| HS Code | 394582 |
| Productname | Chevron Phillips Vytek V205C6 Enhanced LLDPE Blown Film Resin |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene-1 |
| Meltindex 190c 2 16kg | 0.50 g/10 min |
| Density | 0.920 g/cm3 |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 94 °C |
| Crystallizationtemperature | 105 °C |
| Tensilestrengthatbreak Md | 5000 psi |
| Tensilestrengthatbreak Td | 4500 psi |
| Elongationatbreak Md | 600 % |
| Elongationatbreak Td | 700 % |
| Elmendorftearstrength Md | 250 g |
| Elmendorftearstrength Td | 400 g |
| Dartimpactstrength | 300 g |
| Haze | 10 % |
| Gloss 45deg | 60 |
| Coefficientoffriction | 0.20 |
| Recommendedfilmthickness | 1.0 mil |
As an accredited Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Vytek V205C6 resin is supplied in 25 kg (55 lb) polyethylene bags on pallets; bulk quantities available. |
| Container Loading (20′ FCL) | 20′ FCL loading: 25 kg bags of Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin, palletized, stretch-wrapped, and secured. |
| Shipping | Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin ships as nonhazardous solid pellets, typically in 25-kg bags, bulk bags, or bulk trucks/railcars. Transport in clean, dry, covered equipment. Store away from heat, sunlight, and moisture. Maintain package integrity; avoid punctures and contamination. No special DOT/IMDG/IATA hazard classification. |
| Storage | Store Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin in a cool, dry, well-ventilated warehouse at ambient temperature. Keep packaging closed, off the floor, and away from direct sunlight, heat, moisture, and ignition sources. Avoid contamination and excessive stacking. Protect from prolonged UV exposure. Rotate stock first-in, first-out. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typical shelf life is 24 months from manufacture when stored in original packaging, cool, dry, and away from direct sunlight. |
Hexene-based enhanced LLDPE with a narrow short-chain branching distribution is processed into 220–260 µm coextruded three-layer films used as inner liners for FIBCs and heavy-duty chemical sacks. The core layer contains 60–70 wt% Vytek V2050C6, while the skin layers contain 20–30 wt% LDPE with a melt mass-flow rate of 0.25–0.35 g/10 min determined by ISO 1133-1:2022 at 190 °C/2.16 kg and 2–4 wt% of a silica-based antiblock/slip masterbatch; LDPE addition in the skins is held below 30 wt% because exceeding this threshold reduces low-temperature dart impact and increases notch sensitivity at liner fold creases. Regulatory compliance for dangerous goods liners is verified under 49 CFR 178.503, with puncture resistance measured by ASTM D5748-95(2019) and dart impact by ASTM D1709-16ae1 method B. Film conversion takes place on 75–90 mm grooved-feed extruders with 30:1 L/D and a 250–350 mm internal bubble cooling die, using a die gap of 2.4–2.8 mm, melt temperatures of 190–215 °C, and blow-up ratios between 2.2:1 and 2.8:1; heat sealing of finished liners is carried out on impulse sealers at 120–150 °C with 0.3–0.6 s dwell. End products include UN-rated FIBC liners, bulk chemical shipping sacks, and valve sacks for precipitated silica, carbon black, and titanium dioxide transfer.
On 135–200 µm three-layer agricultural films, the enhanced resin is dry-blended at 70–85 wt% with 10–20 wt% metallocene-catalyzed LLDPE and 5–15 wt% LDPE to maintain bubble sleeve stability; hindered amine light stabilizer masterbatch at 2–4 wt% and an anti-fog/anti-dust concentrate at 1–2 wt% are metered into the core and inner skin layers, respectively. Compliance in this segment is anchored to EN 13206:2017 for bale wrap film mechanical stability under silage storage conditions and to ISO 4892-2:2021 for accelerated xenon-arc weathering of the greenhouse film surface. Processing is performed on tower blown-film lines with 300–450 mm dies and internal bubble cooling, operating at a die gap of 1.8–2.4 mm, melt temperatures of 180–210 °C, and blow-up ratios from 2.5:1 to 3.0:1; long-stalk bubble geometries with frost-line heights of 8–12 die diameters are used to suppress bubble instability caused by high HALS loading. End products include silage bale wrap, greenhouse side sheets, and low-tunnel covers where transverse tear propagation at fold edges is the dominant field failure mode.
