Ciplas Llf1019b Linear Low Density Polyethylene

CIPLAS LLF1019B Linear Low Density Polyethylene

    • Product Name: CIPLAS LLF1019B Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 999788
    Polymertype Linear Low Density Polyethylene
    Comonomer Butene-1
    Density 0.919 g/cm³
    Meltflowrate 0.9 g/10 min at 190°C/2.16 kg
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 700%
    Flexuralmodulus 250 MPa
    Dartdropimpact 100 g
    Elmendorftearstrengthmd 150 g
    Elmendorftearstrengthtd 300 g
    Haze 12%
    Gloss 55%
    Meltingpoint 123°C
    Vicatsofteningpoint 96°C
    Brittlenesstemperature -70°C
    Coefficientoffriction 0.2
    Antioxidant Yes
    Slipagent No
    Antiblockagent No

    As an accredited CIPLAS LLF1019B Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLF1019B Linear Low Density Polyethylene supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with CIPLAS LLF1019B Linear Low Density Polyethylene, 25 kg bags, palletized, stretch-wrapped, and secured for transport.
    Shipping CIPLAS LLF1019B Linear Low Density Polyethylene is shipped as non-hazardous polymer pellets, usually in 25 kg PE bags or bulk bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks; protect from moisture, contamination, direct sunlight, and excessive heat. No special dangerous goods handling required.
    Storage Store CIPLAS LLF1019B Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and oxidizing agents. Keep bags or containers closed to prevent moisture and contamination. Store at ambient temperature, protected from weather. Avoid prolonged UV exposure and excessive stacking. Use clean, dry handling equipment and maintain good housekeeping to minimize dust and static hazards.
    Shelf Life Stable under normal storage conditions; no specific shelf life if kept cool, dry, protected from direct sunlight and ignition sources.
    Application of CIPLAS LLF1019B Linear Low Density Polyethylene

    On high-stalk blown film lines producing heavy-duty industrial liners for construction debris, mineral concentrates, and chemical packaging, CIPLAS LLF1019B is processed through a grooved-feed single-screw extruder with an L/D ratio of 30:1 to 36:1. Barrel temperatures are set in a rising profile from 180°C at the feed throat to 230°C at the metering zone, with the adapter maintained at 225°C and the die kept between 225°C and 235°C. The die gap is set at 1.8 mm to 2.3 mm, and the blow-up ratio is held between 2.0:1 and 3.0:1. A high-stalk configuration with the frost line placed high above the die provides the melt relaxation required for tensile property development. Plant audits record output instability when the die gap is reduced below 1.8 mm because the pressure drop across the die lip increases rapidly and edge melt fracture appears on the collapsing frame. A slip/antiblock masterbatch is dosed at 1.0 wt% to 3.0 wt% at the throat, with erucamide concentrations typically held at 500 ppm to 1,000 ppm and synthetic silica antiblock at 1,000 ppm to 3,000 ppm. The coefficient of friction is measured per ASTM D1894 to maintain a range of 0.20 to 0.35 for liner stacking and insertion. Dart impact energy is recorded per ASTM D1709 Method A or B depending on film thickness; tensile properties are measured per ASTM D882 and tear resistance per ASTM D1922. Pre-drying is not required at ambient relative humidity below 60%, but pellets stored outdoors with visible surface moisture should be passed through a hopper dryer at 70°C to 80°C for 1 h to 2 h to prevent surface defects and screw feed slippage. The addition of recycled LDPE above 20 wt% without melt homogeneity verification is not recommended because low-temperature dart impact at −20°C can decline sharply. Additives containing free amines should be avoided in high-temperature processing because of odour and possible organoleptic failures in liners used for food-contact secondary packaging. The following processing window is used as a start-up reference after die and screw cleaning.

