Ciplas Lle1018f2 Linear Low Density Polyethylene

CIPLAS LLE1018F2 Linear Low Density Polyethylene

    • Product Name: CIPLAS LLE1018F2 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 543493
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 240 MPa
    Dart Drop Impact 110 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 350 g
    Haze 13%
    Gloss 45 55
    Coefficient Of Friction 0.2

    As an accredited CIPLAS LLE1018F2 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLE1018F2 Linear Low Density Polyethylene is packaged in 25 kg moisture-resistant paper bags, palletized and shrink-wrapped for industrial handling.
    Container Loading (20′ FCL) CIPLAS LLE1018F2 Linear Low Density Polyethylene loaded in 20′ FCL containers, 25 kg bags, palletized and secured for safe transport.
    Shipping CIPLAS LLE1018F2 LLDPE is shipped as non-hazardous polymer pellets in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry, covered containers or trucks at ambient temperature, avoiding moisture, direct sunlight, heat, and contamination. Follow standard warehouse storage and handling practices.
    Storage Store CIPLAS LLE1018F2 Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep bags or containers tightly closed, clean, and palletized off the floor. Avoid moisture, static buildup, and prolonged UV exposure. Prevent dust accumulation; use grounding where required. Follow manufacturer/SDS guidance and local regulations. No smoking.
    Shelf Life CIPLAS LLE1018F2 typically has a 12-month shelf life when stored cool, dry, and away from direct sunlight in original packaging.
    Application of CIPLAS LLE1018F2 Linear Low Density Polyethylene

    CIPLAS LLE1018F2 Linear Low Density Polyethylene is a butene-copolymer film resin with nominal melt flow rate of 1.0 g/10 min per ISO 1133-1:2022 at 190 °C under 2.16 kg load and nominal density of 0.918 g/cm³ per ISO 1183-1:2019. The F2 designation corresponds to a slip/antiblock additive package formulated for controlled coefficient of friction in thin-gauge films. The molecular architecture incorporates short-chain branching from butene comonomer insertion, producing a melt flow ratio I21.6/I2.16 in the range of 25 to 28 when the high-load melt index is determined under the same standard. Downstream conversion sectors for this grade span blown film extrusion, cast film extrusion, coextrusion, extrusion lamination, flat-die sheet extrusion, and masterbatch compounding.

    Agricultural mulch film produced from LLE1018F2 at 15 µm to 30 µm gauge on single-layer blown film lines with barrier screws of 30:1 to 33:1 L/D operates at melt temperatures between 190 °C and 210 °C. Bubble stability is maintained at blow-up ratios from 1.8:1 to 2.5:1 without internal bubble cooling, provided that frost line height is fixed at 3 to 4 die diameters above the air ring. Machine-direction Elmendorf tear strength measured per ASTM D1922-23 typically exceeds 120 g at 25 µm gauge, permitting mechanical lay-flat installation by tractor-drawn mulch layers without tearing at staple points. Carbon black masterbatch addition at 2.0 wt% to 3.5 wt% loading achieves ultraviolet stabilization for single-season cropping cycles; the masterbatch carrier resin must be butene-copolymer LLDPE chemistry to prevent die-lip phase separation during extrusion. Field tracking of film embrittlement is conducted through tensile elongation at break retention per ISO 527-3:2018 after accelerated weathering under ASTM G154 Cycle 1, with 50% elongation retention at 800 hours exposure constituting the practical service threshold before replacement is scheduled. Production-scale observations on 1200 mm die diameter lines indicate that gauge banding in the transverse direction emerges when frost line oscillation exceeds ±10 mm, creating localized weak points that become evident during soil-contact thermal expansion cycles in equatorial climates.

    What Governs Cast Film Draw Resonance and Pre-Stretch Uniformity in Pallet Wrapping Grades?

