Chevron Phillips Mpact D143sa M Lldpe Linear Low Density Polyethylene

Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene

    • Product Name: Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 733809
    Polymer Type Metallocene Linear Low Density Polyethylene (m-LLDPE)
    Comonomer 1-Hexene
    Density 0.914 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melting Point 118 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield Md 8.6 MPa
    Tensile Strength At Break Md 38 MPa
    Elongation At Break Md 600 %
    Dart Drop Impact 300 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 350 g
    Haze 10 %
    Gloss 45 75
    Coefficient Of Friction 0.20
    Slip Agent Yes
    Antiblock Agent Yes

    As an accredited Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, palletized for bulk industrial shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Chevron Phillips mPact™ D143SA m-LLDPE, stretch-wrapped and secured for safe shipment.
    Shipping Chevron Phillips mPact™ D143SA m-LLDPE is shipped as non-hazardous solid polyethylene pellets, typically in 25 kg moisture-resistant bags or 1,000 kg supersacks, palletized and stretch-wrapped. Transport by dry van, rail hopper car, or bulk truck. Keep dry, cool, and contamination-free.
    Storage Store Chevron Phillips mPact™ D143SA m-LLDPE in a cool, dry, well-ventilated, covered warehouse, away from direct sunlight, heat, ignition sources, moisture, and incompatible materials. Keep original bags or containers closed, palletized, and off the floor. Avoid excessive stacking, prolonged high temperatures, and contamination. Protect from UV radiation and physical damage. Do not store outdoors. Follow FIFO and the supplier’s SDS.
    Shelf Life Shelf life: 24 months from date of manufacture when stored in original packaging, dry, well-ventilated area, away from direct sunlight and heat.
    Application of Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene

    Why Does Seal Initiation Temperature Determine Shelf-Ready Flow Wrap Throughput?

    For high-speed horizontal form-fill-seal (HFFS) lines packaging bakery and confectionery products, the sealant web's seal initiation temperature governs dwell time at the jaw. mPact™ D143SA is specified at a density of 0.918 g/cm³ by ASTM D1505-18 and a melt mass-flow rate of 1.0 g/10 min by ISO 1133-1:2022. In monolayer and three-layer coextruded structures using mPact™ D143SA as the sealant layer, seal initiation values measured by ASTM F88/F88M-21 typically fall between 85°C and 95°C at 0.5 N/15 mm seal force, allowing jaw temperature setpoints to be reduced by 10–15°C compared with conventional Ziegler-Natta LLDPE of equivalent 1.0 g/10 min melt index. The as-delivered slip and antiblock package reduces film-to-jaw release variation on high-speed HFFS lines and is characterized by kinetic coefficient of friction below 0.35 under ASTM D1894-24. Food-contact compliance is defined by FDA 21 CFR § 177.1520(c)3.1a for olefin polymers under Conditions of Use B through H and by EU Regulation No 10/2011 with an overall migration limit of 10 mg/dm² determined by EN 1186-1:2002. In a typical coextruded structure, the sealant layer contains 70–80 wt% D143SA and 20–30 wt% LDPE homopolymer with a melt index of 2.0–4.0 g/10 min to stabilize the bubble and reduce melt fracture during air-cooled blown film extrusion. The process is run on a 60 mm grooved-feed extruder with an L/D ratio of 30:1, die diameter 250 mm, die gap 1.8 mm, blow-up ratio 2.8:1 to 3.2:1, and frost line height maintained between 4 and 6 die diameters. Melt temperature at the adapter is limited to 193–216°C to avoid oxidative gel formation. Terminal finished product types include printed pillow packs for granola bars, bag-in-box cereal liners, and frozen vegetable pouches where low-temperature seal strength measured by ASTM F88/F88M-21 remains above 20 N/15 mm at −20°C storage.

    On a three-layer coextruded blown film line dedicated to 50 kg cementitious product sacks, replacing the outer and inner skins with mPact™ D143SA at 20–30 wt% of the total film formulation shifts the failure mode from brittle tear to ductile puncture propagation when measured by ASTM D5748-19. The middle layer remains a 40–50 wt% blend of in-line edge trim and post-industrial reclaim with LDPE to maintain bubble stability at a blow-up ratio of 2.4:1 to 2.8:1. The process uses a 75 mm grooved-feed extruder with a barrier screw, a 350 mm spiral mandrel die, and internal bubble cooling. Die gap is widened to 2.2 mm to reduce melt fracture associated with the narrow molecular weight distribution of metallocene grades. Melt temperature is controlled between 204°C and 227°C, and frost line height is set at 6–8 die diameters to maintain bubble symmetry. Compliance for industrial packaging is documented under EU Directive 94/62/EC with the sum of lead, cadmium, mercury, and chromium(VI) below 100 mg/kg by weight. Tensile properties are characterized by ISO 527-3:2018 on 25 mm wide strips at a test speed of 500 mm/min. Terminal finished product types include 25 kg and 50 kg form-fill-seal sacks for dry mortar, cement, resin pellets, and granular fertilizer, where the seal region remains the limiting failure point under 1.5 m drop impact testing.

