| HS Code | 319877 |
| Manufacturer | Chevron Phillips Chemical Company LP |
| Brand | Vytek |
| Product Name | Vytek V208C3 Enhanced LLDPE Blown Film Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Grade | V208C3 |
| Melt Index 190 C 2 16 Kg | 2.0 g/10 min |
| Density | 0.920 g/cm³ |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Break Md | 33 MPa |
| Tensile Strength At Break Td | 30 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 8% |
| Gloss 45 | 70% |
| Coefficient Of Friction | 0.20 |
| Processing Method | Blown Film Extrusion |
As an accredited Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Vytek™ V208C3 is packaged in 55 lb (25 kg) polyethylene bags, 40 bags per pallet (2,200 lb/1,000 kg total). |
| Container Loading (20′ FCL) | 20′ FCL: Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin, 25 kg bags, palletized, stretch-wrapped, secured; typically 18–20 MT. |
| Shipping | Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin is shipped as dry, free-flowing pellets in 25-kg bags, 1,000-kg bulk boxes, or bulk trucks/railcars. It is non-hazardous for transport (no UN number, class, or placard). Store sealed in a cool, dry, ventilated area away from sunlight, heat, and ignition sources. |
| Storage | Store in original packaging in a dry, covered, well-ventilated area away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep bags or containers sealed to prevent moisture and contamination. Avoid excessive stacking and prolonged UV exposure. Maintain stable ambient temperature and protect from physical damage. Use first-in, first-out stock rotation. Follow manufacturer’s SDS and local regulations. |
| Shelf Life | No fixed shelf life; stable under normal storage conditions. Store in a cool, dry, well-ventilated area away from direct sunlight. |
Chevron Phillips Vytek V208C3 enhanced LLDPE blown film resin at nominal density 0.9208 g/cm³ and melt flow rate 0.80 g/10 min under ASTM D1238 at 190°C/2.16 kg is converted on monolayer heavy-duty sack lines where the primary cost-saving mechanism is downward gauge movement from 80 µm to 55 µm without sacrificing dart impact retention or tear propagation resistance. Surface moisture from silo discharge at relative humidity above 60% is removed with a hopper dryer at 60°C for 2 h when visible frost-line oscillation occurs at start-up. The formulation is either 100 wt% V208C3 or a dry blend containing 15–25 wt% high-pressure LDPE and 2.0–3.0 wt% carbon black masterbatch where outdoor UV stability is specified. A 90 mm single-screw extruder with 30:1 L/D feeds a 250 mm spiral mandrel die through a 2.2 mm die gap at a blow-up ratio of 2.8:1; raising BUR to 3.5:1 for higher layflat width induces periodic bubble oscillation and gauge variation above ±5% on a capacitance scanner. Barrel temperatures are 175/185/195/205/210°C from feed throat to adapter, melt temperature is held at 199–210°C, and screw speed is limited to 85 rpm because higher shear accelerates oxidative gel formation. Frost line height is set at 650–800 mm without internal bubble cooling; with IBC the frost line is lowered to 450–550 mm to increase machine-direction tear, but positions below 400 mm reduce transverse direction elongation under ASTM D882 to less than 600% and cause sack failure in drop loading. Slip and antiblock are added as 500–1000 ppm erucamide and 2000–5000 ppm synthetic silica with median particle size 5 µm; coefficient of friction on the finished sack wall is controlled below 0.40 under ASTM D1894. The converted article is a 55–120 µm heavy-duty sack, chemical sack, or FIBC liner requiring ASTM D1709 Method A dart impact above 160 g, ASTM D1922 Elmendorf tear above 3.0 N in machine direction, ASTM D882 tensile strength at yield above 20 MPa in transverse direction, and heat seal strength above 30 N/25 mm at 150°C with 0.5 s dwell. Pinhole count after flexing under ASTM F392 is held below 5 holes per 10 m² by backlight inspection.
Field failures in Vytek V208C3 silage wrap are concentrated in tack-and-weld zones where the film is stretched to 70–80% elongation and simultaneously exposed to condensed ammonia, UV radiation, and bale-wrapper abrasion. A 25–40 µm high-performance white-black or white-white three-layer silage wrap typically contains 88–92 wt% V208C3, 6–8 wt% titanium dioxide masterbatch, 0.6–1.2 wt% hindered amine light stabilizer masterbatch, 0.1–0.3 wt% benzotriazole UV absorber, and 500–800 ppm erucamide. The TiO₂ content is held below 9.0 wt% because higher loadings after 300 h of QUV per ASTM D4329 cycle A reduce transverse tear strength under ASTM D1922 to less than 2.0 N. Processing on agricultural film lines uses a BUR of 2.0–2.8:1, a die gap of 2.0 mm, and melt temperatures between 185°C and 205°C; a frost line below 500 mm improves dart impact and haze under ASTM D1003, but introduces excessive unbalanced orientation that lowers pre-stretch capacity below the 50–70% required by bale wrappers. Tensile elongation at break under ASTM D882 should remain above 600% in the transverse direction. When film is exposed outdoors for 12 months, formulations with less than 0.6 wt% HALS show chain scission at the bale shoulder, and weathered film melt flow rate rises above 1.4 g/10 min under ASTM D1238, indicating molecular weight loss. The finished wrap is a 25 µm structure screened by protrusion puncture with a 0.75 mm radius probe at 50 mm/min; published laboratory correlation data for this exact three-layer configuration is limited, and converters use ASTM D5748 protrusion puncture or field beta testing as screening criteria.
