Chevron Phillips Vytek V205e9 Enhanced Lldpe Blown Film Resin

Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin

    • Product Name: Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 449098
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.920 g/cm3
    Melt Index 190 C 2 16 Kg 0.50 g/10 min
    Melting Point 125 °C
    Vicat Softening Point 105 °C
    Tensile Strength At Yield 1500 psi
    Tensile Strength At Break 5000 psi
    Elongation At Break 700%
    Modulus Of Elasticity 30000 psi
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 200 g
    Haze 12%
    Gloss 65%

    As an accredited Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing This resin is packaged in 25 kg (55 lb) polyethylene bags, with 50 bags per pallet (1,250 kg).
    Container Loading (20′ FCL) 20′ FCL loading: Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin, 25 kg bags, palletized, stretch-wrapped, approx. 18–20 MT.
    Shipping Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin is generally shipped in 25 kg polyethylene bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Store and transport in a dry, clean area away from heat, direct sunlight, moisture, and sharp objects. Follow SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers or bags tightly closed to prevent contamination and dust accumulation. Avoid prolonged exposure to high temperatures and UV light. Use first-in, first-out stock rotation. Do not store near strong oxidizers. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 12 months from manufacture when stored cool, dry, and in unopened original packaging; avoid direct sunlight.
    Application of Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin

    In laminated dry-food packaging, the sealant web is often extruded from Chevron Phillips Vytek™ V205E9 enhanced LLDPE on a monolayer blown film line. A production-qualified formulation for a 40 µm sealant web comprises 90 wt% V205E9, 7 wt% high-pressure LDPE with a melt index below 0.4 g/10 min, and 3 wt% silica-based antiblock masterbatch; slip agents are deliberately omitted where the film is intended for ink or solvent-based adhesive lamination to avoid bond-strength decay. The line is typically equipped with a 45 mm grooved-feed extruder at L/D 24:1, a 1.8 mm annular die gap, and a dual-lip air ring. Melt temperature is held between 216 °C and 232 °C, with a blow-up ratio of 2.2:1 to 2.8:1 and a frost-line height of 3 to 5 die diameters. A lower frost line produces a rapidly quenched film with elevated haze and reduced ink adhesion on the outer lamination ply, while an excessively tall frost line can destabilize the bubble when LDPE content drops below 5 wt%. On production lines, melt-pressure spikes above 420 bar have been traced to insufficient LDPE melt miscibility when the LDPE addition is below 5 wt%. The film is corona-treated in-line to 38–42 mN/m surface energy and wound with controlled tension to avoid blocking; the treated surface is stored at 20–25 °C and ≤50% relative humidity to limit additive bloom that reduces adhesion. Regulatory compliance for direct food contact follows FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² tested under EN 1186-1, and GB 4806.7 for China-bound structures. Finished structures are converted into pillow pouches for dry mixes, side-gusseted coffee bags, bakery bag liners, and cereal carton liners.

    Food-contact compliance matrix for V205E9 laminated sealant webs
    RegionStandard / RegulationRequirement Applied to Sealant Web
    United StatesFDA 21 CFR 177.1520Olefin polymer specification; finished food-contact article must meet extraction limits for food types and conditions of use.
    European UnionEU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm² using EN 1186-1; declaration of compliance required under Article 16.
    ChinaGB 4806.7Food-contact plastic resin and article conformity, including sensory and migration testing.

    What Changes When the Sealant Layer Must Survive −40°C Distribution?

    Blown film structures for frozen vegetables, IQF proteins, and ice cream overwrap are produced with V205E9 as the toughness core, but monolayer sealant webs are generally modified with a metallocene polyolefin plastomer when sealing jaws operate below −30 °C. A coextruded three-layer structure may run 80 wt% V205E9 in the core and plastomer-rich skins of 10–20 wt%; the plastomer reduces heat-seal initiation temperature to 85–95 °C on laboratory sealers, but it also lowers film stiffness. The production line uses three extruders feeding a 250 mm annular die with 1.5 mm gap, internal bubble cooling, and an outer stack air ring. Melt temperatures are limited to 210–220 °C because frozen-food film produced above 230 °C may carry oxidized gels that appear as specks in printed areas. Low-temperature fitness is tested by ASTM D1709-16a dart impact at −18 °C, ASTM D1790 brittleness temperature, and ASTM F88/F88M seal strength after conditioning at −40 °C for 24 h. Because heat-seal performance is strongly dependent on jaw pressure, dwell time, and film gauge, published data for V205E9 in plastomer-rich frozen-food configurations is limited; target-line seal curves are required before full-scale conversion. Compliance follows FDA 21 CFR 177.1520 for direct food contact and EU Regulation (EU) No 10/2011; printing inks and varnishes are selected from lists meeting EC 2023/2006 good manufacturing practice. In commercial practice, the finished web is converted into frozen vegetable pouches, IQF seafood bags, ice cream novelty overwrap, and frozen poultry liner films.

