Ciplas Lld1318b Linear Low Density Polyethylene

CIPLAS LLD1318B Linear Low Density Polyethylene

    • Product Name: CIPLAS LLD1318B Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 918482
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Density 0.918 g/cm³
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 240 MPa
    Hardness Shore D 50
    Haze 12%
    Gloss 45 60
    Dart Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Coefficient Of Friction 0.20
    Water Absorption <0.01%
    Thermal Conductivity 0.33 W/m·K
    Volume Resistivity >1.0E15 ohm·cm
    Dielectric Constant 1 Mhz 2.3
    Processing Temperature 180-220 °C

    As an accredited CIPLAS LLD1318B Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing CIPLAS LLD1318B Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) Container Loading (20′ FCL): CIPLAS LLD1318B Linear Low Density Polyethylene in 25 kg bags, approx. 18–20 MT net, securely loaded.
    Shipping CIPLAS LLD1318B Linear Low Density Polyethylene is shipped as non-hazardous resin pellets in 25 kg bags, jumbo bags, or bulk containers. It is not regulated for transport. Store in a cool, dry, clean area away from direct sunlight, heat, moisture, and contamination. Handle with normal industrial care and ensure packaging remains intact.
    Storage Store CIPLAS LLD1318B Linear Low Density Polyethylene indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep bags or containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged stacking or pressure that may cause blocking. Use clean handling equipment and maintain good housekeeping to minimize pellet slip hazards.
    Shelf Life Stable under normal storage conditions; indefinite shelf life if kept cool, dry, sealed, and protected from direct sunlight and heat.
    Application of CIPLAS LLD1318B Linear Low Density Polyethylene
    On three-layer agricultural blown film lines processing butene-LLDPE of nominal melt flow rate 1.0 g/10 min (ISO 1133-1:2022, 190 °C/2.16 kg) and density 0.917–0.920 g/cm³ (ISO 1183-1:2022), LLD1318B is used as the structural layer for silage covers, greenhouse cladding, and nursery tunnel film because the ethylene-butene backbone permits film thicknesses of 180–220 μm when combined with 10–20 wt% high-pressure LDPE for bubble stability. The formulation for a three-layer agricultural grade typically contains 70–80 wt% LLD1318B in the core and outer layers, 10–20 wt% LDPE, 5–10 wt% combined UV/HALS/anti-fog/color masterbatch, and 0.5–1.5 wt% polymer processing aid when die-lip shear stress produces melt fracture at die gaps below 1.8 mm. Extrusion is carried out on grooved-feed extruders of 45–65 mm screw diameter with L/D ratios of 28:1–30:1, barrel set points from 170 °C feed zone to 200–215 °C die zone, die gap 1.8–2.5 mm, blow-up ratio 2.2–2.8, and frost-line height 600–900 mm from the air ring. Internal bubble cooling on the main blown-film tower increases output by 15–30% compared with single-lip air-ring cooling at identical screw speed, but frost-line height must be held within ±50 mm to avoid transverse-direction tensile variation above 5%. Finished-film compliance is normally demonstrated through EN 13206 for agricultural cover films, ISO 527-3 for tensile properties, ISO 7765-1 dart impact with a 25 mm-diameter probe, REACH SVHC screening below 0.1 wt%, and EU 10/2011 overall migration if silage or irrigation contact is incidental. At storage RH above 60%, carbon black or mineral-containing masterbatch should be pre-dried at 70–80 °C for 2–4 h to below 0.03 wt% moisture; otherwise microvoids reduce dart impact by more than 15%. LLD1318B monolayer film is not recommended for direct contact with high-acid silage leachate without an outer barrier layer because carboxylic acid migration can plasticize the seal surface and decrease coefficient of friction below the range needed for mechanical unfolding equipment. Terminal products include silage clamp covers, greenhouse cladding, nursery tunnel film, windbreak sheeting after slitting, and temporary construction enclosure panels.

    Why Do Cast Stretch Film Lines Run Butene-LLDPE Below the Melt Fracture Limit at High Output?

