| HS Code | 403173 |
| Polymer Type | Metallocene Linear Low Density Polyethylene (mLLDPE) |
| Catalyst Type | Metallocene |
| Melt Index 190 C 2 16 Kg | 0.85 g/10 min |
| Density | 0.918 g/cm³ |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 43.4 MPa |
| Elongation At Break | 700% |
| 1 Secant Modulus | 207 MPa |
| Dart Drop Impact | 500 g |
| Elmendorf Tear Strength Md | 350 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 7% |
| Gloss 45 | 80 |
| Coefficient Of Friction D257 | 0.20 |
| Slip Additive D252 | Absent |
| Slip Additive D257 | Present |
| Antiblock Additive D252 | Absent |
| Antiblock Additive D257 | Present |
As an accredited Chevron Phillips mPact™ D252/D257 LLDPE Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips mPact™ D252/D257 LLDPE Film Resin: 25 kg polyethylene bags, 40 bags per pallet (1,000 kg); also 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL loads approx. 18 pallets (24.75 MT) of Chevron Phillips mPact™ D252/D257 LLDPE Film Resin in 25 kg bags. |
| Shipping | Chevron Phillips mPact™ D252/D257 LLDPE Film Resin is shipped as a non-hazardous solid, typically in 25 kg polyethylene bags on stretch-wrapped pallets or in bulk trucks/railcars. Store cool and dry, away from sunlight, heat, moisture, and contaminants; secure loads to prevent shifting. |
| Storage | Store Chevron Phillips mPact™ D252/D257 LLDPE Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep containers or bags closed, palletized, and protected from moisture, dust, and contamination. Avoid prolonged high temperatures. Use first-in, first-out rotation. Follow facility and SDS requirements. |
| Shelf Life | For mPact D252/D257: store cool, dry, in original unopened packaging; typical shelf life is 12 months from date of manufacture. |
Heavy-duty sacks made from mPact™ D257-rich blown film are produced on three-layer coextrusion lines with 70 mm barrier screws, 30:1 L/D ratios, and dual-lip air rings; the melt temperature profile is held between 180°C and 215°C, with the die zone at 215°C and adapter pressure between 320 bar and 420 bar. A typical formulation for a 160 µm sack contains 80 wt% mPact D257, 12 wt% high-pressure LDPE, and 8 wt% clean internal backscrap. The die gap is set at 1.8–2.2 mm, the blow-up ratio at 2.2–2.7:1, and the frost line height at 8–10 die diameters. The LDPE content is the main process conflict: below 10 wt% LDPE, bubble stability deteriorates at high haul-off speeds, while above 25 wt% LDPE the dart impact and Elmendorf tear of the sack decrease. Film properties are tested according to ASTM D1709-16A for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D882-18 for tensile yield and break; filled sacks are evaluated under ISO 21898:2004 for drop resistance. Terminal products include valve sacks for polymer granules, fertiliser, and chemical additives. The operational boundary is a melt temperature above 220°C; this promotes oxidation-induced gel formation in the mLLDPE-rich layer and increases downtime during screen pack changes.
On vertical form-fill-seal lines running polyethylene-based frozen vegetable and IQF poultry films, the sealant layer is compounded from 60 wt% mPact D252, 20 wt% LDPE, and 20 wt% antiblock/slip masterbatch carrier; the outer layer uses a 75/25 mPact D257/LDPE blend for abuse resistance. The film is produced on a three-layer coextrusion blown-film line with 2.0 mm die gap, 2.5:1 blow-up ratio, and melt temperature 193–208°C; the frost line is held at 5–7 die diameters. Seal initiation is evaluated on a J-type ASTM F2029-17 heat sealer at 0.275 MPa seal bar pressure and 0.5 s dwell; the sealant layer is expected to reach seal strength above 12 N/25 mm according to ASTM F88-21. Compliance for direct food contact in the US falls under FDA 21 CFR 177.1520(c) 3.1a/3.2a and in the EU under Regulation (EU) No 10/2011; overall migration must remain below 10 mg/dm² under OM2 test conditions. Terminal films include 350 g to 2.5 kg frozen vegetable bags and IQF poultry pouches. Downgauging from 45 µm to 35 µm is feasible only if the D252-rich sealant layer is maintained at no less than 15 µm. Slip additive loadings above 800 ppm in the sealant layer reduce seal strength and increase leaker rates because frozen-food dust amplifies seal contamination.
