| HS Code | 616851 |
| Density | 0.918 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Comonomer | Hexene-1 |
| Melting Point | 122 °C |
| Vicat Softening Point | 96 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 34.5 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 207 MPa |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Dart Drop Impact | 120 g |
| Haze | 10% |
| Gloss | 70% |
| Coefficient Of Friction | 0.2 |
As an accredited Chevron Phillips Marlex® Marlex® D173 Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex D173 is typically supplied in 55 lb (25 kg) polyethylene bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of Marlex D173 film-grade LLDPE hexene copolymer, shrink-wrapped; approx. 18–20 MT net. |
| Shipping | Chevron Phillips Marlex® D173 Film Grade LLDPE Hexene Copolymer is non-hazardous and typically ships as resin pellets in 25 kg polyethylene-lined bags, stretch-wrapped pallets, or bulk containers. Transport in clean, dry trucks, railcars, or containers at ambient temperature. Not regulated for transport; keep sealed, avoid moisture, UV, and contamination. |
| Storage | Store in a cool, dry, well-ventilated warehouse. Keep bags or containers closed, off the floor, and away from heat, sparks, open flames, direct sunlight, and strong oxidizers. Protect from moisture, dust, and contamination. Use first-in, first-out rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is typically two years when stored in original unopened packaging, cool, dry, away from direct sunlight and heat. |
Production-scale blown film lines producing heavy-duty sacks for form-fill-seal (FFS) filling of polyolefin pellets, granular fertilizers, and concentrated masterbatches incorporate Chevron Phillips Marlex® D173 at 15–35 wt% of the film structure, typically in HDPE-rich skins or cores. The hexene comonomer distribution produces a higher tie-chain density than equivalent butene LLDPE grades, shifting failure mode from brittle crack propagation to ductile puncture resistance under loaded drop. Verification follows ASTM D1709 Method B dart drop, ASTM D1922 Elmendorf tear, and ISO 6383-2 tear propagation, with minimum dart impact values for FFS sacks typically specified between 600 g and 1,200 g depending on fill mass. Dies of 1.2–2.0 mm gap and blow-up ratios of 2.0–3.2:1 are run at melt temperatures of 190–230°C on extruders with 25:1–30:1 L/D; grooved-feed sections and screen packs of 60–100 mesh are standard. Incoming D173 lots are checked by ISO 1133-1 at 190°C with 2.16 kg to confirm melt mass-flow rate before start-up. Bubble flutter and edge-weave are reduced by dry-blending D173 with high-pressure LDPE at 10–20 wt%, although field observations on lines exceeding 200 kg/h indicate that bubble stability degrades when ambient temperatures fall below 10°C unless melt-pressure-based air ring control is active. For hazardous-material sacking, UN Model Regulations Chapter 6.5 drop, stacking, and tear requirements are demonstrated through ISO 7965-1 vertical impact and ASTM D5276 drop tests. Terminal products include FFS sacks for resin plants, fertilizer bags containing ammonium phosphate, and packaging for carbon black masterbatch pallets.
For silage bale wrap, puncture and tear resistance during high-speed baling depend on the same tie-chain population that governs FFS performance, but the critical failure criterion shifts to oxygen transmission control under farm storage. D173 is typically let down at 70–85 wt% of the film layer, with 15–30 wt% of a butene or metallocene LLDPE and a UV stabilizer masterbatch metered by gravimetric dosing at 2–5 wt%. Hindered amine light stabilizers are compounded to active concentrations of 0.1–0.5 wt%; their retention after field weathering is evaluated by ISO 4892-3 artificial weathering and ASTM D3826 degradation endpoint, not by visual inspection. Blown film towers with 30:1 L/D barrier screws, rotating dies of 400–600 mm, and dual-lip air rings maintain bubble geometry, with frost line height held at 4–8 die diameters to preserve MD/TD tear balance. Oxygen transmission is measured by ASTM F2622 or ISO 15105-2; D173-rich webs at 25–38 µm thickness provide the required oxygen barrier through thickness rather than EVOH or PVOH layers. Tensile properties are tested according to ISO 527-3, and compliance with DIN EN 13206:2017 for agricultural covering films covers longitudinal and transverse tensile strength, tear propagation, and impact resistance. Terminal products include round bale silage wrap, square bale enveloping film, and silage pit cover films.