    On cast stretch film lines running butene-LLDPE at 15–25 μm thickness, the main processing conflict is not barrel cooling capacity but the point at which die-lip shear rate exceeds the critical shear rate and initiates sharkskin on the chill-roll side. On a 2.4 m-wide cast extrusion line with a 120 mm single-screw extruder at 30:1 L/D, the maximum stable output is typically determined by die-lip flow conditions rather than by downstream winding torque. The processing window uses a slot die gap of 0.5–1.0 mm, an air gap of 20–50 mm, a chill roll temperature of 15–25 °C, and a melt temperature of 240–260 °C; vacuum boxes, air knives, or electrostatic pinning are required above 250 m/min to hold the melt curtain on the chill roll. The stretch-film formulation generally contains 88–96 wt% LLD1318B, 2–5 wt% polyisobutylene-based cling masterbatch, and 1–3 wt% antiblock/slip masterbatch; pre-stretch ratio at the pallet wrapper is set at 150–250% depending on load containment and film memory. Compliance testing for industrial pallet wrap uses ASTM D5458 for cling, ASTM D5748 for puncture resistance, ISO 527-3 for tensile strength and elongation, and REACH SVHC screening below 0.1 wt%; if the film is later used as primary food-contact stretch wrap, migration testing under EU 10/2011 must be commissioned separately because the standard pallet wrap formulation is not automatically compliant. Terminal products include machine pallet wrap, hand wrap, silage bale wrap, coil protection film, and bundling film.

    On cast lines wider than 3.0 m, edge-bead thickness exceeding 250 μm is a recurring field failure when the air gap remains above 50 mm; the resulting hard roll edges generate slitter dust and require trim recycling at 5–8 wt%. Published data for LLD1318B at line speeds above 500 m/min is limited; converters should qualify melt-curtain stability on their specific die geometry and confirm the absence of draw resonance before automatic gauge control is activated. The principal operational boundary is that die-lip gaps below 0.5 mm can reduce melt-curtain stability at low output, while gaps above 1.0 mm raise neck-in and increase edge trim, so the die gap must be re-optimized if extruder melt pressure fluctuates more than 3% because of regrind feed variation.

    Extrusion Coating onto Woven Polypropylene Backing in Flexible Intermediate Bulk Container Liners

    Polypropylene woven backing that is extrusion-coated with LLD1318B requires blending with high-pressure LDPE because the butene-LLDPE component alone exhibits excessive neck-in and insufficient melt draw at coating speeds above 80 m/min. Typical coating blends contain 20–50 wt% LLD1318B, 50–80 wt% LDPE coating grade, and 0.5–1.5 wt% processing aid masterbatch, with coating weights of 15–30 g/m² for woven sack lamination and 35–60 g/m² for FIBC liner webs. The extrusion coating line uses 90–150 mm single-screw extruders with 30:1 L/D, barrel temperatures from 230 °C at the feed zone to 300–320 °C at the feedblock and die, a slot die gap of 0.3–0.8 mm, and a chill roll temperature of 15–25 °C; nip pressure is set at 250–400 N/cm. The woven substrate is corona-treated to 40–46 mN/m measured by ASTM D2578, and adhesion development is verified by ASTM F88 seal strength testing on 25 mm-wide specimens after lamination. Food-adjacent packaging compliance includes FDA 21 CFR 177.1520(c) for olefin polymers, EU 10/2011, EC 2023/2006 good manufacturing practice for food contact materials, and REACH SVHC screening below 0.1 wt%. Amine-based antistatic agents in the coating should be avoided because they can accelerate auto-oxidation at die temperatures above 300 °C, generating gel particles that diminish coating uniformity. Terminal products include laminated woven polypropylene sacks, FIBC inner liners, paper/polyethylene sachet lamination, technical textile coating, and carpet backing.