Agricultural silage and greenhouse films formulated with mPact D252/D257 are manufactured on high-output monolayer or two-layer blown-film lines with die diameters from 150 mm to 450 mm, die gap 1.8–2.6 mm, blow-up ratio 2.4–3.0:1, and melt temperature 188–216°C. A typical bale wrap formulation contains 88–94 wt% mPact D252, 7–12 wt% polyethylene-based HALS/UV masterbatch containing hindered amine light stabilizers, and 1–2 wt% antiblock masterbatch with synthetic silica; for greenhouse covers, the coextruded skin layer carries 0.5–1.5 wt% HALS and 0.2–0.7 wt% UV absorber package, while the core retains unmodified D257 for tear resistance. The inflated bubble is quenched with chilled air at 12–18°C to suppress haze caused by overly rapid cooling. Critical threshold: the frost line must be held within ±2 die diameters of the set point; if frost line rises above 10 die diameters, TD elongation and dart impact become inconsistent. Compliance is assessed under ASTM D5748-19 for puncture propagation resistance, ASTM D882-18 for tensile modulus, and ISO 527-3:2018 for elongation at break; UV stability is verified by accelerated weathering per ASTM G154-23 Cycle 1 with retention of elongation at break above 50% after 2000 h. Silage acid resistance is simulated by immersion in 3 wt% acetic acid at 40°C for 72 h, with mass uptake below 0.2 wt%. Terminal products include 750 mm round bale silage wrap, 12 m-wide greenhouse covers, and silo cover sheeting. Operational boundary: slip masterbatch should not exceed 0.15 wt% free erucamide equivalent in bale wrap because reduced film-to-film friction lowers winder tension and causes telescoping rolls.
Stretch hood pallet films are extruded on a three-layer coextrusion line with a 250 mm die, 1.4–2.0 mm die gap, 2.0–2.6:1 blow-up ratio, and melt temperature 195–215°C. The core layer contains 70–85 wt% mPact D257; the skin layers combine 10–20 wt% metallocene plastomer with LDPE and 0.5–1.2 wt% slip/cling masterbatch. The film is drawn in machine direction and then converted on a stretch hood machine with pre-stretch ratio 1.8:1 to 2.2:1; final film thickness is 80–140 µm. Puncture energy is tested according to ASTM D5748-19 at 23°C ±2°C; tensile impact is measured by ISO 8256:2004 Method A. The melt pressure at the adapter is maintained within 300–400 bar; exceeding 420 bar indicates excessive screen pack pressure drop and triggers gel formation in metallocene-rich layers. The critical processing conflict is the balance between cling and machine unwind tension: if the coefficient of friction in the skin exceeds 0.6 as measured by ASTM D1894-14, the film may block on the stretch hood machine; if it drops below 0.25, the film loses load stability on smooth palletized surfaces. End products include pallet wraps for PET bottle bundles, OSB panels, and bagged cement. Operational limitation: coextruded film with D257-rich cores should not be stored below 5°C for more than 48 h before stretching, because low-temperature stiffness shifts the pre-stretch force curve and raises the incidence of puncture at sharp pallet corners.