    Cast stretch film production using LLE1018F2 as the primary resin or in blends with polyolefin plastomers at 60 wt% to 80 wt% primary content is executed on chill-roll cast lines running at 300 m/min to 600 m/min line speed. Melt temperature at the slot die is maintained between 240 °C and 260 °C, and the die-to-chill-roll air gap is set at 25 mm to 40 mm to minimize neck-in while drawing to final thicknesses of 12 µm to 17 µm. The resin’s short-chain branching distribution provides ultimate elongation exceeding 500% per ASTM D882-18, a precondition for powered pre-stretch rollers operating at 250% elongation without film fracture. Cling force is regulated through polyisobutylene or low-density polyolefin additive incorporation at 1.0 phr to 3.0 phr; migration to the film surface reaches functional equilibrium within 24 hours of winding, with coefficient of friction falling below 0.6 when measured per ISO 8295:1995. Draw resonance manifests when the ratio of take-off velocity to die exit velocity exceeds the stability threshold, producing periodic thickness oscillation at frequencies between 10 Hz and 30 Hz; suppression is achieved by maintaining melt temperature above 245 °C and melt pressure at the die entrance below 180 bar. These conditions have been documented on extruders with 90 mm screw diameter and 30:1 L/D ratio equipped with gear pumps, where shear-thinning behavior of the resin at apparent shear rates of 100 s⁻¹ to 500 s⁻¹ stabilizes the melt curtain.

    Heavy-duty shipping sacks and polymer granule silo bags at 80 µm to 120 µm total gauge are produced on five-layer coextrusion blown film lines with LLE1018F2 occupying the core layer at 50 wt% to 70 wt% of total structure. High-density polyethylene outer layers provide stiffness and print adhesion, while the LLDPE core contributes puncture resistance measured by slow-puncture probe according to ASTM D5748-23, with energy-to-break values routinely exceeding 3.0 J at 100 µm gauge when processed at die gap 1.6 mm to 2.0 mm and blow-up ratio 2.0:1 to 2.5:1. Creep rupture extrapolation at 23 °C indicates hoop-stress capacity of 4.0 MPa to 4.5 MPa at 10,000 hours following ISO 9080 methodology on pressurized pipe specimens fabricated from the resin. Internal corona treatment of the tubular film at 2.0 kW to 3.5 kW per meter of film width raises surface energy to 40 mN/m to 42 mN/m for water-based flexographic ink adhesion, without degrading fin-seal strength at the bottom gusset, which remains above 30 N/15 mm per ASTM F88/F88M-22. Batch-to-batch variance in slip additive concentration is observed when the extruder barrel temperature profile is reversed from 195 °C at the feed zone to 230 °C at the die, a condition that reduces gel formation from higher molecular weight fractions but accelerates slip agent thermal degradation; the resulting coefficient of friction drift is quantified by surface lubricity measurement at 24-hour intervals post-conversion.

    Dart Impact Retention and Seal Initiation Temperature in Coextruded Food-Packaging Sealant Layers

    Coextruded structures pairing LLE1018F2 as a sealant layer with biaxially oriented polypropylene or polyethylene terephthalate outer layers require seal initiation temperatures between 95 °C and 105 °C, determined on gradient heat-seal equipment per ASTM F2622-20 and reported as the temperature at which 8.8 N/25 mm seal strength is achieved. The grade’s compliance position for Indian food-contact applications is established through the positive list requirements of IS 10146:1982 and overall migration limit testing under IS 9845:1998 at 40 °C for 10 days in aqueous food simulants. Oxygen transmission rate through a 20 µm sealant layer at 23 °C and 0% relative humidity is approximately 7,500 cm³/m²·day·atm per ASTM D3985-17, functionally irrelevant as a barrier but compatible with five-layer structures incorporating EVOH or polyamide core layers. Dart impact strength of coextruded laminates containing 40 µm LLDPE sealant layer, tested per ASTM D1709-22 Method A, exceeds 300 g when the resin is processed with a reverse temperature profile from 195 °C at the feed zone to 230 °C at the die. Migration of erucamide slip additive to the sealant surface is governed by diffusion coefficients on the order of 10⁻¹² m²/s at ambient temperature, leading to full coefficient of friction stabilization within 72 hours of film production; verification is performed by slip measurement on the sealed package interior according to ASTM D1894-14.