    For wide-sheet geomembrane production, carbon black masterbatch partitioning across the extruder profile is preferred over hopper dry blending because poor dispersion of carbon black agglomerates creates local stress concentrations that reduce puncture resistance under ASTM D4833 by more than 10%. A 5-layer smooth geomembrane formulation for 0.5–2.5 mm thickness typically consists of 80–90 wt% LLD1318B, 10–20 wt% MDPE or HDPE to raise yield strength, 2–3 wt% carbon black masterbatch, 1–3 wt% antioxidant/UV stabilizer masterbatch, and 0.5–1.0 wt% polymer processing aid. Extrusion is performed on internally cooled blown-film towers of 5–8 m lay-flat width or flat-die calender lines, with die gaps of 1.5–2.5 mm, melt temperatures of 195–215 °C, and haul-off speeds below 20 m/min to control thickness variation below ±5%. At storage relative humidity above 60%, carbon black masterbatch must be pre-dried at 70–80 °C for 2–4 h until moisture is below 0.03 wt%; otherwise microbubbles in flat-die webs reduce weld seam shear strength and create visible pinholes in thin sections. The following GRI-GM17 table lists representative minimum acceptance values for a 1.5 mm smooth LLDPE geomembrane; the current revision and project specification must be checked for the exact threshold. Published data for LLD1318B long-term oxidative induction time under high-pH leachate contact is limited, so comparative qualification under GRI-GM17 Appendix and EN 13492 is required before fixed service-life predictions are made. Terminal products include landfill cell liners, pond liners, canal liners, mining heap leach pads, and temporary containment curtains.

    Property and test method1.5 mm smooth LLDPE minimum acceptance valueTypical verification frequency
    Thickness, ASTM D5199Minimum average 1.5 mm; lowest individual not less than 90% of stated minimumper roll
    Tensile break strength, ASTM D6693 Type IVMinimum average 29 kN/m machine and transverse directionper batch
    Elongation at break, ASTM D6693Minimum average 800%per batch
    Tear resistance, ASTM D1004Minimum average 125 Nper batch
    Puncture resistance, ASTM D4833Minimum average 480 Nper batch
    Carbon black content, ASTM D16032.0–3.0%per batch
    Oxidative induction time, ASTM D3895Minimum average 100 minper batch

    When Form-Fill-Seal Lines Demand Hot-Tack Above 85 °C in Frozen Food Packaging

    When form-fill-seal lines demand hot-tack above 85 °C in frozen food packaging, LLD1318B is normally used as the sealant layer in a three-layer blown film structure rather than as a monolayer, because butene-LLDPE by itself may not maintain sufficient hot-tack at packaging speeds above 80 packs/min. Sealant-layer formulations for vertical or horizontal form-fill-seal applications use 60–80 wt% LLD1318B, 10–25 wt% metallocene plastomer to lower seal initiation, 10–20 wt% high-pressure LDPE for bubble stability, and 2–4 wt% slip/antiblock masterbatch; total film thickness is 35–70 μm, with the sealant layer at 10–20 μm. Coextrusion is run on 45–65 mm grooved-feed blown-film extruders with 28:1–30:1 L/D, die gap 1.8–2.5 mm, blow-up ratio 2.0–2.5, and frost-line height 500–800 mm; downstream VFFS sealing jaws are set at 115–140 °C, dwell time 0.5–1.2 s, and seal pressure 3–5 bar. Amine-containing antistatic or slip packages should be avoided in the sealant layer because they can react with oxidized metallocene phases and reduce hot-tack reproducibility. Terminal products include frozen food pouches, cereal liners, snack bags, bag-in-box liners, and pharmaceutical intermediate packaging. The food-contact compliance matrix below covers the main regulatory pathways; compliance must be re-verified for each specific finished film structure because the presence of plastomers, colorants, or recycled content can change the migration profile.