Greenhouse cover film operating in mid-latitude radiation environments imposes a different set of requirements than silage wrap; haze retention and diffuse light transmission are controlled by additive selection rather than resin density alone. D173 is compounded into three-layer greenhouse covers at 60–80 wt% of the core and 40–60 wt% of the skin layers, with UV and thermal stabilizer masterbatches fed at 5–10 wt% by weight of total film. The outer skin commonly contains 0.2–0.6 wt% hindered amine light stabilizer and a triazine or benzophenone UV absorber at 0.1–0.3 wt%, while the inner skin receives anti-fogging additives tested by EN 13206:2017 Annex C for condense spread. On blown film lines with 2.5–4.0:1 blow-up ratios and die gaps from 1.6 mm to 2.2 mm, melt temperature is held between 195°C and 215°C to limit additive degradation. Haze is measured according to ASTM D1003; tensile property retention after accelerated ageing is quantified by ISO 527-3 and ISO 4892-2 exposure of 1,000 h. Compliance with REACH Annex XVII restricts UV absorber migration; the film is not suitable for direct contact with agricultural chemicals containing highly concentrated sulfur or halogen compounds. Terminal products include multi-season greenhouse covers, low tunnel covers for early vegetable forcing, and side-roll polytunnel film.
Maintaining seal integrity at -20°C in frozen food vertical form-fill-seal lines depends on seal bar dwell time, jaw temperature, and sealant layer composition. D173 is incorporated as the sealant skin in three-layer coextrusions at 50–70 wt% of the sealant layer, with the remainder split between metallocene LLDPE and a low-seal-initiation LDPE. Slip and antiblock masterbatches are added at 2–5 wt%; erucamide slip migration is evaluated by coefficient of friction testing per ISO 8295 after 24–72 h of storage at 23°C. Heat seal strength is measured according to ASTM F88 with a 25 mm strip at 0.50 N/mm minimum peel strength for most frozen food converters; hot tack is assessed by ASTM F1921 Method A using a 500 g load. Published seal initiation temperature data for D173 specifically is limited; industrial LLDPE sealant webs typically initiate seals between 110°C and 135°C at 0.5 s dwell and 0.35 MPa jaw pressure. Compliance with food contact regulations is established under FDA 21 CFR 177.1520(c)(3.2) for olefin polymers and EU Regulation 10/2011; overall migration must not exceed 10 mg/dm² in aqueous, 10% ethanol, and 3% acetic acid simulants. Blown film towers with 1.8–2.4 mm die gaps, 2.0–2.8:1 blow-up ratios, and internal bubble cooling have reduced blocking in D173-rich sealant webs; melt temperatures above 230°C degrade the slip package and increase plate-out on stabilizer bars. Terminal products include VFFS pouches for frozen blueberries, IQF shrimp film bags, and coextruded films for ice cream novelties.
Cast stretch film lines operating above 400 m/min require melt-phase homogeneity and controlled crystallinity quenching; D173 is used in core and back layers at 30–50 wt% of total structure, with metallocene LLDPE at 45–65 wt% and polyisobutylene cling agent at 1–3 wt%. The hexene copolymer contributes to plastic deformation hysteresis without the film fibrillation seen in homopolymer-heavy blends. Puncture resistance is measured by ASTM D5748; cling force is quantified by ASTM D5458 after 24 h at 23°C and 50% RH. Cast film extrusion through 0.5–1.0 mm flex-lip dies onto chrome-plated chill rolls at 12–18°C produces webs of 8–15 µm for hand wrap and 15–30 µm for machine wrap. Draw ratios are set at 2.5:1 to 4.5:1; the air gap is held at 15–25 mm to control neck-in. Compliance is typically limited to ISO 9001 process control and REACH substance registration unless food contact is intended, in which case EU 10/2011 applies. Terminal products include pre-stretched hand film, machine stretch film for pallet unitization, and heavy-gauge stretch hoods for cold-chain logistics.