    ParameterStart-up setpointOperating rangeMonitoring reference
    Extruder L/D ratio32:130:1 to 36:1Gearbox nameplate and screw drawing
    Zone 1 temperature180°C170°C to 190°CHead pressure recorder and melt thermocouple
    Zone 2–3 barrel temperature210°C200°C to 220°CBarrel zone thermocouples
    Adapter and die temperature230°C225°C to 235°CDie body thermocouple
    Die gap2.0 mm1.8 mm to 2.3 mmFeeler gauge after die cleaning
    Blow-up ratio2.5:12.0:1 to 3.0:1Layflat width check
    Frost line height8 die diameters6 to 10 die diametersVisual marker on collapsing tent
    Output70 kg/h60 kg/h to 80 kg/hGravimetric feeder calibration

    Why Does Cast Stretch Film Require a Narrower Molecular Weight Distribution Than Blown Film?

    Cast stretch film lines using LLF1019B in a core or monolayer hand-wrap construction operate with a flat die gap of 0.5 mm to 1.0 mm and a melt temperature of 240°C to 275°C at the die exit. The draw from the die lip to the chill roll is accompanied by neck-in and edge bead formation, both of which are governed by the resin's melt flow ratio rather than melt index alone. The I21.6/I2.16 melt flow ratio is measured per ASTM D1238 or ISO 1133-1:2022; published data for this specific configuration is limited, and converters compare the value against an established line reference resin before stringing the line. Chill roll temperature is controlled at 15°C to 25°C; temperatures below 10°C produce condensation-related optical defects, while temperatures above 30°C reduce quench rate and increase blocking on the winder. Polyisobutylene cling agent is injected at 0.5 wt% to 2.0 wt% directly into the barrel; direct dry blending of high-viscosity PIB into the feed throat causes screw slip and output fluctuation. Machine-side problems include cling-agent plating on the chill roll, and roll cleaning intervals shorten from 72 h to 24 h when PIB dosage exceeds 2.0 wt%. Cling force is tested per ASTM D5458 after conditioned storage at 23°C and 50% relative humidity for 24 h. Dart impact for cast stretch film is not normally used as a specification; tensile properties per ASTM D882 and tear resistance per ASTM D1922 provide the lot-control data. Film thickness from 12 µm to 25 µm is measured per ASTM D2732. At the die, edge deckle widths are expanded by 15% to 25% per side to compensate for neck-in before edge trim. If the film is used for food-contact hand wrap, the formulation must comply with FDA 21 CFR 177.1520(c) 3.1a or 3.2a and EU Regulation (EU) No 10/2011; no claim of compliance should be made for a finished structure without migration testing specific to the cling additive package.

    Agricultural Silage Barrier Film and UV Stabilizer Loading Limits

    Agricultural silage film conversion routes use three-layer blown film dies with an outer layer containing a hindered amine light stabilizer package. HALS loading is maintained at 0.2 wt% to 0.8 wt%, UV absorber at 0.1 wt% to 0.3 wt%, and titanium dioxide at 3 wt% to 6 wt% when a white opaque outer layer is specified. The die gap is set at 1.8 mm to 2.2 mm, blow-up ratio at 2.0:1 to 2.5:1, and melt temperature at 190°C to 210°C. High TiO₂ loading raises melt viscosity and accelerates screen pack pressure build-up; backflush filter units are mounted upstream of the die to reduce die-lip deposit formation. Tensile properties are measured per ISO 527-3, tear resistance per ISO 6383-2, and dart drop impact per ISO 7765-1. Weathering resistance is evaluated by tensile retention after accelerated exposure per ISO 4892-2; published data for this specific configuration is limited, and outdoor exposure trials under the intended silage storage period are required before commercial specification. Direct contact with fermented silage leachate can extract stabilizers and accelerate embrittlement; sulfur-containing fumigants and halogenated disinfectants must not be stored in contact with unstabilized film. The film is not recommended as a direct seal for silage stacks unless the outer stabilizer layer is maintained at a minimum thickness of 25 µm to reduce migration of additives into the barrier layer. Batch-to-batch variance in TiO₂ dispersion is measured by screen pack pressure differential and film gel count per ASTM D3351 or an inline optical gel counter.

