Chevron Phillips Vytek V205a Enhanced Lldpe Blown Film Resin

Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin

    • Product Name: Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 171295
    Melt Index 190 C 2 16 Kg 0.5 g/10 min
    Density 0.920 g/cm³
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1400 psi
    Tensile Strength At Break Md 5000 psi
    Tensile Strength At Break Td 4500 psi
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Dart Drop Impact F50 300 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 10 %
    Gloss 45 70 %
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin is packaged in 25 kg (55 lb) polyethylene bags, palletized for bulk shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin loads as palletized 25kg bags, securely stowed.
    Shipping Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin is shipped as free-flowing pellets in 25-kg bags, 1,000-kg bulk boxes, or bulk hopper trucks/railcars. Store in a cool, dry, ventilated area, away from direct sunlight, moisture, and contaminants. Keep containers sealed until use; no special hazardous handling is required.
    Storage Store Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep bags or containers closed to prevent moisture, dust, and contamination. Avoid excessive stacking and protect from physical damage. Maintain good housekeeping; follow the manufacturer’s SDS and local regulations. Use first-in, first-out inventory.
    Shelf Life Shelf life: Typically 24 months from manufacture when stored unopened in a cool, dry, well-ventilated area, away from direct sunlight.
    Application of Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin

    On high-speed vertical form-fill-seal lines running polyolefin food-contact film at package speeds above 80 packages/min, Vytek™ V205A is typically fed as a neat letdown resin with a slip/anti-block masterbatch at 2–4 wt% depending on film gauge and packaging machine coefficient-of-friction targets. The formulation is adjusted so that the final slip additive concentration remains below 1200 ppm; higher levels bloom to the seal surface after 48 h at 23 °C and 50% RH per ASTM D618, creating haze and jaw contamination on form-fill-seal equipment. The blown-film process on a 90 mm grooved-feed extruder with 30:1 L/D uses a 200 mm spiral mandrel die, die gap 1.8 mm, blow-up ratio 2.3:1, and melt temperature 216 °C to 238 °C. The frost line is held at 3 die diameters to balance bubble stability and transverse orientation. In-line corona treatment is set to 38–40 dynes/cm measured per ASTM D2578 to anchor water-based flexo ink on the outer surface. The terminal films are used for produce bags, bakery overwrap, and frozen-food pouches. Food-contact conformity is established by the following matrix:

    MarketStandardEnd-use condition
    United StatesFDA 21 CFR 177.1520Olefin polymer clearance; extraction testing based on food type and temperature
    European UnionRegulation (EU) No 10/2011Overall migration ≤ 10 mg/dm²; specific migration limits apply to slip/antiblock additives
    ChinaGB 4806.6-2016 and GB 9685-2016Positive list for food-contact plastic resin and additives
    REACHRegulation (EC) No 1907/2006, Annex XVIISubstance restriction screening for monomers and processing aids

    Why does haze remain the controlling specification in over-wrap and produce-film applications?

    For produce overwrap and bakery film, haze is governed less by the base resin than by the kinetic competition between slip additive bloom and anti-fog surface wetting after film is cooled below the frost line. V205A-rich film is extruded with an antiblock masterbatch at 0.5–1.5 wt% and an anti-fog masterbatch at 1.0–2.0 wt% when the packaged product has high respiration moisture. The die gap is reduced to 1.6–2.2 mm, blow-up ratio is set at 2.5:1 to 3.2:1, and melt temperature is kept between 204 °C and 221 °C to avoid oxidative gel discoloration. Haze and clarity are measured per ASTM D1003 and ASTM D1746 after 48 h conditioning, because immediate on-line haze values underreport bloom-related haze development. Anti-fog persistence is evaluated by cold-room fog testing with a 4 °C water bath and is specified by the packaging buyer, not by the resin clearance. Batch-to-batch variance in anti-fog masterbatch carrier resin can shift the frost line by several die diameters; the line crew must record die lip build-up and film blocking at each shift change. Published data for this specific configuration is limited; the valid additive window must be established by plant trials because die lip build-up and film blocking vary with ambient humidity and line speed. Finished products include leafy-green bags, bread bags, and floral sleeves where clarity and anti-fog persistence are the primary saleable properties.

    Tensile elongation at break and dart impact thresholds determine agricultural film downgauging limits.

