| HS Code | 182490 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.923 g/cm3 |
| Melt Index | 2.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 99 °C |
| Tensile Strength At Yield | 11.7 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 241 MPa |
| Hardness Shore D | 50 |
| Environmental Stress Crack Resistance | >1000 h |
| Brittleness Temperature | < -70 °C |
As an accredited Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® K203 LLDPE is supplied in 25 kg polyethylene-lined multiwall paper bags, 40 bags per pallet, shrink-wrapped. |
| Container Loading (20′ FCL) | Container loading: 20′ FCL loaded with Chevron Phillips Marlex® K203 LLDPE resin bags, palletized, stretch-wrapped, and secured for sheet extrusion shipment. |
| Shipping | Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion is shipped as solid resin pellets, typically in 25 kg moisture-barrier bags on stretch-wrapped pallets, or in bulk trucks/railcars. It is non-hazardous and not regulated for transport. Store cool and dry, away from sunlight, moisture, contamination, and ignition sources. |
| Storage | Store Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed, clean, and palletized off the floor. Protect from moisture, dust, oils, and other contaminants. Avoid prolonged high temperatures and UV exposure. Reseal unused material promptly. Do not stack excessively. Follow local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored in original packaging, cool, dry, and away from direct sunlight and moisture. |
On geomembrane production lines, Marlex® K203 is processed into smooth and textured sheet at nominal thicknesses between 0.75 mm and 3.0 mm using single-screw extruders with 30:1 L/D and barrier screws fitted with Maddock mixing sections. The melt temperature measured at the adapter is typically held within 220°C to 240°C; exceedance above 250°C accelerates gel formation and generates oxidized specks that are unacceptable under GRI-GM13 visual inspection. A 120 mm extruder running at 90 rpm with a 2,800 mm flex-lip die and a three-roll stack set at 70°C/85°C/70°C can sustain 800 kg/h to 1,100 kg/h when the screen pack is 20/40/60 mesh and back pressure remains between 180 bar and 240 bar. For textured sheet, the middle polishing roll is engraved and maintained at 80°C to 85°C to preserve embossment depth after the sheet exits the nip. A 40% carbon black masterbatch in an LLDPE carrier is let down at 2.5 wt% to 3.0 wt%, yielding 1.0% to 1.2% carbon black content in the finished sheet; lower addition rates fail the puncture requirement under ASTM D4833 after 1,000 h of xenon-arc exposure, while loadings above 3.5 wt% increase melt viscosity enough to disturb gauge uniformity at the die lips. Seaming by hot-wedge welding requires a weld zone temperature of 400°C to 430°C and a travel speed of 1.2 m/min to 1.8 m/min for 2.0 mm sheet; peel adhesion tested per ASTM D6392 must exceed 80% of sheet yield strength. Compliance is anchored to GRI-GM13 for HDPE/LLDPE geomembranes, ASTM D5199 for nominal thickness, ASTM D1004 for tear resistance, ASTM D4833 for puncture, and ASTM D5397 for notched constant tensile load stress-crack resistance. Terminal components are containment liners, heap-leach pads, and floating covers for anaerobic digesters and reservoirs.