During adhesive lamination to aluminium foil or metallised PET, D173-rich sealant webs generate static charge that affects machinability; antistatic agent migration must be balanced against heat seal strength. The sealant layer is blown from a D173/LDPE blend at 60–80 wt% D173 and 20–40 wt% LDPE, with glycerol monostearate antistat at 0.5–1.5 wt% of the layer. Static decay is measured by IEC 61340-2-3; surface resistivity is evaluated at 23°C and 50% RH. The blown web, typically 20–50 µm, is adhesive-laminated to 12 µm PET or 18 µm aluminium foil using solventless polyurethane adhesives applied at 1.5–2.5 g/m²; lamination bond strength is measured by ASTM F904 or ASTM D1876. Compliance follows FDA 21 CFR 177.1395 for laminating adhesives and EU 10/2011 for the composite, with specific migration limits for aromatic amines from polyurethane systems verified by EN 13130-1. Processors on tandem laminators running 150–300 m/min have observed that antistat bloom beyond 1.5 wt% reduces heat seal strength below 4 N/15 mm; corona treatment to 38–42 mN/m dyne level is applied immediately before laminating. Terminal products include low-migration dry food pouches, metallised snack packaging, and tear-resistant lamination film for liquid stick packs.
Competitive Chevron Phillips Marlex® Marlex® D173 Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® D173 is a film-grade linear low density polyethylene resin produced by ethylene-1-hexene copolymerization. The nominal density is 0.917 g/cm³ when measured according to ASTM D1505, and the nominal melt index is 1.0 g/10 min when measured according to ASTM D1238 at 190 °C under 2.16 kg load. These two values position the grade within the LLDPE film segment where converters must balance bubble stability, downgauging, tear resistance, and optical clarity. The use of 1-hexene as the comonomer, rather than 1-butene, introduces C6 short-chain branches that alter crystallization kinetics and tie-chain concentration in the final film. Typical application areas for D173 include heavy-duty shipping sacks, industrial liners, agricultural films, and blends with low-density polyethylene. Nominal resin properties are not specifications; lot-specific physical-property data and certificate-of-analysis values should be obtained from the supplier before machine qualification.
At a constant density of 0.917 g/cm³, a hexene-copolymer LLDPE differs from a butene-copolymer LLDPE primarily in the length of the short-chain branch and its effect on the semicrystalline network. The C6 branch is more effective than a C4 butene branch at interrupting the linear ethylene sequences that form crystalline lamellae. This interruption reduces average lamellar thickness and increases the probability that a polymer chain will exit one lamella, traverse the amorphous region, and enter another lamella as a tie chain. The resulting tie-chain population is a major reason why hexene-based LLDPE grades of similar density and melt index are selected when enhanced dart impact and Elmendorf tear resistance are required. Because the difference is morphological, it is not directly visible in density or melt index data alone; a comparison based solely on ASTM D1505 and ASTM D1238 therefore cannot distinguish hexene LLDPE from butene LLDPE of the same nominal density and flow rate.
The mechanistic difference is observed most clearly in film toughness tests such as ASTM D1709-22 and ASTM D1922-23. Under ASTM D1709-22, a free-falling dart with a 38 mm hemispherical head is used to measure the impact failure energy of a clamped film specimen. In butene-copolymer LLDPE of comparable density, tensile failure can propagate along relatively weak interlamellar regions once a critical crack is initiated. The longer C6 branch in D173 is associated with a higher population of load-bearing tie chains, which increases the local strain required for crack propagation and shifts failure toward a more ductile response. Under ASTM D1922-23, Elmendorf tear testing uses a pendulum impact device and a pre-slit specimen; the measured tear energy per unit thickness reflects the energy consumed as the tear propagates through the oriented film. Hexene-copolymer LLDPE films typically show higher machine-direction and transverse-direction tear values than butene-copolymer films at the same gauge, although the magnitude depends on blow-up ratio, frost-line height, and melt orientation. Direct D173-versus-butene data for a specific film line should be generated by comparative testing because published data for this specific configuration is limited.