    When LLF1019B is used as an extrusion coating sealant layer on woven polypropylene sacks, aluminium foil, and paper-based sachets, the melt temperature is raised to between 280°C and 320°C because low melt temperature produces poor adhesion and excessive neck-in at the die lips. The flat die gap is set at 0.4 mm to 0.6 mm, the air gap between die lip and chill roll is maintained at 100 mm to 200 mm, and the chill roll surface temperature is controlled at 10°C to 20°C. Coat weights between 12 g/m² and 30 g/m² are typical for sealant layers. Polymer film substrates require corona discharge treatment to 40 dyn/cm to 42 dyn/cm immediately before coating; aluminium foil adhesion depends on the primer or anchor coat rather than on the polyethylene alone. Heat seal initiation temperature for butene-copolymer LLDPE coatings is typically between 90°C and 105°C; seal strength is tested per ASTM F88/F88M after the coated structure is converted into sachets or pouches. Neck-in at the die edges is compensated by increasing deckle width by 15% to 25% per side before edge trim. If the extruder is operated above 320°C, oxidative gel particles form in the melt and deposit on the die lip, leading to coating streaks and uncoated lanes. The melt temperature and residence time should therefore be recorded continuously; a shift of more than 5°C at the die lip relative to centre-line should trigger die heater inspection. Compliance of the finished food-contact structure is governed by FDA 21 CFR 177.1520(c) 3.1a or 3.2a and EU Regulation (EU) No 10/2011; migration testing must be conducted on the final laminate because coatings and primers contribute to overall extractives. The following matrix lists the mechanical and regulatory evaluation points for extrusion-coated structures.

    Evaluation pointStandard designationConditionData requirement
    Melt mass-flow rateISO 1133-1:2022 / ASTM D1238190°C, 2.16 kgLot acceptance
    Coating thicknessASTM D273212 g/m² to 30 g/m² converted to µmLine record
    Seal strengthASTM F88/F88MSeal dwell 1 s, 0.5 MPaMinimum seal integrity
    T-peel adhesionASTM D1876Crosshead speed 254 mm/minLaminate adhesion value
    Food-contact resin statusFDA 21 CFR 177.1520(c)3.1a / 3.2aSupplier letter
    EU food-contact statusEU 10/2011Overall migrationMigration test on final laminate

    When Thin-Wall Container Moulding Replaces Blown Film Conversion

    The injection moulding route for LLF1019B is constrained by the resin's low melt flow and high shrinkage relative to high-flow HDPE. The process is appropriate only when the cavity wall thickness exceeds 1.2 mm; thin-wall containers with wall sections below 0.8 mm usually require a higher-flow grade to prevent short shots and high clamp force demand. Barrel temperatures are set from 180°C to 230°C, with the nozzle held at 220°C and the mould surface temperature maintained between 10°C and 40°C. Injection speed is set at 50 mm/s to 150 mm/s, holding pressure at 30 MPa to 60 MPa, and back pressure at 5 MPa to 10 MPa. Linear mould shrinkage is recorded per ASTM D955 at 1.5% to 2.5%; this is higher than HDPE and requires tooling allowance in the cavity dimensions. Tensile properties are measured per ASTM D638 Type IV at 50 mm/min, flexural modulus per ASTM D790, and notched Izod impact per ASTM D256. Warpage at gate bosses and ejector pin marks are recorded when holding pressure exceeds 60 MPa or when the gate freezes before packing is complete. The processing window is narrow for closures with deep draw ratios because the resin's low crystallinity retards dimension stability after demoulding. A mould release agent may be used at 0.1 wt% to 0.3 wt%, but excessive release agent migrates to the surface and reduces print adhesion. Processors should verify the melt temperature at the nozzle with a needle pyrometer; a drop below 180°C increases injection pressure and gate freeze-off risk.