    Five-Layer Silage Film Tear Resistance Data

    In agricultural bale wrap and bunker cover film, mPact™ D143SA is introduced into the two outer skin layers at 12–18 wt% of the total film mass, while a UV masterbatch with hindered amine light stabilizer is added at 3–6 wt% and a white pigmented masterbatch at 8–10 wt% in the core layer. This formulation targets puncture and tear resistance after 12 months of outdoor exposure, with retained tensile elongation at break measured by ISO 527-3:2018 and tear resistance by ISO 6383-2:1983. Published data for prolonged outdoor exposure of this specific resin configuration in silage film is limited; therefore, laboratory screening per ISO 4892-2:2013 is required for each incoming UV masterbatch lot. The film is specified against EN 13206:2017 for thermoplastic stretch films for silage and against REACH Annex XVII restrictions on certain phthalates and heavy metals. The downstream process is a five-layer coextruded blown film line using one 90 mm extruder for the core, two 60 mm extruders for the skins, and two 45 mm extruders for tie layers. Die diameter is 400 mm, die gap is 2.0 mm, blow-up ratio is 2.0:1 to 2.5:1, and melt temperature is held at 191–210°C. Because metallocene LLDPE narrow molecular weight distribution reduces bubble stability at high frost line heights, the line is run with a frost line height of 5–7 die diameters and a low stalk height configuration. Terminal finished product types include 750 mm × 1500 m round bale wrap, 500 mm × 1800 m square bale wrap, and 12 m wide bunker cover sheet.

    When stand-up pouches for dry foods and frozen seafood do not require retort conditions, a sealant web based on mPact™ D143SA at 60–80 wt% blended with a low-melt-index LDPE at 20–40 wt% provides a seal initiation temperature below 100°C measured by ASTM F88/F88M-21 at 0.5 N/15 mm, reducing dwell time on rotary pouch-converting machines. The compliance profile for the food-contact sealant layer includes FDA 21 CFR § 177.1520(c)3.1a, EU Regulation No 10/2011, and for export to China, GB 4806.7-2016 with overall migration not exceeding 10 mg/dm². The downstream process begins with a three-layer coextruded blown film line equipped with a 50 mm grooved-feed extruder, die diameter 200 mm, die gap 1.5 mm, and blow-up ratio 2.5:1 to 3.0:1. The sealant film is then solventless-laminated to a reverse-printed 12 µm BOPET or 18 µm BOPP outer web using a 1.8–2.2 g/m² polyurethane adhesive. Lamination speed is limited to 180–220 m/min to maintain film tension below 40 N/m and prevent neck-in. Terminal finished product types include 250 g stand-up pouches for dried fruit, 1 kg quad-seal pouches for frozen vegetables, and side-gusseted coffee valve pouches.

    Compliance and test method matrix
    Application segmentRegulatory or consensus standardPrimary test methodCritical specification
    Food-contact flow wrapFDA 21 CFR § 177.1520(c)3.1a, EU Regulation No 10/2011ASTM F88/F88M-21, EN 1186-1:2002Seal initiation 85–95°C at 0.5 N/15 mm; overall migration below 10 mg/dm²
    Heavy-duty FFS sacksEU Directive 94/62/ECISO 527-3:2018, ASTM D5748-19Heavy metals sum below 100 mg/kg; puncture propagation mode
    Agricultural silage filmEN 13206:2017, REACH Annex XVIIISO 6383-2:1983, ISO 4892-2:2013Outdoor tear retention after 12 months
    Stand-up pouch sealant webFDA 21 CFR § 177.1520(c)3.1a, EU Regulation No 10/2011, GB 4806.7-2016ASTM F88/F88M-21, EN 1186-1:2002Seal initiation below 100°C; overall migration below 10 mg/dm²
    Free Quote

    Competitive Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Chemical’s mPact™ D143SA is a metallocene-catalyzed linear low-density polyethylene, abbreviated m-LLDPE. The grade is a 1-hexene ethylene copolymer with a nominal density of 0.918 g/cm³ determined by ASTM D1505 and a nominal melt index of 1.0 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238 and ISO 1133-1. The “SA” suffix in commercial documentation identifies a formulated slip and antiblock package intended for film separation and converting. In blown film applications, D143SA is used for monolayer packaging films, lamination skins, overwrap, and coextruded sealant webs. The product is selected where gauge reduction, puncture resistance, seal integrity, and optical clarity are specified in the same film structure. Typical processing and converting conditions must be validated against lot-specific technical data because the additive package and comonomer distribution can shift secondary properties such as coefficient of friction and blocking force.

