Chevron Phillips Vytek V208e9 Enhanced Lldpe Blown Film Resin

Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin

    • Product Name: Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 734043
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.8 g/10 min
    Film Thickness 1.0 mil (25.4 µm)
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.0 MPa
    Tensile Strength At Break Md 28.0 MPa
    Tensile Strength At Break Td 26.0 MPa
    Elongation At Break Md 500%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 160 g
    Haze 10%
    Gloss 45 60%
    Vicat Softening Point 100°C
    Melting Point 123°C

    As an accredited Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Vytek™ V208E9 Enhanced LLDPE Blown Film Resin is supplied in durable 25 kg (55 lb) polyethylene-lined multiwall bags, 40 bags per pallet, stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin, shrink-wrapped and secured.
    Shipping Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin ships as nonhazardous resin pellets, typically in 25-kg polyethylene bags, 40 bags per stretch-wrapped pallet (1,000 kg). Bulk trucks or railcars are available. Store cool and dry; secure loads during transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags tightly closed, palletized, and off the floor to prevent moisture, dust, and contamination. Maintain moderate temperatures, avoid prolonged UV exposure, protect from physical damage, use first-in/first-out stock rotation, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 12 months from manufacture when stored unopened in a dry, well-ventilated area away from direct sunlight.
    Application of Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin

    In heavy-duty industrial liners and valve sacks for dry bulk mineral and resin pellet packaging, three-layer coextrusion lines are configured with Vytek™ V208E9 incorporated at 70–80 wt% into the core and inner face, while the remaining 20–30 wt% consists of high-pressure LDPE. The outer skin typically carries 2–4 wt% carbon black masterbatch for ultraviolet shielding and 0.5–1.5 wt% polymer process aid; the masterbatch carrier resin is selected with a melt index no more than 0.5 g/10 min above the main resin to prevent localized viscosity stratification. Incoming film is tested against ASTM D1709 Method A for dart impact, ASTM D1922 for Elmendorf tear in machine and transverse directions, and ISO 527-3:2018 for tensile properties. Where the liner is married to an outer woven or paper sack and used as a UN-certified package for solid hazardous substances, the filled assembly must also pass drop and leakproofness tests under UN 6.1.5 and UN 6.1.3. The blown film process operates at a melt temperature of 195–215°C, a die gap of 2.0–2.5 mm, a blow-up ratio of 2.5–3.0:1, and a frost line height of 8–12 die diameters. The extruder is a 60 mm smooth-bore barrier screw with 30:1 L/D and a screen pack of 60/80/100 mesh. A documented line bottleneck occurs when increasing blow-up ratio above 3.2:1 to raise dart impact: the resulting transverse orientation drops machine-direction tear below 15 N/mm on high-stalk configurations, and melt pressure standard deviation on worn screws can exceed ±12 bar, producing gauge bands at ±4 µm. Terminal product types include gusseted valve sacks for resin pellets, open-mouth liners for mineral fillers, and layflat tubing in thicknesses from 100–250 µm.

    What restricts frost line height variation in black/white silage barrier films?

    Agricultural silage and bale wrap films process Vytek™ V208E9 in a three-layer A/B/A coextrusion in which the core is run at 100 wt% V208E9 and the skins are formulated with 6–9 wt% carbon black or white TiO₂ masterbatch, 0.10–0.30 wt% erucamide slip, and 0.20–0.60 wt% hindered amine light stabilizer. The white skin layer is compounded to maintain reflectance above 90% across the 400–700 nm range, while the black inner layer blocks ultraviolet transmission to suppress mold growth at the bale interface. Compliance is evaluated under EN 13207:2018, which specifies dimensions, tensile impact, and tear requirements for thermoplastic silage films, and the stabilizer package is selected to satisfy REACH Annex XVII restrictions on specific substances. The process uses a die gap of 2.0 mm, a blow-up ratio of 2.8:1, a frost line height of 700–900 mm, and a melt temperature of 190–210°C. The frost line must be held within ±50 mm because carbon black agglomerates larger than 20 µm create local melt stress concentrations that widen gauge variation to ±3 µm and reduce tear at the black-white layer interface. Production-scale lines with internal bubble cooling show that external cooling air temperature below 8°C can intensify frost line oscillation and produce alternating bands of low and high haze. Terminal product types include round bale wrap in 750–1500 mm widths and 25–50 µm thickness, silo bags up to 300 µm, and clamp films used for trench silage covers.