    Agricultural silage covers and mulch films produced from V205A require a balance between ultraviolet screening and puncture propagation resistance. Three-layer coextrusion on a 120 mm grooved-feed extruder with internal bubble cooling and a 350 mm die uses die gap 2.4 mm, blow-up ratio 2.8:1, and melt temperature 218 °C to 235 °C. The outer skins are formulated with white, black, or green masterbatch at 6–10 wt%; carbon black final-film loading is maintained at 2.0–3.0 wt% when UV protection is critical. A hindered amine light stabilizer package is added according to the masterbatch supplier’s recommendation for outdoor service, and the complete film is evaluated against EN 13206 for silage covering films. Tensile elongation at break per ISO 527-3 and dart impact per ASTM D1709 Method A at film thickness 120 µm to 180 µm are used to determine downgauging capacity; downgauging trials show the puncture resistance can fall sharply when the frost line height or blow-up ratio is moved outside the validated window. Elmendorf tear per ASTM D1922 is measured in both machine and transverse directions after 72 h at 23 °C. The terminal articles are silage bags, round bale stretch films, and mulch films laid by tractor-mounted applicators. Published data for this specific configuration is limited because soil abrasion and UV exposure are regional variables.

    Heavy-duty shipping sacks and industrial liners are produced on grooved-feed blown-film lines where bubble stability and drawdown capacity determine maximum output rate. At layer ratios of 100% V205A or 80/20 V205A/LDPE, the bubble is maintained under high-stalk conditions with frost line height set at 4 to 6 die diameters to promote machine-direction orientation and reduce sag at the haul-off. Die gap is 2.0–2.6 mm, blow-up ratio is 2.0:1 to 2.5:1, and melt temperature is 218 °C to 235 °C. For valve sacks and FIBC liners, film thickness is 125 µm to 250 µm, and slow-rate puncture resistance is measured per ASTM F1306 while dart impact is measured per ASTM D1709 Method B. Tensile properties are checked per ASTM D882. Surface treatment for flexographic or gravure printing is set to 42–46 dynes/cm per ASTM D2578. The terminal articles are heavy-duty shipping sacks, mineral and chemical liners, and FIBC inner liners. Published data for this specific configuration is limited; output ceilings are best established by measuring back pressure and bubble stability on the target line rather than by extrapolating from laboratory film data.

    When pallet unitization shifts from cast stretch to blown stretch-hood film.

    When pallet unitization shifts from cast stretch to blown stretch-hood film, the film must combine high transverse elongation with controlled elastic recovery after being pulled over a pallet at pre-stretch ratios up to 200%. V205A-rich stretch-hood film is extruded on a 250 mm die with 2.0 mm die gap, blow-up ratio 3.0:1 to 3.8:1, and a low-frost-line condition to reduce crystallinity and raise dart resistance. A 60/40 or 70/30 V205A/metallocene LLDPE core is used to increase dart; the outer skins contain anti-block only at 500–1000 ppm, because slip additives can reduce surface friction engagement on stretch-hood machines. Elongation at break per ISO 527-3 and hysteresis after 100% elongation per ASTM D5459 are used to compare elastic recovery. The terminal articles are stretch-hood films for building materials, beverage pallets, and bagged resin pallets. Published data for this specific configuration is limited; the pre-stretch ratio and elastic recovery are machine-specific and must be validated on the target packaging line.

    Low-COF collation shrink and frozen-food packaging layer ratios.

    Low-COF collation shrink and frozen-food packaging layer ratios are established on three-layer blown-film lines with V205A in the core and skins. A three-layer structure of 30/40/30 or 20/60/20 is used as the starting point; the final layer distribution is adjusted by hot-tack tests on the packaging machine. The sealant skin is blended with a lower-melting plastomer or butene LLDPE to reduce seal initiation temperature, while the core maintains shrink force and stiffness. Slip additive is staged so that the kinetic coefficient of friction measured per ASTM D1894 falls below 0.20 after 72 h conditioning, without generating sufficient bloom to contaminate the seal bar or reduce seal strength per ASTM F88. Hot tack is measured per ASTM F1921. Shrink orientation is performed on a double-bubble or high-stalk process where orientation temperature is maintained 10–15 °C below the crystalline melting peak determined by differential scanning calorimetry per ASTM D3418. Frozen-food packaging requires low-temperature dart impact per ASTM D1709 Method A at -20 °C. The terminal articles are collation shrink for canned goods and bottled beverages, and frozen-food pouches for IQF vegetables and prepared meals.