| Property | Test method | QC conditioning |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg |
| Density | ISO 1183-1:2019 | 23 °C, immersion |
| Tensile properties | ISO 527-3 | 500 mm/min |
| Dart impact | ISO 7765-1 method A | 23 °C, 50% RH |
| Elmendorf tear | ISO 6383-2 | 23 °C, 50% RH |
| Puncture resistance | ASTM D5748-95(2019) | 250 mm/min |
| Kinetic coefficient of friction | ISO 8295 | 23 °C |
| Haze | ISO 14782:2021 | 23 °C |
| Gloss | ASTM D2457-13 | 60° angle |
| Water vapor transmission rate | ASTM F1249-20 | 38 °C, 90% RH |
| Oxygen transmission rate | ASTM D3985-17 | 23 °C, 0% RH |
Blown film structures destined for frozen vegetables, IQF seafood, and ice cream packaging are run at total gauges of 50–90 µm and must retain seal integrity after product impact at −20 °C. In these structures, V2050C6 is used at 65–80 wt% with 20–30 wt% LDPE and 5–10 wt% EVA containing 18% vinyl acetate to lower seal initiation temperature; slip/antiblock masterbatch is added at 1–3 wt%, with erucamide levels limited to 300–600 ppm in the food-contact layer to prevent void formation during frozen product drop tests. Food-contact compliance is verified under 21 CFR 177.1520(c) 3.2 and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; seal strength is measured by ASTM F2029-16 using 25 mm strips sealed at 110–135 °C and 0.5 s dwell. Processing is completed on coextrusion lines with 200–300 mm dies, die gaps of 1.5–1.9 mm, melt temperatures of 175–200 °C, and BUR 2.3:1–2.7:1; flame or corona treatment is avoided on the seal side to retain hot-tack strength. End products include frozen vegetable bags, seafood pouches, ice cream sleeves, and stand-up pouches with zipper reclosure.
Sealant webs for dry soup powders, beverage sachets, and spice pouches are configured as three-layer asymmetric blown films in which the food-contact layer contains 65–85 wt% V2050C6, 15–30 wt% LDPE, and optionally 5–10 wt% ethylene-1-octene plastomer to reduce seal initiation below 95 °C. Compliance is established under 21 CFR 177.1520 for the polyolefin layer, EU Regulation (EU) No 10/2011 for overall migration, and 21 CFR 175.105 for the solventless laminating adhesive placed on the outside web. The sealant film is produced at 50–80 µm on 250–330 mm dies with a die gap of 1.4–1.8 mm, melt temperatures of 185–210 °C, and BUR 2.0:1–2.5:1; after wind-up, the film is corona-treated to 42–46 mN/m and laminated to BOPP, PET, or metallized OPP using a two-component solventless adhesive at 2.0–2.5 g/m² coating weight. Seal strength is controlled to ≥18 N/25 mm at 130 °C and 1 s dwell per ASTM F88/F88M-21, while kinetic coefficient of friction is targeted below 0.25 by ASTM D1894-14 to permit reliable belt tracking on auger fillers. End products include four-side-seal dry soup pouches, stick packs for instant coffee, and spice sachets.
Vertical form-fill-seal lines running at 90–110 pouches/min with 0.15–0.25 s jaw dwell expose films to high seal-area stress in detergent and surfactant-containing powder packaging. In these applications V2050C6 is used at 80–90 wt% with 10–15 wt% LDPE and 0.5–1.0 wt% of a fluoropolymer processing aid to delay die-lip buildup at mass output rates above 180 kg/h; the formulation is intentionally not plasticized because ester additives used in similar films can accelerate environmental stress cracking in contact with nonionic surfactants. Compliance is verified by ASTM D1693-15b condition A with 10% Igepal CO-630, with converter internal controls requiring ≥500 h to 50% failure at 50 °C. The blown film process uses 45–65 mm extruders equipped with barrier screws, 75–130 mm dies, die gaps of 1.0–1.4 mm, melt temperatures of 190–220 °C, and BUR 2.0:1–2.4:1; slit widths are held to ±1 mm to avoid tracking drift on high-speed FFS units. End products include detergent unit-dose overwrap, dishwasher powder sachets, and swimming pool chemical stick packs.