    What separates metallocene hexene mLLDPE from conventional butene LLDPE and high-pressure LDPE?

    Ziegler-Natta butene LLDPE grades exhibit a broad interchain comonomer distribution and a heterogeneous short-chain branch profile because of multi-site active centers. D143SA is polymerized on a single-site metallocene catalyst; the resulting narrow molecular weight distribution and uniform intramolecular and intermolecular branching alter solid-state morphology. At the same nominal density, the lamellae are thinner and more uniformly distributed, which reduces bulk haze when measured by ASTM D1003 and increases dart impact at a given gauge when tested by ASTM D1709, Method A. The reduction in low-molecular-weight material also reduces extractable fractions and improves organoleptic performance in food-contact films, provided that the additive package meets the applicable migration limits under EU Regulation 10/2011 and US FDA 21 CFR 177.1520(c) 3.2a.

    High-pressure LDPE possesses long-chain branching, which imparts strain-hardening and melt strength. D143SA is essentially linear and has lower extensional viscosity; bubble stability in high-stalk processing is therefore lower than that of LDPE of the same melt index. The practical consequence is that D143SA requires closer control of die gap, cooling air velocity, and internal bubble pressure. Coextruding the mLLDPE core between LDPE skins or blending 10–20 wt% high-pressure LDPE is a standard method to recover bubble geometry on conventional lines. The metallocene resin also exhibits less shear thinning; extruder head pressures at identical screw speed and output are commonly higher than those of LDPE, requiring a pressure-rated die and possibly a higher-torque drive.

    Under high-shear extrusion conditions typical of cast film and small-die-gap blown film lines, the rheology of D143SA must be matched to screw geometry and die design rather than to melt index alone. The melt index by ASTM D1238 measures flow at low shear rate and does not predict high-shear viscosity; metallocene LLDPE generally requires a barrier screw with mixing sections and a length-to-diameter ratio of at least 24:1. On grooved-feed extruders in the 45–75 mm size range, melt temperature measured at the adapter can rise by several degrees Celsius as screw speed is increased because of viscous dissipation under high backpressure. Production-scale blown film lines have reported shark-skin melt fracture when die lip temperatures drop below the recommended melt temperature window or when die shear stress exceeds the critical value for narrow-MWD mLLDPE. Die gaps of 1.5–2.5 mm are assigned to reduce shear stress and to accommodate the higher melt pressure observed with metallocene resins.

    When D143SA is processed in high-stalk blown film at blow-up ratios above 2.5:1

    High-stalk configurations with blow-up ratios above 2.5:1 impose two measurable process risks on D143SA: stalk instability and gauge variation. To maintain a stable neck and prevent fluctuation, the internal bubble pressure must be held within a narrow band, and the frost line height should be fixed with a segmented cooling ring rather than by manual adjustment. On 55 mm extruders with a 100 mm die, LDPE skins of 10–20 wt% are often used to reduce deforming stresses near the die exit. The die gap is typically increased from 1.5 mm to 2.3 mm when the mLLDPE content in the structure exceeds 70 wt% to lower shear heating and delay melt fracture. Internal bubble cooling is often necessary for mLLDPE because of limited melt strength; a conventional air ring designed for LDPE can create a broad frost line and gauge bands at high output. The resulting gauge variation is quantified by scanning capacitance or beta transmission gauge. Film thickness variation above ±5% at 2σ can cause blocking in wound rolls and intermittent sealing at high form-fill-seal speeds. At melt temperatures above 240 °C, gel and oxidized speck formation increases, particularly where the resin residence time exceeds 10 min at high backpressure; published data for prolonged residence in this specific configuration is limited but the boundary is consistent with narrow-MWD metallocene ethylene copolymers.

    In coextruded sealant webs, D143SA is selected for low seal initiation temperature and elevated hot tack strength relative to higher-density LLDPE grades. Seal strength is evaluated according to ASTM F88/F88M, heat sealability of flexible barrier materials according to ASTM F2029, and hot tack according to ASTM F1921. The uniform comonomer distribution depresses the melting endotherm; low-temperature sealing on flat-seal equipment typically falls below 110 °C when validated with 0.3–0.7 MPa seal bar pressure and 0.5–1.0 s dwell, but the exact threshold depends on film gauge, seal bar geometry, and the thermal resistance of the outer printable layer. In high-speed form-fill-seal operations, hot tack performance must be verified on the target machine because seal cooling and contamination of the seal interface by product dust can shorten the processing window by several degrees. The grade is frequently coextruded with ethylene vinyl acetate or polyolefin plastomers when a seal-through-contamination requirement is specified.

