Chevron Phillips Marlex M358y3 Lldpe Pipe And Corrugated Extrusion Resin

Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin

    • Product Name: Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 584287
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.935 g/cm³
    Melt Index 190 C 2 16 Kg 0.25 g/10 min
    Tensile Strength At Yield 17 MPa (2400 psi)
    Tensile Strength At Break 27 MPa (3900 psi)
    Elongation At Break 700%
    Flexural Modulus 620 MPa (90,000 psi)
    Vicat Softening Temperature 115°C (239°F)
    Brittleness Temperature < -70°C (< -94°F)
    Environmental Stress Crack Resistance Escr > 1000 h
    Shore D Hardness 55
    Melting Point 125°C (257°F)
    Thermal Conductivity 0.33 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2 × 10^-4 /°C
    Specific Heat 2.3 J/g·°C
    Water Absorption < 0.01%
    Dielectric Strength 20 kV/mm
    Volume Resistivity > 1 × 10^15 ohm·cm

    As an accredited Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg (55.1 lb) polyethylene bags, 40 bags per pallet (1,000 kg), stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with 25-kg bags of Chevron Phillips Marlex M358Y3 LLDPE Pipe and Corrugated Extrusion Resin, palletized, stretch-wrapped.
    Shipping Chevron Phillips Marlex® M358Y3 LLDPE is typically shipped as free-flowing pellets in 25-kg moisture-barrier bags on pallets, stretch-wrapped, or in bulk trucks/railcars. Store in a cool, dry area away from direct sunlight. It is non-hazardous under normal transport regulations.
    Storage Store Chevron Phillips Marlex® M358Y3 LLDPE resin in a cool, dry, well-ventilated warehouse, away from heat, ignition sources, direct sunlight, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture and contamination. Stack pallets securely to avoid bag damage or collapse. Use first-in, first-out inventory. Avoid prolonged UV exposure; maintain normal ambient temperatures.
    Shelf Life No defined shelf life; typically stable under normal storage in cool, dry, ventilated areas away from heat, sunlight, and contaminants.
    Application of Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin

    Application Subsection: Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin

    Chevron Phillips Marlex® M358Y3 is positioned for non-pressure and low-pressure polyethylene pipe systems where slow crack growth resistance, flexural toughness, and stable corrugator output determine long-term service performance. The downstream scenarios below isolate six separate extrusion environments by compliance regime, formulation let-down ratio, production equipment configuration, and finished article geometry. Processing ranges assume pellet feedstock with a melt index of 0.35 g/10 min at 190°C/2.16 kg per ASTM D1238 and a density reported at 0.938 g/cm³ per ASTM D1505. Line data reflect production-scale single-screw extruders of 45–120 mm screw diameter and 28:1–36:1 L/D ratio unless otherwise stated.

    Formulation addition ratios and governing standard matrix for M358Y3 downstream applications
    ApplicationAddition ratioPrimary standardsProcessing constraint
    Agricultural single-wall drain97.0–98.0 wt% M358Y3, 2.0–2.5 wt% carbon black masterbatch, 0.5–1.0 wt% fluoropolymer processing aidASTM F405, ASTM F667, AASHTO M252Corrugator vacuum 16–22 kPa; melt temperature 218–232°C
    Highway edge drain inner wall60–80 wt% M358Y3, 20–40 wt% HDPE pipe resin, 2.0–2.5 wt% carbon black masterbatchAASHTO M294, ASTM F2306, ASTM F2648LLDPE inner layer not to exceed 65 wt% of total wall; corrugator vacuum below 18 kPa
    Drip irrigation lateral body95–98 wt% M358Y3, 2–3 wt% color concentrate, 0.5–1.5 wt% UV stabiliser masterbatch, 0.3–0.6 wt% slip/processing aidISO 9261, ISO 8779, ISO 13460Wall thickness tolerance ±0.05 mm; melt temperature 215–235°C
    Underground cable duct96.5–98.0 wt% M358Y3, 2.0–3.0 wt% carbon black masterbatch, 0.5–1.0 wt% non-halogenated flame retardant where acceptedUL 651A, ASTM D3485, NEMA TC 7, NFPA 70 Article 350Not validated for plenum-rated raceway; halogenated FR packages are excluded due to acid corrosion risk
    Landfill leachate collection pipe96.5–97.5 wt% M358Y3, 2.5–3.0 wt% carbon black/UV masterbatch, no calcium carbonate fillerASTM F2987, 40 CFR Part 258, ISO 13479Post-extrusion anneal 70–85°C for 2–3 h to reduce residual stress
    Livestock water replacement lateral96.0–98.0 wt% M358Y3, 2.0–3.0 wt% UV-stabilised carbon black masterbatch, 0.5–1.0 wt% processing aidASTM D2239, NSF/ANSI 14 optional potable contact45–65 mm single-screw extruder, melt temperature 210–225°C, coil winding 50–150 m