| Segment | Jurisdiction | Standard or regulation | Critical test limit or requirement |
|---|---|---|---|
| Heavy-duty sack liners | US DOT | 49 CFR 178.503 | UN 13H2 drop and stacking endurance |
| Agricultural silage | EU | EN 13206:2017 | Mechanical stability under silage storage |
| Frozen food packaging | US/EU | 21 CFR 177.1520(c) 3.2, EU 10/2011 | OML 10 mg/dm² |
| Dry-powder pouch converting | US | 21 CFR 175.105 | Adhesive residual compliance |
| Detergent FFS film | US | ASTM D1693-15b | ≥500 h to 50% failure |
| Collation shrink hood | EU | ISO 14616 | Internal shrink force threshold |
| Greenhouse film | EU | ISO 4892-2:2021 | 3500 h xenon-arc tensile retention |
Collation shrink hood films of 100–150 µm thickness are produced with V2050C6 at 60–70 wt%, LDPE at 30–40 wt%, and anti-block concentrate at 1–2 wt%; the relatively high LDPE fraction broadens the shrinkage temperature window and reduces machine-direction tear susceptibility at corner impact points. Shrinkage in this segment is characterized by ASTM D2732-14, while shrink force is measured by ISO 14616; published data for this specific V2050C6 configuration is limited, so converter internal validation sets maximum shrink force thresholds before film stretching on direct-fired tunnel lines. Processing uses either double-bubble or hot-air blown film equipment with die gaps of 1.2–1.8 mm, first-bubble melt temperatures of 180–200 °C, second-bubble inflation at 105–120 °C, and stabilization at 70–80 °C; film is slit and sealed on hood formers with longitudinal seal temperatures of 130–160 °C. End products include shrink hoods for beverage bottle trays, appliance corner protection, and corrugated bundle overwrap.
Accelerated xenon-arc weathering under ISO 4892-2:2021 cycle A1 for 3500 h is used to qualify greenhouse glazing films containing V2050C6 at 80–85 wt%, metallocene LLDPE at 10–15 wt%, and a UV stabilizer masterbatch at 3–5 wt%; the masterbatch is split between the outer skin at 70–80% of total loading and the core to maintain stabilization efficiency after air dust abrasion. Tensile retention is evaluated by ISO 527-3/2/500 at a separation speed of 500 mm/min, and film transparency is quantified by ISO 14782:2021; compliance for silage applications under the same extrusion platform is covered by EN 13206:2017. Production of 150–200 µm film occurs on 400–600 mm dies with internal bubble cooling, die gaps of 1.6–2.0 mm, melt temperatures of 175–200 °C, BUR 2.8:1–3.2:1, and frost-line heights of 8–12 die diameters; bubble collapse is controlled by differential air velocity to minimize haze caused by HALS migration to the inner surface. End products include greenhouse roofing sheets, low-tunnel covers, and silage storage bags.
Competitive Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Vytek™ V205C6 is an Enhanced LLDPE blown film resin based on an ethylene-hexene copolymer. The C6 suffix denotes hexene as the short-chain branching comonomer, distinguishing the grade from C4 butene-type LLDPE products in the same melt index class. Converter specification control for V205C6 should include density measured under ASTM D1505, melt index measured under ASTM D1238 at 190 °C/2.16 kg, and certificate-of-analysis release limits for slip and antiblock additive concentration. The enhanced designation refers to polymerization and additive modifications intended to reduce melt fracture and improve bubble stability relative to earlier hexene LLDPE grades.
Compared with butene-comonomer LLDPE, the longer hexene branch length in V205C6 disrupts lamellar crystallization more efficiently at equivalent density. The resulting solid-state morphology tends to increase dart impact when films of 25 µm gauge are tested under ASTM D1709 and can narrow machine-direction/transverse-direction tear imbalance when Elmendorf tear is measured under ASTM D1922. These comparisons are valid only when film gauge, blow-up ratio, frost line height, and die gap are held constant; pellet density alone does not predict film toughness.
Vytek V205C6 is not a metallocene-catalysed narrow-composition-distribution resin. It is positioned between conventional butene LLDPE and metallocene hexene LLDPE on the basis of extrusion pressure, seal initiation behaviour, and melt fracture onset. Relative to metallocene LLDPE, the grade may show lower clarity and higher extractables but generally requires lower extruder torque on conventional smooth-bore and grooved-feed blown film lines. Relative to butene LLDPE, the main trade-off is higher raw-material cost and a possible 2–6 °C upward shift in seal initiation temperature.
