| HS Code | 856208 |
| Manufacturer | Chevron Phillips Chemical Company LP |
| Product Name | Marlex M248 LLDPE Carbon Black Concentrate |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Product Form | Pellets |
| Color | Black |
| Carrier Resin | LLDPE |
| Carbon Black Content | 40% |
| Melt Flow Rate 190 C 2 16 Kg | 20 g/10 min |
| Density | 1.12 g/cm³ |
| Bulk Density | 0.60 g/cm³ |
| Pellet Size | 2-3 mm |
| Moisture Content | <0.1% |
| Volatile Content | <0.5% |
| Recommended Let Down Ratio | 5% |
| Compatibility | Polyolefins |
| Processing Method | Melt blending/extrusion |
As an accredited Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg (55 lb) polyethylene-lined bags, 40 bags per 1,000 kg pallet; bulk packaging also available. |
| Container Loading (20′ FCL) | Container loading (20′ FCL) of Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate; 25 kg bags, palletized, shrink-wrapped, securely stowed. |
| Shipping | Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate typically ships as non-hazardous plastic pellets in sealed 25-kg bags, boxes, or octabins. It is not DOT/IMDG/IATA/ADR regulated. Keep containers closed, dry, and cool; avoid heat, moisture, ignition sources, and dust generation. Follow the SDS and local transport rules. |
| Storage | Store Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed, off the floor, and away from moisture, contaminants, and incompatible materials. Avoid excessive stacking and dust generation. Maintain ambient storage conditions and follow all local regulations and safety data sheet guidance. |
| Shelf Life | Marlex® M248 shelf life is typically indefinite when sealed in original packaging, cool, dry, away from sunlight and contamination. |
Blown film extrusion lines processing 25–75 mm grooved-feed extruders typically introduce Marlex® M248 as a 3.0–6.0 wt% let-down in an LLDPE base resin with 0.9–1.0 g/10 min melt flow rate when measured under ISO 1133-1:2022 condition 190 °C/2.16 kg. The target actual carbon black content in finished silage cover or mulch film is 1.8–2.5 wt%; the exact let-down must be corrected against the carbon black loading shown on the lot certificate of analysis because concentrate loading variations above ±1.5 wt% shift opacity, UV screening efficiency, and melt fracture threshold. The concentrate is tumble-mixed at 20–30 rpm for 10–15 min or metered by a loss-in-weight gravimetric feeder, then dispersed during film extrusion without a separate compounding pass. Melt temperature at the die is maintained at 195–215 °C, and a 1.6–2.2 mm die gap with a blow-up ratio of 2.5–3.0 suppresses bubble instability that can tear thin-gauge sections. Frost line height is controlled at 6–8 die diameters to stabilize the bubble below the crystalline orientation zone. Screen packs of 60/100/60 mesh are changed when backpressure exceeds 34.5 MPa on melt pressure transducers.
Finished agricultural film is converted into 25–60 μm opaque-black mulch, 120–180 μm silage cover, and 200–250 μm fumigation barrier film. UV resistance is assessed by tensile elongation retention after xenon-arc exposure under ISO 4892-2:2013, with acceptance typically set at ≥50% retained elongation after 2,000 h for multi-season film. Carbon black aggregate size must remain below 20 μm on pressed film inspected per ISO 18553:2002 to avoid pinholes during machine-direction orientation. Regulatory documentation for EU agricultural film requires a REACH compliance statement under 1907/2006 and, where silage film contacts animal feed, migration testing under EU 10/2011; for North America, FDA 21 CFR 177.1520 covers olefin polymers and may be included in lot-specific food-contact certification.
In LLDPE geomembrane production, carbon black dispersion governs weld seam ductility because undispersed carbon black agglomerates above 25 μm act as stress concentrators in the weld root when sheet is peeled at 23 °C under ASTM D6392. The LLDPE sheet specification GRI-GM17 requires carbon black content 2.0–3.0 wt% by ASTM D1603 and dispersion Category 1 or 2 by ASTM D5596. A concentrate with nominal carbon black loading in the 40–50 wt% range is let down at 5.0–7.0 wt% into LLDPE with a 0.5–1.0 g/10 min melt index, extruded through a 1.8–3.2 mm flat die onto chill rolls at 70–85 °C.