    On alluvial clay soils where the water table rises above drain invert for 30–60 days annually, M358Y3 is extruded into single-wall corrugated drain tubing with slotted perforations sized to exclude fine sand while maintaining inlet area under AASHTO M252 for highway underdrain laterals. The governing product specifications are ASTM F405 for corrugated polyethylene drainage tubing and ASTM F667 for larger-diameter corrugated pipe, with the resin selected because its strain-hardening response at low strain rates reduces the incidence of wall cracking when backfill settlement imposes bending loads after installation. On a typical agricultural drain line, virgin M358Y3 is metered at 97.0–98.0 wt% with a 40% carbon black LLDPE masterbatch at 2.0–2.5 wt%, yielding a compounded carbon black concentration of 0.8–1.0 wt% for outdoor UV resistance. A fluoropolymer processing aid masterbatch is added at 0.5–1.0 wt% when corrugator speeds exceed 12 m/min to suppress die-lip buildup and intermittent melt fracture in the 0.35 g/10 min melt index resin. The extrusion line uses a 60–90 mm grooved-feed single-screw extruder with a 33:1 L/D ratio, barrier screw, 20/40/60/80 mesh screen pack, and melt temperature 218–232°C. Vacuum-assisted corrugated forming is operated at a differential pressure of 16–22 kPa with internal air pressure maintained between 1.5–2.0 bar, allowing wall thickness to be held at 0.8–1.2 mm across pipe diameters from 75 mm to 300 mm. Finished product types include 100 mm, 150 mm, 200 mm, and 300 mm coiled single-wall drains, sock-wrapped sand-protection drains, and slit-perforated field laterals supplied in 10–30 m coils with snap-in fittings.

    Does Highway Edge Drain Demand a Higher Melt Strength Profile Than LLDPE Can Deliver?

    For dual-wall highway edge drain and storm water culverts, the local buckling resistance required by AASHTO M294 and ASTM F2306 for annular corrugated HDPE pipe typically exceeds the stiffness of an all-LLDPE wall, so M358Y3 is used as the inner corrugated wall layer in coextrusion with a high-density PE outer shell, or blended with HDPE at 20–40 wt% to raise the flexural modulus of the inner layer without sacrificing stress crack resistance. The inner-layer formulation is 60–80 wt% M358Y3, 20–40 wt% HDPE pipe resin, 2.0–2.5 wt% carbon black masterbatch if the inner layer is externally exposed, and 0.5–1.0 wt% antioxidant/photostabiliser masterbatch per ISO 1167 long-term hydrostatic testing protocols. Coextrusion is carried out on a 75–110 mm main extruder running M358Y3 at 220–235°C and a 45–60 mm coextruder running HDPE at 210–225°C, both feeding a corrugating die head with a die gap of 1.2–1.6 mm and lug depth control of 12–18 mm. The critical processing threshold is the melt strength differential between LLDPE and HDPE: if the inner LLDPE layer exceeds 65 wt% of total wall thickness, the corrugator vacuum must remain below 18 kPa and haul-off speed should not exceed 4.5 m/min, otherwise inner-wall fold-over and non-uniform wall thickness occur before the product reaches the water spray cooling station. Finished product types include 150–600 mm dual-wall perforated edge drain, 300–1500 mm storm water culverts, and coupling bands meeting ASTM F2648.