| Property | Test method | Sampling frequency |
|---|---|---|
| Nominal thickness | ASTM D5199 | 1 per roll |
| Tear resistance | ASTM D1004 | 1 per 5,000 m² |
| Puncture resistance | ASTM D4833 | 1 per 5,000 m² |
| Stress-crack resistance | ASTM D5397 | Quarterly per formulation |
| Carbon black content | ASTM D4218 | 1 per shift |
| Melt flow rate | ASTM D1238 at 190°C/2.16 kg (or ISO 1133-1:2022) | 1 per silo |
Deep-draw thermoforming of extruded K203 sheet for automotive cargo trays and load-floor panels is governed by low melt strength relative to fractional-melt HDPE. Sheet blanks of 4.0 mm to 6.0 mm thickness are clamped in a shuttle thermoformer and heated by ceramic or quartz IR elements until the surface temperature reaches 132°C to 148°C. Below 128°C the sheet exhibits excessive elastic recovery and corner tearing; above 155°C sag exceeds 25 mm across a 1,200 mm clamp frame, causing wall thinning beyond 40% in the deepest draw areas. Plug assist is mandatory for draw ratios exceeding 1:1, with syntactic foam or POM plugs preheated to 90°C to 110°C to prevent chill marks. The forming mold is maintained at 30°C to 50°C; higher mold temperatures improve surface replication but extend cycle time beyond 90 s for 6.0 mm sheet. Post-trimming tensile properties are evaluated per ASTM D638 Type IV specimens cut from the thinnest wall section; elongation at break below 400% indicates excessive thermo-oxidative degradation or draw-induced orientation. Formulation adjustments include the addition of 0.5 wt% to 1.0 wt% of a fluoropolymer processing aid to reduce die-lip build-up and a 2.0 wt% UV stabilizer masterbatch for interior cargo applications. Finished parts include trunk tubs, wheel-well liners, and rear load-floor covers with carpet lamination. Compliance for automotive interior materials normally invokes VDA 275 for formaldehyde release and OEM flammability standards such as FMVSS 302; K203 is not flame-retardant, so any application requiring UL 94 V-0 is outside the stated use envelope.
When K203 replaces a fractional-melt HDPE in secondary containment and spill-pallet fabrication, the sheet is extruded at 5.0 mm to 12.0 mm thickness and then cut, butt-fused, or extrusion-welded into sump liners and spill decks. The lower flexural modulus of LLDPE relative to HDPE permits the formed sump to conform to uneven substrates without stress whitening, but it also reduces the load-bearing capacity of unsupported spans. For a 10 mm sheet, a 500 mm unsupported span under 1,000 kg/m² service load requires reinforcement ribs or steel backing to keep deflection below 6 mm. Extrusion welding with a 4 mm round or triangular welding rod uses a hot-air gun set at 300°C to 340°C, with a welding speed of 0.2 m/min to 0.4 m/min and parameters aligned with DVS 2207-4; weld factor per DVS 2203-4 must exceed 0.8 for chemical storage applications. Formulation for chemical containment typically includes 2.0 wt% to 2.5 wt% carbon black masterbatch and, when oxidizing acids are present, no metal stearate slip additives, because copper-based or cobalt-based catalyst residues can accelerate oxidative degradation. The terminal products are secondary containment pallets, tank base liners, and cut-to-size sump sheets used in battery charging rooms and agrochemical storage. Compliance is specified by EPA 40 CFR 264.175 for secondary containment, ASTM D1998 for polyethylene tanks, and ASTM D638 Type IV for weld tensile strength.
Extruded sheet in the 0.2 mm to 0.5 mm range from K203 is deployed as a vapor barrier and radon retarder beneath concrete slabs, where tensile and puncture properties must survive construction traffic before the pour. Lines for this thin-sheet application use a 90 mm extruder with a 30:1 L/D barrier screw, an automatic screen changer with 40/60/80 mesh packs, and a three-roll vertical stack with roll temperatures of 60°C to 75°C. Gauge control at 0.3 mm requires either a gravimetric hopper system or an X-ray thickness scanner because melt-pressure variation of ±5 bar can shift thickness by ±4%. The sheet is typically supplied in 3 m to 6 m wide rolls and installed with 150 mm overlaps that are taped or sealed to block radon and moisture. Formulation requires no migratory slip agents if the underside will be bonded; where peelable protective film is laminated, a 0.1 wt% erucamide or oleamide slip package may be added, but this reduces the coefficient of friction to below 0.3 and can compromise worker footing on sloped roofs if used in above-grade vapor-barrier service. Compliance for underslab vapor barriers is defined by ASTM E1745 Class A, B, or C, which sets minimum tensile strength, puncture resistance, and water-vapor permeance; typical LLDPE sheet at 0.3 mm exhibits water-vapor permeance below 0.1 perm per ASTM E96 Procedure B. For radon applications, ASTM E2121 governs installation practices in the United States. Operational boundary: installation below 5°C is not recommended because sheet stiffness increases and seam tape adhesion falls below the 0.2 N/mm peel threshold.