    Rotomoulding of Intermediate Bulk Container Liners Demands a Different Thermal Profile

    After LLF1019B pellets are ground to a 35-mesh (500 µm) powder and dry-blended with a carbon black masterbatch at 0.5 wt% to 1.0 wt% for UV protection, the mould is rotated in an oven at 260°C to 300°C. The peak internal air temperature is held at 190°C to 210°C for 20 min to 40 min depending on wall thickness. Rotation ratio is set at 4:1 to maintain uniform wall coverage; pinholes along the parting line are observed when the peak internal air temperature remains below 185°C. Demoulding is conducted at 70°C to 80°C to minimise distortion. The butene-copolymer structure of the resin provides a lower environmental stress crack resistance than hexene or octene copolymers; for diesel or surfactant storage, ASTM D1693 Condition C in 10% Igepal should be reviewed before specification. Tensile properties are measured per ASTM D638, flexural modulus per ASTM D790, and low-temperature impact per ASTM D256 at −40°C for cold-weather liner service. The powder must be dried to below 0.05 wt% moisture before charging; surface moisture causes steam pinholes and delamination at the inner wall. Published data for this specific configuration is limited, and field trials with the actual mould geometry and service chemical are required to confirm long-term retention of mechanical properties.

    Free Quote

    Competitive CIPLAS LLF1019B Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    CIPLAS LLF1019B Linear Low Density Polyethylene is a pelletized linear low-density polyethylene grade intended for thin-gauge blown and cast film conversion. A procurement-grade technical profile must be extracted from the manufacturer’s lot release certificate and safety data sheet; the following text positions the grade within class-level LLDPE film extrusion boundaries and identifies the values that require verification before insertion into a qualified production specification. Published data for the specific CIPLAS LLF1019B configuration is limited, so class ranges are presented only where they are supported by ISO and ASTM test designations.

    Material Identity and Grade Designation Logic

    Under polyolefin producer nomenclature, the prefix “LL” denotes linear low-density chemistry, while the “F” position commonly indicates film-grade rheology. The numeric sequence “1019” can correspond to a nominal melt mass-flow rate of 1.0 g/10 min and a nominal density of 0.919 g/cm³, but this decoding is not a substitute for certificate-of-analysis values. The final letter may identify the antioxidant package, slip/antiblock level, or comonomer generation. If the grade is butene-based, class-level dart impact and Elmendorf tear are typically lower than for hexene- or octene-based LLDPE at equivalent density and MFR. Because the comonomer type is not declared in the available public designation, the end-use specification must verify whether the product meets high-dart or high-tear requirements under ASTM D1709-16ae2 and ASTM D1922-23.

    Substitution of CIPLAS LLF1019B for a general-purpose autoclave LDPE in a blown-film line without adjustment of die gap, haul-off, and frost-line height is not recommended because the linear backbone produces lower melt strength and a different strain-hardening response. In contrast to high-pressure branched LDPE, LLDPE film grades typically exhibit higher solid-state tensile and puncture resistance at equivalent thickness. Class-level LLDPE film values include tensile strength at break from 20 MPa to 45 MPa under ISO 527-3:2018, elongation at break above 400 %, and dart impact values in the 80 g to 250 g range at 25 µm under ASTM D1709-16ae2. Compared with a conventional HDPE film grade, LLF1019B-class resin is expected to provide lower stiffness but higher tear and impact resistance, making it more suitable for down-gauged flexible packaging than for rigid thermoformed trays.

    What Limits Melt Fracture Onset in LLF1019B Film Extrusion?

    On blown-film lines equipped with a 25:1 L/D to 30:1 L/D single-screw extruder and a spiral mandrel die with a 1.5 mm to 2.5 mm die gap, melt fracture onset is governed by wall shear stress at the die lip. For linear low-density film grades with a nominal melt mass-flow rate near 1.0 g/10 min, production lines typically reach throughput constraints when die pressure exceeds 35 MPa to 45 MPa; the exact threshold must be measured on the specific line. Barrel settings from 180 °C at the feed throat to 220 °C at the die are typical, but melt temperature must not exceed 250 °C to limit oxidation-induced gel formation. Surface condensation can introduce moisture-related bubble defects when pellets are stored at relative humidity above 60 %, so hopper feeding under dry-air purge or short residence time is recommended. Cross-contamination with polypropylene scrap above 2 wt% may create discrete domains that increase visible gel counts and reduce dart impact under ASTM D1709-16ae2.

    Mechanical and Thermal Property Windows for LLF1019B-Class Film Resins

    The table presents class-level property windows reported for general-purpose LLDPE film grades; it does not constitute a certificate of analysis for CIPLAS LLF1019B.