    Where subsurface drip irrigation laterals are installed under 0.5–1.5 bar pulsed pressure and exposed to chlorine-based water treatment, M358Y3 is processed into thin-wall cylindrical laterals and flat drip tape with an emitter bonding surface. Compliance for such products is defined by ISO 9261 for agricultural irrigation emitters and laterals, ISO 8779 for polyethylene pipes for irrigation laterals, and ISO 13460 for drip tapes, with chlorine resistance verified under accelerated immersion protocols such as ASTM D6284 or ISO 24454. The formulation addition ratio for the lateral body consists of 95–98 wt% M358Y3, 2–3 wt% white or black high-opacity color concentrate, 0.5–1.5 wt% UV stabiliser masterbatch in the outer skin, and 0.3–0.6 wt% slip or processing aid to maintain surface smoothness at the emitter bond line. Extrusion takes place on a 45–65 mm single-screw extruder with 30:1 L/D, melt temperature 215–235°C, and a spiral mandrel die drawing a wall thickness of 0.25–0.75 mm; inline vacuum calibration and laser micrometer thickness control maintain a dimensional tolerance of ±0.05 mm along the emitter insertion path. Terminal product types include 16 mm and 22 mm round drip laterals, flat emitter-integrated tapes with wall thickness 0.15–0.30 mm, and coextruded white-over-black lateral tubing for root-resistant buried installation.

    Cable Duct Outer Sheath Wall Thickness and Flame Compliance

    Underground LLDPE cable duct produced from M358Y3 is specified where pull force during cable installation and long-term earth load require ductile wall deformation without cracking. The applicable compliance framework includes UL 651A for Schedule 40 and Schedule 80 HDPE conduit, ASTM D3485 for smooth-wall coilable PE conduit, NEMA TC 7 for smooth-wall coilable electrical conduit, and NFPA 70 Article 350 for raceway installations where underground direct burial is permitted. The formulation is 96.5–98.0 wt% M358Y3, 2.0–3.0 wt% carbon black masterbatch for UV resistance, and 0.5–1.0 wt% non-halogenated flame retardant masterbatch only where the local specification accepts a non-plenum-rated duct; LLDPE itself is inherently combustible, and published data for M358Y3-specific plenum applications is limited. Extrusion runs on a 70–90 mm single-screw extruder with 30:1 L/D, melt temperature 215–230°C, vacuum sizing tank pressure of 0.08–0.12 MPa, and controlled haul-off to avoid sheath thinning below 1.5 mm. Finished product types include 25–100 mm coilable HDPE/LLDPE duct, pre-lubricated telecommunication duct, and color-coded low-voltage power raceway.

    Landfill Leachate Collection Lines and the 100-Year Stress Crack Window

    Under a cap or basal liner, leachate collection pipes remain under constant compressive stress and in contact with surfactant-bearing leachate, making slow crack growth the dominant failure mode. M358Y3 is specified for corrugated leachate collection pipe under ASTM F2987 for specification of polyethylene corrugated pipe for leachate collection, and under 40 CFR Part 258 for US EPA Subtitle D operational requirements. The formulation is 96.5–97.5 wt% M358Y3 with 2.5–3.0 wt% carbon black/UV masterbatch, and no calcium carbonate filler because filler reduces notched stress crack resistance under ISO 13479 notched pipe testing. Downstream processing uses a 75–100 mm grooved-barrel single-screw extruder at 205–225°C, with a pipe die and corrugator capable of 12–18 mm corrugation pitch; post-extrusion anneal at 70–85°C for 2–3 hours is applied on some lines to minimise residual hoop stress before slitting. Terminal product types include 100–300 mm corrugated leachate collection pipes, slotted, with perforation area 2,000–10,000 mm²/m and a smooth internal surface for cleaning access.

    When Livestock Water Line Replacement Prioritises Flexibility Over Pressure Rating

    For farm-to-barn water replacement lines that are pulled through irregular trenches, M358Y3 is formed into 32–63 mm flexible LLDPE pipe with a wall thickness of 2.0–3.0 mm under ASTM D2239 for controlled inside-diameter PE pipe and optional NSF/ANSI 14 potable contact compliance, using 96.0–98.0 wt% M358Y3 with 2.0–3.0 wt% UV-stabilised carbon black masterbatch and 0.5–1.0 wt% processing aid on a 45–65 mm single-screw extruder at 210–225°C, yielding 50–150 m coils and towing-compatible quick-coupler tails for stock-water laterals.

