    Specifications
    HS Code 109975
    Density 0.920 g/cm³
    Melt Index 0.50 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 102 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 700%
    Dart Drop Impact 250 g
    Elmendorf Tear Strength Md 400 g
    Elmendorf Tear Strength Td 600 g
    Haze 12%
    Gloss 50%
    Coefficient Of Friction 0.2
    Seal Initiation Temperature 105 °C

    As an accredited Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading: Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin, palletized bagged resin securely stowed for ocean freight.
    Shipping Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin is typically shipped in 25-kg polyethylene bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Keep cool, dry, and away from sunlight, heat, moisture, and contaminants. It is not DOT/IATA regulated as dangerous goods; follow the SDS and local shipping rules.
    Storage Store Vytek™ V205C3 Enhanced LLDPE Blown Film Resin in a clean, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, ignition sources, and strong odors. Keep bags or containers closed to prevent moisture, dust, and contamination. Use first-in, first-out rotation. Avoid prolonged UV exposure and excessive stacking. Protect from physical damage and incompatible materials. Good housekeeping.
    Shelf Life Stable under normal storage conditions; keep cool, dry, and sealed. No specific expiration date is assigned if stored properly.
    Application of Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin

    In blown-film lines producing heavy-duty shipping sacks and FIBC inner liners, Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin is introduced as the primary layer resin while gauge reduction from 200 µm to 150 µm is evaluated through retained dart impact and Elmendorf tear after film conditioning at 23°C ± 2°C and 50% ± 5% RH per ASTM D1709 Method A and ASTM D1922. The formulation addition ratio in two- or three-layer sack film typically places V205C3 at 70–85 wt%, high-pressure LDPE at 10–20 wt% for increased bubble stability, post-industrial LLDPE reclaim at 5–15 wt%, and processing aid masterbatch at 0.05–0.2 wt% to suppress sharkskin on high-output lines. Extrusion is carried out on blown-film lines with L/D 30–36, die gap 1.8–2.4 mm, BUR 2.0–3.0, and melt temperature 185°C–215°C; a dual-lip air ring with internal bubble cooling is used because the elevated stalk height required for MD/TD tear balance becomes unstable when frost line height exceeds 700–900 mm unless cooling is actively managed. Downstream conversion includes flexographic or CI printing, in-line gusseting, bottom tape or heat sealing, and valve insertion. Terminal film structures include FIBC inner liners tested to ISO 21898 and UN 13H4 performance conditions, heavy-duty valve sacks for cement and construction chemicals, resin packaging bags, and bulk bags for dry-flowable industrial solids. Compliance at resin level for food-contact uses references FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011 with overall migration limit 10 mg/dm²; non-food industrial sacks are screened under REACH (EC) No 1907/2006 and RoHS Directive 2011/65/EU when packaging electrical goods.

    What Changes in Three-Layer Greenhouse Film Coextrusion When V205C3 Replaces Conventional Butene LLDPE?

    Three-layer agricultural film coextrusion introduces V205C3 into the core or outer polyethylene fraction at 75–90 wt% of the hydrocarbon base; the remaining 10–25 wt% is divided between EVA with vinyl acetate content 9–18% and metallocene LLDPE to retain dart impact and elongation after UV exposure. A HALS/NOR HALS UV stabilizer masterbatch is let down at 5–12 wt% in the outer skin, while anti-fog and anti-dust additives are metered at 1–3 wt%; batch-to-batch variation in masterbatch carrier resin can shift frost line height by 50–100 mm at constant air settings, so let-down ratio and extruder backpressure must be monitored. Process parameters use die gap 1.5–2.5 mm, BUR 2.5–3.5, melt temperature 180°C–210°C, and extruders at L/D 28–34; the critical conflict is the viscosity increase from the UV masterbatch in the outer layer, which raises backpressure and can force gauge bands near the frost line unless internal bubble cooling and an adjustable-lip air ring hold frost line height within 400–700 mm. Downstream operations include gusseting, slitting, perforation for mulch film, and anti-drip coating or corona treatment at 38–42 dyn/cm. Terminal finished products are greenhouse covers under EN 13206, low-tunnel films, silage wrap, and conventional mulch films under EN 13655; compliance for food-adjacent agricultural contact references REACH (EC) No 1907/2006 and EU Regulation No 10/2011, with migration testing by EN 1186 using 3% acetic acid and 10% ethanol simulants for wet acidic produce.