    Compliance ParameterStandard / MethodTypical Value or Requirement
    Melt flow rate, 190 °C / 2.16 kgISO 1133-1:20221.0 g/10 min
    DensityISO 1183-1:2019 Method A0.918 g/cm³
    Tensile elongation at break (film)ISO 527-3:2018>600%
    Dart impact, 40 µm filmASTM D1709-22 Method A>300 g
    Elmendorf tear, 25 µm film, MDASTM D1922-23>120 g
    Oxygen transmission rate, 20 µm filmASTM D3985-17≈7,500 cm³/m²·day·atm
    Water vapor transmission rate, 25 µm filmASTM F1249-20≈2.0 g/m²·day at 38 °C, 90% RH
    Food contact (Indian market)IS 10146:1982 / IS 9845:1998Compliant per manufacturer CoC
    Food contact (US market)FDA 21 CFR 177.1520Olefin polymer, conditions of use A–H
    EU registrationREACH (EC) No 1907/2006Registered as polymer (monomer: 1-butene)

    Extrusion lamination of woven polypropylene sack substrates with 20 µm to 30 µm of LLE1018F2 melt at 290 °C to 310 °C produces peel bond strengths above 2.0 N/15 mm when measured per ASTM D903-98, conditional upon corona pre-treatment of the woven substrate to 42 mN/m surface energy and an air gap of 100 mm to 150 mm permitting melt curtain oxidation before contact. The resin’s melt viscosity at apparent shear rates from 100 s⁻¹ to 500 s⁻¹ within the T-die maintains sufficient melt strength to prevent sag-induced thinning of the melt curtain at coating weights above 15 g/m². Operational data from flat-die laminators with 2500 mm working width indicate that neck-in at the substrate edges increases from 20 mm at 15 g/m² coating weight to 35 mm at 30 g/m², requiring scheduled deckle adjustment during grade transitions on the same line. The lamination layer functions as a moisture barrier with water vapor transmission rate of approximately 2.0 g/m²·day at 38 °C and 90% relative humidity per ASTM F1249-20 at 25 µm thickness, a specification condition sufficient for cement, fertilizer, and pet food packaging formats in tropical distribution chains.

    Geomembrane Sheet Extrusion, High-Frequency Welding, and Stress-Crack Resistance Under Landfill Leachate Exposure

    LLDPE geomembrane sheet in 1.0 mm to 2.0 mm thickness is flat-die extruded from LLE1018F2 at melt temperatures of 220 °C to 250 °C on single-screw machines with 45:1 L/D and grooved feed sections. Sheet tensile properties at yield, measured per ASTM D6693-20, fall within 15 MPa to 18 MPa in both machine and transverse directions, with elongation at yield between 13% and 16%. Seam integrity is established through wedge welding at 350 °C to 380 °C wedge temperature with roller pressure calibrated to 70 N to 100 N per 25 mm seam width; shear strength of welded seams per ASTM D6392-12 exceeds 80% of parent sheet strength, and peel strength exceeds 60% of parent sheet strength. Notched constant tensile load testing in 10% Igepal CO-630 at 50 °C according to ASTM D5397-21 provides stress-crack transition times exceeding 50 hours, adequate for secondary containment and agricultural lining but below the threshold for hazardous waste primary impoundments requiring high-density polyethylene. Multiaxial strain at break measured per ASTM D5617-04 exceeds 15% at 2.0 mm sheet thickness, absorbing differential settlement without brittle fracture. Published data on long-term leachate immersion for this specific grade is limited, and field performance validation per GRI-GM13 test methods should be conducted prior to specification for municipal solid waste landfill primary liner service.