The process conflict arises during hot wedge or extrusion fillet welding. If actual carbon black content exceeds 3.5 wt%, the seam frequently transitions from ductile film-tearing bond to brittle weld delamination under ASTM D6392 peel and shear. If dispersion falls below Category 2, the weld gap becomes thermally unstable because carbon black agglomerates absorb infrared unevenly, producing local viscosity gradients at the 350–420 °C wedge-nip temperature. Weld trial parameters are recorded on dual-track hot wedge equipment with wedge speed 2.0–3.5 m/min, nip pressure 0.4–0.7 MPa, and air preheat 300–350 °C. Lot-specific validation includes ASTM D5596 compression-molded plaque inspection at 100× magnification and ASTM D792 density checks to detect filler concentration drift.
Operational boundary: if bagged concentrate is stored at ambient RH above 60%, it must be dried at 70–80 °C for 2 h in a desiccant hopper dryer before flat-die extrusion; steam bubbles from absorbed moisture generate localized dispersion faults that are not removed by the chill-roll polishing stack. Finished products include landfill basal liners, mining heap-leach pads, agricultural slurry lagoon liners, and secondary containment dikes. Published data for Marlex® M248 in GRI-GM17 LLDPE geomembrane formulations is limited to lot-specific plant validation; the above setpoints are operational starting points rather than product-specific guarantees.
During extrusion blow molding of 10–30 L multilayer agri-chemical jerrycans, 2.0–4.0 wt% of LLDPE-based carbon black concentrate is commonly metered into the outer layer of a three-layer coextrusion structure, yielding an outer-layer carbon black concentration of 1.0–1.8 wt%. The core layer is a post-consumer or in-plant regrind fraction at 20–30 wt%, and the inner layer remains unpigmented to reduce chemical interaction with ester solvents and emulsifiable concentrates. Carbon black concentrate is fed into the outer-layer extruder throat by gravimetric feeder; melt temperatures are held at 190–210 °C in the accumulator head machine, and the parison programmer is adjusted to thicken the top shoulder and bottom pinch-off by 12–18% relative to the sidewall to compensate for reduced melt strength at high regrind fractions.
Containers are tested for UN performance certification under 49 CFR 178.509 for hazardous materials. Drop impact at −18 °C from 1.2 m and hydraulic pressure testing at 100 kPa for 30 min are common acceptance criteria. Carbon black agglomerates larger than 30 μm in the outer skin can initiate environmental stress-cracking under ASTM D1693 when the surface is in contact with aromatic solvents. Batch-to-batch variance is controlled by checking outer-layer melt flow ratio before start-up and limiting regrind to 30% to avoid carbon black heat-history buildup that embrittles the pinch-off weld. Finished products include UN-marked 5–25 L jerrycans, induction-sealed dosing containers, and closed-loop dispensing systems.