In blown-film processing, the final morphology of D173 is created during film fabrication rather than during pellet production. Melt temperature, die-gap geometry, draw-down ratio, and cooling rate determine the orientation and crystalline texture of the film. Increasing the frost-line height generally allows more crystal growth and can increase stiffness while lowering dart drop impact. Reducing melt temperature below 190 °C may raise die pressure and promote surface melt fracture, while operating above 230 °C can reduce melt strength and destabilize the bubble. Spiral mandrel dies with a diameter of 100 mm to 250 mm and die gaps from 1.5 mm to 2.5 mm are common for this product class. Narrow die gaps increase shear rate and die pressure, improving gauge control but potentially generating sharkskin if the melt stress at the die lip exceeds the critical shear stress of the linear polyethylene. A wider die gap reduces die pressure but requires a higher draw-down ratio to reach final gauge, shifting the balance between machine-direction and transverse-direction properties.
| Resin type | Branch architecture | Typical density | Typical melt index | Primary film toughness test |
|---|---|---|---|---|
| Marlex® D173 hexene LLDPE | C6 short-chain branches | 0.917 g/cm³ | 1.0 g/10 min | ASTM D1709-22, ASTM D1922-23 |
| Butene-copolymer LLDPE of equal density and melt index | C4 short-chain branches | 0.917 g/cm³ | 1.0 g/10 min | ASTM D1709-22, ASTM D1922-23 |
| High-pressure LDPE | Long-chain branches with short-chain branches | 0.918–0.925 g/cm³ | 0.2–2.0 g/10 min depending on grade | ASTM D1709-22, ASTM D882-22 |
| Metallocene LLDPE of similar density | Uniform C6 or C8 short-chain branches | 0.917 g/cm³ typical | 1.0 g/10 min depending on grade | ASTM D1709-22, ASTM F1921 |
A typical blown-film line processing D173 uses a grooved-feed extruder or a smooth-bore extruder with a barrier screw and a mixing section. A screw with an L/D ratio of 24:1 to 30:1 is generally selected for LLDPE because the resin’s relatively narrow molecular-weight distribution reduces shear heating during melting. Compression ratios of 2.5:1 to 3.5:1 are common for 1.0 g/10 min LLDPE film resins. Barrel set points are frequently reverse-profiled, with the feed zone set below 180 °C and the metering zone held between 190 °C and 210 °C. The die and adapter are often set from 200 °C to 220 °C to maintain bubble stiffness without excessive oxidation. A melt-pressure transducer and melt-temperature thermocouple should be installed in the adapter; if pressure before the screen changer exceeds the screen-pack rating, output should be trimmed or the screen pack replaced. Screen-pack configurations of 20/40/60/100 mesh are used in LLDPE film operations, but the final configuration depends on the level of recycled trim and the required back-pressure.
Bubble stability is governed by die geometry, air-ring performance, and frost-line height. If blow-up ratio is increased above 3.0:1, transverse-direction orientation increases and machine-direction tear strength may decline. If blow-up ratio is held below 2.0:1, bubble stiffness improves but transverse-direction tear may become limiting. Frost-line height is commonly maintained between 2 and 5 die diameters, depending on output and ambient humidity. A very low frost line quenches the melt rapidly and can increase surface haze, while a very high frost line can reduce dart impact by permitting excessive lamellar thickening. The appropriate line conditions for D173 must be established on the individual film line because air-ring design, die diameter, ambient air temperature, and cooling-air humidity interact with the crystallization kinetics of the hexene copolymer.