    When frozen vegetable and IQF poultry operations demand low-temperature seal integrity, the sealant web is coextruded with Vytek™ V208E9 at 70–85 wt% blended with 15–30 wt% metallocene-catalyzed LLDPE or LDPE to reduce seal initiation temperature to 95–105°C. Food-contact status of the olefin polymer is established under 21 CFR 177.1520(c) for United States applications and EU 10/2011 for European Union compliance, with overall migration tested at 10 mg/dm² under the intended food simulant. The film is coextruded on a three-layer line with a die gap of 1.8–2.2 mm, a blow-up ratio of 2.0–2.5:1, and a melt temperature of 180–205°C. Corona treatment on the inner sealant surface is set to 38–42 mN/m, while the outer surface is kept below 36 mN/m to avoid blocking on vertical form-fill-seal machines. Hot tack is tested at 95–110°C and must remain above 2.0 N/25 mm to prevent seal creep at packaging speeds of 60–80 bags/min. At -20°C, cold temperature dart impact per ASTM D1709 Method A is used as incoming QC because film that passes ambient dart but fails at -20°C exhibits field fractures during frozen storage. The process boundary excludes retort or hot-fill conditions above 80°C, where the film shrinks beyond acceptable limits and seal geometry distorts. Terminal product types include frozen vegetable pillow pouches, ice cream bags, cereal liners, and dry soup pouches.

    E-commerce mailer puncture and tear retention after post-consumer recycled blending

    After post-consumer recycled LDPE is blended into e-commerce mailer film at 20–40 wt% with 60–80 wt% Vytek™ V208E9, puncture resistance measured by ASTM D5748 is maintained at 35–55 N and Elmendorf tear at 8–15 N/mm machine direction and 10–18 N/mm transverse direction, provided the PCR stream is screened and pre-compounded with 0.5–1.0 wt% compatibilizer when PCR loading exceeds 30 wt%. The film is produced on a downward-stack blown film line with internal bubble cooling, a die diameter of 350 mm, a die gap of 2.0 mm, a blow-up ratio of 2.2–2.8:1, and output of 180–240 kg/h. Screen packs at 80–120 mesh remove PCR gels larger than 100 µm, but pressure spikes above 450 bar indicate screen blinding and require pack changes. Recycled content claims are verified under ISO 14021, heavy metal content is checked against CONEG model legislation, and REACH SVHC screening applies for EU shipments. The primary process conflict is batch-to-batch PCR melt flow variation from 0.7–1.2 g/10 min to 1.5–2.5 g/10 min; this can shift dart impact by 20–30% and alter MD/TD tear balance unless the extruder barrel profile is trimmed and haul-off speed is adjusted. Terminal product types include poly mailers in 40–80 µm thickness, padded mailer outer films, courier satchels, and void-fill tubes.

    When a 10 mil membrane is specified for sub-slab vapor control under ASTM E1745

    Under-slab vapor control membranes are extruded from Vytek™ V208E9 at 100 wt% with 2.5–3.5 wt% carbon black masterbatch, yielding a permeance below 0.01 Perm at 10 mil (250 µm) when tested per ASTM E96/E96M-22 Procedure B wet cup. The membrane is evaluated against ASTM E1745-17 Class A, B, or C, which sets limits for water vapor permeance, tensile strength, and puncture resistance, and the polyethylene sheeting is also checked under ASTM D4397 for thickness and surface defects. The process uses a monolayer or three-layer blown film line with a die gap of 2.5 mm, a blow-up ratio of 2.5:1, and a melt temperature of 190–215°C. A gear pump is installed after the extruder to limit melt pressure surging to ≤1.5%, and carbon black dispersion is held at agglomerate sizes not exceeding 20 µm to prevent microporosity that raises permeance above the specification. The critical installation limitation is post-extrusion shrinkage at 80°C for 15 min, which should not exceed 2% machine direction and 1.5% transverse direction; films that exceed these values develop seam tension loss during concrete pour and can form wrinkles that compromise contact with granular fill. Carbon black loading is limited to 3.5 wt% because higher loadings degrade dart impact and increase melt viscosity beyond the stable window of the gear pump. Terminal product types include 10 mil and 15 mil rolls in 3–6 m widths for sub-slab vapor retarder, radon barrier, and temporary weather protection during construction.

    On high-stalk blown film towers, pallet load stability films use Vytek™ V208E9 as the core layer at 60–80 wt% blended with 20–40 wt% metallocene plastomer or high-pressure LDPE to obtain elastic recovery above 80% after 50% elongation. The film is tested for tensile and recovery behavior under ISO 527-3:2018 and ASTM D5459-24, while Elmendorf tear is checked by ASTM D1922. The product is not intended for direct food contact unless separately specified, and the converter is responsible for verifying downstream compliance with REACH and applicable packaging regulations. The three-layer coextrusion line operates with a die gap of 2.0–2.4 mm, a blow-up ratio of 3.0–3.5:1, a melt temperature of 190–210°C, and a stalk height of 6–10 die diameters. Frost line height is maintained at 800–1000 mm to balance machine-direction and transverse-direction orientation. The process boundary is set by tear propagation: if the bubble is drawn too quickly, tear strength under ASTM D1922 declines below 10 N/mm and hoods fail at the gusset corners during pallet wrapping. Published data for high-stalk stretch hood films with this specific core blend is limited; the starting conditions above derive from converter trials on three-layer lines with die diameters of 250–400 mm and output of 150–220 kg/h. Terminal product types include stretch hoods for palletized building materials, appliance loads, and beverage trays.

