Chevron Phillips Marlex Hhm Tr 232 Polyethylene Enhanced

Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced

    • Product Name: Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 264075
    Productname Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced
    Chemicalfamily Polyethylene
    Polymertype High Density Polyethylene (HDPE)
    Density 0.952 g/cm³
    Meltindex 0.10 g/10 min (190°C/21.6 kg)
    Meltingpoint 130 °C (266 °F)
    Tensilestrengthatyield 28 MPa (4,000 psi)
    Tensilestrengthatbreak 34 MPa (5,000 psi)
    Elongationatbreak >600%
    Flexuralmodulus 1,380 MPa (200,000 psi)
    Environmentalstresscrackresistance >1,000 hours (10% Igepal CO-630, F50)
    Vicatsofteningpoint 127 °C (260 °F)
    Hardnessshored 65
    Brittlenesstemperature < -70 °C (< -94 °F)

    As an accredited Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced is supplied in 25 kg polyethylene-lined bags, palletized, and 1,000 kg bulk bags.
    Container Loading (20′ FCL) Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced loaded in 20′ FCL dry container, palletized bags, secured for ocean freight, maximum payload.
    Shipping Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced is a non-hazardous polyethylene resin. It typically ships in 25 kg bags, bulk bags, or bulk trucks/railcars, palletized and secured. No UN number, hazard class, or special transport labels required. Keep dry, cool, and away from ignition sources.
    Storage Store Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Store on pallets, off the floor, and avoid dust generation or static discharge. Do not store near strong oxidizers. Follow the manufacturer’s SDS and local regulations.
    Shelf Life No specific shelf life; stable under normal storage conditions. Store cool, dry, well-ventilated, away from heat, sunlight, and ignition sources.
    Application of Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced

    Multilayer Automotive Fuel Systems Under SAE J1737 Permeation Limits

    Six-layer coextrusion blow molding of automotive fuel systems uses Chevron Phillips Marlex® HHM TR-232 primarily in outermost and innermost HDPE layers, where the resin’s high-molecular-weight distribution sustains parison wall integrity during mold close. The layer sequence outer HDPE / regrind / tie / EVOH / tie / inner HDPE runs on lines with 120 mm extruders and 25 kg accumulator heads, with total parison length above 2,200 mm on large-tank machines. HDPE-layer melt temperature is held at 210–230°C, die gap at 2.5–4.0 mm, blow pressure at 0.8–1.2 MPa, and mold temperature at 15–25°C. Formulation addition in the HDPE fraction comprises 2.0–3.0 wt% carbon black masterbatch, 0.05–0.10 wt% primary antioxidant, and internally generated flash regrind at 25–40 wt% of the combined HDPE layers. The EVOH barrier layer is metered at 2.0–3.5 wt% of total wall thickness and the two tie layers together at 2.0–3.0 wt%. Tail flash and pinch flash are reground only after passing a 2.0 mm screen pack and drying to below 0.08 wt% moisture to avoid microvoids at the pinch-off seam. Permeation and durability compliance is evaluated under SAE J1737 for fuel system permeation, UN ECE R34 for tank mechanical integrity, and EPA Title 40 CFR Part 86 for evaporative emissions. Tensile and stress crack resistance are confirmed using ASTM D638 Type IV specimens and ASTM D1693 Condition B in 100% Igepal CO-630. Terminal products include passenger vehicle fuel tanks, light commercial vehicle fuel systems, and off-road fuel cells.