    When frozen-food packaging converters evaluate blown sealant webs for lamination to biaxially oriented polyamide and BOPET, seal-initiation trials are run at 115°C–135°C and low-temperature dart impact at -20°C; V205C3 is formulated in the sealant layer at 70–90 wt% with 10–30 wt% lower-density metallocene LLDPE to widen the seal plateau and prevent seal-through-contamination failure on high-speed vertical form-fill-seal machines. The blown web is extruded at 40–80 µm, die gap 1.5–2.0 mm, BUR 2.2–3.0, and melt temperature 185°C–205°C, then surface-treated to 40–44 dyn/cm before adhesive lamination to BOPA or BOPET. The critical property is retention of seal strength after corona and lamination, measured by ASTM F88/F88M at or above 0.4 N/mm after 24 h aging; low-temperature tear is reported by ASTM D1922 and puncture by ASTM D5748 for freezer punctures from sharp-edged IQF vegetables. Terminal finished products include IQF vegetable and fruit pouches, seafood bags, frozen bakery wrap, and ice cream packaging films. Food-contact compliance is anchored to FDA 21 CFR 177.1520 and EU Regulation No 10/2011, with fatty-food simulants per EN 1186; the converter must verify that adhesive and ink systems also meet FDA 21 CFR 175.105 and 21 CFR 175.300 when indirect contact is used.

    Bag-in-Box Liner Flex-Crack Resistance and Tie-Layer Compatibility

    Bag-in-box liner structures use V205C3 in the polyethylene skin layers at 65–85 wt% of the total film, coextruded with a mid-layer barrier of EVOH at 5–8 wt% and tie layers at 4–8 wt%; the remaining 10–20 wt% is a lower-crystallinity sealant polyethylene selected for flex-crack resistance and fitment weld integrity. The process is coextrusion blown film at die gap 1.5–2.2 mm, BUR 2.0–2.8, and melt temperature 190°C–215°C, followed by corona treatment, slitting, and welding into pillow or gusseted bags with heated-bar seals around LLDPE-compatible fitments. The critical failure mode is flex-crack pinhole formation along bag corner creases during repeated filling and dispensing cycles; this is evaluated by Gelbo flex testing ASTM F392 using 50 cycles and pinhole count, and by film tensile elongation ASTM D882 after flexing. Terminal finished products include bag-in-box liners for wine, liquid eggs, dairy concentrates, edible oil, and water dispenser reservoirs. Compliance is governed by FDA 21 CFR 177.1520 for polyethylene layers and EU Regulation No 10/2011 for the finished multilayer structure; overall migration must not exceed 10 mg/dm², and the EVOH barrier and tie layers must be qualified under the applicable national or EU food-contact provisions for multilayer films.

    At 45–60 cycles/min, form-fill-seal equipment imposes simultaneous hot-tack and coefficient-of-friction demands on the film web; V205C3 is formulated at 80–95 wt% of the blown film, with 2–5 wt% slip/antiblock masterbatch and 0.05–0.2 wt% processing aid, because excessive slip migrates to the seal interface and widens heat-seal initiation temperature beyond the 125°C–155°C window required for high-speed jaw sealing. The film is extruded on L/D 30–36 blown-film lines with die gap 1.8–2.4 mm, BUR 2.0–2.8, and melt temperature 185°C–210°C; after slitting and corona treatment to 38–42 dyn/cm, the web is printed and run on vertical or horizontal form-fill-seal machines with dwell times of 0.3–0.6 s. Seal integrity is measured by ASTM F88/F88M and hot-tack by ASTM F1921, while coefficient of friction is tested by ISO 8295 or ASTM D1894; the target kinetic COF is 0.15–0.30 to prevent film tracking drift on forming collars. Terminal finished products are pet food bags, dry food pouches, fertilizer bags, salt bags, and detergent pouches. Food-contact compliance is established by FDA 21 CFR 177.1520 and EU Regulation No 10/2011; non-food chemical packaging is screened under REACH (EC) No 1907/2006 and RoHS Directive 2011/65/EU for electronics-adjacent bulk goods.