K203 can function as the skin or cap layer in coextruded barrier sheet where the core contains EVOH or polyamide and the tie layer is maleic anhydride-grafted polyethylene, provided the resin is supplied with a food-contact compliance declaration. A typical structure for thermoformed food trays is K203 / tie / EVOH / tie / K203 with layer distribution 35% / 5% / 20% / 5% / 35%. The outer K203 layers provide sealability and moisture protection, while the EVOH core contributes oxygen transmission below 0.5 cm³·mm/(m²·day·atm) at 23°C and 50% RH when dried. Coextrusion feedblocks or multi-manifold dies must maintain the K203 melt stream at 220°C to 232°C; excursions above 245°C generate acetic acid odor from EVOH degradation and can reduce interlayer adhesion below 4 N/15 mm when tested by ASTM F904. For food-contact compliance, the K203 layer must be covered by a manufacturer’s declaration under 21 CFR 177.1520(c) and, for the European Union, EU Regulation 10/2011 with overall migration limit below 10 mg/dm². The addition of regrind is limited to 20 wt% in the outer layers and must not be used in direct food-contact surfaces unless the regrind is generated from the same food-compliant structure. Thermoforming of the coextruded sheet requires equilibrium moisture content below 0.1% for EVOH; pre-drying at 80°C for 4 h is mandatory if the sheet has been stored at relative humidity above 60%. Terminal products include refrigerated dairy trays, fresh meat trays, and microwaveable lidding bases where the peelable seal is applied to the K203 cap layer. When the same coextruded sheet is converted into reusable electronics component trays, EU 2011/65/EU RoHS and EC 1907/2006 REACH SVHC declarations are required; the K203 layer does not contain restricted phthalates, lead, cadmium, mercury, or hexavalent chromium above the 0.1 wt% homogeneous-material threshold.
For silo, chute, and hopper liner service in bulk solids handling, K203 sheet at 6.0 mm to 10.0 mm thickness is bolted or welded to the interior surfaces of carbon-steel vessels to reduce wall friction and prevent rat-holing in powders and sticky ores. The lower crystallinity and higher ESCR of LLDPE relative to HDPE provide better resistance to abrasive wear from angular particles and to stress cracking at fastener holes. Liners are normally cut from extruded sheet and fastened with countersunk bolts; the bolt holes are spaced at 300 mm to 450 mm centers and gasketed with EPDM washers to isolate the steel from the process material. Installation requires pre-curving the sheet to the vessel radius; at ambient temperatures below 10°C, bending radii below 8 times sheet thickness can induce stress whitening. A formulation with 0.5 wt% of a high-molecular-weight silicone masterbatch lowers the dynamic coefficient of friction to 0.15–0.20 against dry limestone, measured per ASTM D1894 using a 100 mm/min sled speed. Compliance for mining use frequently references MSHA 30 CFR Part 18 for flame resistance if the liner is used in underground coal conveyance; K203 without flame-retardant modification does not meet that requirement and is restricted to surface operations. Terminal components are feeder hopper liners, truck-bed liners, railcar hopper liners, and chain-conveyor trough liners. Published data for the coefficient of friction of K203 against specific mineral ores is limited; laboratory tests on representative bulk materials are required before specifying liner thickness and fastening layout.