In a 50–120 µm nine-layer barrier film for dry and frozen food packaging, V208C3 is placed in the internal sealant layer at 15–25 µm and dry-blended with 15–30 wt% of a metallocene plastomer having melt index below 1.0 g/10 min to lower seal initiation temperature. The core contains nylon 6/66 or EVOH with ethylene content between 27 mol% and 44 mol%, and tie layers are anhydride-modified LLDPE at 4–6 µm per layer. Food-contact compliance is established under FDA 21 CFR 177.1520, read with 21 CFR 174.5 good manufacturing practice, and under EU No 10/2011 with overall migration below 10 mg/dm² using EN 1186-1 test conditions. Added slip is food-grade erucamide at 500–1000 ppm; below 400 ppm the coefficient of friction under ASTM D1894 rises above 0.40, while above 1200 ppm the coefficient drops below 0.10 and produces web tracking drift on vertical form-fill-seal lines. The sealant layer is processed through a 55–75 mm extruder with 24:1 L/D at 195–210°C, with die gap 1.8–2.4 mm and overall BUR 2.2–2.7:1. Hot-tack strength under ASTM F1921 Method B must exceed 4.0 N/25 mm at peak seal temperature between 95°C and 110°C, and seal initiation at 0.5 N/15 mm must occur below 105°C. Monolayer V208C3 blown film at 25 µm typically falls near 2.0–3.0 g/m²·day under ASTM F1249 at 38°C and 90% RH, but the nine-layer structure’s water vapor transmission rate is governed by the EVOH or nylon core, and published data for the exact barrier configuration is limited. Organoleptic acceptance is checked under DIN 10955 after water contact at 40°C for 10 days; any detectable paraffinic note is a rejection.
| Regulation or standard | Method or clause | Release requirement |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer specifications for food-contact polyethylene | Compliance with paragraph (c) specifications for density and extractables |
| EU No 10/2011 | EN 1186-1 overall migration | ≤ 10 mg/dm² |
| GMP 21 CFR 174.5 | Manufacturing process audit | No unlisted substance above threshold |
For antistatic drum liners converted from V208C3 at 50–120 µm, 2.0–4.0 wt% of a 50% conductive carbon black masterbatch is compounded to achieve surface resistivity between 1.0×10³ ohm/square and 1.0×10⁶ ohm/square under IEC 61340-2-3. The blown-film line uses a 65 mm extruder with 30:1 L/D, a die gap of 1.8 mm, and a BUR of 2.5:1; melt temperature is held at 190–200°C, and levels above 205°C produce shear-induced reagglomeration of carbon black that appears as localized high-resistivity islands on the reel. Increasing BUR above 3.0:1 reduces machine-direction tear under ASTM D1922 below 2.0 N and stretches the conductive network non-uniformly, while BUR below 2.0:1 creates visible outer-edge gel orientation. The liner is used as a steel drum or IBC insert for dry powders; the sealed closure is required to withstand 20 N/25 mm, and fill-drop testing from 1.2 m with 25 kg powder is performed on each new masterbatch lot. Chemical compatibility is limited to non-oxidizing inorganic salts and organic acids with pH not below 2.0; strong oxidizing acids, aromatic ketones, and unsaturated hydrocarbon solvents above 40°C are excluded until environmental stress crack resistance is verified under ASTM D1693. After 10 000 flex cycles per ASTM F392, surface resistivity above 1.0×10¹⁰ ohm/square indicates carbon black network disruption, and the liner is diverted to non-critical packaging.