    When Pallet Loads Require Stretch Hood Containment Without LDPE Dilution

    Because stretch hood application subjects the sleeve to 70–90% pre-stretch, V205C3 is formulated at 85–100 wt% with optional 10–20 wt% metallocene LLDPE to replace conventional LDPE-rich formulations and increase puncture resistance and elastic recovery; the addition ratio is constrained by the need to maintain low-speed stretchability without wing tear at die-cut edges. The blown film is produced at die gap 1.8–2.4 mm, BUR 4.0–4.5, melt temperature 185°C–205°C, and layflat widths matched to pallet dimensions; the high BUR shifts tear anisotropy toward transverse direction, which is desirable for hood opening but requires a collapsing frame with low-friction slats to prevent MD scratch lines. Downstream conversion includes gusseted sleeve sealing, corner welding, and application through four-corner stretch-hood machines with 0.5–1.5 s stretch cycles. Terminal finished products are pallet hoods for beverage trays, appliance panels, bagged resins, and construction materials. Compliance for industrial packaging references ISO 527-3 tensile elongation, ASTM D882, ASTM D5748 puncture, and load stability under EUMOS 40511 if specified by the transport buyer; chemical registration is covered by REACH (EC) No 1907/2006, and heavy metals restrictions by RoHS Directive 2011/65/EU for electronics-containing pallets. Published data for V205C3 in high-BUR stretch-hood configuration is limited; processors should run a designed experiment varying BUR 4.0–4.5 and frost line height to map dart impact and Elmendorf tear before qualifying pallet-wrap replacement.

    Free Quote

    Competitive Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin is a pelletized linear low-density polyethylene supplied for blown film extrusion. The manufacturer assigns a nominal melt index of 0.5 g/10 min at 190 °C/2.16 kg when tested under ASTM D1238-20 and a nominal density of 0.920 g/cm³ at 23 °C when tested under ASTM D1505-18. These values place the product in the fractional-melt-index blown film segment, where bubble tension and tear balance are controlled by molecular architecture as much as by melt temperature. The “Enhanced LLDPE” designation distinguishes the resin from early-generation butene C4-LLDPE; the exact α-olefin comonomer and catalyst package are not disclosed in the public technical datasheet. Published data for the complete film-property matrix of this specific configuration is limited, and conformance is therefore maintained through certificate-of-analysis values rather than a single universal film-property table.

    The corresponding international methods are ISO 1133-1:2022 for melt flow rate and ISO 1183-1:2019 for density. When comparative data are generated across standards, sample preparation and temperature tolerance differences must be recorded because they can create small numerical offsets that are larger than lot-to-lot variance.

    Which Melt Flow and Density Boundaries Define the Process Envelope?

    At 0.5 g/10 min, the resin has higher melt strength and higher die pressure than 1.0 g/10 min grades. For linear polyethylene, zero-shear viscosity scales with weight-average molecular weight to the 3.4 power, so small shifts in the high-molecular-weight tail alter die pressure and bubble tension before the melt index changes significantly. At 0.920 g/cm³, the solid-state crystallinity is lower than in medium-density grades, reducing secant modulus but improving low-temperature dart impact. Secant modulus at 1% strain for this density class is typically 190–240 MPa on 25 µm blown film under ASTM D882-18; exact product-specific values should be taken from the manufacturer technical datasheet. Density variation of ±0.002 g/cm³ shifts crystalline content enough to alter modulus, dart impact, and seal initiation temperature; therefore, density should be treated as a boundary condition rather than a nominal value.

    At 190 °C and shear rates between 10 s⁻¹ and 100 s⁻¹, this resin class exhibits pseudoplastic behavior with a power-law index near 0.45–0.55. A 10 °C increase in melt temperature lowers viscosity by roughly 5–8%, so die pressure responds measurably to small zone adjustments. However, raising melt temperature also reduces melt strength and raises frost line height; corrections are therefore not free of film property consequences.