Substitution of D173 for a butene-copolymer LLDPE may not require a complete screw redesign, but the converter should expect changes in melt pressure, bubble geometry, and film mechanical response. Hexene-copolymer LLDPE can exhibit higher melt elasticity and different shear-thinning behavior than butene-copolymer LLDPE at the same melt index. The result may be a measurable shift in die pressure at constant screw speed. A die-pressure change greater than 10% at constant screw speed is an early indication that melt viscosity or feed-temperature conditions have changed, and it should be investigated before adjusting the line speed. Because D173 is designed for film applications requiring toughness, the largest improvements are usually observed in dart drop impact and Elmendorf tear, while gauge uniformity and output capability depend on the extrusion equipment. Converters should not assume that the same frost-line height and blow-up ratio used for a butene LLDPE will yield identical film properties; comparative trials should be run with the same die gap, target gauge, and haul-off speed.
Edge trim and scrap film from D173 can be recycled back into the film process. Trim that has been stored in high-relative-humidity conditions may require drying at 60 °C to 70 °C for at least 2 h before reintroduction. Trim levels above 20% can amplify die-lip streaking and reduce bubble stability if the recycled material is not melt filtered through a 60 mesh screen pack. Oxidative stability of LLDPE is sensitive to melt residence time at high temperature. At melt temperatures above 250 °C, oxidation of the polyethylene backbone can produce gel particles that appear as fish-eye defects. The supplier’s recommended melt-temperature limits should be followed. If a line uses an automatic screen changer, dead zones in the breaker plate can increase localized residence time and promote gel formation. Incoming-resin evaluation may include oxidation-induction time testing according to ASTM D3895, but published OIT data for D173 under this specific configuration is limited.
Compared with high-pressure LDPE, D173 contains no long-chain branching of the type produced in autoclave or tubular low-density polyethylene reactors. High-pressure LDPE typically has higher melt strength and better bubble stability at low melt temperatures, but lower dart impact and tensile strength at the same film gauge. D173 relies on short-chain branching and orientation-induced toughness rather than long-chain branching. Compared with metallocene-catalysed LLDPE of similar density, a conventional LLDPE such as D173 may show a broader short-chain branching distribution and a different heat-seal initiation temperature. The difference is relevant in packaging operations using vertical or horizontal form-fill-seal equipment. Hot-tack strength should be measured according to ASTM F1921-18, and seal strength should be measured according to ASTM F88/F88M-23, because heat-seal behavior cannot be predicted from the melting peak alone.
In blends with LDPE, D173 can increase dart impact and tear strength while retaining some of the processability benefits of long-chain branched LDPE. The optimum blend ratio depends on the melt-index mismatch between the two resins and on the intended film gauge. If the LDPE component has a much lower melt index, bubble stability may be dominated by the LDPE phase while the LLDPE phase contributes to toughness. The blend ratio must be confirmed by comparative film testing, and film properties should be reported with full test method descriptions, including specimen thickness and conditioning according to ASTM D618. Filled-sack performance for D173-based industrial liners is often evaluated by drop-impact testing of filled packages according to ASTM D5276-19 or ISO 7965-1:2013, because film-level dart drop impact alone does not capture seam failure or creep under load.
Food-contact use of D173 must be evaluated under the applicable regulatory framework. If the grade is used in food-packaging layers, the converter must verify that the supplier’s product stewardship documentation references 21 CFR 177.1520(c) for olefin polymers or the relevant EU plastics regulation. No direct food-contact claim should be based solely on resin type. For industrial packaging and heavy-duty liners, slow-speed puncture resistance can be evaluated according to ASTM D3763-22, and puncture propagation resistance can be evaluated according to ASTM D5748-19. Because D173 is a semicrystalline polyolefin, it is not inherently resistant to aromatic hydrocarbon solvents, strong oxidizing agents, or severe ultraviolet exposure without stabilizing additives. The product should not be blended with low-molecular-weight wax-based concentrates in high loadings because exudation can reduce seal strength and increase coefficient of friction. Published data for D173 in aggressive chemical packaging configurations is limited; end-use compatibility must be confirmed by actual package testing under the intended service conditions.