For retortable stand-up pouch structures, the sealant web is produced from mPact D252-rich blown film with a thickness between 25 µm and 40 µm and is subsequently laminated to aluminium foil or metallized polyester by solventless adhesive. The sealant layer formulation contains 70–80 wt% mPact D252, 10–20 wt% butene LLDPE, and 5–15 wt% LDPE to balance hot-tack and seal-through-contamination; the film is produced on a three-layer blown-film line with 1.6–2.0 mm die gap, 2.2–2.8:1 blow-up ratio, and melt temperature 190–208°C. Hot-tack performance is measured on a J&B hot-tack tester at 0.5 N/mm² seal bar pressure and 0.5 s dwell; the sealant must maintain hot-tack strength above 2 N/25 mm over a sealing temperature range of 85–120°C. Heat seal curves per ASTM F2029-17 are generated with 25 mm-wide specimens and a dwell time of 0.5 s. The laminated structure is evaluated for interlayer adhesion according to ASTM F904-16, and the finished pouch is retortable at 121°C for 30 min in a counter-pressure autoclave if the external layers are designed for retort conditions. End products include retort pouches for ready-to-eat rice, sauce pouches, and pet food packs. The key limitation is that the D252-rich sealant web must not be exposed to corona treatment intensities above 2.5 kW·min/m² before lamination; higher intensities create low-molecular-weight oxidation products that reduce seal strength after sterilisation.
On horizontal form-fill-seal lines running liquid sachet and powder stick applications, the sealant web is coextruded as a three-layer film with a core of 80 wt% mPact D257 and 20 wt% LDPE; the skin layer contains 60 wt% mPact D252, 25 wt% butene LLDPE, 10 wt% LDPE, and 5 wt% masterbatch with slip and antiblock at 0.3–0.8 wt% inorganic silica. The film is blown on a 200 mm die with 1.5 mm die gap, 2.0:1 blow-up ratio, and melt temperature 196–212°C. At film thickness below 25 µm, the bubble must be stabilised with internal bubble cooling and a dual-lip air ring; otherwise TD gauge variation exceeds ±8%, causing seal window narrowing. Seal initiation temperature is measured on an ASTM F2029-17 sealer at 0.275 MPa, 0.5 s dwell; the sealant layer is required to reach 8 N/25 mm seal strength by 105°C. The film must pass FDA 21 CFR 177.1520(c) 3.1a for food contact and Regulation (EU) No 10/2011 with overall migration below 10 mg/dm²; where used for pharmaceutical powder stick packaging, extractables are screened per USP <661.1>. Terminal products include single-serve beverage powder sticks, liquid detergent sachets, and cosmetic sample pouches. Operational boundary: the slip package must not exceed 1200 ppm erucamide equivalent; above this level, seal strength drops and delamination at the seal area occurs after horizontal form-fill-seal jaw release.
| Application Segment | Standard Designation | Test Purpose |
|---|---|---|
| Heavy-duty sacks | ASTM D1709-16A, ASTM D1922-15, ISO 21898:2004 | Dart impact, Elmendorf tear, filled-sack drop resistance |
| Frozen food packaging | FDA 21 CFR 177.1520(c) 3.1a/3.2a, Regulation (EU) No 10/2011, ASTM F88-21, ASTM F2029-17 | Food contact compliance, seal strength, seal initiation |
| Agricultural silage/greenhouse | ASTM D5748-19, ASTM G154-23, ISO 527-3:2018 | Puncture propagation, UV weathering, elongation at break |
| Stretch hood pallet wrap | ASTM D5748-19, ASTM D1894-14, ISO 8256:2004 | Puncture energy, coefficient of friction, tensile impact |
| Retortable pouch sealant web | ASTM F2029-17, ASTM F904-16 | Heat seal, interlayer adhesion |
| High-speed pouching sealant | FDA 21 CFR 177.1520(c) 3.1a, Regulation (EU) No 10/2011, ASTM F88-21 | Food contact compliance, seal strength |
Competitive Chevron Phillips mPact™ D252/D257 LLDPE Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips mPact D252 and D257 are metallocene-catalysed linear low-density polyethylene film resins based on hexene comonomer. Grade positioning places D252 at a nominal density of 0.921 g/cm³ when tested under ASTM D1505 or ISO 1183-1:2019 and at a melt index near 2.0 g/10 min under ASTM D1238, 190 °C/2.16 kg. D257 is positioned at a nominal density near 0.917 g/cm³ and a melt index in the 2.3–2.6 g/10 min range under the same conditions. The single-site catalyst architecture produces a narrow short-chain branching distribution and a reduced fraction of high-density backbone segments relative to conventional Ziegler-Natta butene LLDPE. The resulting property balance is lower heat-seal initiation temperature, higher Elmendorf tear propagation resistance, and higher dart impact at equivalent gauge. D252 is intended for converters requiring greater stiffness, yield strength, and web handling; D257 is intended for thin-gauge packaging webs where toughness, optics, and puncture resistance limit performance. Both grades are supplied as pelletized film resins with antioxidant stabilization and are used in monolayer or coextruded blown film equipment.