    On a 75 mm grooved-feed single-screw extruder with 30:1 L/D and a 300 mm internal bubble cooling die, start-up conditions for this density/MI class are commonly barrel zones 170/185/195/205/210 °C, adapter and die zones 210–220 °C, and target melt temperature 215–225 °C. For 25 µm film, die gap is 1.6–2.0 mm; for 80–120 µm film, die gap is increased to 2.2–2.5 mm to reduce die-lip stress. Blow-up ratio is set at 2.2:1–2.8:1, and frost line height is held at 5–7 die diameters. These are starting points, not guaranteed production windows.

    When specific output approaches 1.4 kg/h/mm die circumference, die land shear rates remain below 100 s⁻¹. Pressure below 350 bar on a clean screen pack is typical for this melt index class. If surface melt fracture appears, increasing die temperature by 5–10 °C or widening the die gap by 0.3 mm reduces die-lip stress. Lowering melt temperature below 205 °C may increase unmelted high-molecular-weight fraction at the die lip and promote die-lip plateout. Bubble stability is the primary throughput limitation: at BUR 3.0:1, oscillation can begin before extruder capacity is reached; reducing BUR to 2.2:1 stabilizes the bubble but lowers TD tear as measured by ASTM D1922-09. On an air-cooled line, increasing lower-nip airflow can intensify oscillation at high BUR; increasing stalk height and reducing lower-nip air flow return the frost line to a stable position. The trade-off is a cliff-edge, not a linear loss.

    Gauge variation is influenced by die gap, air ring uniformity, and frost line height. For this density class at 25 µm nominal gauge and 2.5:1 BUR, transverse gauge variation of ±4–6% is typical on a well-centered die; increasing die gap to 2.5 mm without adjusting frost line can raise variation to ±8%. Because dart impact is highly thickness-sensitive, gauge variation amplifies impact variability; a trial with poor gauge control cannot resolve resin differences.

    When Replacing a Conventional C4-LLDPE in High-Stalk Blown Film Systems

    Conventional butene C4-LLDPE at the same 0.920 g/cm³ and 0.5 g/10 min tends to show lower dart impact and a more MD-biased tear balance because short-chain branch length and composition distribution influence tie-chain concentration. In comparative trials normalized to 25 µm film and 2.5:1 BUR, enhanced LLDPE grades may show dart impact improvements of 20–40% under ASTM D1709-16a; Vytek™ V205C3-specific values must be confirmed from the manufacturer technical datasheet. Elmendorf tear tested under ASTM D1922-09 shifts from MD to TD dominance as BUR increases, and the product is selected where TD tear retention at high BUR is required.

    Drop-in replacement is not automatic. Die pressure at equal output may differ by 5–15% because molecular weight distribution influences shear viscosity; screen pack, die gap, or zone settings may need adjustment. Compared with metallocene-catalyzed C6/C8 grades, this resin class can offer a broader processing window, lower die pressure, and higher melt strength, but seal initiation temperature may be higher and optical haze may be higher. Seal strength should be evaluated under ASTM F88/F88M-21 on the final film structure because coextrusion and gauge variation affect the seal response more than pellet properties.

    Compared with tubular LDPE of the same melt index, the resin has higher tensile strength and puncture resistance but lower melt strength and lower clarity. LDPE addition is used to improve bubble stability in high-stalk lines; the resulting film may show lower haze but also lower dart impact. If optical haze below 8% under ASTM D1003-13 is required, the formulation must be adjusted with an LDPE or a metallocene grade; Vytek™ V205C3 is not a high-clarity resin by design.

    Blending with 10–20 wt% LDPE improves bubble stability in high-stalk lines, but dart impact under ASTM D1709-16a can decline by 10–20%. Blend ratio should be controlled to ±2 wt% because density and melt index differences between components create composition-driven gauge variation. Addition of C6-mLLDPE at 30 wt% can lower seal initiation but may reduce bubble tension; this must be tested on the target die rather than inferred from pellet properties.

