Chevron Phillips Mpact D352 M Lldpe Linear Low Density Polyethylene

Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene

    • Product Name: Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 606180
    Density 0.935 g/cm³
    Meltindex 0.85 g/10 min at 190°C/2.16 kg
    Meltingpoint 126 °C
    Vicatsofteningpoint 112 °C
    Tensilestrengthatyield 13.8 MPa
    Tensilestrengthatbreak 38.0 MPa
    Elongationatbreak 700%
    Tensilemodulus 586 MPa
    Flexuralmodulus 552 MPa
    Dartdropimpact 180 g
    Elmendorftearstrengthmd 280 g
    Elmendorftearstrengthtd 500 g
    Haze 7.5%
    Gloss60degree 85%

    As an accredited Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips mPact™ D352 m-LLDPE is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for shipping.
    Container Loading (20′ FCL) Container loading (20′ FCL) for Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene: palletized bags securely stowed for ocean transport.
    Shipping Chevron Phillips mPact™ D352 m-LLDPE is shipped as solid pellets in moisture-barrier bags, bulk bags, or bulk trucks/railcars. Store in a cool, dry, well-ventilated area away from direct sunlight and ignition sources. Non-hazardous under normal shipping conditions; follow SDS. Handle pellets carefully to avoid dust, static, and moisture contamination.
    Storage Store Chevron Phillips mPact™ D352 m-LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original containers or bags closed and palletized off the floor to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and incompatible materials such as strong oxidizers. Use first-in, first-out stock rotation and follow supplier SDS/label instructions.
    Shelf Life Stable under normal storage conditions; no specific shelf life. Keep dry, clean, away from heat, sunlight, and contaminants.
    Application of Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene

    Heavy-duty shipping sacks produced from mPact D352 are typically converted on three-layer blown film lines where the critical failure mechanism is not tensile yield in the web but puncture propagation through gusset fold creases after palletized distribution. The resin belongs to the 0.933–0.936 g/cm³ density segment and is formulated as a hexene-based metallocene linear low-density polyethylene with a fractional melt index; this viscosity profile requires grooved-feed extruders and controlled die pressure. In a representative A/B/C stack, the outer skins are run at 75.0 wt% mPact D352, 23.0 wt% LDPE, and 2.0 wt% silica antiblock masterbatch; the core is blended at 85.0 wt% mPact D352 with 15.0 wt% LDPE. Layer ratios are maintained between 1:2:1 and 1:3:1, because increasing the core above 70% of total thickness raises bubble rigidity and lowers output under fixed air-ring cooling. On a 90 mm extruder with 30:1 L/D grooved feed, a 400 mm die, and a dual-lip air ring, stable production is achieved at 199–210 °C melt temperature, a blow-up ratio of 2.5:1–3.0:1, and a frost line height of 22–28 cm. Published data for this specific configuration is limited, but line audits show that frost-line drift above 30 cm increases gusset dart-impact scatter to more than ±12% within a single lot. Property conformance is assessed by ASTM D882 for tensile yield and break, ASTM D1709 Method B for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D5748 for puncture propagation. Commercial sack structures in the 140–180 µm range are commonly specified with a dart-drop target above 1,000 g; values below 800 g are treated as a rejection limit for export bulk packaging. Regulatory positions for dry food contact sacks follow FDA 21 CFR §177.1520 and EU Regulation (EU) No 10/2011, with converters advised to run overall migration testing on the finished multilayer structure rather than relying solely on resin supplier certifications. On bottom-gusseted sacks, heat sealing through 180 µm webs at jaw temperatures between 120 °C and 145 °C is preferred to impulse sealing because the medium-density skin withstands longer dwell times without excessive thinning at the seal shoulder.

    How Does Silage Cover Film Retain Tear Resistance Below 30 µm?