    Free Quote

    Competitive Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® M358Y3 is a linear low-density polyethylene resin formulated for pipe and corrugated extrusion. The product is characterized by a nominal density of 0.941 g/cm³ when tested in accordance with ASTM D1505 and a melt index of 0.35 g/10 min at 190 °C under a 2.16 kg load as determined by ASTM D1238. The low melt index reflects a high molecular-weight backbone that provides the melt tension and sag resistance required to maintain wall symmetry in corrugated profiles. In solid-wall pipe and profile applications, the same molecular architecture contributes to elevated elongation at break and low-temperature impact toughness relative to high-density pipe grades. The resin is supplied as natural pellets without a pre-compounded carbon black or ultraviolet stabilizer package; therefore, outdoor formulations require a controlled let-down of color concentrate or weathering masterbatch before final extrusion. Principal application areas include small- to medium-diameter agricultural drainage pipe, land-drain tubing, annular corrugated drainage pipe conforming to AASHTO M252 or AASHTO M294, and non-pressure conduit where flexibility and installation survivability are prioritized over the higher flexural modulus of PE 4710 high-density polyethylene.

    PropertyMethodNominal value
    DensityASTM D15050.941 g/cm³
    Melt indexASTM D1238, 190 °C/2.16 kg0.35 g/10 min
    Flexural modulusASTM D790760 MPa
    Tensile strength at yieldASTM D63819 MPa
    Elongation at breakASTM D638>800%
    Environmental stress-crack resistance, F50ASTM D1693, Condition B, 100% Igepal>1000 h
    Vicat softening temperatureASTM D1525122 °C
    Brittleness temperatureASTM D746< -75 °C

    The tabulated values are representative data from manufacturer documentation and are not intended as release limits or guaranteed specifications. The pipe-grade designation is evaluated under ASTM D3350, but the final cell classification depends on the weathering package, carbon black content, and property testing of the compounded pipe material rather than on the neat resin alone.

    How does the melt strength of M358Y3 control corrugated wall thickness uniformity?

    Corrugated extrusion imposes a periodic stretching and vacuum-forming step in which the molten tube is drawn into moving profile blocks. Melt strength governs whether the web remains intact during block closure and whether the corrugation valley and crest achieve consistent thickness without draw resonance or melt sag. The low melt index of 0.35 g/10 min for M358Y3 indicates a comparatively high melt viscosity that resists gravitational thinning between the die exit and the corrugator. This property is particularly relevant in small-diameter corrugated pipe where the unsupported melt length may be short but the forming cycle is rapid. A high-molecular-weight LLDPE of this type generally produces a stable melt balloon or parachute at typical corrugator haul-off speeds, provided the extruder head pressure and vacuum level are adjusted to the rheology of the grade. Capillary rheometry data generated according to ISO 11443 would be required to derive the complete viscosity curve; published data for this specific resin may be limited to standard melt index, density, and mechanical property values.

    On a corrugated pipe line equipped with a 75 mm single-screw extruder having a 30:1 L/D grooved-feed barrel, the barrel profile is typically set from 180 °C at the feed throat to 225 °C in the metering zone. The head adapter and die are maintained between 215 °C and 230 °C. Screen packs of 20/60/100 mesh with a breaker plate generate pre-die back pressures in the range of 15–25 MPa, depending on throughput, screen cleanliness, and melt temperature. In this regime, the resin permits stable operation on small-diameter corrugators without severe melt fracture, but corrugator block temperature must remain sufficiently above the polyethylene crystallization onset to avoid surface drag marks and fold-over at the block parting line. Vacuum forming levels at the blocks are normally held between 0.05 MPa and 0.08 MPa to fill corrugation valleys without excessive draw of the melt web.