| Downstream segment | Standard designation | Parameter or limit |
|---|---|---|
| Agricultural mulch/silage film | ISO 4892-2:2013, ISO 18553:2002, ASTM D882 | Elongation retention, aggregate size < 20 μm, tensile properties |
| LLDPE geomembrane | GRI-GM17, ASTM D1603, ASTM D5596, ASTM D6392 | Carbon black 2.0–3.0 wt%, dispersion Category 1–2, seam peel and shear |
| Blow molded chemical containers | 49 CFR 178.509, ASTM D1693, ASTM D256 | Drop impact, ESCR, impact strength |
| Drip irrigation micro-tubing | ISO 4427:2019, EN 12201-2, ISO 18553:2002, ASTM D1603 | Wall tolerance, carbon black content, dispersion |
| Cable sheathing | IEC 60502-1, ISO 4892-2:2013, RoHS 2011/65/EU | Jacket physicals, UV aging, heavy-metal limits |
| Rotomolded storage tanks | ASTM D1998, ASTM D256, FDA 21 CFR 177.1520 | Tank performance, impact, food-contact compliance |
When micro-irrigation tape wall thickness falls below 0.40 mm, carbon black plate-out at the die lip becomes a rate-limiting defect. Production lines commonly run 150–300 μm wall tape at 15–30 m/min using an LLDPE base resin of 0.8–1.0 g/10 min melt index let down with 5.0–7.0 wt% black concentrate. Actual carbon black concentration in the tape is maintained at 2.0–2.5 wt% and verified by ignition loss under ASTM D1603. The extruder is typically a 30:1 L/D single-screw machine with a gear pump, and melt temperature is held at 215–230 °C upstream of the gear pump; barrel zones are profiled from 160 °C feed to 220 °C metering to avoid premature carbon black agglomeration.
Screen packs are set to 100/200/100 mesh, and the melt pump is protected by a slide-plate screen changer with a 25 μm nominal filtration rating. Backpressure is limited to 20–25 MPa because higher shear heating can degrade the LLDPE carrier and generate carbon black domains that pass the screen but reagglomerate at the exit die land. The die land length is maintained at 12–18 mm to allow melt relaxation, and the outer air ring is set to 1.5–2.0 m/s air velocity. Die lip build-up produces machine-direction weld lines and wall-thickness variation exceeding ±0.02 mm when the carbon black dispersion rating exceeds 2 on ISO 18553:2002. Published data for Marlex® M248 at this exact thin-wall let-down in drip tape is limited; on-line capacitance wall-thickness scanning and ISO 4427:2019 documentation are required to validate the downstream lot before commercial release.
Finished drip tapes, micro-sprayer tubes, and pressure-compensating inline emitter tubing are produced with the carbon black dispersion requirement functioning as a mechanical leak barrier rather than a cosmetic specification. Agglomerates near the emitter weld point create channel leaks at 0.7–1.0 bar operating pressure. Compliance documentation for export markets includes ISO 4427:2019 for water transport, EN 12201-2 for dimension and pressure tolerance, and REACH 1907/2006 for EU import.
| Application | Let-down ratio | Melt temperature | Critical control point |
|---|---|---|---|
| Mulch/silage film | 3.0–6.0 wt% | 195–215 °C | Screen pack 60/100/60; blow-up ratio 2.5–3.0 |
| Geomembrane | 5.0–7.0 wt% | 204–227 °C | Chill roll 70–85 °C; ASTM D5596 Category 1–2 |
| Blow molded containers | 2.0–4.0 wt% | 190–210 °C | Parison shoulder 12–18%; regrind ≤ 30% |
| Drip irrigation tape | 5.0–7.0 wt% | 215–230 °C | Screen pack 100/200/100; die lip build-up |
| Cable sheathing | 4.0–6.0 wt% | 150–210 °C | Pre-dry 70–80 °C; spark test 3–10 kV |
| Rotomolded tanks | 0.5–1.5 wt% | 260–320 °C oven | Actual carbon black ≤ 0.75 wt%; internal air 180–200 °C |
In high-humidity cable sheathing operations, black concentrate with residual moisture is dry-blended into LLDPE at 4.0–6.0 wt% and extruded directly onto copper or aluminium conductors at 1.0–3.0 mm wall thickness. Steam pinholes form when the water vapor pressure exceeds melt strength at the die exit. The target actual carbon black level in the outer sheath is 2.0–2.6 wt% for UV stabilization of low-voltage distribution cable. Before processing, bagged concentrate stored at ambient RH above 60% is dried at 70–80 °C for 2–4 h in a desiccant-bed hopper dryer with dew point ≤ −30 °C. The sheathing line is usually a 24:1 L/D single-screw extruder with temperature zones from 150 °C feed to 210 °C head and a haul-off speed of 20–80 m/min depending on conductor diameter.