    Framework / standardRelevant clause or test methodApplication scope
    FDA 21 CFR 177.1520(c)Olefin polymers, extractables in n-hexane and xyleneDirect dry and aqueous food contact sealant layer
    EU 10/2011Overall migration 10 mg/dm²; specific migration limits for additivesFrozen and refrigerated food bags
    EC 2023/2006Good manufacturing practice for food contact materialsFilm converter hygiene and traceability
    REACH SVHCCandidate list threshold 0.1 wt%Resin, masterbatch, and finished film screening
    RoHS 2011/65/EULead, cadmium, mercury, hexavalent chromium, PBB, PBDEPackaging inserts for electrical and electronic goods
    Free Quote

    Competitive CIPLAS LLD1318B Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    CIPLAS LLD1318B Linear Low Density Polyethylene is supplied as pelleted butene-comonomer resin for blown-film extrusion, cast-film conversion, and selected coextrusion structures. The nominal melt flow rate is 1.3 g/10 min at 190 °C under a 2.16 kg load tested according to ISO 1133-1, and the density is reported as 0.918 g/cm³ under ISO 1183-1. The resin belongs to the linear low density polyethylene class; the backbone is essentially linear, with short-chain branches introduced through butene incorporation. This structure differentiates it from high-pressure low density polyethylene, which contains long-chain branching, and from hexene- or octene-based linear low density products, where longer short-chain branches modify tie-molecule formation and impact resistance. Product designation often encodes nominal density and melt-flow class, but the exact lot-to-lot release limits must be taken from the manufacturer certificate of analysis rather than from a general datasheet description. The product is supplied in pellet form and packaged in 25 kg bags or bulk containers; packaging lot identification follows the supplier’s internal traceability system.

    The Molecular Architecture Controls Thermal Transitions and Crystallisation

    The short-chain branch distribution of CIPLAS LLD1318B influences crystallisation temperature, crystal thickness, and solid-state mechanical response. Differential scanning calorimetry per ISO 11357-3 typically records a peak melting temperature near 121 °C and an onset of crystallisation in the range of 106 °C to 110 °C for this density class. The density of 0.918 g/cm³ corresponds to a crystalline volume fraction of approximately 45 %; the residual amorphous phase contributes low-temperature impact resistance and permeability to small molecules. Rapid quenching during blown-film extrusion reduces lamellar thickness and increases the number of interlamellar tie molecules. This is the primary structural reason why dart impact and Elmendorf tear resistance in finished film are sensitive to frost-line height and cooling-air flow. Butene comonomer creates ethyl branches that are less efficient than hexene-derived butyl branches in suppressing crystal perfection at equivalent comonomer content; therefore a butene resin at 0.918 g/cm³ may exhibit slightly higher crystallinity than a comparable hexene resin. Melt flow ratio, calculated as the quotient of melt flow rate at 21.6 kg and 2.16 kg, generally lies between 25 and 30 for this resin class; such shear-thinning behaviour is relevant to die-lip shear stress and screw-torque control. Published data for this specific configuration is limited, and thermal transitions should be treated as class-typical for butene-based LLDPE.

    Film property values for CIPLAS LLD1318B shift with film thickness, blow-up ratio, and frost-line height. The following table presents class-typical values for a 40 µm blown film produced at a blow-up ratio of 2.2:1 and a melt temperature of 205 °C; they are not guaranteed minima and should be read with the manufacturer release certificate.

    PropertyUnitClass-typical valueTest method
    Densityg/cm³0.918ISO 1183-1
    Melt flow rateg/10 min1.3ISO 1133-1
    Vicat softening temperature°C92ISO 306 A50
    Peak melting temperature°C121ISO 11357-3
    Tensile stress at break, machine directionMPa35ISO 527-3
    Tensile stress at break, transverse directionMPa28ISO 527-3
    Elongation at break, machine and transverse directions%>700ISO 527-3
    Secant modulus, 1% strain, machine directionMPa200ISO 527-3
    Dart impact, 40 µmg110ISO 7765-1
    Elmendorf tear, transverse directionN7ISO 6383-2
    Haze%12ISO 14782
    Gloss, 60°GU50ASTM D2457
    Environmental stress-cracking resistanceh>1000ASTM D1693B