    Thick-Gauge Liners Fail by Tear Propagation Before Tensile Yield

    Tear propagation, rather than tensile yield, typically determines service life in thick-gauge industrial liners. In a heavy-duty FIBC liner or drum liner, V205E9 is processed at 125–250 µm gauge with 92–100 wt% V205E9 and 0–8 wt% post-industrial reclaim; carbon black masterbatch is added at 2–3 wt% only when the liner is stored outdoors. The extrusion line is specified with a 65 mm grooved-feed extruder at L/D 30:1, a 350 mm die with 2.2–3.0 mm lip gap, and internal bubble cooling. Output ranges from 200–350 kg/h; melt temperature should not exceed 245 °C, because elevated gel formation appears as puncture-initiation sites. A low blow-up ratio of 1.8:1 to 2.2:1 is preferred for tear resistance in the machine direction, while a higher BUR improves transverse direction tear but reduces MD stiffness. Screen packs of 100–120 mesh are installed ahead of the die to remove carbon specks and oxidized film fragments that would otherwise act as tear nuclei. Qualification test battery: ASTM D1709-16a for dart impact, ASTM D1004 for initial tear, ASTM D1922 for Elmendorf tear, ASTM F88/F88M for heat seal, and ISO 21898 for FIBC component fitness where the liner is inserted into a woven outer bag. Commercial articles produced from this film include FIBC liners for hygroscopic powders, drum liners for resins and coatings, hazardous-waste collection bags, and construction debris liners.

    Qualification test battery for thick-gauge industrial liners produced from V205E9
    TestStandardCondition / Purpose
    Dart impactASTM D1709-16aMethod A, 38 mm dart, 23 °C; puncture energy absorption.
    Initial tearASTM D1004Die-cut geometry; tear initiation force.
    Elmendorf tearASTM D1922Propagating tear in MD and TD; compare orientation.
    Seal strengthASTM F88/F88MHeat-seal seam at production dwell and pressure.
    FIBC linerISO 21898Component suitability for flexible intermediate bulk containers.

    When silage clamp covers are stretched over a horizontal bunker after compaction, the film must retain oxygen barrier properties after six months of UV exposure and contact with silage effluent. V205E9 serves as the core layer in a three-layer white/black cover film at 150–200 µm. A production formulation comprises 60–75 wt% V205E9 core, 15–25 wt% metallocene LLDPE for tear recovery, and 10–15 wt% white or black masterbatch containing hindered amine light stabilizers and carbon black or titanium dioxide. The white outer layer contains 2–4 wt% TiO₂ to reflect solar load, and the black inner layer contains 2–3 wt% carbon black to suppress light transmission to the crop. Extrusion is performed on a three-layer blown film line with die gap 2.0–2.4 mm, BUR 2.5:1 to 3.5:1, and melt temperature 200–220 °C. Wide-web units of 1.5–3.0 m collapsed width are used, requiring automatic gauge control to maintain variation within ±5%. Roll hardness is controlled by taper tension to avoid blocking during outdoor storage, because blocked film tears at the unwinding brake and creates spoilage points on the bunker. Compliance for agricultural covering films is assessed under EN 13206:2017, with tensile properties per ISO 527-3 and ultraviolet stability per the standard's exposure conditions. REACH Annex XVII restrictions apply to any hazardous masterbatch components. Roll widths are slit to bunker dimensions and delivered as silage clamp covers, grain bunker covers, temporary silage bags, and compost heap covers.