    Free Quote

    Competitive Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin is a linear low-density polyethylene grade supplied as free-flowing pellets for tubular blown film extrusion. The material is classified under ASTM D883 as a polyethylene plastic with a density below 0.940 g/cm³. The designation “enhanced LLDPE” reflects a resin architecture and additive package developed to improve bubble stability, melt strength, and film toughness relative to conventional Ziegler-Natta LLDPE film grades. The resin is intended for monolayer and coextruded film structures in which a balance of puncture resistance, tear propagation resistance, and optical clarity governs end-use acceptance. Processing and property performance should be verified against the manufacturer’s certificate of analysis for lot-specific values; where the supplier’s current datasheet is not publicly available, published product-specific numerical data should not be reproduced without batch verification.

    What Distinguishes Vytek™ V205A from Conventional LLDPE Blown Film Grades?

    Enhanced LLDPE grades differ from conventional butene-based LLDPE in the distribution of short-chain branching and molecular weight. In conventional Ziegler-Natta LLDPE, comonomer incorporation is heterogeneous: lower-molecular-weight fractions contain less comonomer, while higher-molecular-weight fractions contain more, producing a broad orthogonal composition distribution. That heterogeneity can improve processability but often limits dart impact and tear resistance at a given density. An enhanced LLDPE such as Vytek™ V205A is designed to modify that balance, typically through catalyst selection and post-reactor compounding, so that toughness-critical fractions are more uniformly incorporated into the film network. The practical result is that the resin may show improved film performance in ASTM D1709 dart impact, ASTM D1922 Elmendorf tear, and ASTM D5748 puncture resistance when compared with conventional LLDPE grades of equivalent melt index and density. No claim is made that the resin is a single-site metallocene product; the enhancement may arise from multiple resin design strategies.

    Resin suppliers in this market segment typically specify melt index by ASTM D1238 at 190 °C/2.16 kg and density by ASTM D1505 or ISO 1183-1:2019. Blown film LLDPE grades commonly fall between 0.5 g/10 min and 2.0 g/10 min melt index and between 0.915 g/cm³ and 0.940 g/cm³ density. Within that envelope, lower density improves toughness and sealing performance but reduces modulus and may increase blocking tendency. Higher melt index improves extrusion output and reduces melt pressure but typically sacrifices dart impact and tear. The selection of Vytek™ V205A over a standard LLDPE grade therefore depends on whether the film converter requires improved toughness at a given gauge or whether gauge downgauging is the primary economic target.

    On production-scale blown film lines, the practical differences between enhanced LLDPE and conventional LLDPE are most visible in two areas: bubble stability and gauge uniformity. Because LLDPE has lower melt elasticity than LDPE, it is often more sensitive to draw resonance and bubble breathing. A grade with enhanced melt strength can tolerate higher blow-up ratios and deeper frost lines without losing bubble geometry. That allows the converter to operate at blow-up ratios from 2.0:1 to 3.5:1 while maintaining film-thickness variation within ±5% on lines equipped with automatic air rings and gauge-control systems. Such behavior is evaluated on annular dies with die diameters from 150 mm to 400 mm; published data for this specific resin configuration may be limited to supplier trial reports.

    Compared with LDPE, LLDPE film generally exhibits higher tensile strength and puncture resistance at equivalent gauge but lower melt elasticity and optical clarity. The addition of LDPE to LLDPE is common in monolayer and coextruded films to improve bubble stability and optical appearance. However, excessive LDPE addition reduces the toughness contribution of the LLDPE. In practice, many converters blend 10 wt% to 30 wt% LDPE into LLDPE-rich film structures, with the exact ratio determined by the required balance of tear, dart impact, and clarity. Vytek™ V205A is positioned as a resin that may reduce or eliminate the need for such LDPE processability blends, although this must be confirmed on the specific film line because die geometry, air ring design, and cooling air temperature influence the result.