Dart impact is sensitive to resin density and film orientation. In converter trials comparing C6 and C4 LLDPE at a fixed density of 0.920 g/cm³ and a fixed film thickness of 25 µm, dart impact values obtained under ASTM D1709 Method A often differ by 30–80 g in favour of the hexene grade. The improvement is not uniform across film orientations; transverse-direction tear may increase by 50–150 gf under ASTM D1922, while machine-direction tear can remain flat or decrease if the line runs a low frost line height. Converter trial design must therefore report both directions and the orientation state.
On a 65 mm single-screw extruder with a 30:1 L/D barrier screw and a 200 mm low-stalk die, a blow-up ratio of 2.5:1 can produce a tear ratio between machine and transverse directions that differs by 0.3–0.7, depending on frost line height. Hexene branching alters the balance because the longer branches delay crystallite orientation under hoop stress. The result is a less splitty film in the transverse direction, which is relevant for side seal integrity in can liners and heavy-duty sacks.
Heat-seal behaviour is a further differentiator. Hexene branches are less effective at reducing crystalline melting point than ethyl branches. The seal initiation temperature of the C6 class may shift upward by 2–6 °C relative to butene LLDPE of equal density. Packaging lines with short dwell times should verify seal strength under ASTM F88 or ASTM F2029 before replacing a butene grade with V205C6.
During film conversion on a grooved-feed extruder with a 40:1 L/D barrier screw and a spiral mandrel die, barrel temperatures from 170 °C to 210 °C and a die temperature of 210–230 °C are class-typical starting points. Melt temperature at the die exit should not exceed 240 °C unless the additive package is confirmed for such conditions; otherwise oxidative gel formation can increase at the die lip. Hopper condensation, when ambient relative humidity exceeds 60 %, can introduce surface moisture that appears as bubble pinholes and dart impact variability. The resin is not generally hygroscopic, but pre-drying at 60–70 °C for 2–4 h may be used only when hopper condensation is observed.
Bubble stability is controlled by blow-up ratio and frost line height. In high-stalk configurations, a BUR of 2.0:1 to 3.0:1 with a frost line height of 6–10 die diameters is typical. In low-stalk oscillating haul-off configurations, a frost line height of 1–3 die diameters and a die gap of 1.2–2.0 mm support bubble centering and gauge control but may reduce the dart impact benefit of the C6 resin. When gauge variation exceeds ±8 % at a target thickness of 20 µm, die centering or melt temperature uniformity is usually the dominant cause rather than lot-to-lot resin viscosity shift.
Output limits are governed by melt fracture onset and bubble resonance. Enhanced hexene LLDPE grades generally shift sharkskin melt fracture to a higher shear rate than conventional butene LLDPE of equal melt index, allowing higher screw speed before surface roughness appears. The onset of melt fracture should be mapped by a step-trial on the target die gap rather than assumed from another grade. Die pressure can increase by 5–15 % relative to butene LLDPE and should be monitored against the die manufacturer’s pressure rating. Extruder motor load should remain below the drive nameplate limit.
Rheological comparison of V205C6 with butene LLDPE can be generated by capillary rheometry under ISO 11443 at 190 °C. Shear viscosity curves in the 100–1000 s⁻¹ range are more relevant to die flow than melt index alone. Enhanced hexene LLDPE resins often show a steeper shear-thinning slope than butene grades, with a power-law index lower by 0.05–0.15 over the die shear-rate window. This behaviour reduces head pressure at high output but may increase gauge sensitivity to screw speed changes. Process engineers should use the shear viscosity curve rather than melt index alone when adjusting die temperature profiles.
Regulatory control for Vytek V205C6 should treat the grade as an olefin polymer within the ethylene-hexene copolymer class. Food contact status is commonly evaluated under FDA 21 CFR 177.1520(c), and European food contact applications require verification under EU No 10/2011 for overall migration and specific migration of additives. The additive package present in V205C6 must be disclosed through the supplier’s regulatory certificate, because the same base resin can be produced with different slip and antiblock loadings for different film markets.