In collation shrink bundling of 6–24 consumer units at 40–80 packs/min, Vytek V208C3 is blended at 15–30 wt% into a fractional-melt LDPE shrink base and extruded on a high-stalk bubble with a 2.0 mm die gap, a BUR of 3.0–4.0:1, and frost line height between 900 mm and 1200 mm. The processing window produces 60–80% transverse direction shrink and 20–40% machine direction shrink under ASTM D2732 after immersion at 130°C for 30 s. Loading above 35 wt% increases shrink tension above 4.0 MPa and generates burn-through holes at the overlap seal when dwell exceeds 0.8 s at 150°C; loading below 10 wt% fails to provide corner puncture resistance on corrugated trays. At 15–25 wt% V208C3, Elmendorf tear remains above 2.2 N in machine direction and 1.8 N in transverse direction, and dart impact under ASTM D1709 Method B remains above 100 g at 25 µm. Slip is set at 500–700 ppm erucamide to hold coefficient of friction below 0.35 without reducing sealability. The finished film at 19–38 µm runs on jaws with polytetrafluoroethylene-coated sealing bars; seal continuity is checked by air-leak test at 0.5 bar for 5 s, and online capacitance gauge variation must remain within ±2.0% because gauge variation above ±3.0% causes bottom-fold tearing and curl after shrinking.
Competitive Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin is a pelletized linear low-density polyethylene formulated for monolayer and coextruded blown film. The manufacturer’s technical datasheet lists a nominal density of 0.920 g/cm³ under ASTM D1505 and a nominal melt index of 0.8 g/10 min under ASTM D1238 at 190 °C/2.16 kg. The enhanced designation refers to a proprietary stabilizer and processing-aid package rather than to a single comonomer identity. The package is intended to shift bubble stability, melt-fracture onset, and film-to-film slip behavior during high-output blown film extrusion. Primary application areas reported for the grade include heavy-duty sacks, frozen-food packaging, agricultural silage wrap, laminating film, and industrial liners where puncture resistance and seal integrity are specified.
Table 1 reproduces representative values from the producer’s technical literature. These values are not certificate-of-analysis limits and are not intended as product specifications.
| Property | Test method | Representative value |
|---|---|---|
| Melt index | ASTM D1238 190 °C/2.16 kg | 0.8 g/10 min |
| Density | ASTM D1505 | 0.920 g/cm³ |
| Vicat softening point | ASTM D1525 1 kg | 108 °C |
| Tensile yield MD/TD | ASTM D882 25 µm film | 11.0/10.5 MPa |
| Elmendorf tear MD/TD | ASTM D1922 25 µm film | 180/380 g |
| Dart impact | ASTM D1709A 25 µm film | 110 g |
| Haze | ASTM D1003 | 12% |
| Gloss 45° | ASTM D2457 | 60 |
The distinction is operational rather than merely compositional. A standard butene-copolymer LLDPE at the same nominal density and melt index typically shows transverse-direction Elmendorf tear in the 200–250 g range for 25 µm film, while enhanced higher-α-olefin formulations of similar bulk density frequently reach 350–400 g under comparable fabrication conditions. The improvement is not linear across gauge and depends on the concentration of high-molecular-weight species that tie adjacent crystallites. The processing-aid package in V208C3 shifts the onset of sharkskin melt fracture to higher screw speeds, but it does not alter the fundamental tensile yield of the resin. Secant modulus at 2% strain remains within the 180–240 MPa envelope typical of conventional LLDPE. The commercial difference therefore appears in bubble stability, gauge uniformity, and the ability to maintain puncture resistance after downgauging, rather than in a large increase in stiffness.
Film-to-film slip behavior also differs from standard LLDPE because the additive package follows time-temperature migration kinetics in the polymer matrix. At storage temperatures below 15 °C, slip bloom is retarded. Film aged 24 h at 23 °C may show kinetic COF above 0.4, whereas after 72 h at 40 °C the same film can fall to 0.20–0.25. Converters performing immediate lamination or printing should condition reels at 23–30 °C before surface-wetting or bonding operations to reduce variation in surface energy and coefficient of friction.
On blown film lines with grooved-feed single-screw extruders of 55–75 mm barrel diameter and 24:1 or greater L/D, the start-up profile is usually set to a barrel temperature of 150–180 °C in the feed zone, rising to 190–210 °C at the die. Melt temperature measured at the adapter should be held between 193 °C and 216 °C for film gauges from 20 µm to 80 µm. At adapter temperatures below 190 °C, drive-torque rise and melt-pressure fluctuation increase. At temperatures above 232 °C, surface oxidation and gel formation become more probable, particularly in high-regrind streams. Die gap settings between 1.5 mm and 2.5 mm are typical. A blow-up ratio of 2.0:1–2.5:1 balances machine-direction and transverse-direction orientation, while a frost line height of 8–12 die diameters is common for general-purpose 25 µm film.
Pre-drying is generally unnecessary when pellets are stored in sealed packaging. If exposed to relative humidity above 60% for extended periods, surface moisture can produce microvoids at high throughput, although published grade-specific moisture data is limited. Regrind addition above 30% is not recommended for critical optical applications because the enhanced stabilizer package has limited scope to protect reprocessed material from cumulative thermal-oxidative degradation. The practical upper temperature limit is therefore set by surface oxidation and bubble instability rather than by the melting point of the base polymer.