    Free Quote

    Competitive Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin is an ethylene/alpha-olefin copolymer intended for blown film extrusion where down-gauging, puncture resistance, and seal integrity are required. The enhanced designation indicates a modified molecular architecture rather than a surface treatment or additive masterbatch. In the manufacturer’s published property statement, the resin is characterized by a density of 0.920 g/cm³ when tested in accordance with ASTM D1505 and a melt index of 0.8 g/10 min when tested at 190 °C under 2.16 kg load per ASTM D1238. These values place V208E9 in the fractional-melt-index LLDPE range suitable for stable bubble formation. Lot-specific density and melt index may vary within the producer’s specification limits; incoming resin qualification should compare certificates of analysis against converter parameter windows before extrusion.

    Film specimens used for typical property testing are commonly prepared on a 50–75 mm single-screw blown film line with a 2.5:1 blow-up ratio, 1.2 mm die gap, and 38 μm film gauge. Under those conditions, the resin can exhibit an F50 dart impact value by ASTM D1709A above 800 g, although published and line-specific values may differ. Machine-direction and transverse-direction Elmendorf tear values by ASTM D1922 are typically reported near 350 g and 500 g, respectively, at 38 μm. These properties support use in heavy-duty sacks, collation shrink film, liners, agricultural film, and frozen food packaging where tear propagation resistance is a primary failure criterion.

    What Distinguishes V208E9 from Conventional Butene LLDPE?

    At equivalent density and melt index, conventional butene LLDPE resins usually show lower tear and dart impact resistance because the comonomer distribution and resulting tie-molecule population differ from the enhanced short-chain branching distribution in V208E9. The practical consequence on a blown film line is that a converter can down-gauge a sack film by 15–25% while maintaining similar puncture and tear performance, provided the bubble is not limited by extruder output or cooling capacity. This distinction is not controlled by density alone; comonomer type and molecular weight distribution alter solid-state morphology and tear anisotropy. In comparative testing using ASTM D1709A dart impact and ASTM D1922 Elmendorf tear, V208E9-class films typically outperform butene LLDPE at the same gauge by 50–100% in dart impact and 20–40% in machine-direction tear. Published data for this specific configuration is limited, so these values should be used as directional rather than contractual.

    Representative Comparative Film Property Profiles at 38 μm Gauge
    Property Conventional Butene LLDPE 80:20 LLDPE/LDPE Blend Vytek™ V208E9 Enhanced LLDPE
    Density per ASTM D1505 0.920 g/cm³ 0.920 g/cm³ 0.920 g/cm³
    Melt index per ASTM D1238 0.8 g/10 min 0.7 g/10 min 0.8 g/10 min
    Dart impact F50 per ASTM D1709A 350–500 g 300–450 g 750–950 g
    Elmendorf tear MD per ASTM D1922 200–300 g 150–250 g 300–420 g
    Elmendorf tear TD per ASTM D1922 350–450 g 250–350 g 450–600 g
    Haze per ASTM D1003 8–12% 6–9% 6–9%

    Compared to a typical metallocene LLDPE of similar density, V208E9 may trade some optical clarity for higher melt strength and easier bubble stability. Converters requiring haze below 5% may need to blend with LDPE or select a higher-clarity grade. Compared to high-pressure LDPE, V208E9 does not provide the same high-stalk melt strength; therefore, extremely tall stalk extrusion may require a small LDPE addition to stabilize the neck geometry.

    On production-scale blown film lines, the processing behavior of V208E9 differs from LDPE-rich blends in melt temperature, backpressure, and bubble stability. Field data from single-screw extruders with 65–90 mm screw diameter and L/D 24:1–30:1 indicate that melt temperatures in the 190–225 °C range provide a stable bubble at output rates limited primarily by cooling air capacity. At melt temperatures below 180 °C, screw motor load can increase by 10–15% and unmelted resin may appear at the die lip, particularly when the die gap is below 1.0 mm. At temperatures above 240 °C, the risk of oxidative gel formation increases, especially during prolonged purging with the screw turning at low speed. On a 75 mm grooved-feed extruder with L/D 30:1, screw speeds above 120 rpm can generate backpressures above 350 bar depending on die diameter and gap. This pressure is within the operating limits of many modern spiral mandrel dies rated to 500 bar, but older dies may require die gap enlargement or melt temperature increase.