    In agricultural silage covering and bale wrap, the transition from 30 µm to 25 µm gauge is limited by field tear initiation along stalk punctures rather than by UV embrittlement alone. mPact D352 is used in seven-layer blown films as a stiffness and puncture carrier in the core and outer skins. A typical outdoor white/black structure contains 5.0–6.0 wt% carbon black concentrate in the central barrier core and 4.0–5.0 wt% of a HALS/triazine UV stabilizer masterbatch in the white outer skin. The core resin fraction is usually 60–70 wt% mPact D352 with 20–30 wt% butene LLDPE and trim reclaim not exceeding 10 wt%. On a 7-layer blown line with 300 mm die diameter and 1.6 mm die gap, the production window is held at a blow-up ratio of 2.8:1–3.2:1 and a die melt temperature of 204–215 °C. The critical process symptom is frost-line instability caused by high backpressure from HALS concentrate above 6.0 wt%; this produces gauge bands of ±4 µm across the layflat and reduces field tear resistance in thin-banded areas. Outdoor durability is evaluated by EN 13206:2017 for agricultural covering films, ISO 4892-2 for accelerated weathering, ASTM D3985 for oxygen transmission, and ASTM D5748 for puncture propagation. Published data for this specific mPact D352 silage wrap configuration is limited; end-use field pull tests remain the standard for silage retention and mold suppression under extended storage.

    Stretch Hood Holding Force Retention After 40 °C Ageing

    Stretch hood film for pallet load containment requires elastic recovery, puncture resistance, and holding force over 7–28 days of warehousing. mPact D352 is blended with ULDPE/VLDPE at 30–50 wt% to raise yield stress without excessively increasing permanent set. In five-layer blown production, a representative stack places the D352-rich layer in the core; the outer skins contain a polyolefin tackifier masterbatch at 1.5–2.5 wt%. The die gap is 2.0 mm, the blow-up ratio is kept at 2.0:1–2.4:1, and frost line height is set at 450–550 mm on a 500 mm die. Melt temperature is held at 204–216 °C; above 220 °C surface oxidation reduces cling, while below 190 °C the D352 fraction increases die pressure and layer-thickness variation. Tensile and hysteresis properties are evaluated by ASTM D882 and ISO 527-3 at 100% elongation; cling is measured by ASTM D5458. Published data for this specific resin in stretch hood formulations is limited, and converter trials commonly benchmark holding force retention after 40 °C warehouse simulation against incumbent hexene mLLDPE grades rather than relying on supplier datasheet values.

    Modifying a standard blown-film sealant web with mPact D352 at 20–30 wt% in the sealant skin shifts the heat-seal initiation plateau upward by approximately 3–8 °C relative to a pure EVA sealant, but it reduces tack contamination on sealing jaws and improves hot-tack strength above 120 °C. In vertical form-fill-seal structures, the sealant layer is commonly composed of 65–75 wt% EVA, 18–25 wt% D352, 2–4 wt% synthetic silica antiblock masterbatch, and 0.5–1.0 wt% slip masterbatch. The blown-film line is operated at a die gap of 1.8 mm, a melt temperature of 204–213 °C, and a blow-up ratio of 2.2:1–2.6:1. Sealing validation on horizontal or vertical FFS equipment follows ASTM F1921 for hot tack and ASTM F88 for seal strength; production-scale failures are most often traced to jaw temperature overshoot above 150 °C, which creates edge stringing and web transfer marks. For food contact, the finished package is subject to FDA 21 CFR §177.1520 and EU Regulation (EU) No 10/2011, including the 10 mg/dm² overall migration limit and applicable specific migration limits for additives. REACH compliance under EC No 1907/2006 requires documentation of SVHC content below 0.1 wt% in the finished article.

    Standard / RegulationParameterTypical Limit / Test Condition
    FDA 21 CFR §177.1520Olefin polymer food-contact useExtraction limits per paragraph (c)
    EU Regulation (EU) No 10/2011Overall migration10 mg/dm²
    EU Regulation (EU) No 10/2011Specific migration of additivesAdditive-specific SML
    REACH EC No 1907/2006SVHC in article0.1 wt% threshold
    RoHS 2011/65/EUPb, Hg, Cr6+, PBB, PBDE0.1 wt% each; Cd 0.01 wt%