    Greenhouse Roof Film and IR Retention in Forced-Air Polytunnels

    A greenhouse roof film produced with V205E9 must balance photosynthetically active radiation transmittance, condensation control, and multi-season mechanical stability. A three-layer coextruded greenhouse film commonly blends 70–85 wt% V205E9 with 10–20 wt% high-transparency LDPE and 5–10 wt% ethylene-vinyl acetate containing 14–18% vinyl acetate for infrared retention and flexibility at low night temperatures. UV stabilizer masterbatch is added at 1.5–2.5 wt% in the outer layer. The die gap is 2.0 mm, blow-up ratio 2.5:1 to 3.5:1, melt temperature 190–220 °C, and collapsed width may reach 3–7 m. Blown film lines used for greenhouse production are often fitted with internal bubble cooling and automatic layflat width control; gauge non-uniformity above ±7% has been associated with premature mechanical failure at gutter attachments. Die lip build-up from EVA decomposition at 220 °C after 6–8 h of continuous extrusion requires purge schedules on longer production campaigns. Standard references include EN 13206:2017 for agricultural covering films, ASTM D1003 for luminous transmittance and haze, and ISO 527-3 for tensile modulus and elongation. Published data for V205E9 in EVA-containing multi-season greenhouse structures is limited; outdoor weathering trials at the target site are required before selecting a stabilizer package. The greenhouse market procures the film as multi-season cladding, low tunnel film, shade film, and polytunnel door panels.

    Below concrete slabs placed on grade, a polyethylene membrane extruded from V205E9 is positioned as a capillarity break and vapor retarder. The film is produced from 95–100 wt% V205E9 with 0–5 wt% carbon black masterbatch; post-industrial reclaim is excluded when the membrane is specified as a radon barrier or when ASTM criteria demand virgin material. Production is performed on a wide-web blown film line with a die diameter of 600–1,200 mm, a lip gap of 2.0–2.8 mm, BUR 1.8:1 to 2.4:1, and melt temperature 215–235 °C. The collapsed width is typically 3.0–7.5 m, and thickness ranges from 150–300 µm. On such lines, edge-curl and blocking can interrupt flatness during slab placement; antistatic or anti-block additives are used at 0.5–1.5 wt% where field handling requires immediate lay-flat performance. The membrane is field-seamed with double-sided butyl tape at overlaps, so tear resistance and thickness uniformity at the seam are critical to prevent moisture intrusion. Compliance is established by ASTM E96/E96M-22 for water vapor transmission, ASTM D4397 for polyethylene sheeting suitable for construction, and ACI 302.2R sub-slab vapor barrier recommendations. The construction distribution channel handles this film as underslab vapor barriers, crawl space liners, radon barriers, and temporary weather-protective membranes.

    Free Quote

    Competitive Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin is a pelletized ethylene-alpha-olefin copolymer developed for high-output blown film conversion. The manufacturer’s published data identify a nominal melt index of 0.9 g/10 min when measured under ASTM D1238 at 190 °C with a 2.16 kg load and a nominal density of 0.920 g/cm³ when measured under ASTM D1505. The “Enhanced” designation refers to a controlled molecular architecture intended to reduce melt-fracture sensitivity and to elevate dart impact relative to conventional linear low density polyethylene grades of equivalent melt index. Lot-specific certification values govern the conversion process; nominal published values do not replace a certificate of analysis.

    The resin is positioned for monolayer and coextruded film structures requiring down-gauging, puncture resistance, and seal integrity. Typical blown film lines include annular dies from 50 mm to 150 mm diameter and single-screw extruders with 24:1 to 30:1 length-to-diameter ratio. Because the resin is an enhanced ethylene-alpha-olefin system, it differs from simple butene-copolymer LLDPE in that the comonomer distribution and molecular weight distribution are balanced to preserve machine-direction tear while improving dart impact and reducing film haze. Published data for this specific configuration in all film structures are limited; converter trials on the target line remain necessary for final gauge and property confirmation.

    Product differentiation is also evident in extrusion energy consumption. On grooved-feed extruders with 25:1 L/D, the enhanced resin generally displays lower specific energy input than a conventional Ziegler-Natta butene copolymer at equivalent melt temperature and screw speed. The reduction is not uniform across all conditions; if the screw has a restrictive Maddock mixing section, the lower viscosity may permit higher screw speed before motor current limits are reached, but melt quality depends on the mixing element design. Published comparative data are limited to specific extruder configurations; measured amperage, melt pressure, and output rate should be collected for the target line.

    Does the Comonomer Distribution Explain the Difference in Dart Impact and Elmendorf Tear?

    Dart impact and Elmendorf tear respond differently to comonomer placement in linear low density polyethylene. In conventional butene-copolymer LLDPE, short-chain branches from butene are distributed across the molecular weight spectrum; the result is improved toughness relative to high-pressure LDPE, but machine-direction tear is often lower after orientation because the lamellar network and tie-chain population are not fully optimized. Enhanced LLDPE grades such as V205E9 are designed with a structured comonomer insertion that increases the population of tie molecules between lamellae. A film formed under a 2.5:1 blow-up ratio and a 25 µm gauge may exhibit a more isotropic tear balance than a butene copolymer of similar density. Comparative data should be generated under ASTM D1922 and ASTM D1709 Method A; published data for this specific configuration is limited, so laboratory values should not be extrapolated to high-speed form-fill-seal films without pilot-line verification.