    On conventional monolayer blown film lines equipped with grooved-feed extruders having screw diameters from 45 mm to 90 mm and length-to-diameter ratios of 24:1 to 30:1, melt temperatures at the adapter are commonly held between 190 °C and 230 °C, depending on die size, output rate, and coextruder distribution. Die gaps for LLDPE are typically set between 1.5 mm and 2.5 mm, wider than LDPE die gaps, to control melt fracture by reducing die-land shear stress. Melt temperatures below 180 °C may reduce thermal degradation of the polymer backbone but can also increase melt pressure and reduce output, particularly on older single-flighted screws without mixing elements. Melt temperatures above 240 °C are generally unnecessary for LLDPE film production and may promote gel formation or additive decomposition.

    Die land shear rate is a critical processing variable for LLDPE film quality. On production lines equipped with spiral mandrel dies, sharkskin melt fracture may appear when die land shear rate exceeds approximately 500 s⁻¹, although the actual threshold shifts with die temperature, molecular weight distribution, and the presence of polymer processing aids. Fluoropolymer processing aids are frequently added at 200 ppm to 800 ppm to suppress melt fracture and reduce die build-up. These additives function by coating the die steel and lowering the interfacial friction between the polymer melt and the metal surface. Their effectiveness depends on shear rate, die land length, and conditioning time; line operators often observe a temporary increase in haze or gel-like specks during the first 30 min to 60 min of processing-aid purge.

    Bubble cooling and frost line placement influence the property balance of Vytek™ V205A. For a die diameter of 250 mm and a die gap of 2.0 mm, frost line heights between 5 and 10 die diameters are typical. Lower frost line heights increase quench rate and can improve optical clarity while reducing tear resistance in the machine direction. Higher frost line heights allow greater molecular orientation to develop, increasing machine-direction tensile strength but often reducing transverse-direction elongation. The optimum frost line height therefore depends on the anisotropy required in the final film. A blow-up ratio near 2.5:1 is commonly targeted when balanced machine-direction and transverse-direction properties are required, while a blow-up ratio above 3.0:1 may be used to improve transverse-direction tear at the expense of line stability.

    Film Mechanical Property Benchmarks and Test Methods

    Qualification of enhanced LLDPE film requires conditioning of specimens at 23 °C and 50% relative humidity in accordance with ASTM D618 unless otherwise specified. Film gauge is determined by ASTM D6988; thickness variation across the web is often evaluated with a capacitance or beta gauge. Tensile properties are measured by ASTM D882 or ISO 527-3, with jaw separation and test speed selected according to film elongation. Dart impact is determined by ASTM D1709 Method A or Method B depending on expected impact range; results are reported in grams and are strongly affected by film gauge, gauge uniformity, and conditioning. Elmendorf tear is measured by ASTM D1922 or ISO 6383-2, with machine-direction and transverse-direction values reported separately. Haze and clarity are measured by ASTM D1003, and puncture resistance is often evaluated by ASTM D5748.

    Blown film characterization methods applied to enhanced LLDPE grades
    PropertyReference methodReported unit
    Melt indexASTM D1238 / ISO 1133-1:2022g/10 min
    DensityASTM D1505 / ISO 1183-1:2019g/cm³
    Dart impactASTM D1709 Method Ag
    Elmendorf tearASTM D1922 / ISO 6383-2gf or mN
    Tensile strength at breakASTM D882 / ISO 527-3MPa
    Elongation at breakASTM D882 / ISO 527-3%
    HazeASTM D1003%
    Puncture resistanceASTM D5748N or lbf

    Comparative interpretation of these values requires strict attention to film gauge. Dart impact values scale with gauge in a nonlinear manner, so direct comparison without gauge normalization is not valid. For LLDPE-based films in the 25 µm to 50 µm range, published dart impact values for high-toughness grades commonly range from 100 g to 400 g, but the wide spread reflects differences in comonomer type, density, molecular weight, and extrusion orientation. Similarly, Elmendorf tear values are strongly dependent on blow-up ratio and frost line height. A resin that exhibits high machine-direction tear at a blow-up ratio of 2.0:1 may show lower machine-direction tear at 3.5:1 because molecular orientation shifts toward the transverse direction.

    Secant modulus is measured by ASTM D882 or ISO 527-3; for LLDPE film-grade resins with densities between 0.915 g/cm³ and 0.940 g/cm³, 1% secant modulus values published for blown film are typically in the range of 150 MPa to 350 MPa, depending on orientation, gauge, and test speed. Enhanced LLDPE grades may exhibit modulus values near the upper end of that range when density is raised, but density increases above 0.930 g/cm³ generally reduce dart impact and low-temperature toughness. The trade-off between stiffness and impact is therefore not unique to Vytek™ V205A; it is a fundamental density-property relationship across linear low-density polyethylene resins.