    Seal initiation temperature for this resin is typically in the range 105–115 °C for the density class, but coextruded skin layer and heat seal equipment settings determine final values; heat-seal testing should follow ASTM F88/F88M-21 with dwell time, pressure, and anvil temperature recorded.

    Heavy-duty monolayer and multilayer blown film structures use Vytek™ V205C3 in industrial liners, can liners, agricultural silage covers, and frozen food packaging. In heavy-duty sacks, performance is specified by dart impact under ASTM D1709-16a, tear resistance under ASTM D1922-09, and puncture propagation resistance under ASTM D5748-18. Film thickness in these applications generally ranges from 30 µm to 150 µm; above 150 µm, cooling rate becomes the limiting factor and gauge variation can mask resin differences.

    In a three-layer coextruded film with HDPE skins, the resin is commonly placed in the core layer at 60–80% of total thickness to contribute dart impact and tear resistance while the skins control modulus, moisture barrier, and seal behavior. On a 250 mm die running 60/80/60 µm layer distribution, the core layer may be blended with process aid to reduce die-lip plateout. For agricultural silage covers, UV stabilization is not incorporated; a HALS/UVA masterbatch must be added and dispersed through high-shear mixing or an efficient distributive section. Field experience on 70–90 mm grooved-feed extruders shows that output limitation at 80 µm is frequently bubble instability rather than screw recovery when BUR exceeds 2.8:1.

    In frozen food packaging, low-temperature dart impact at -20 °C is generally higher than C4 grades of the same density, but slip and antiblock additives are not included at final-use levels; surface coefficient of friction should be controlled with additive masterbatch and verified under ASTM D1894-14. Corona treatment to 38–42 mN/m is typical for polyethylene film before printing or lamination, but treatment decay must be confirmed on the specific film.

    Regulatory Status, Food Contact, and Handling Boundaries

    The base polyethylene may be suitable for food contact under FDA 21 CFR 177.1520, paragraphs (c) 3.1a and 3.2a, provided the end-use food type and thermal treatment remain within the regulation. European Union compliance with Regulation (EC) No 10/2011 requires supplier documentation and final-film overall migration below 10 mg/dm². Under REACH Regulation (EC) No 1907/2006, substances of very high concern must remain below 0.1% w/w; this is confirmed through the safety data sheet rather than assumed from the base resin classification. If the film is incorporated into electrical or electronic equipment, the applicable homogeneous material must be assessed under RoHS Directive 2011/65/EU, Annex II.

    RequirementPrimary clause or methodApplicability to Vytek™ V205C3
    Food contact, United StatesFDA 21 CFR 177.1520Olefin polymer conditions of use; food type and temperature restrictions apply
    Food contact, European UnionRegulation (EC) No 10/2011, Article 12Overall migration 10 mg/dm²; supplier declaration required
    Chemical substances, EUREACH 1907/2006, Article 33SVHC below 0.1% w/w; verify SDS
    Restricted substances in EEERoHS 2011/65/EU, Annex IIApplicable only if film becomes part of homogeneous material in EEE

    Moisture absorption is low, but storage at relative humidity above 60% can produce surface condensation when the resin is moved into a colder processing area; for critical film, pre-drying at 80 °C for 2–4 h in a desiccant dryer reduces micro-bubble formation. Processing above 250 °C accelerates oxidative chain scission; melt residence times above 15 min at temperature increase gel formation and off-odor. The resin should not be combined with copper-containing colorants or certain metal carboxylate process aids if die-lip plateout increases; after such runs, purge with a cast acrylic or HDPE purge compound may be required. Pneumatic conveying lines must be grounded to prevent static dust ignition, and storage should remain below 50 °C away from direct ultraviolet exposure.

    Slip, antiblock, UV stabilizer, and processing aid are not incorporated at levels sufficient for all end uses. These additives must be predispersed; inadequate dispersion creates gel streaks and uneven surface coefficient of friction as measured by ASTM D1894-14. Product-specific maximum processing temperature, additive compatibility, and food-contact status should be verified against the current safety data sheet and technical datasheet.