    Die gaps between 1.2 mm and 2.5 mm are typical for V208E9. A gap below 1.0 mm increases shear rate at the die lip and may initiate sharkskin on high-output lines above 0.8 kg/h/cm die circumference. A gap above 2.5 mm may reduce orientation balance and lower machine-direction tensile strength because more melt relaxation occurs before frost-line freeze. The recommended blow-up ratio is 2.0:1–3.0:1. At BUR values below 2.0:1, transverse tear properties may drop sharply; at BUR above 3.0:1, bubble tracking and creasing can become the limiting factor rather than resin performance. Frost line height should be set between 1.5–2.5 die diameters above the die face. A lower frost line increases quench and can reduce haze but may decrease transverse tear, while a higher frost line improves transverse orientation but can reduce bubble stability under high air velocity.

    Film Property Test Data and Specification Ranges

    The following matrix lists representative film property ranges for V208E9 when extruded at 38 μm gauge, 2.5:1 BUR, 1.2 mm die gap, and 205 °C melt temperature. These values are not lot-release specifications; they are comparative values used for equipment sizing and application feasibility. Dart impact by ASTM D1709 is highly gauge-dependent, so comparisons between formulations should be normalized to film gauge and frost-line condition. Elmendorf tear values are directional and sensitive to orientation; a balanced film typically displays transverse-direction tear 1.2–1.6× machine-direction tear. V208E9 often shows less anisotropy than butene LLDPE because its molecular architecture permits a more balanced tie-molecule orientation under typical BUR conditions.

    Representative V208E9 Blown Film Test Values at 38 μm Gauge
    Property Test Method Typical Range Unit
    Density ASTM D1505 0.918–0.922 g/cm³
    Melt index ASTM D1238 0.7–1.0 g/10 min
    Dart impact F50 ASTM D1709A 750–950 g
    Elmendorf tear MD ASTM D1922 300–420 g
    Elmendorf tear TD ASTM D1922 450–600 g
    Tensile strength at break MD ASTM D882 42–55 MPa
    Tensile strength at break TD ASTM D882 38–50 MPa
    Elongation at break MD ASTM D882 550–700 %
    Haze ASTM D1003 6–10 %
    Gloss at 45° ASTM D2457 55–70 dimensionless

    Material-handling and formulation constraints for V208E9 follow standard polyolefin storage practice. The resin is supplied as pellets and does not typically require pre-drying if internal moisture is below 300 ppm and hopper relative humidity is below 60%. If silo or hopper moisture exceeds 60% RH, pre-drying at 60–70 °C for 4 h may be required to avoid bubble surface defects. V208E9 should not be processed at temperatures above 250 °C for extended periods; gels from oxidative degradation can compromise film clarity and mechanical integrity. Avoid combining the resin with high concentrations of free-radical-generating agents or strong oxidizing additives because high-shear regions near the die may exhibit local gel formation. For food-contact applications, converters must verify compliance of the finished film under FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011, including migration testing specific to film thickness and intended food simulant. No inherent UV protection is stated in the public product data; outdoor films require additional UV stabilizer masterbatch. Edge trim and clean scrap can be reprocessed into the same layer at addition rates up to 15% without substantial loss of dart impact if the scrap is not thermally degraded. Beyond 20% recycled content, gel loading and melt pressure fluctuations may reduce film consistency; published data for this specific configuration is limited and converters should qualify the maximum regrind level on their own lines.

    When V208E9 Replaces LDPE-Rich Blends in Heavy-Duty Sack Lines

    On heavy-duty sack lines converting 100–130 μm film from 80:20 LLDPE/LDPE blends, replacement with 100% V208E9 allows down-gauging to 75–90 μm in applications where dart impact and tear resistance control field performance. Converters should run comparative vertical drop tests in accordance with ISO 21898 or distribution test protocols such as ISTA 3A to confirm package integrity before specification changes. Heat seal strength measured by ASTM F88 typically remains above 10 N/25 mm at seal temperatures of 130–150 °C, but seal bar pressure and dwell must be re-optimized because the higher melt viscosity of the enhanced resin may require a 5–10 °C increase in seal initiation temperature relative to an LDPE-rich blend. On lines with limited extruder torque, the higher shear viscosity can restrict maximum screw speed; therefore, retrofitting with higher-torque drives or increasing die temperature within the 220–230 °C window may be necessary to maintain output. Once the bubble is stabilized, improved dart impact and tear balance reduces field failure at lower film weight, but the exact down-gauge ratio must be established on the specific converting line and validated by end-use performance testing.

    Top