    When Silage Wrap Formulation Replaces Low-Density Homopolymer in Round Bale Encapsulation Systems

    Round bale silage wrap at 25 µm gauge produced from LLE1018F2 is stretched to 55% to 70% pre-stretch during application using mechanical bale wrappers with powered rollers. The resin’s elongation at break above 600% per ISO 527-3:2018 and resistance to puncture under stalk pressure maintain bale integrity during the 12-month storage interval between harvesting cycles. Tackifier compatibility requires formulation trials on each film line because the F2 slip package containing glyceryl monostearate may interfere with polyisobutylene tackifier migration when long-chain polyisobutylene concentrates are added at 1.5 wt% to 2.5 wt% on an ethylene vinyl acetate carrier. Comparative testing against low-density homopolymer baselines on the same blown film equipment quantifies 35% lower probe penetration energy for the homopolymer at equal gauge per ASTM D5748-23. Ultraviolet stabilization for 12-month outdoor storage is achieved with hindered amine light stabilizer concentrate addition at 0.3 wt% to 0.5 wt%; without this addition, elongation retention drops below 50% after 6 months of equatorial sun exposure, a failure mode observed as circumferential splitting during round bale handling.

    Masterbatch and compounding applications employ LLE1018F2 as a carrier resin for carbon black, mineral filler, or additive concentrates at loadings from 20 wt% to 50 wt% active component. The low melt flow rate of 1.0 g/10 min requires twin-screw compounding at 180 °C to 220 °C barrel temperature with screw designs providing 2.0 to 2.5 kWh/kg specific mechanical energy input for homogeneous pigment dispersion. Let-down ratios of 20:1 to 50:1 in target resins are achievable when the carrier resin molecular architecture matches the end-use polyolefin chemistry, preventing dispersion phase separation visible as surface specks in thin-gauge film. Batch-to-batch viscosity consistency of the carrier is monitored through melt flow rate determination per ISO 1133-1:2022, with rejection criteria set at ±0.15 g/10 min deviation from nominal to preserve consistent dilution behavior in downstream converters.

    Free Quote

    Competitive CIPLAS LLE1018F2 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    CIPLAS LLE1018F2 is designated as a linear low-density polyethylene extrusion resin in which the ethylene backbone carries a controlled short-chain branch distribution introduced by an α-olefin comonomer during low-pressure polymerization. The numeric string 1018 corresponds to a nominal melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg and a nominal density of 0.918 g/cm³ at 23 °C. The suffix F2 is interpreted as a film-conversion variant; open technical literature does not fully reproduce the supplier’s lot certificate, so exact slip, antiblock, and processing-aid loadings should be confirmed with the supplier before line trials. Density conformity is assessed by ISO 1183-1:2019 or ASTM D1505-18, and melt flow rate by ISO 1133-1:2022 or ASTM D1238-23.

    Typical physical-property envelope for a film-grade LLDPE of nominal 0.918 kg/dm³ density and 1.0 g/10 min MFR; supplier Certificate of Analysis required for CIPLAS LLE1018F2.
    PropertyTest methodTypical rangeLot verification
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:2022 / ASTM D1238-231.0 g/10 min nominalCertificate of Analysis required
    Density, 23 °CISO 1183-1:2019 / ASTM D1505-180.918 g/cm³ nominalCertificate of Analysis required
    Peak melting temperature, DSC second heatISO 11357-3:2018 / ASTM D3418-15120–124 °CCertificate of Analysis required
    Vicat softening temperature, method A50ISO 306:2022 / ASTM D1525-1795–105 °CCertificate of Analysis required
    Tensile yield stress, compression-molded sheetISO 527-2:2012 / ASTM D638-1410–13 MPaCertificate of Analysis required
    Tensile elongation at break, compression-molded sheetISO 527-2:2012 / ASTM D638-14>800% class-typicalCertificate of Analysis required

    On a production-scale blown-film line comprising a 75 mm grooved-feed extruder with 30:1 L/D and a 250 mm spiral mandrel die, the most visible lot-to-lot variable for F2-formulated resin is not usually output rate but bubble position and die-lip deposit formation at extended run lengths. The linear backbone provides lower melt tension than an equivalent-density LDPE; when LLE1018F2 is blended at above 70% in an LLDPE/LDPE mix, frost-line height and lower neck height typically require independent adjustment. Published LLE1018F2-specific production logs are limited in the open literature, so the above observation should be treated as class behavior rather than a supplier-guaranteed operating point.