Moisture-induced voids reduce sheath integrity and create surface pinholes that fail spark testing at 3–10 kV depending on jacket thickness. The black concentrate is therefore metered by loss-in-weight feeder into the main resin stream, not pre-blended in bulk boxes that can condense moisture overnight. Carbon black dispersion is checked in a pressed sheath specimen under ISO 18553:2002; agglomerates above 20 μm are associated with screen pack pressure spikes. Use a 60/100/60 mesh screen pack and replace at 30–35 MPa differential pressure. Finished products include UV-resistant LLDPE cable jackets, optical fibre duct, and submersible pump drop cable. Compliance testing includes IEC 60502-1 for low-voltage cable sheath physicals, ISO 4892-2:2013 for accelerated UV aging, and RoHS 2011/65/EU for lead and cadmium.
For rotational molding of 2,000–10,000 L seamless storage tanks, 0.5–1.5 wt% carbon black concentrate is dry-blended into 35-mesh pulverized LLDPE, producing an actual carbon black level of 0.25–0.75 wt%. The lower concentration preserves low-temperature impact strength because carbon black above 1.0 wt% can shift the ductile-brittle transition and cause brittle failure in the tank sidewall when tested under ASTM D1998 and ASTM D256. Oven temperature is set to 260–320 °C with an internal air temperature ramp to 180–200 °C, followed by forced-air cooling to 70 °C before mold release. Dry-blending is preferred over compounded micropellets because it avoids a heat history that can increase concentrate carrier viscosity and reduce wall impact.
Carbon black dispersion in rotomolded parts is checked on a 40× microscope after a 1.0 mm microtome section is cut from the thinnest corner radius. The failure mode is not visible agglomerates but internal porosity when moisture remains in the concentrate after storage at RH above 65%; pre-drying at 60–75 °C for 1 h is applied before blending if the concentrate has been exposed. Finished products include rainwater harvesting tanks, agricultural sprayer tanks, and potable water storage vessels. Potable-water contact requires FDA 21 CFR 177.1520 or EU 10/2011 overall migration compliance, and export shipments typically require REACH 1907/2006 registration confirmation.
Competitive Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate is a pelletized carbon black concentrate dispersed in a linear low-density polyethylene carrier. The product is not a finished polyethylene molding or extrusion grade and is not intended for use at full strength. Its function is to be melt-compounded into a natural LLDPE, MDPE, or HDPE stream at a controlled letdown ratio. Published data for this specific configuration is limited; carbon black content, ash, density, melt flow rate, and moisture must be obtained from the lot certificate of analysis and the current technical data sheet. General statements in this document refer to LLDPE-based carbon black concentrates as a class and are not product specifications unless confirmed by the supplier.
Because carbon black is present in concentrated form, pellet attrition during handling can release black fines. The material should be conveyed with a dense-phase system or another low-attrition method, and the feed throat should be connected to suitable dust collection. Long dilute-phase pneumatic conveying distances should be minimized to prevent pellet fracture and carbon black segregation before the extruder.
Incoming lots should be screened for carbon black content by ASTM D1603, melt flow rate by ISO 1133-1:2022 at 190 °C/2.16 kg, density by ISO 1183-1, ash by ASTM D5630, and moisture by ISO 15512 or ASTM D6869. The carbon black content is the primary control because it sets the gravimetric letdown ratio. A sampling plan should include composite samples drawn from multiple packages within the lot, because carbon black distribution can vary and a single grab sample may not represent the supplied batch. The melt flow rate of the concentrate is expected to be lower than that of the uncut LLDPE carrier because carbon black increases viscosity; the exact value must be read from the lot certificate.