Competitive Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical’s Marlex® K203 linear low density polyethylene (LLDPE) sheet extrusion resin is designated for flat-sheet production and downstream thermoforming operations in which a nominal density of 0.920 g/cm³ (ASTM D1505) and a nominal melt index of 2.0 g/10 min (ASTM D1238, 190 °C/2.16 kg) are used to balance melt strength, drawdown, and low-temperature ductility. The resin is supplied as stabilized pellets, and the nominal values are material-selection data rather than lot release specifications; the lot certificate of analysis governs each shipment. In sheet extrusion, K203 is typically processed into heavy-gauge industrial sheet, dunnage, agricultural sheet, and thermoformed parts that require a broader impact-tolerance window than high-density polyethylene but greater stiffness than high-pressure low-density polyethylene. The linear backbone of LLDPE introduces a different shear response, melt-fracture sensitivity, and neck-in behavior than branched low-density polyethylene; these differences must be accommodated in die design, temperature profiling, and cooling-roll setup rather than treated as direct substitutions.
The designation “K203 LLDPE Sheet Extrusion” identifies the product by target process rather than by additive package. A 2.0 g/10 min melt index is low enough to provide rupture resistance in heavy-gauge sheet, yet high enough to fill the die at moderate head pressure. The 0.920 g/cm³ density class is below the typical 0.940 g/cm³ threshold that defines high-density polyethylene; it yields lower crystallinity and therefore lower modulus but greater ductility. In sheet form, the lower crystallinity also reduces the sharp yield point that can cause stress whitening during die cutting. Because density and melt index are inversely related through comonomer content, each lot will vary within supplier control limits; a lot at the low-density end of the band may exhibit lower chill-roll plate-out but also lower stiffness, while a lot at the high-density end may show improved drawdown but increased warpage. These trade-offs are measurable only through lot-specific density and melt-index data, not through product name.
Transitioning from a previous polyolefin campaign to K203 requires attention to purging because the lower density and higher comonomer content can leave an intermediate layer that is not visible on the sheet surface. A purging resin with a melt index below 1.0 g/10 min or a commercial polyethylene purge compound is used until the melt-pressure signal at the breaker plate stabilizes. The hopper, feed throat, and screw should be free of HDPE pellets because high-density residues can survive in the boundary layer and appear as unmelted translucent domains in thin sheet. Lot-to-lot transitions should be segregated by silo and dated, because density drift of 0.002 g/cm³ is sufficient to alter sag resistance in a thermoforming oven even when the melt index remains within specification.
On single-screw sheet lines with 24:1 to 30:1 L/D barrier screws and Maddock mixing sections, the most common process deviation is uneven melt-temperature distribution at the adapter. A temperature spread greater than approximately 5 °C across the melt stream can produce transverse gauge bands because local viscosity differences alter die flow. Sheet processors typically install melt pumps between the extruder and flat die to reduce screw-induced surging; suction pressure is commonly held between 3.4 MPa and 10.3 MPa, while discharge pressure depends on die restriction. Melt-temperature ranges for LLDPE sheet grades in the 2.0 g/10 min melt-index class are usually held between 221 °C and 246 °C. The lower bound is set by backpressure and incomplete homogeneity; the upper bound is set by gel formation and loss of melt strength. Flat dies used for this product class are normally equipped with a restrictor bar and flex lip; die gap settings from 0.8 mm to 1.5 mm are used for sheet thicknesses between 0.3 mm and 6.0 mm. Chrome-plated chill rolls with closed-loop water temperature control are required for consistent surface replication. The first chill roll is commonly set in the range of 21 °C to 38 °C, depending on sheet thickness and line speed.
Barrel temperature profiles should not be copied from an HDPE sheet campaign. In the feed zone, a lower temperature of 100 °C to 130 °C is sufficient to melt the surface of the pellets while avoiding premature melting in the feed throat. In the compression zone, temperatures rise progressively to the metering zone at 190 °C to 220 °C, and the adapter and die are usually set at 220 °C to 240 °C. The exact set points depend on extruder diameter, screw design, and output rate. On a 90 mm single-screw extruder with 30:1 L/D, LLDPE sheet of 1.2 mm gauge can be run at outputs that place the screw speed between 40 rpm and 80 rpm, but these figures are equipment-specific and should be confirmed by screw-performance data.