    The film retains measurable anisotropy: machine-direction tensile stress at break is typically higher than transverse-direction stress at break, while tear resistance in the transverse direction is higher than in the machine direction. This imbalance controls gusset placement, bag-opening behaviour, and pallet-wrap load retention. Additive packages containing slip and antiblock agents lower coefficient of friction; the coefficient of friction measured by ISO 8295 can be reduced from 0.8 to below 0.2 depending on additive concentration, but this reduces gloss and increases haze. Gas permeability of CIPLAS LLD1318B film follows polyethylene class behaviour: oxygen transmission rate at 40 µm is approximately 2000 cm³/(m²·d·bar) to 3000 cm³/(m²·d·bar) at 23 °C and 0 % relative humidity under ISO 15105-2. Carbon dioxide transmission is roughly 3 to 4 times higher than oxygen, and water vapour transmission rate is typically 1.5 g/(m²·d) to 3.0 g/(m²·d) at 38 °C and 90 % relative humidity under ISO 15106-2.

    The Die Gap and Air Ring Settings Required for Stable Bubble Operation

    Stable bubble formation for CIPLAS LLD1318B is obtained at melt temperatures from 195 °C to 225 °C. The lower bound prevents excessive backpressure and screw-motor overload; above 225 °C, oxidative degradation can generate gel defects and reduce dart impact. Die gaps between 1.2 mm and 2.0 mm are used because linear low density polyethylene exhibits higher die-lip shear stress than high-pressure LDPE at the same output. If the die gap is reduced below 1.0 mm, sharkskin melt fracture may appear at shear stresses above approximately 0.18 MPa. Blow-up ratios between 2.0:1 and 2.8:1 are common, with frost-line height adjusted to balance machine-direction and transverse-direction tear. On a 65 mm single-screw extruder with a barrier screw and L/D ratio of 30:1, cylinder temperatures are often set from 160 °C at the feed throat to 200 °C at the die adapter. Dual-lip air rings or internal bubble cooling improve output and bubble stability; without these, the upper output limit may be governed by bubble flutter and film thickness variation rather than extruder capacity. Blending with 10 % to 30 % high-pressure LDPE increases melt strength and reduces draw resonance, at a slight penalty in dart impact and haze. Screen packs of 60 mesh to 100 mesh are typically installed upstream of the breaker plate to trap agglomerated additives; pressure drop across the screen pack should not exceed 2 MPa to avoid excessive melt heating. Film blocking can occur after winding when low-slip formulations are used; therefore surface-treated film for printing or lamination should be allowed to cool to below 40 °C before winding at high tension.

    In cast-film operation, CIPLAS LLD1318B is processed at melt temperatures between 220 °C and 240 °C, with die gap settings from 0.5 mm to 0.8 mm. Chill-roll temperature is typically held between 15 °C and 25 °C to control crystallinity and optical clarity. The absence of long-chain branching reduces melt strength and increases neck-in relative to LDPE; therefore the die deckle is set wider than the target film width and edge trim is reprocessed at controlled levels. Melt pump operation at a pressure setpoint of 8 MPa to 12 MPa reduces surging and film-thickness variation. In coextrusion, the grade is combined with polypropylene or HDPE to modify stiffness and moisture barrier; layer thickness ratios are set by rheological matching to avoid interfacial instability. Corona treatment at a power density of 2.0 W·min/m² typically raises surface tension from 31 mN/m to 42 mN/m according to ASTM D2578; the treatment decays slowly over 30 days, so printing and lamination should be scheduled as close as possible to surface treatment.

    How Does Butene-LLDPE Compare with Hexene and Metallocene Alternatives in Blown Film?