The matrix below identifies the controlling test methods and the reporting basis for grade-specific lot release. It is not a substitute for the manufacturer’s product datasheet.
| Parameter | Test Method / Standard Designation | Reporting Basis | Grade-Specific Control |
|---|---|---|---|
| Density | ASTM D1505 | g/cm³ | Certificate-of-analysis target required |
| Melt index | ASTM D1238 Procedure A, 190 °C/2.16 kg | g/10 min | Certificate-of-analysis target required |
| Dart impact | ASTM D1709 Method A or B | g | Film gauge and line condition dependent |
| Elmendorf tear | ASTM D1922 | N/mm or gf | Machine and transverse direction required |
| Tensile yield/break | ASTM D882 | MPa | Machine and transverse direction required |
| Haze | ASTM D1003 | % | Film thickness normalized |
| Food contact status | FDA 21 CFR 177.1520(c) | EU No 10/2011 | Migration limit verification required |
Certificate-of-analysis data for each lot should include density, melt index, additive concentrations, and gel count if the resin is used in high-clarity film. A grade-specific document is especially important when comparing V205C6 with other Enhanced LLDPE grades because a melt-index difference of 0.1 g/10 min can shift head pressure and melt temperature by several degrees on a 65 mm extruder. Lot-to-lot viscosity data should be archived in a converter’s incoming-material database to detect drift before extrusion trials.
Incoming inspection should also record gel count and visual surface defects on a 25 µm blown film sample, because gel count variability can influence haze and dart impact. For food packaging, the certificate of analysis should include hexane extractable or xylene solubles data if required by FDA 21 CFR 177.1520. Pulverized or densified regrind should be screened for metal contamination before blending with virgin V205C6; ferrous and non-ferrous metal contamination above 0.1 wt% can damage extruder screws and increase gel formation.
Replacement of a fractional-melt butene LLDPE with V205C6 is not a direct drop-in when the film contains high percentages of recycled in-plant trim. Because the C6 resin has a different shear response, blending with butene-rich regrind above 20–30 wt% may reintroduce tear anisotropy and reduce dart impact more than predicted by linear mixing rules. The effect is most visible at film gauges below 20 µm, where orientation state becomes sensitive to minor changes in molecular weight distribution. Trials should evaluate blend ratios in 10 wt% increments and test film under ASTM D1709 and ASTM D1922 before committing the line.
High-stalk lines using a 300 mm die with a 0.8 mm die gap and internal bubble cooling may observe a narrower processing window if the resin’s melt strength is not matched to haul-off speed. Bubble flutter can be suppressed by raising the frost line height within the allowable range, but this action reduces transverse orientation and can lower dart impact. Die temperature should not be raised beyond the additive package’s oxidative stability limit solely to recover bubble clarity because die-lip deposit and gel accumulation increase with exit temperature. Incompatibilities with amine-based stabilizer concentrates should be avoided in coextrusion structures where halogenated purging compounds are also used.
Coextruded film with a V205C6 core and a metallocene LLDPE skin is used to combine high dart impact with low seal initiation. In this configuration, the C6 core contributes toughness and the mLLDPE skin controls seal behaviour and optics. The tie layer, if present, should be a maleic anhydride-grafted polyolefin with a melt index within 0.5 g/10 min of the core to prevent interfacial flow instability. Interfacial instability can increase when the skin layer viscosity is more than 30 % below the core viscosity. The core should therefore be paired with a skin resin of comparable melt index or a low-shear match determined by capillary rheometry.
Compared with a butene grade of identical nominal melt index and density, V205C6 may retain dart impact better as film thickness falls below 25 µm. Compared with metallocene hexene LLDPE, V205C6 may exhibit higher haze and higher extractables but lower extruder torque and less sensitivity to die-gap cleanliness. These differences should be validated on the target line because additive loading and molecular weight distribution modify all direct comparisons.
For heavy-duty sacks, industrial liners, and agricultural silage wrap, the product is specified where film toughness and puncture resistance are primary requirements. Monolayer evaluation is typically conducted on 50–70 mm extruders, while coextrusion studies use layer ratios of 20/60/20 or 30/40/30. The converter’s standard gauge, blow-up ratio, and frost line height must be fixed before comparative dart impact and tear testing; otherwise differences may be confounded by orientation state. No conclusion regarding fitness for a specific packaging article should be drawn from pellet properties alone.
A designed experiment with two blow-up ratios (2.2:1 and 3.0:1), two frost line heights (4 and 8 die diameters), and two gauge targets (20 µm and 50 µm) can separate resin performance from line effects. The trial should record head pressure, motor load, film haze under ASTM D1003, dart impact under ASTM D1709, and Elmendorf tear under ASTM D1922 in both machine and transverse directions. Published data for this specific V205C6 configuration is limited in open literature; the manufacturer’s technical service bulletins provide the required starting conditions for the additive package and melt temperature limits.