Ash analysis by ASTM D5630 reveals non-carbon inorganic residues that may affect screen pack life and die buildup. A high ash load can require finer melt filtration or more frequent screen changes. Moisture is reported in ppm because LLDPE carriers are not strongly hygroscopic, but condensation during storage or transport can introduce surface water. If storage has occurred at relative humidity above 60%, pre-drying of polyethylene pellets at 80 °C for 2–4 h is a general drying practice; M248-specific drying conditions should be taken from the supplier’s technical data sheet. Avoid exposure to open flame, prolonged heating above the maximum processing temperature, or direct high-intensity sunlight during storage.
| Property | Test method | Reporting basis | Process control function |
|---|---|---|---|
| Carbon black content | ASTM D1603 | wt% | Sets gravimetric letdown ratio for final carbon black window |
| Melt flow rate | ISO 1133-1:2022 | g/10 min | Indicates carrier fluidity and blend melt flow displacement |
| Density | ISO 1183-1 | g/cm³ | Checks carrier density for blend mass balance |
| Ash | ASTM D5630 | wt% | Detects inorganic residue beyond carbon black |
| Moisture | ISO 15512 or ASTM D6869 | ppm | Determines whether pre-drying is required |
In LLDPE film extrusion, a gravimetric feeder is placed above the main feed throat and is set to deliver the letdown mass based on the measured concentrate carbon black content. The letdown ratio is calculated as the target final carbon black weight percent divided by the concentrate carbon black weight percent, multiplied by 100 and expressed as weight percent of the total blend. For a target final carbon black content Cf and concentrate carbon black content Cc, the concentrate weight percentage is L = (Cf / Cc) × 100. If the concentrate contains 40 wt% carbon black and the final article requires 2.5 wt% carbon black, the letdown ratio is 6.25 wt%; if the concentrate contains 45 wt%, the letdown ratio is 5.56 wt%. These are arithmetic examples and do not define the M248 lot value. The diluted blend should be checked by ASTM D1603 before full production.
For film and geomembrane, carbon black dispersion is evaluated by ISO 18553 or ASTM D5596 on microtomed specimens. Equipment used for this dispersion duty typically includes a co-rotating twin-screw extruder with an L/D of at least 32:1, kneading and distributive mixing elements, vacuum venting, a melt pump, and a screen changer with 100–200 mesh breaker plates. At letdown ratios below 10 wt%, distributive mixing is often more important than dispersive mixing because the carrier is chemically similar to the natural resin. Process melt temperatures for LLDPE-based blends generally fall between 190 °C and 230 °C. Temperatures above 240 °C may cause localized polymer degradation, while temperatures below 180 °C may generate high melt pressure and poor concentrate dilution.
For pressure pipe compounds that rely on carbon black for ultraviolet stabilization, final carbon black content is commonly controlled within a window of 2.0 wt% to 3.0 wt% when measured by ASTM D1603. The applicable pipe standard may require additional dispersion assessment. Under ISO 18553, polyolefin pipe and fittings are inspected at defined magnification for undispersed pigment agglomerates, with count and size thresholds that vary by product class. A concentrate with poorly dispersed carbon black cannot be corrected solely by raising letdown ratio; it requires higher shear mixing, lower throughput, or screen pack adjustment. Carbon black content alone does not demonstrate dispersion. If the final product is subject to ASTM D3350, the cell classification is assigned only after carbon black content and dispersion are verified by the specified test methods.
Production-scale experience with LLDPE-based black concentrates shows that pellet breakup and carbon black dust generation are more likely when pellets are conveyed over long distances with dilute-phase pneumatic systems. Dense-phase conveying, minimal bends, and a cyclone filter can reduce fines. Volumetric dosing is not recommended when the final carbon black window is narrow; a gravimetric feeder with a short-term feed accuracy of at least ±0.5% of set rate is typical for these letdown operations. A 1.0 wt% concentrate loading error at a 6 wt% letdown changes final carbon black content by approximately 0.06 wt%, which can consume a meaningful portion of the allowed tolerance in ultraviolet-stabilized pipe classifications.
In a pressure pipe plant, the concentrate is metered into the main resin before compounding or extrusion. If the base resin is a natural polyethylene grade, the final carbon black content is determined by the letdown ratio. If the base resin is already a pre-compounded black polyethylene, adding M248 will increase carbon black content beyond the designed value and may move the material outside its classification. The processor must confirm whether the receiving resin is natural or already black. M248 should be let down only into natural or low-carbon black resins whose final formulation has been reviewed against the applicable product standard.