Because linear low-density polyethylene has a narrower distribution of long-chain branching than high-pressure LDPE, the onset of sharkskin and stick-slip melt fracture can occur at lower apparent shear stress. For LLDPE extruded through a flat die, the critical wall shear stress for visible sharkskin is frequently reported near 0.1 MPa to 0.3 MPa; the exact value depends on die metallurgy, temperature, and molecular weight distribution. Die-lip build-up is accelerated by low-molecular-weight species, oxidized surface material, and excessive die-gap residence time. The use of a polymer processing aid at 200 ppm to 500 ppm is a common remediation, but the additive must be dispersed uniformly in the melt stream by the mixing section; otherwise, pressure fluctuations remain. Backpressure should be measured at the breaker plate and logged against screw speed. A rising backpressure at constant screw speed, exceeding approximately 10 % of baseline, indicates screen-pack plugging or die-lip accumulation. Filtration packs in the range of 60/100/60 mesh are standard for sheet lines running LLDPE; coarser packs reduce pressure but do not remove gels and oxidized droplets from regrind streams.
Regrind incorporation alters the shear response of K203 sheet. Because the resin is stabilized for extrusion, up to 20 % of clean in-house regrind is commonly tolerated without loss of melt integrity, but the regrind must be sourced from sheet produced under the same thermal history; thermoformed scrap that has undergone multiple heat cycles may contain carbonyl groups that accelerate die-lip oxidation and lower the onset of discoloration. A gravimetric blender with better than 0.5 % dosing accuracy is preferred when regrind ratio is varied, because uneven regrind distribution appears as flow lines and gloss variation. The moisture content of the feedstock should remain below 0.02 %; although LLDPE is not hygroscopic in the manner of polyamide or PET, surface condensation on cold pellets stored outdoors or in unheated silos can generate steam bubbles at sheet thicknesses above 2.0 mm.
If the first chill roll is set below the crystallization onset temperature of LLDPE of this density, the sheet surface quenches rapidly while the core continues to crystallize more slowly. The result is a through-thickness morphology gradient, which can appear as curl, warpage, and frozen-in stress in thermoformed parts. For LLDPE in the 0.918 g/cm³ to 0.922 g/cm³ density band, crystallization onset measured by differential scanning calorimetry under cooling rates of 10 °C/min per ASTM D3418 is typically below 105 °C; therefore, the typical chill-roll range of 21 °C to 38 °C already imposes a large thermal gradient in thick sheet. When sheet thickness exceeds 2.5 mm, processors should use higher chill-roll temperatures, lower line speed, or multistage cooling to reduce warpage. Air-knife velocity should be adjustable between 2 m/s and 10 m/s; excessive air velocity can produce surface haze and uneven chill-roll contact. Thermoformed K203 parts exhibit stress whitening if the sheet was overquenched; this failure mode can be detected by incremental forming-temperature trials and by instrumented puncture testing according to ASTM D3763 or tensile impact testing according to ASTM D1822.
The molecular architecture of K203 also affects drawdown and neck-in. Sheet extrusion lines designed for high-pressure LDPE often use a die width calculated for a specific neck-in allowance. With LLDPE of 2.0 g/10 min melt index, neck-in can be greater than with a branched LDPE of the same melt index, depending on die-land length and melt temperature. To maintain edge trim within 25 mm per side, processors typically raise the die lip temperature by 5 °C to 10 °C relative to the center, reduce the die gap to sheet thickness ratio below 1.2:1, or increase the land length to reduce die-end stagnation. These adjustments are not defects of the resin but consequences of reduced melt elasticity. A lower-shear melt elasticity difference can be observed as lower die swell and reduced sag resistance in thermoforming; therefore, ovens should be profiled with lower top-heat intensity than an HDPE sheet of equivalent gauge.