    What Limits Melt Pressure Homogeneity When LLE1018F2 Runs on General-Purpose Extrusion Lines?

    The limiting variable is normally screw melting capacity before the adapter. LLDPE of this melt flow and density has a higher zero-shear viscosity than a comparable autoclave LDPE and no long-chain branching to promote strain hardening; as a result, a general-purpose screw with a compression ratio below 2.8:1 may deliver a partially melted plug into the metering section. On a 60 mm single-screw extruder with 28:1 L/D producing 40 µm monolayer film, this condition appears as melt-pressure oscillation of 5–15 bar at constant screw speed, along with an increase in gauge-band scatter. A reverse-taper or Maddock mixing section, a barrel profile of 160–180 °C in the feed zone and 200–220 °C in the die zone, and a barrier screw with a compression ratio of 3.0:1 to 3.5:1 normally restore melt quality.

    Capillary rheometry on analogous 0.918 kg/dm³, 1.0 g/10 min resins indicates apparent shear viscosity at 100 s⁻¹ between 450 Pa·s and 750 Pa·s at 190 °C. However, published rheological data for CIPLAS LLE1018F2 specifically are limited; a 20 kg pilot-trial charge is therefore advised before full silo conversion. Cast-film lines feeding a chill roll typically require melt temperature of 240–265 °C with a slot die gap of 0.5 mm for uniform web formation. At those temperatures, oxidative gel risk increases, so the resin should not be held above 260 °C for more than 10 min during stoppage; purging with a higher-MFR polyolefin is recommended after extended dwell. If the F2 formulation allows a fluoroelastomer processing aid, die-lip deposit formation can be reduced at a dosage specified in the supplier’s technical bulletin.

    Mechanical performance in 50 µm monolayer blown film is controlled by short-chain branch type, frost-line height, and gauge uniformity. In directional terms, LLE1018F2 is expected to provide higher dart impact and puncture resistance than a 0.922–0.924 g/cm³ LDPE at equal thickness, while haze and elastic recovery may be less favorable because the linear chains lack long-chain branching. Dart impact according to ASTM D1709-16a should be measured on a minimum of 10 specimens per direction; tear propagation is anisotropic and is commonly higher in the transverse direction for blown film. Published data for the specific CIPLAS F2 variant are limited, and production-line film values are routinely shifted by 20–40% relative to laboratory cast specimens by die-gap, orientation, and frost-line conditions.

    Thin-Gauge Cast Film Property Divergence Versus Butene-Copolymer LLDPE

    If the comonomer in LLE1018F2 is butene, the primary separation from hexene- or octene-copolymer LLDPE appears in dart impact and tear at identical density and gauge. The following table provides a directional comparison for a 25 µm cast film converted on a chill-roll line; values are class envelopes and require lot-specific verification for CIPLAS LLE1018F2.

    Directional comparison of film properties at 25 µm thickness for class-equivalent resins; CIPLAS LLE1018F2 lot data required.
    AttributeCIPLAS LLE1018F2 expected class zoneLDPE 0.923 g/cm³, 2.0 g/10 minHexene mLLDPE 0.918 g/cm³, 1.0 g/10 min
    Dart impact, method A120–180 g60–100 g200–400 g
    Seal initiation temperature, gradient bar95–112 °C90–105 °C85–105 °C
    Haze, no antiblock3–7%2–5%2–6%
    Elmendorf tear anisotropyMD lower than TD; supplier data requiredModerate anisotropyMD lower than TD; supplier data required

    These differences imply that a direct replacement of LDPE by LLE1018F2 on a cast-film line should not be made solely on density and MFR. The converter must re-establish the extruder temperature profile, chill-roll temperature, and air-knife settings because the LLDPE’s lower melt strength and different crystallization behavior alter neck-in and strip adhesion. In applications requiring high clarity and low seal initiation temperature, a hexene- or octene-based metallocene LLDPE may outperform a butene-copolymer F2 variant; if F2 is a hexene-copolymer grade, that property separation narrows.