    When High Dart Impact and Tear Resistance Govern Heavy-Duty Sack Specifications

    Heavy-duty shipping sacks and industrial liners often specify minimum dart impact and Elmendorf tear values at a given film thickness. In those applications, an enhanced LLDPE may be selected because it allows the converter to meet the specification without increasing film gauge or incorporating excessive LDPE. A typical 80 µm sack film may require dart impact above 300 g and transverse-direction tear above 15 gf/µm, but these values are not product-specific and must be verified on the target line. The film structures used for such sacks frequently combine an LLDPE core with LDPE or HDPE skin layers. In a three-layer A/B/A structure, the core may represent 60 wt% to 80 wt% of the total film, while the skins provide surface friction control, sealing performance, or stiffness. Vytek™ V205A may be used as the core layer or as the dominant resin in the formulation when toughness is the controlling specification.

    On a production line equipped with a three-layer annular die and three extruders of 60 mm, 90 mm, and 60 mm screw diameter, the core layer is commonly processed at a melt temperature 5 °C to 15 °C higher than the skin layers to promote interfacial mixing without increasing total melt temperature. Coextrusion feedblock and die-body temperatures are maintained between 200 °C and 220 °C unless a fluoropolymer processing aid reduces die pressure. Output rates are often limited by bubble cooling rather than extruder capacity. When the bubble becomes unstable at high output, the usual corrective sequence is to lower melt temperature, reduce frost line height, increase LDPE content, or adjust the air ring internal deckle position. A resin with enhanced melt strength may permit output-rate increases of 5% to 15% relative to a conventional LLDPE before bubble instability occurs, based on general industry experience with enhanced film-grade LLDPE resins. Published data for this specific product on a given line configuration should be obtained from Chevron Phillips Chemical technical service.

    In coextruded structures used for food packaging, the surface layer may also contain antiblock and slip additives. Interaction between the enhanced LLDPE and those surface additives can affect sealing performance and hot-tack strength. Hot-tack testing is performed by ASTM F1921 or ASTM F2627; seal strength is measured by ASTM F88. The sealing window of LLDPE is generally broader than that of LDPE because LLDPE retains seal strength at higher temperatures, but the exact hot-tack curve depends on comonomer type, density, and additive package. A film containing Vytek™ V205A in the core or skin layer should be sealed on equipment with calibrated jaw temperatures and uniform pressure. Sealing temperatures below 110 °C may produce incomplete seals, while temperatures above 150 °C may induce edge thinning or film distortion depending on dwell time and sealing geometry.

    Regulatory compliance for food-contact applications is assessed under 21 CFR 177.1520, which covers olefin polymers. End-use suitability depends on food type, temperature, and duration. The fabricator must verify the specific conditions of use in 21 CFR 177.1520(c) and any applicable limitations for the finished article. European food-contact compliance may require evaluation under Regulation (EC) No 1935/2004 and, where applicable, Commission Regulation (EU) No 10/2011. For electrical or electronic film applications, RoHS compliance should be demonstrated by declarations supported by IEC 62321 test methods. REACH compliance requires confirmation that the substance or mixture does not contain a candidate-list substance of very high concern above the stated threshold. These compliance statements are supplier-specific and must be obtained from the resin manufacturer; generic statements based on resin class are insufficient for final article certification.

    Storage conditions influence processability and film quality. Polyolefin pellets should be stored in sealed containers or silos to prevent airborne contamination. LLDPE resins are generally not hygroscopic, but condensation on cold pellet surfaces can introduce surface moisture into the extruder feed throat. If pellets are transferred from unheated storage to a warm production area at relative humidity above 60%, surface condensation may occur. In such cases, a desiccant dryer operated at 60 °C for 2 h to 4 h may be used to remove surface moisture before extrusion. Extended storage at elevated temperatures above 40 °C may accelerate additive migration and antioxidant depletion, particularly if silo turnover times exceed several months. Inventory should therefore follow first-in-first-out rotation, and any stored resin exceeding the supplier’s recommended shelf life should be evaluated for melt flow stability and film appearance before use.

    Top