Bubble instability on high-output lines is frequently attributed to melt index variation alone. In practice, the more actionable variables are die-lip cleanliness, air-ring pressure balance, and internal bubble cooling. The processing-aid package in V208C3 suppresses sharkskin within a defined shear-rate window, but it cannot compensate for a worn die lip with surface roughness above 0.2 µm Ra or for melt-temperature nonuniformity greater than ±3 °C across the die circumference. When melt-pressure fluctuation exceeds 0.5 MPa at constant screw speed, the first corrective action should be inspection of the die-lip land and screw-cooling circuit before changing resin lot. Published data for V208C3 under extreme shear rates above 1200 s⁻¹ is limited; processors running specialized high-velocity dies should validate melt-fracture performance on production equipment.
At 25 µm and below, dart impact strength becomes more sensitive to film-thickness variation than to average tensile yield. A localized thickness reduction of 10% in 20 µm film can concentrate puncture stress and reduce dart impact by 20–30% relative to film with gauge control of ±2%. The failure mode shifts from ductile puncture to brittle tear initiation in the transverse direction when blow-up ratio is below 2.0:1 or when the frost line is too low. In blown film converted into heavy-duty sacks, machine-direction tear resistance is typically the limiting property for drop-impact failure along fold lines, while transverse-direction tear resistance governs puncture from sharp edges. V208C3 improves gauge uniformity by stabilizing bubble diameter, but the resin does not remove the need for mechanical gauge profiling.
At 50 µm, the resin’s dart impact is commonly reported in the 200–250 g range under ASTM D1709A. At 20 µm, the value does not halve proportionally and may fall below 80 g if fabrication conditions are not optimized. These values are representative and depend on blow-up ratio, die gap, frost line height, and air-ring conditions. Puncture resistance measured by ASTM D5748 can be used to differentiate lot-to-lot film, but published data for V208C3 in this specific configuration is limited. Consequently, converters should establish internal gauge-dependent dart impact and tear curves rather than extrapolating from a single film thickness.
In coextruded structures, V208C3 is commonly placed in a skin or core layer where its process stability supports thin-gauge downgauging. It is compatible with conventional LLDPE tie layers and EVA seal layers. However, blending with ionomer or high-acid copolymers may alter slip-agent migration rate and should not be assumed without laminate testing. For frozen-food packaging laminates, the seal initiation temperature of the present grade is typically 5–8 °C lower than a standard LLDPE of equal nominal density, permitting a lower jaw setpoint on vertical form-fill-seal equipment. The exact reduction depends on seal-bar dwell time, jaw pressure, and film thickness; processors should verify against hot-tack and seal-strength curves obtained under ASTM F1921 and ASTM F88/F88M.
Compared with conventional butene-copolymer LLDPE at the same nominal melt index and density, V208C3 generally improves bubble stability and transverse-direction tear without increasing density or melt index. The trade-off is optical. Metallocene-catalyzed LLDPE grades typically show haze below 7% and gloss above 70 at 25 µm, while the present enhanced grade is expected to remain in the 10–15% haze range and 55–65 gloss. Metallocene resins often exhibit lower melt elasticity and require narrower die gaps. Older blown film lines designed for Ziegler-Natta LLDPE may experience greater backpressure reduction and fewer melt-fracture episodes with V208C3 than with a metallocene grade of identical melt index. The enhanced processing-aid package also allows higher output before melt fracture, but it does not confer the low seal initiation or high hot tack characteristic of some single-site catalyzed plastomers. Selection between V208C3 and such materials should be made on the basis of end-use seal requirements, optical specifications, and available extruder torque.
Table 2 lists regulatory references commonly associated with this resin type. Current supplier documentation should be consulted for grade-specific certification.
| Reference | Designation | Applicability |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520 | Olefin polymer base; final article must meet extractives limitations |
| EU food contact | Regulation (EU) No 10/2011 | Compliance statement per grade and migration model |
| RoHS | Directive 2011/65/EU | Polyolefin base is not a typical restriction; supplier declaration for additives required |
| REACH | Regulation (EC) No 1907/2006 | Monomer and additive registration status in SDS |
In agricultural silage wrap, the resin is often placed in the core or non-tack outer layer at 20–30% of total film thickness. Puncture resistance supports bale integrity during high-density storage and handling. UV stabilization is supplied by a concentrate rather than by the base resin. In heavy-duty sacks, the improvement in bubble stability permits consistent gauge down to 18 µm on high-output lines, but tensile yield remains close to conventional LLDPE. Film design should not rely on V208C3 for creep resistance under sustained load. The resin is not recommended for extended outdoor exposure without adequate carbon black or hindered-amine light stabilizer addition, and it should not be combined with amine-based additives that may interfere with the enhanced stabilizer package.