    Differences from metallocene-catalyzed LLDPE are relevant. Metallocene grades usually exhibit narrow molecular weight distribution, low extractables, and high clarity, but they may generate higher extruder backpressure and can be sensitive to melt fracture at high shear rates. Vytek™ V205E9 Enhanced LLDPE is intended to reduce that sensitivity while retaining clarity and toughness. The melt index of 0.9 g/10 min places the grade in a viscosity band suitable for blown film without excessive barrel pressure; however, pressure is also a function of die gap, melt temperature, and throughput. Increasing melt temperature from 190 °C to 220 °C lowers viscosity and reduces die pressure but can delay frost line stabilization if air-ring cooling is not adjusted. The practical processing window is therefore defined not by melt index alone, but by the interaction of extruder screw speed, die gap, blow-up ratio, and air-ring temperature.

    Capillary rheometry at 190 °C over shear rates from 100 s⁻¹ to 1,000 s⁻¹ is used to compare lot-to-lot consistency. The melt flow ratio determined as I21.6/I2.16 is often used as a rough indicator of shear sensitivity; a higher ratio indicates greater shear thinning. For Vytek™ V205E9, the melt index and density define the grade, but the melt flow ratio should be obtained from the certificate of analysis. Variation in melt flow ratio beyond the supplier specification may affect die pressure and bubble stability, even when the melt index remains within nominal limits.

    Test method designations commonly referenced for blown film property reporting
    PropertyMethodUnit
    Melt indexASTM D1238g/10 min
    DensityASTM D1505g/cm³
    Dart impactASTM D1709 Method Ag
    Elmendorf tearASTM D1922gf
    Tensile propertiesASTM D882MPa
    HazeASTM D1003%
    Gloss 45°ASTM D2457GU
    Hot-tack strengthASTM F1921N

    Die Gap, Frost Line Position, and Bubble Cooling

    Blown film extrusion of Vytek™ V205E9 is commonly run with die gaps from 0.8 mm to 2.0 mm. Narrow die gaps increase shear rate, reduce melt residence time in the die, and improve gauge uniformity, but they may increase melt fracture unless melt temperature is raised or polymer processing aid is added. Wide die gaps reduce backpressure but can produce thicker melt webs that require higher frost line position to control orientation. The frost line is typically maintained at 5 to 7 die diameters above the die face; a lower frost line freezes the bubble before sufficient transverse orientation develops, while a higher frost line increases crystallinity and often reduces dart impact. The relationship is process-specific and must be validated with on-line gauge profiling.

    At high output rates above 150 kg/h, dual-lip air rings or internal bubble cooling are used to remove heat from the bubble without deforming the melt. If the air-ring velocity is too high, the bubble may oscillate in the transverse direction, producing thick-thin lanes. Bubble stabilizers, calibrated iris, or ultrasonic film scanners can detect gauge variation. The resin’s enhanced molecular architecture reduces the onset of draw resonance relative to high-melt-index linear low density resins, but it does not eliminate the need for a stable air and temperature environment. Ambient air drafts below 0.5 m/s are preferred; open windows, floor fans, or adjacent chillers can produce localized cooling defects.

    During start-up, a lower-viscosity high-pressure LDPE purge grade may be used to clear polypropylene, EVA, or ionomer residues. Transitioning from a higher-density polyethylene to V205E9 requires a die purge at 180 °C to 200 °C until the melt is free of gels and specks. Avoid prolonged hold times above 240 °C, because oxidative chain scission or crosslinking can degrade film appearance and reduce impact strength. The resin should not be pre-dried unless condensation is present; if pellets have been stored below dew point, hot-air drying at 60 °C to 80 °C for 2 h to 4 h removes surface moisture. Internal moisture is negligible, so drying is not a substitute for proper purging.

    Surface melt fracture appears as sharkskin on the film and is usually observed at die gaps below 0.8 mm and high output rates. Adding fluoropolymer processing aid at 200 ppm to 600 ppm conditions the die lip and reduces sharkskin, but the benefit may require 20 min to 60 min to develop after the processing aid is introduced. Die lip build-up can also occur with some antiblock or slip masterbatches; ceramic-coated die lips or periodic purging may be required on long campaigns.