    Property Test Method LLDPE Film Class Range LDPE Film Class Range HDPE Film Class Range
    Density ISO 1183-1:2019 0.915–0.930 g/cm³ 0.917–0.930 g/cm³ 0.940–0.965 g/cm³
    Melt mass-flow rate 190 °C/2.16 kg ISO 1133-1:2022 0.5–2.0 g/10 min 0.2–2.0 g/10 min 0.1–1.2 g/10 min
    Tensile strength at break, 25 µm film ISO 527-3:2018 20–45 MPa 10–25 MPa 25–40 MPa
    Elongation at break, 25 µm film ISO 527-3:2018 400–800 % 100–600 % 300–700 %
    Dart impact at 25 µm ASTM D1709-16ae2 80–250 g 50–150 g 60–150 g
    Elmendorf tear, MD/TD at 25 µm ASTM D1922-23 100–400 gf 50–250 gf 80–300 gf
    Vicat softening temperature, A50 ISO 306:2013 90–110 °C 85–100 °C 120–130 °C

    Because the specific certificate of analysis for CIPLAS LLF1019B is not publicly reproduced here, the table is a class-level screening reference. A converter must replace the ranges with lot-specific values before setting barrel profiles, die gaps, and haul-off ratios.

    Blown-film equipment with internal bubble cooling and dual-lip air rings is commonly used for heavy-duty sacks, agricultural silage film, and carrier bags. The class-specific balance of dart impact and tear resistance enables down-gauging from 50 µm to 35 µm in some structures without dropping dart impact below 100 g under ASTM D1709-16ae2, but this trade-off must be confirmed on the film line because gauge variation above ±5 % across the web will dominate film failure. For cast film, chill-roll temperatures between 18 °C and 30 °C and a 0.5 mm to 1.0 mm die gap are common starting points, with drawdown ratios adjusted until the desired gauge profile and tensile isotropy are achieved.

    When Hexene or Octene Comonomer Distinguishes LLF1019B from Butene-Only LLDPE Film Grades

    If CIPLAS LLF1019B is produced with hexene or octene comonomer, it differs from butene-only LLDPE by a more uniform short-chain branch distribution; this increases dart impact at identical density and MFR under ASTM D1709-16ae2 and improves Elmendorf tear under ASTM D1922-23. Butene-based LLDPE often exhibits lower extrusion head pressure due to lower high-shear viscosity but may show lower puncture resistance under ASTM D5748-19. At a density of 0.919 g/cm³, the resin is in the medium-low density segment where the branch distribution—not density alone—controls the balance between stiffness, hot-tack, and tear propagation. Converters replacing a metallocene LLDPE with a Ziegler-Natta LLF1019B-class resin should compare seal initiation temperature and hot-tack force on the target film structure because catalyst and comonomer differences can shift the sealing window by more than 5 °C in some cases.

    Regulatory Conformance Pathways for LLF1019B Film Resin

    For food-contact applications, the resin must be compliant under FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation 10/2011 with specific migration limits for total migration of 10 mg/dm² according to EN 1186-1:2002 and subsequent parts. Electrical and heavy-metal requirements may be evaluated under RoHS Directive 2011/65/EU and the REACH SVHC candidate list, but the final article—not only the resin—must be tested for non-intentionally added substances under Regulation 10/2011 Article 19. Because additive packages vary, a written compliance statement from the producer is required before using LLF1019B in direct food contact. Incompatible additive combinations include unsaturated fatty acid amide slip agents above 500 ppm in high-temperature extrusion when organoleptic performance is critical; such systems can increase taste and odor transfer under EN 1186-2:2002.

    For packaging lines converting CIPLAS LLF1019B into collation shrink film, the limiting factor is not tensile strength but seal initiation temperature and hot-tack force, which must be measured on a JIS K 7127 or ASTM F1921-12 hot-tack tester before line speed is set. Published data for this specific configuration is limited, so the converter must replace class-level ranges with lot-specific results before enabling automatic gauge control or wide-spec film qualification.