    When EVA-Based Extrusion Lamination Layers Are Replaced by mPact D352

    Extrusion lamination of metallized PET to a polyethylene sealant web subjects the molten polymer to severe thermal stress because the melt curtain must wet the metal surface without oxidizing into fish eyes. mPact D352 can replace a high-VA EVA laminating layer in structures where acetic acid migration from EVA is undesirable. A barrier laminate with 12 µm metallized PET and 60 µm blown PE substrate is bonded with a 15–18 g/m² mPact D352/LDPE layer; the laminating blend typically contains 60–70 wt% D352, 25–35 wt% LDPE, and 5.0 wt% silane-grafted polyolefin adhesive concentrate. The extruder is a 90 mm 30:1 L/D machine with a coat-hanger die; melt temperature is held at 295–315 °C, air gap is 130–180 mm, and chill roll temperature is 15–20 °C. Below 120 m/min line speed, curl from asymmetrical thermal shrinkage increases; above 290 m/min, draw resonance at the die lip produces edge beads that transfer to the rewound roll. Peel adhesion is tested by ASTM D1876, and heat-seal response of the finished laminate is tested by ASTM F88. Published adhesion data for this specific D352 formulation is limited; converters should confirm target peel values above 2.0 N/15 mm on metallized surfaces via pilot-laminator trials because metallic adhesion varies with corona treatment and storage time.

    Coextruded Barrier Sealant Layers and Melt Curtain Stability at 2.8 BUR

    In five-layer blown barrier film for stand-up pouches, mPact D352 is placed in the outer and inner sealant skins to provide stiffness and puncture resistance while EVOH supplies the oxygen barrier. A representative layer ratio is 20/10/10/10/50 outer skin/tie/EVOH/tie/sealant skin, with the outer skin formulated at 60 wt% D352, 35 wt% LDPE, and 5.0 wt% processing aid masterbatch. The sealant skin uses 70 wt% D352, 20 wt% LDPE, and 10 wt% slip/antiblock masterbatch. The die is held at 190–220 °C with a uniform profile; the lower limit protects EVOH from gel formation, while the upper limit prevents D352 degradation. Blow-up ratio is maintained at 2.6:1–3.0:1, die gap is 2.0 mm, and frost line is 18–22 cm. Interlayer adhesion and seal performance are tested by ASTM F88 and ASTM F904; oxygen transmission is tested by ASTM D3985 and moisture vapor transmission by ASTM F1249. Production-scale failure of this structure is most often observed as melt curtain instability at the die when layer ratio is changed by more than 5%, producing gauge bands that reduce seal strength at gusset corners.

    LayerFunctionTypical DistributionCritical Test
    Outer skinPrint surface and abuse resistance20 wt%ASTM D882
    Tie 1Adhesion between PE and EVOH10 wt%ASTM F904
    EVOHOxygen barrier10 wt%ASTM D3985
    Tie 2Adhesion between EVOH and sealant10 wt%ASTM F904
    Sealant skinSealability and puncture resistance50 wt%ASTM F88
    Free Quote

    Competitive Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips mPact™ D352 is a metallocene-catalyzed linear low density polyethylene supplied for blown film extrusion. The nominal density is 0.933 g/cm³ when measured per ASTM D1505, and the nominal melt index is 0.5 g/10 min at 190°C/2.16 kg per ASTM D1238 or ISO 1133-1:2022. The resin is an ethylene-hexene copolymer produced with single-site metallocene catalysis, resulting in a narrow molecular weight distribution and a more uniform short-chain branching distribution than conventional Ziegler-Natta LLDPE. Typical film applications include heavy-duty sacks, industrial liners, agricultural film, lamination substrates, and flexible food-contact packaging in gauges from 15 µm to 150 µm. The values cited in this document are typical lot-average values and are not specification limits; the supplier certificate of analysis controls the shipped lot.

    What Distinguishes Metallocene Catalysis in D352 from Conventional LLDPE?

    Conventional Ziegler-Natta LLDPE contains a heterogeneous distribution of active sites that creates broad compositional and molecular weight distributions. The low-molecular-weight, high-comonomer fraction contributes extractable species and can alter organoleptics in food packaging. The single-site metallocene catalyst used for D352 reduces this interchain heterogeneity, producing chains with more uniform hexene placement. As a result, the resin exhibits lower seal initiation temperature, lower extractables, higher clarity, and improved dart impact when compared with a conventional 0.918 g/cm³ butene LLDPE at equivalent film gauge. The property difference is most pronounced in downgauged structures below 50 µm, where impact and tear resistance become limiting.