The distinction between D252 and D257 is density-driven. The 0.004 g/cm³ nominal density difference shifts the balance between modulus and tear resistance. In film structures where machine-direction tear initiation is a failure mode, D257 may be preferred because lower crystallinity permits greater plastic deformation before crack propagation. D252 provides higher secant modulus and better web stiffness. Actual property response depends on film gauge, die geometry, blow-up ratio, and frost line height; published data for this specific resin pair under standardized conditions is limited, and converter trials are required for final qualification.
Blown film processing of metallocene-catalysed LLDPE grades requires narrower operating windows than Ziegler-Natta LLDPE because of reduced shear thinning and higher extensional stress response. Converters operating single-screw extruders with L/D ≥ 24:1 and barrier screw designs typically set reverse-temperature profiles from 170 °C to 210 °C, with die zones between 210 °C and 230 °C and melt temperature at the die not exceeding 240 °C. A die gap of 1.5–2.5 mm is generally used to mitigate melt fracture at high shear rates. Blow-up ratio commonly ranges from 2.0:1 to 2.7:1; lower blow-up ratios may reduce transverse direction tear resistance, while higher blow-up ratios can induce bubble instability unless the frost line is raised to 8–12 die diameters. Because melt strength of D252 and D257 is lower than that of high-pressure LDPE or long-chain-branched LLDPE, a bubble stabilizer such as LDPE may be added at 10–20 wt% when drawing films below 25 µm. The addition of LDPE reduces bubble sag and lowers melt pressure, but it raises haze and reduces dart impact; converters producing optically critical films should minimize LDPE content or select a high-pressure LDPE with narrow molecular weight distribution.
Compared with a conventional butene LLDPE of similar melt index, the narrow molecular weight distribution can raise extruder motor load by 5–15% at equivalent screw speed, especially in grooved-feed extruders. The use of a wider die gap and higher temperatures within the stated window reduces this load at the expense of transverse direction orientation. Slip and antiblock additives are lot-specific. Coefficient of friction should be measured under ASTM D1894 after 48 h conditioning at 23 °C and 50% RH because migratory slip compounds reach equilibrium slowly in metallocene matrices.
The following table consolidates grade-positioning ranges compiled from producer technical literature and comparative converter data. The values are representative, not batch-release certificates. Incoming material should be specified against the supplier certificate of analysis, not generic literature ranges.
| Property | Test method | mPact D252 | mPact D257 |
|---|---|---|---|
| Density | ASTM D1505 / ISO 1183-1:2019 | 0.920–0.922 g/cm³ | 0.916–0.918 g/cm³ |
| Melt index | ASTM D1238, 190 °C/2.16 kg / ISO 1133-1:2022 | 1.9–2.1 g/10 min | 2.3–2.6 g/10 min |
| Melting temperature | DSC, ASTM D3418 | 119–123 °C | 117–121 °C |
| Vicat softening temperature | ASTM D1525 | 102–106 °C | 99–103 °C |
| Tensile strength at break, MD | ASTM D882 | 40–48 MPa | 42–50 MPa |
| Elongation at break, MD | ASTM D882 | 550–650% | 600–700% |
| Dart drop impact, F50, 50 µm blown film | ASTM D1709A | 600–900 g | 900–1300 g |
| Haze, 50 µm blown film | ASTM D1003 | 6–10% | 4–8% |
These ranges are not specifications; specific lot certificates may fall outside the indicated intervals because of additive package, film fabrication, and conditioning history. For critical sealing applications, the supplier certificate of analysis and a trial on the target film line remain the controlling references.