    In heavy-duty sacks and bulk liners, the film is often coextruded as a three-layer A/B/A structure. The outer layers may contain a higher-density polyethylene to provide abrasion resistance, while the core or seal layer uses an enhanced LLDPE such as Vytek™ V205E9 to provide seal strength and dart impact. On a 40 mm grooved-feed blown film line running at 2.5:1 BUR and 25 µm gauge, film evaluations under ASTM D882 measure tensile properties after machine and transverse direction conditioning; seal initiation data are generated on laboratory heat sealers with 0.5 MPa seal pressure and 1 s dwell. The product is used in form-fill-seal packaging, agricultural silage wrap, frozen food pouches, collation shrink film, and carrier bags. The selection of slip and antiblock masterbatch is line-specific; typical antiblock loadings range from 2,000 ppm to 6,000 ppm in the outer layer, and slip is often added at 500 ppm to 1,500 ppm to reduce coefficient of friction. Because the resin contains a base stabilization package, additional antioxidant dosage should only be made after oven-aging or oxidative induction time data are reviewed.

    Differences from high-pressure LDPE are substantial. LDPE has long-chain branching, which provides high melt strength and easy bubble control, but lower dart impact and limited down-gauging relative to linear low density polyethylene. V205E9 provides higher puncture resistance and can be drawn to lower thicknesses while maintaining load retention. However, blending with 10 wt% to 30 wt% LDPE is common when improved optical appearance, deeper draw, or higher shrink tension is required. The blend ratio changes bubble stability and seal behavior; converters should not assume that the same temperature profile and frost line position can be used for pure V205E9 and LDPE-containing formulations.

    The film is often corona treated to improve ink adhesion. Surface tension should be raised to at least 38 mN/m for solvent-based inks or 42 mN/m for water-based inks. Excessive treatment above 46 mN/m can create low molecular weight oxidized species and reduce seal strength. Treatment level depends on film thickness, line speed, and electrode condition; dyne pens and contact-angle measurements are used for verification.

    When LDPE Blending Is Required for Shrink, Seal, or Optical Performance

    LDPE blending modifies the long-chain branching content and can reduce the film’s tensile modulus while increasing shrink tension. In a V205E9/LDPE system, the addition of 10 wt% LDPE improves bubble stability on high-stalk extrusion lines because the long-chain branching increases strain-hardening. At 30 wt% LDPE, the film may exhibit lower dart impact and higher haze than pure V205E9; therefore, the selection is a compromise between optical clarity and process stability. Blends should be tumble-mixed uniformly before entering the extruder hopper, or metered by gravimetric feeders. Static mixing and screen-pack selection at 80 mesh to 120 mesh can reduce gel streaks. The use of high-shear barrier screws may generate overheating in the LDPE phase; melt temperature should be monitored at the die adapter rather than the barrel zones, because localized shear heating can exceed the setpoint by 10 °C to 15 °C.

    The heat seal performance of V205E9-containing films is governed by seal bar temperature, dwell time, and sealing pressure. Standard laboratory seals are made at 0.5 MPa for 1 s; hot-tack strength is measured under ASTM F1921. In form-fill-seal packaging, the seal layer must survive package weight immediately after sealing; higher molecular weight linear low density resins typically provide greater hot-tack than high-pressure LDPE, but the exact value depends on comonomer distribution. Converters often set the seal bar temperature 10 °C to 20 °C above the film’s seal initiation temperature to ensure seal through contaminant. Because Vytek™ V205E9 is an enhanced LLDPE, seal initiation is generally lower than that of high-density polyethylene but higher than that of metallocene plastomers. The final seal specification should be verified under ASTM F88 peel testing on the target packaging machine.

    Regulatory references relevant to polyethylene blown film
    ReferenceScopeConverter obligation
    FDA 21 CFR 177.1520Olefin polymers for food-contact useVerify density, extractables, and end-use conditions
    Regulation (EU) No 10/2011Plastic food-contact materialsDeclaration of compliance and migration testing

    Regulatory status should be confirmed through the supplier’s compliance documentation. Polyethylene grades in this class are generally evaluated for food contact under 21 CFR 177.1520 and Regulation (EU) No 10/2011; specific migration limits, additive restrictions, and end-use conditions remain the converter’s responsibility. The resin is not intended for medical implant use. Storage should be in a clean, dry area below 50 °C and away from direct sunlight. Open bags should be protected from dirt and condensation. If a bag is exposed to high humidity, surface moisture on pellets can create splay or bubbles; dry air purging of the hopper may be used. The product should not be blended with amine-based masterbatches unless compatibility is confirmed, because some amine stabilizers can cause color bodies or odor. Fluoropolymer processing aid is compatible at recommended dosages of 200 ppm to 600 ppm when melt fracture or die lip build-up occurs.