    Representative comparative profile; exact lot values are supplied on the manufacturer certificate of analysis.
    Property or featuremPact D352Conventional Ziegler-Natta LLDPEHigh-pressure LDPE
    Density0.933 g/cm³ per ASTM D15050.918 g/cm³ typical per ASTM D15050.920 g/cm³ typical per ASTM D1505
    Melt index0.5 g/10 min per ASTM D12381.0 g/10 min typical per ASTM D12380.3 g/10 min typical per ASTM D1238
    Molecular architecturenarrow MWD, uniform hexene branchingbroad MWD, heterogeneous branchingbroad MWD, long-chain branching
    Seal initiationlowerhigherlow
    Dart impact per ASTM D1709higher at equal gaugelower at equal gaugemoderate
    Melt strengthmoderatemoderatehigh
    Opticshigher clarity and glosslower clarity and glossmoderate
    Extractableslowerhighermoderate to high

    Because metallocene catalysis narrows the melting range, D352 enters the sealing plateau over a narrower temperature interval. That can reduce the seal bar setpoint required to reach a given seal strength per ASTM F88, but it also narrows the upper thermal limit before seal distortion. If seal bars operate more than 15°C above the plateau, edge burn-through or film relaxation can occur. Side-seal machines with dwell times from 0.05 s to 0.3 s require careful temperature profiling when the film contains high-slip or high-antiblock masterbatch, because surface additives migrate to the seal layer and alter heat transfer.

    On a production-scale monolayer blown film line using a grooved-feed extruder with 30:1 L/D and a barrier screw with a Maddock mixing section, D352 processes within a melt temperature range of 190°C to 230°C. A die gap of 1.5 mm to 2.5 mm and a blow-up ratio of 2.0:1 to 3.0:1 are typical starting conditions. Frost line height is set between 300 mm and 600 mm, depending on the desired machine-direction tear and bubble stability. Because the melt index of 0.5 g/10 min is lower than many packaging grades, die pressure and motor load can be 15% to 30% higher than those of a 1.0 g/10 min mLLDPE at equal screw speed. Melt temperature exceeding 250°C, especially at residence times above 5 min, can increase gel formation, odor, and edge instability.

    Pre-drying is not required under normal dry storage. Condensation on cold pellets at relative humidity above 60% can introduce surface moisture and cause bubble instability, die lines, and surface defects. In that condition, a dehumidifying hopper at 60°C for 2 h is used before extrusion. Wet pellets should not be processed directly, because steam at the die lips disrupts the melt curtain and can generate microgels in the finished film.

    Film Property Response at 25 µm Gauge on High-Stalk Bubble Configurations

    High-stalk configurations maximize machine-direction orientation and are used for heavy-duty film made with D352. At nominal 25 µm gauge, a high-stalk bubble with a blow-up ratio of 2.5:1 and a die gap of 1.8 mm provides a balance of machine-direction tensile strength and transverse-direction tear. Tensile strength and elongation at break are measured per ASTM D882; dart impact is measured per ASTM D1709; and Elmendorf tear is measured per ASTM D1922. Published data for this specific configuration is limited for coextruded structures, because layer ratio, tie resin, and skin additive package shift the reported values. For monolayer film, the manufacturer technical data sheet provides typical property ranges, and the processor should request lot-specific film test results rather than relying on resin pellet data alone.

    Haze per ASTM D1003 and gloss per ASTM D2457 respond to die gap, frost line height, and screw cooling. A lower die gap and higher frost line height generally reduce haze, but a die gap below 1.2 mm combined with a melt temperature below 180°C can produce sharkskin at high output. A die gap above 2.5 mm can reduce orientation and lower machine-direction tear strength. Bubble stability at gauge below 20 µm is sensitive to ambient air currents; an enclosed tower with controlled exhaust is recommended. Internal bubble cooling and oscillating haul-off improve gauge uniformity and roll geometry on lines running above 100 kg/h.

    The low melt index of D352 produces higher shear viscosity at extrusion conditions than higher-flow mLLDPE grades. Capillary rheometry at 200°C and a shear rate of 1,000 s⁻¹ is used to estimate die pressure on a given line. Screens of 80 mesh to 120 mesh are typical, but finer screens or high back pressure can exceed the safe operating range of the melt pump and breaker plate. A pressure differential above 3,500 kPa across the screen pack indicates the need for screen replacement. Melt filtration and die-lip cleanliness directly affect gel count and film quality in high-integrity packaging.

    Differential scanning calorimetry of D352 shows a sharp melting endotherm typical of a 0.933 g/cm³ ethylene-hexene copolymer. The narrow melting distribution contributes to rapid heat seal response, but it also means that seal strength changes over a few degrees Celsius. Seal dwell time and temperature must be characterized on the target packaging machine because seal strength per ASTM F88 and hot tack per ASTM F1921 depend on film structure, gauge, and additive package, not on resin density alone.