    Compared with a high-density polyethylene of 0.954 g/cm³ and 0.30 g/10 min MFR, this grade gives lower tensile yield stress but higher strain-at-break, lower Vicat softening temperature, and lower moisture-vapor barrier. It should not be substituted for HDPE in blow-molded containers or geomembranes without redesigning wall thickness and weld strength.

    When Blown Film Bubble Stability at High Blow-Up Ratios Becomes the Controlling Variable

    For a 300 mm mono-layer die producing 40 µm film at a blow-up ratio of 2.8:1 and output of 180–220 kg/h, the linear architecture of LLE1018F2 generates lower melt tension than an equivalent high-pressure LDPE. Bubble support at the frost-line boundary therefore becomes the controlling variable. The usual corrective sequence is to raise the frost-line height to 2.0–2.5 die diameters, reduce cooling-air temperature to 8–15 °C, and, where fitted, increase internal bubble cooling air exchange. If transverse bubble oscillation occurs, the lower neck height should be lowered in increments of 10 mm while the thickness profile is recorded. A conventional single-lip air ring can hold 2-sigma thickness variation near ±3%; a dual-lip air ring generally reduces that variation to ±1.5% for class-equivalent resins. Published LLE1018F2-specific plant data remain limited, and the above values should be treated as factory norms for linear-low resins in this melt-flow and density class.

    Moisture drying is generally unnecessary if pellets are stored at <25 °C and <50% relative humidity.

    Incoming inspection for CIPLAS LLE1018F2 should replicate the supplier’s certified test conditions. A transfer line sample should be injection- or compression-molded according to ISO 1872-2:2007; density columns calibrated with isopropanol/water mixtures are used. Gel count is assessed by extruding a 50 µm tape through a laboratory cast line and counting visible fish-eyes per 100 cm². Acceptable thresholds are product-specific; technical literature for film-grade LLDPE commonly reports visible gels in the range of 10–50 per 100 cm², but published limits for the F2 variant are limited. The resin should be sampled from at least 3 positions per silo or container to detect feed-segregation effects.

    Additive Chemistry, Food-Contact Boundaries, and Migration Pragmatics

    The F2 suffix may denote a selected slate of slip and antiblock additives rather than a bare-polymer grade. If erucamide slip is present at 500–1000 ppm and synthetic silica antiblock at 1000–2000 ppm, the coefficient of friction against polished stainless steel can fall from 0.30–0.40 immediately after extrusion to 0.08–0.15 after 48 h at 23 °C when measured by ISO 8295:1995. The same additive migration that lowers friction may reduce corona-discharge retention, print adhesion, or seal strength on high-speed packaging lines; surface treatment should be adjusted only after tests on the F2 film.

    For direct food-contact use, a written conformity statement against 21 CFR 177.1520(c) 3.1a or 3.2a is required for the specific film composition, and against EU Regulation 10/2011 for specific migration limits applicable to the comonomer and additives. Compliance is not automatically inherited from the polymer class because slip, antiblock, or fluoroelastomer processing aids can carry independent restrictions under REACH and RoHS Directive 2011/65/EU. The grade should not be presumed acceptable for fatty-food contact above 40 °C unless the supplier’s migration data support the condition.

    Thermal degradation begins to form measurable gel particles above 260 °C; melt-temperature excursions beyond 250 °C should be time-limited. Extended contact with strong oxidizing acids, halogens, or aromatic and chlorinated solvents at elevated temperature can promote swelling and environmental stress cracking. At shutdown, if LLE1018F2 is to remain in the barrel above 180 °C for more than 15 min, a purge with a higher-MFR polyolefin should be used to reduce subsequent gel formation. The same limitation applies when the line is cycled back to LDPE; a full tail-packing purge of the die lips prevents cross-contamination of the F2 additive package into non-film regrind.