Thermoforming K203 sheet is commonly performed in double-sided infrared ovens with sheet-surface temperatures in the range of 132 °C to 150 °C, measured with a contact pyrometer; the forming window is narrower than HDPE because lower crystallinity produces a sharper sag transition. Plug-assisted forming with heated plugs at 80 °C to 110 °C reduces webbing and thin-out. Mold temperature should be held below 60 °C to prevent premature release and part distortion. For deep-draw parts, sheet pre-stretch of 30 % to 60 % is used; above this range, local thinning in corner regions can reduce burst strength below the value predicted by the base resin.
The operational boundary between K203 and high-pressure LDPE is clearest in melt strength and melt-fracture sensitivity. High-pressure LDPE carries long-chain branching that imparts strain-hardening and allows thin edges to hold shape; K203, as an LLDPE, has a more linear backbone and relies on molecular weight and short-chain branching for melt strength. On lines without melt pumps, this difference can appear as gauge oscillation when the screw speed is changed. At the same mass output, K203 can require 10 °C to 20 °C higher barrel temperatures in the metering zone to reach target melt temperature, because the viscosity of LLDPE remains higher at low shear rates. The flat die should be inspected for chrome roughness below 0.1 µm Ra; rough die lips increase sharkskin and die-lip build-up. Edge pinning, air knife angle, and vacuum box settings must be re-tuned because LLDPE has a narrower adhesion window to the chill roll than oxidized LDPE.
Compared with high-density polyethylene sheet grades of comparable melt index, K203 at 0.920 g/cm³ density has lower flexural modulus and lower Vicat softening temperature, but better low-temperature impact and environmental stress-crack resistance in many sheet applications. This trade-off is relevant in dunnage and agricultural sheet, where impact at -20 °C to 0 °C may be more important than top-load rigidity. For applications requiring continuous service above approximately 60 °C under load, HDPE or a higher-density LLDPE should be evaluated, because creep resistance of a lower-density grade is reduced. Conversely, when high-pressure LDPE sheet provides insufficient puncture resistance or tear propagation resistance, K203 may be selected if the line is configured for higher backpressure and greater neck-in control. Environmental stress-crack resistance comparisons should be based on ASTM D1693 condition B, not on Izod impact values alone, because the failure mechanism in detergent or surfactant contact is slow crack growth.
When compared with metallocene-catalyzed LLDPE sheet grades, K203 may exhibit broader short-chain branching distribution and less extreme clarity. Metallocene grades often provide lower extractables and better organoleptic properties, but they can require narrower processing temperatures and may be more sensitive to screw-speed changes. If downstream use requires a Declaration of Compliance for low migration in fatty-food contact, the choice between K203 and a metallocene alternative should be based on extraction tests conducted according to Regulation (EU) No 10/2011 and on measured hexane extractables where applicable under FDA 21 CFR 177.1520 methodology.
Food-contact suitability is not established merely by the polyolefin designation. The converter must obtain a supplier letter of assurance that references FDA 21 CFR 177.1520 for food-contact olefin polymers and any applicable European migration limits under Regulation (EU) No 10/2011. The base resin may meet the compositional requirements of the regulation, but the final sheet must be tested under the migration conditions of the intended food type and temperature. For medical or sterilization uses, K203 should not be assumed to be gamma-stable unless the supplier has qualified the specific formulation; oxidative degradation under sterilizing radiation can shift melt flow and embrittle the web. Storage at relative humidity above 60 % may require hopper drying at 60 °C to 70 °C for 2 h to 4 h, particularly when the resin is transferred from cold outdoor silos into a warm production building. The resin should not be processed at melt temperatures above 260 °C for extended periods, because thermal degradation can form oxidized gels that deposit on the die lip and produce pinholes in thermoformed parts.