdoor exposure performance depends on additive package and film thickness. In lamination sealant layers, the LLDPE film is often 20–50 µm thick and combined with biaxially oriented PET or BOPP; seal strength is evaluated under ASTM F88 and hot tack under ASTM F1921.

    When Seal Initiation Temperature and Hot Tack Force Become Limiting Parameters

    In form-fill-seal packaging, the conversion performance of an LLDPE-rich sealant web is controlled by seal initiation temperature, hot tack force, and ultimate seal strength. LLDPE film-class resins typically exhibit seal initiation values in the range 95–110 °C when tested according to ASTM F1921 at a dwell time of 0.5 s and pressure of 275 kPa; in comparison, LDPE seal initiation is often 105–120 °C. Hot tack becomes the limiting parameter when a machine cycle requires the seal to hold before crystallization is complete. Hexene-based LLDPE grades usually deliver a wider hot tack window than butene-based grades at equivalent melt index and density. For CIPLAS LLF1019F, the sealing window cannot be established from the grade name; the supplier’s technical data sheet or a sealing curve generated on the intended packaging line is required. If the resin is used as a food-contact sealant layer, compliance with FDA 21 CFR 177.1520(c) or EU No 10/2011 must be verified on the finished article under the intended food-simulant conditions. Grade-level compliance statements do not address adhesive, ink, or coating migration.

    Compared with metallocene-catalyzed hexene LLDPE, a conventional Ziegler-Natta film-grade resin of the LLF1019F class generally has a broader molecular weight distribution, which lowers extruder head pressure and improves bubble stability but reduces dart impact and clarity at equal film thickness. A metallocene hexene film at 25 µm can show ASTM D1709 dart impacts above 300 g and ASTM D1003 haze below 5%, whereas the conventional LLDPE class may require a thicker web to meet the same dart requirement. Compared with HDPE, the LLDPE class exhibits lower modulus and lower moisture vapor barrier but substantially higher Elmendorf tear and puncture resistance under ASTM D1922 and ASTM D5748. The appropriate replacement decision is therefore application-specific: down-gauging thin films generally favors metallocene LLDPE; heavy-duty sacks and liners requiring process robustness often favor broader-MWD Ziegler-Natta LLDPE or LLDPE/LDPE blends.

    Regulatory Submission Requires Lot-Specific Migration Data, Not Generic Class Statements

    For packaging-grade polyethylene, regulatory acceptance is article-based. A resin may be manufactured under conditions that permit a supplier to issue a food-contact declaration under FDA 21 CFR 177.1520(c), but the declaration is limited by the specified density range, additive loading, and end-use extraction limits. Under EU No 10/2011, overall migration must not exceed 10 mg/dm² of food-contact surface area when tested with the prescribed food simulants; specific migration limits apply to additives and monomers. A converter cannot rely on the resin grade name alone when the finished structure includes recycled layer material, printing inks, or adhesives. REACH Regulation (EC) No 1907/2006 imposes communication obligations for substances of very high concern above 0.1% w/w in articles, and RoHS Directive 2011/65/EU restricts lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE when the material is incorporated into electronic equipment. The matrix below summarizes the documentation boundary.

    RequirementScopeAcceptance basisBoundary
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactASTM D1238 density and extraction limits; finished articleGrade declaration not sufficient for final article
    EU No 10/2011Plastic materials and articles in food contactOverall migration <10 mg/dm²; specific migrationRequires simulant testing on finished structure
    REACH Regulation (EC) No 1907/2006SVHC communicationArticle 33; 0.1% w/w thresholdApplies to articles, not raw resin as supplied
    RoHS Directive 2011/65/EURestricted substances in EEEXRF or wet chemistry for Pb, Hg, Cd, Cr(VI), PBB, PBDEOnly when incorporated into electrical/electronic equipment

    Storage and handling boundaries for the LLF1019F-class resin follow standard LLDPE practice but require discipline in humid plants. The pellets are not hygroscopic, yet surface condensation on cold pellets transferred into a warm production area can introduce moisture into the feed throat at relative humidities above 60%; purging hoppers with dry air or extended residence at ambient conditions is necessary. Reprocessing of trim and edge scrap should be controlled because LLDPE rheology and gel formation are sensitive to oxidative history. Oxidative induction time can be evaluated by ASTM D3895 to detect antioxidant depletion in regrind stored for extended periods. Melt temperature should not exceed 250 °C; at higher temperatures, chain scission produces volatile compounds and surface defects on the film.

    Top