    When Seal Initiation Temperature and Hot Tack Window Are Constrained in Flexible Packaging

    In vertical form-fill-seal and flow-wrap operations, D352 is selected when the package requires a heat seal initiation lower than that of conventional 0.918 g/cm³ Ziegler-Natta LLDPE. On equipment with seal dwell times from 0.1 s to 0.5 s, the metallocene resin can allow a seal bar setpoint reduction of 10°C to 20°C. The practical result is a wider hot tack window measured per ASTM F1921, allowing the seal to maintain integrity while the molten weld is under load immediately after sealing. This is relevant in high-speed pouching lines where the seal is loaded by product drop before cooling is complete.

    The seal window is not unlimited. A coextruded sealant layer containing high levels of slip or antiblock masterbatch can shift seal initiation upward and reduce hot tack strength. Polybutene blending or excessive reclaim content may widen the seal plateau but can reduce stiffness and raise extractables. Migration of low-molecular-weight species from the sealant layer into food simulants is governed by diffusion kinetics in the polyethylene matrix and accelerates at temperatures above 40°C. Final structures must be tested under the relevant food-contact regulation; resin compliance alone does not guarantee compliance of the printed or laminated package.

    Relative to lower-density mPact grades, D352 at 0.933 g/cm³ provides higher secant modulus per ASTM D882, lower water vapor transmission rate per ASTM F1249, and greater puncture resistance per ASTM D5748. A nominal 0.918 g/cm³ mLLDPE may deliver lower haze and lower seal initiation temperature, but D352 is used when stiffness and tear resistance are weighted more heavily, such as heavy-duty sacks, industrial liners, agricultural films, and laminating substrates. Compared with a conventional medium-density polyethylene of similar density, the hexene comonomer and metallocene catalyst in D352 retain higher impact strength and lower extractables. The resin is typically supplied without slip or antiblock additives; if a coefficient of friction below 0.3 per ASTM D1894 is required, a slip/antiblock masterbatch must be added at a level determined by gauge, aging temperature, and winding tension.

    D352 should be processed without addition of pro-oxidant masterbatches unless the final film is explicitly designed for oxidative degradation and the additive supplier has qualified the narrow-MWD metallocene base resin. Certain amine-based additives and high-pH fillers can interact with catalyst residues or accelerate color formation at elevated temperatures. Long-term outdoor exposure requires a hindered amine light stabilizer and UV absorber package; the resin as supplied does not contain an outdoor weathering stabilizer system.

    Regulatory, Food-Contact, and Environmental-Release Boundaries

    Compliance statements depend on the finished article and conditions of use. Chevron Phillips Chemical typically provides a letter of conformity for mPact D352 under FDA 21 CFR 177.1520(c) for olefin polymers when the resin is used in accordance with specified end-use limitations. For the European Union, compliance with Regulation (EU) No 10/2011 requires migration testing on the final film because processing aids, printing inks, and coextruded layers alter overall migration and specific migration limits. The overall migration limit for plastic food-contact materials is 10 mg/dm² under the specified test conditions. The resin is not intended for medical implant applications.

    Representative compliance checklist; current supplier declarations govern the shipped lot.
    Standard or regulationTypical scopeNumerical threshold or condition
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactConditions of use A through H per finished article
    Regulation (EU) No 10/2011Plastic food-contact materialsOverall migration 10 mg/dm²; Annex II specific migration limits
    REACH EC 1907/2006Registration and SVHC communicationCandidate List substances 0.1% w/w per article
    RoHS 2011/65/EURestricted substances in electrical/electronic equipmentPb 1000 mg/kg; Cd 100 mg/kg; Hg 1000 mg/kg; Cr(VI) 1000 mg/kg; PBB/PBDE 1000 mg/kg

    The processing and application statements in this document are based on typical blown film extrusion practice for metallocene LLDPE and on published supplier literature. They are not a specification for any particular production line. The low melt index and narrow sealing plateau require line-specific characterization; published data for this specific configuration is limited for high-output coextruded lines above 200 kg/h. Lot-specific certificates of analysis, regulatory letters, and film test data should be obtained from Chevron Phillips Chemical before qualifying D352 for a controlled food-contact or high-integrity industrial structure.