D252 is used in collation shrink film, overwrap, and high-stiffness packaging where rapid bag opening and web handling are required. The higher modulus reduces film sag on vertical form-fill-seal machines and allows down-gauging by 10–20% relative to conventional butene LLDPE of equivalent modulus. D257 is used in high-integrity liquid packaging, heavy-duty sacks, and freezer film, where puncture, cold-temperature impact, and tear propagation limit performance. In coextruded structures, D257 has been placed in sealant layers to reduce heat-seal initiation temperature and to extend the hot-tack plateau across jaw dwell times from 0.3 s to 0.6 s when tested with ASTM F1921. The lower seal initiation supports higher sealing speeds on horizontal flow-wrap equipment; the practical limit is controlled by thermal transfer through the reverse-printed substrate rather than by resin melting alone.
Cast film operation with D257 requires a chill-roll temperature between 20 °C and 35 °C to preserve film clarity and reduce post-crystallisation haze. For blown film, the frost line height must be adjusted upward when gauge variation exceeds ±5%; bubble diameter control using digital gauge profilers is recommended. In deep-freeze packaging, D257 retains ductile deformation at freezer temperatures typical of -18 °C storage, but the converter must qualify the complete structure under the target cold-chain distribution profile because sealing-layer thickness and orientation affect puncture resistance in frozen distribution.
Conventional Ziegler-Natta butene LLDPE of similar density and melt index typically exhibits broader short-chain branching distribution and higher extractable fractions. The consequence is measured as higher haze after heat-seal cycles and lower dart impact at frozen storage. With D257, the narrower branching distribution reduces low-molecular-weight extractables and shifts the heat-seal initiation temperature downward by 5–10 °C in laboratory sealing trials conducted under ASTM F88/F88M and ASTM F1921. The shift allows sealing jaws to operate at lower setpoint temperatures while maintaining seal strength above 1.5 N/15 mm, a common minimum for snack packaging integrity. A lower jaw setpoint also reduces substrate shrinkage and reverse-print distortion in oriented polyester and biaxially oriented polypropylene lamination.
Compared with high-pressure LDPE, D252 and D257 have lower melt strength and lower bubble stability. Drawdown to gauges below 20 µm on high-stalk bubble geometry may require blending with 15–25 wt% LDPE. The addition of LDPE broadens the processing window but increases seal initiation temperature and reduces elongation at break. Compared with octene metallocene LLDPE, the hexene-based D252 and D257 may show slightly lower dart impact and tear at equivalent density and melt index; however, field reports from blown film converters indicate that the hexene grades provide adequate toughness at lower compound cost while maintaining lower gel counts in cast film. Published data for this specific resin pair under identical high-speed packaging conditions is limited; direct side-by-side evaluation on the target line is required.
In the United States, polyolefin film resins in this product family are generally manufactured to meet FDA 21 CFR 177.1520(c) 3.1a or 3.2a conditions for food-contact articles, subject to the thickness and extraction limitations specified in the regulation. The converter must verify the current supplier food-contact letter because additive formulation changes may alter the migration profile. For European Union conversion, compliance should be established under Commission Regulation (EU) No 10/2011 and its amendments, with overall migration tested under EN 1186-1 and specific migration limits for additives under EU 10/2011 Annex II. In applications involving fatty foods, the simulant D2 or 95% ethanol may be required under Annex V of EU 10/2011.
Storage should be in a dry, contaminant-free silo or lined bulk container at ambient temperature below 40 °C. Prolonged exposure to ultraviolet light during outdoor storage can generate free radicals and reduce oxidative induction time; resin should be purged with nitrogen during long-term silo storage. Regrind addition is limited to 10–20 wt% in high-clarity films because higher levels raise gel counts and haze. Drying is not normally required when the material is stored in sealed containers; with an ambient relative humidity above 60%, surface moisture on pellets can be removed by hopper drying at 60–70 °C for 2 h. Avoid dense-phase conveying air temperatures above 80 °C because pellet deformation can obstruct rotary feeders.