    Dart impact, tear, and puncture qualification protocols

    Mechanical toughness of D143SA film is not described by a single value. Dart impact is measured by ASTM D1709 using a staircase technique; results shift with film gauge, blow-up ratio, and frost line height. Elmendorf tear by ASTM D1922 reflects propagation resistance and is not interchangeable with trouser tear or Graves tear values. Puncture resistance is quantified by ASTM D5748 with a 9.5 mm probe; in coextruded films the puncture value often registers the outer layer stiffness as much as the core toughness. For specification purposes, a 25 µm monolayer film produced at a 2.5:1 blow-up ratio and a 2.0 mm die gap may be used as a reference configuration, but the user must establish control film samples on the actual line. Published data for this specific configuration is limited; therefore, incoming QC should include dart impact at the intended gauge rather than relying on resin data generated at a different gauge. Secant modulus reported at 1% strain by ASTM D882 can be used to estimate film stiffness but should not be confused with tensile modulus reported at 2% strain for injection molded plaques.

    Typical property values for mPact™ D143SA; not specification limits
    PropertyTypical ValueTest Method
    Nominal density0.918 g/cm³ASTM D1505
    Nominal melt index at 190 °C, 2.16 kg1.0 g/10 minASTM D1238 / ISO 1133-1
    Peak melting endotherm118–124 °CASTM D3418
    Comonomer1-hexeneManufacturer documentation
    Additive packageSlip/antiblockManufacturer documentation

    A 0.918 g/cm³ density is not interchangeable with higher-density octene mLLDPE grades in all flexible packaging structures

    Although D143SA sits at the lower end of the LLDPE density range, its density and comonomer type alone do not define performance in every laminate. Octene mLLDPE grades with similar melt index may provide higher dart impact and different tear balance at equivalent density, but D143SA is differentiated by its additive package and by its narrower processing window in high-stalk film. Substitution without revalidation of seal range, coefficient of friction, and blocking force can create converting failures on high-speed bag machines. The heat seal window must be re-established with ASTM F88/F88M data on the final laminate because the outer layers and adhesive in a laminate shift the apparent seal initiation temperature. Likewise, the printability and corona retention of the film are affected by the slip/antiblock package; surface treatment should be measured according to ASTM D2578 and sustained at a minimum level required by the ink system.

    In coextrusion, the narrow melt index distribution of D143SA permits a more uniform layer thickness at low gauge; however, the interfacial viscosity match with adjacent high-pressure LDPE or ethylene vinyl alcohol must be controlled to avoid interfacial instability. Layer-to-layer melt viscosity mismatch can produce wavy interfaces and optical defects. The resin is commonly placed in the core or sealant layer rather than the skin when surface gloss and slip must be controlled by the additive package. Coextrusion feedblock and die design should be reviewed when the D143SA layer exceeds 40% of total film thickness because the higher melt viscosity can alter the layer distribution.

    Frozen food packaging and heavy-duty ice bags require abuse resistance at sub-ambient temperatures. D143SA is used in these structures because metallocene-catalyzed ethylene-hexene copolymers retain ductility below −20 °C; puncture resistance and dart impact are evaluated after conditioning films for 48 h at the intended storage temperature. Failure modes observed on production lines include seal popping on overfilled bags, fold-lining along gusset edges, and film fracture at staple or tape closures. These defects are not solely resin-related; they arise from gauge distribution, seal bar contamination, and film tension control. The grade must be evaluated in the final package geometry rather than through flat-film tensile data alone. Tensile properties are measured by ASTM D882; elongation at break and secant modulus values are reported on the machine and transverse directions to detect orientation imbalance.

    Regulatory and compliance verification scope
    Regulatory ReferenceTypical Claim Boundary
    US FDA 21 CFR 177.1520(c) 3.2aOlefin copolymer for food contact; final packaging must be evaluated for additive migration and end-use temperature.
    EU Regulation 10/2011Plastic material and article compliance; overall migration limit 10 mg/dm² unless reduced by surface area-to-volume calculation.
    REACHNo substance of very high concern above 0.1 wt% per manufacturer safety data sheet.
    RoHSNot a typical packaging criterion; applicable only if the film enters electrical and electronic equipment articles.

    At film storage and handling, the slip/antiblock package can migrate to the surface over time. Blocking force and coefficient of friction should be rechecked after warehouse aging at 30 °C for 28 days or according to the intended shelf life before release to high-speed form-fill-seal equipment. Moisture is not a primary degradation pathway for polyolefins, but surface condensation on film rolls stored below dew point can interfere with sealing and surface treatment. Pre-drying is not normally required for D143SA if pellets are stored in closed containers and purged with dry air; however, bulk railcar unloading into outdoor silos should be evaluated for fines and condensation at high relative humidity above 60%. The operational boundary is therefore defined by additive bloom, surface treatment decay, and converting line speed rather than by resin hydrolysis.