    Relative to a hexene-comonomer LLDPE of the same melt index and density, CIPLAS LLD1318B produces films with lower dart impact strength and lower transverse-direction tear resistance. The difference is most evident below 25 µm, where butene-based films can show 20 % to 30 % lower dart impact than hexene grades due to reduced tie-molecule concentration after rapid quenching. Short-chain branch length in hexene resins generates a more flexible tie-molecule population and delays crystal perfection more effectively; this is reflected in puncture resistance sustained under ISO 7765-1 and tear propagation under ISO 6383-2. Compared with metallocene-catalysed octene LLDPE, the butene resin has lower puncture resistance, higher haze, and a higher seal initiation temperature; metallocene grades also display narrower composition distribution, which reduces random-chain branching and improves optical and mechanical uniformity. However, metallocene resins often require tighter die gap control and internal bubble cooling due to lower melt elasticity. Compared with high-pressure LDPE, CIPLAS LLD1318B offers approximately 1.5 times higher tensile stress at break and greater dart impact at equivalent film thickness, but lower melt strength limits bubble stability and neck-in on high-stretch extrusion coating lines. The following table presents class-typical comparative values for blown film resins; absolute values are process-dependent and should be verified with first-article inspection.

    Material classDart impact at 25 µm, ISO 7765-1Elmendorf tear TD at 25 µm, ISO 6383-2Haze at 40 µm, ISO 14782Seal initiation temperature, ASTM F2029 (°C)
    C4-LLDPE class including CIPLAS LLD1318B90 g4 N12 %105
    C6-LLDPE130 g7 N9 %104
    Metallocene C8-LLDPE180 g9 N4 %95
    High-pressure LDPE60 g3 N7 %102

    When CIPLAS LLD1318B Is Deployed in High-Strength Sack and Liner Applications

    In heavy-duty sack and industrial liner conversion, CIPLAS LLD1318B is run in monolayer or coextruded structures at film thicknesses between 60 µm and 120 µm. A blend containing 70 % CIPLAS LLD1318B and 30 % LDPE processed on a 65 mm barrier-screw blown-film line at 120 kg/h has produced 80 µm film with dart impact above 300 g and sufficient tear propagation resistance for 50 kg packed bags. The grade is also used as a sealant skin in coextruded structures with HDPE or polypropylene; seal strength measured by ASTM F88 and hot-tack performance measured by ASTM F1921 are controlled through comonomer type, seal-bar temperature, and dwell time. In cast-film stretch applications, CIPLAS LLD1318B functions as a cling layer or a machine-direction orientation layer; the resin permits pre-stretch ratios up to 250 % when formulated with suitable tackifying additives. In agricultural silage films, the resin is combined with UV stabiliser masterbatch at 0.5 % to 1.5 % addition levels; outdoor service life is thickness- and stabiliser-dependent, and published data for this specific configuration is limited. Extrusion coating lamination is possible where melt drawdown and neck-in are controlled with LDPE blending; the higher shear viscosity of LLDPE requires barrel temperatures at the upper end of the 200 °C to 240 °C range and die gaps above 0.5 mm to prevent liner tear.

    Operational Boundaries, Storage, and Incompatibilities

    Storage of CIPLAS LLD1318B at ambient temperature below 40 °C and relative humidity below 60 % avoids surface moisture uptake. The polymer is not hygroscopic, but condensation on pellet surfaces can create steam pinholes during extrusion at melt temperatures above 200 °C; if condensation is observed, drying at 60 °C to 80 °C for 2 h is sufficient. The processing melt temperature should not exceed 240 °C because thermal oxidation accelerates and can form crosslinked gel defects. The resin is not recommended for direct contact with concentrated nitric acid, fuming sulfuric acid, or halogenated solvents at processing temperatures; halogenated flame-retardant packages that release acidic species can accelerate thermo-oxidative degradation. Prolonged contact with copper ions in metal equipment should be avoided because copper catalysis lowers oxidative induction time measured by ISO 11357-6. Food-contact suitability must be confirmed with the supplier certificate; the base olefin polymer may be covered under FDA 21 CFR 177.1520 when extraction limits and density conditions are met. For REACH and RoHS declarations, the supplier should provide a compliance statement referencing EU 10/2011 migration limits if the film is intended for food contact. Outdoor exposure without UV stabiliser leads to embrittlement within 6 to 12 months at temperate latitudes; addition of 1 % carbon black or hindered amine stabiliser packages extends service life but changes film optical properties.

    Top