For pipe production, the extruder screw should provide sufficient distributive mixing without excessive shear heating. A grooved-feed single-screw extruder or a co-rotating twin-screw extruder may be used depending on whether the concentrate is compounded into a separate compound or diluted inline. The melt temperature should be monitored at the die adapter rather than only at the barrel thermocouples. Melt filtration through a screen pack with 100–200 mesh screens is common to retain agglomerates and foreign particles. Die pressure should be recorded continuously; an abrupt pressure rise may indicate screen blockage from carbon black agglomerates or inorganic ash.
If the final pipe is intended for outdoor storage or above-ground service, weathering classification may require carbon black content, dispersion, and minimum mechanical properties. The final compound may be tested under ISO 527-1 for tensile properties and under the designated weathering method, such as ISO 4892-2 or ASTM G154, depending on the product specification. Carbon black is not the only stabilizer system present in a formulated pipe compound; it does not automatically provide long-term weathering classification without the complete additive package.
Substitution of an LDPE-based concentrate with an LLDPE-based concentrate changes the carrier architecture and may alter blend rheology. The LLDPE carrier has a lower frequency of long-chain branching than LDPE and may respond differently under shear. Direct substitution should not be made without measuring melt flow rate by ISO 1133-1:2022 and, where a broader viscosity curve is required, capillary rheometry by ISO 11443. A fully compounded black resin differs from a concentrate because the carbon black is already dispersed at the resin supplier’s facility; the processor does not need to validate a letdown ratio or dispersion level to the same extent. A concentrate such as M248 allows the extruder to adjust carbon black concentration across multiple natural resins and product families but places responsibility for dispersion validation on the processor.
| Material form | Carbon black placement | Dispersion validation burden | Line flexibility | Processing requirement |
|---|---|---|---|---|
| LLDPE-based black concentrate | Concentrated in LLDPE carrier | High; lot and blend checks required | High; letdown can be varied | Gravimetric dosing and intensive distributive mixing |
| LDPE-based black concentrate | Concentrated in LDPE carrier | High; blend-specific | High; letdown can be varied | Shear compatibility must be checked in LLDPE-rich systems |
| Fully compounded black PE | Pre-dispersed at resin supplier | Lower; supplier certification applies | Low; carbon black content fixed | Direct extrusion |
| Carbon black powder | Free powder | Very high; dust and agglomerate control required | High in principle | Not recommended for standard polyethylene lines |
In geomembrane sheet extrusion, the concentrate is metered into the feed throat before the extruder. The molten blend passes through a screen changer and often a gear pump before the flat die. Because geomembranes are welded and exposed outdoors, carbon black content, dispersion, and oxidative induction time may be specified. Oxidative induction time is measured by ISO 11357-6 or ASTM D3895; carbon black can interact with antioxidant packages, so the final formulation and processing heat history must be evaluated. In soil burial or potable water service, the applicable product standard may require carbon black content and dispersion in addition to mechanical properties measured under ISO 527-1.
If M248 is used in electrical jacketing or electrostatic discharge applications, the final surface or volume resistivity must be measured under IEC 62631-3-2 or ASTM D257. The concentrate cannot be treated as a conductive grade unless the supplier confirms that its carbon black loading and dispersion can form a percolation network in the target matrix. Published data for this specific configuration is limited.
Regulatory status requires end-use verification. A polyethylene carrier and carbon black colorant may be used in food-contact articles only if the final formulation meets applicable requirements, such as 21 CFR 177.1520 for the polymer and 21 CFR 178.3297 for the colorant when applicable. RoHS Directive 2011/65/EU applies only to electrical and electronic equipment within scope; it does not automatically govern all pipe or film applications. REACH Article 33 communication obligations may apply to substances of very high concern present above the threshold; the concentrate supplier should provide regulatory information for the specific lot.