    Density, comonomer distribution, and the stress-crack boundary versus conventional HDPE pipe grades

    Compared with high-density polyethylene pipe grades having density near 0.959 g/cm³, M358Y3 exhibits lower flexural modulus and a more ductile low-temperature response. The nominal density of 0.941 g/cm³ places the material near the upper end of the LLDPE density range, allowing sufficient stiffness for buried profile-wall pipe while avoiding the higher crystallinity that can reduce slow-crack-growth resistance in many HDPE homopolymers. The comonomer distribution and molecular-weight architecture also shift the failure mode under sustained localized stress from brittle slit propagation toward ductile deformation at moderate stress intensities. In comparison with high-melt-index LLDPE film resins, the 0.35 g/10 min melt index of M358Y3 provides measurably higher melt tension and sag resistance, but at the cost of higher specific energy consumption and reduced output per screw revolution in conventional smooth-bore extruders. Unlike bimodal PE 4710 high-density pipe resins, this grade is not typically supplied with a pre-certified hydrostatic design basis. In pressure pipe applications, long-term strength must be established by regression analysis according to ISO 9080 or ASTM D2837. Published data for this specific LLDPE resin in pressure-pipe configurations is limited, so direct substitution for PE 100 or PE 4710 materials without hydrostatic verification is not appropriate.

    Outdoor service requires carbon black or an alternative ultraviolet stabilizer. The neat resin is unpigmented; a carbon black masterbatch is typically let down at 2–3 wt% to achieve a finished-pipe carbon black content of 2.0–2.5 wt%. This addition level is selected to satisfy the weathering categories of ASTM D3350 for buried and exposed drainage applications. Dispersion of carbon black is assessed by ISO 18553 or ASTM D5596, with poor dispersion recognized as a source of pinholes, localized oxidative embrittlement, and reduced slow-crack-growth resistance during extended outdoor storage. Final pipe materials intended for potable water contact must be evaluated under NSF/ANSI 61; the neat resin does not by itself convey certification. Similarly, base-resin compliance with 21 CFR 177.1520 or food-contact legislation must be confirmed through the supplier’s lot-specific regulatory statement because converted article status depends on additives, regrind quality, and processing aids.

    If an existing PE 4710 pressure-pipe die is used, what modifications prevent excessive wall orientation?

    Because M358Y3 has lower melt viscosity and lower yield stress than high-density PE 4710, a die developed for 0.959 g/cm³ high-density resin may require changes to die land length and draw-down ratio when converted to this LLDPE grade. Lower melt strength can lead to excessive longitudinal orientation when haul-off speed is high relative to melt velocity; that orientation reduces environmental stress-crack resistance in the hoop direction and may cause pipe to split during installation. The die gap should be set to produce a draw-down ratio below 1.5:1, and the land length should be increased relative to the gap to allow melt relaxation before the forming step. If the corrugator uses differential pressure forming, vacuum may need to be increased or haul-off reduced to maintain female block fill while preventing melt fracture at the corrugation crest. Residual stress should be verified by measuring pipe longitudinal reversion according to ISO 2505 after 24 h at 110 °C. These modifications are not required for dedicated M358Y3 tooling, but they become necessary when converting older high-density polyethylene corrugation lines or pressure-pipe dies to this grade.

    Quality control for M358Y3 begins with incoming resin lot testing for melt index and density. A shift of melt index above 0.45 g/10 min or below 0.25 g/10 min may indicate polymer lot variation, regrind contamination, or cross-contamination with another polyolefin and should trigger a purging procedure before corrugator start-up. The resin is not hygroscopic, and pre-drying is generally unnecessary when the hopper and regrind system maintain internal relative humidity below 60%. During start-up, low screw speeds near 20–30 min⁻¹ are used to fill the die and forming blocks before ramping to target throughput, which reduces the probability of melt surging and fold-over at the corrugation valleys. Clean post-industrial corrugated pipe regrind can be blended at 20–30 wt% depending on final physical property requirements, provided the regrind is free of degraded material, moisture, and foreign polymer. Residence time above 240 °C should be kept below 5 min to limit thermal-oxidative degradation and loss of process stabilizer. When purging or shutdown is required, a low-melt-index polyolefin purge compound is preferred because high-melt-index purge resins may leave lower-viscosity residues that destabilize the corrugated wall at restart.

    Top