    Flat-die sheet extrusion of HDPE geomembrane for waste containment and mining liners relies on the elevated environmental stress crack resistance of Marlex® HHM TR-232 when processed into 1.5–3.0 mm sheet. The extrusion line typically comprises a 120 mm single-screw extruder with L/D 30:1, a 2,500–3,200 mm coat-hanger die, and a polished three-roll stack held at 70–90°C. Barrel zone set points are staged from 190°C to 230°C, with die zone temperature maintained within ±3°C of the final barrel zone to limit transverse thickness drift below ±5%. Carbon black masterbatch is introduced at 2.0–3.0 wt% to achieve 2–3% carbon black content under ASTM D1603, and a hindered amine light stabilizer package is added at 0.3–0.6 wt% for long-term UV exposure. Where liner specifications demand additional oxidation resistance during the extrusion heat history, phenolic-phosphite stabilizer is metered at 0.1–0.2 wt%. Compliance is governed by GRI GM13, with single-point notched constant tensile load under ASTM D5397 at 50°C in 10% Igepal CO-630 for 500 h minimum failure time, tensile yield stress tested under ASTM D638, density under ASTM D1505, and puncture resistance under ASTM D4833. Terminal products include landfill base and cap liners, heap-leach pads, produced water pond liners, and secondary containment barriers beneath chemical tank farms.

    What Limits Parison Sag in 1,000-L Industrial Container Blow Molding?

    In accumulator-head extrusion blow molding of 1,000-L IBC inner bottles and 200-L open-head drums, parison sag after die exit determines wall thickness distribution and reject rate. Marlex® HHM TR-232 is processed on a 120 mm extruder with L/D 30:1 and a 20–25 kg accumulator head at melt temperature 210–225°C. Die gap is set between 2.5 mm and 4.5 mm, and parison length is controlled by head tooling geometry rather than line speed alone. Blow air pressure of 0.6–1.0 MPa and mold temperature of 15–25°C are used; clamp force on dedicated IBC machines is typically above 800 kN. The formulation includes 25–35 wt% regrind from deflashed top and bottom sections, screened through 6 mm and dried to below 0.05 wt% moisture before re-entry. Color concentrate is added at 1.5–3.0 wt% and a zinc-free antioxidant package at 0.05–0.10 wt% to avoid discoloration in high-residence-time head passages. Compliance for dangerous goods packaging includes UN 31A/Y for composite IBCs and UN 1H1 for tight-head plastic drums, with mechanical verification under ASTM D1998, environmental stress crack resistance under ASTM D1693 Condition A, and transport suitability under ADR/RID/IMDG. Terminal products include UN-certified IBC inner bottles, industrial export drums, and heavy-wall open-top chemical containers.

    Twin-sheet thermoforming lines converting Marlex® HHM TR-232 sheet into reusable material-handling platforms operate from extruded sheet of 6.0–9.5 mm thickness. The sheet section is produced on a 90–120 mm single-screw extruder with barrier screw and L/D 30:1, using a flat die and vertical three-roll stack at 70–90°C. Humidity above 80% RH requires pre-drying at 70–80°C for 1–2 h; below that threshold, hopper residence time and vent vacuum are sufficient to prevent surface moisture defects. Twin-sheet forming requires both sheets to reach 160–175°C surface temperature by infrared pyrometer before vacuum draw onto matched aluminum tools. Formulation for outdoor-rated pallets includes internally generated regrind at 25–40 wt%, carbon black or color masterbatch at 2.0–4.0 wt%, and UV stabilizer masterbatch at 0.3–0.6 wt%. Load performance is verified under ISO 8611-1, tensile properties under ASTM D638, flexural modulus under ASTM D790, and repeated food contact under FDA 21 CFR 177.1520 for reusable pallet applications. Terminal product types include nestable export pallets, rackable warehouse pallets, collapsible bulk containers, and returnable automotive component trays.

    When High-Density Polyethylene Replaces PVC in Non-Pressure Drainage Extrusion

    In non-pressure industrial drainage and cable conduit extrusion, Marlex® HHM TR-232 is processed on corrugated pipe lines with a 75–120 mm grooved-feed single-screw extruder at L/D 30:1. The melt enters a crosshead die and is drawn over a moving corrugator with vacuum slots holding 0.06–0.08 MPa against polished aluminum mold blocks. Barrel zone temperatures are staged from 180°C at the feed throat to 225°C at the die, with melt pressure of 15–25 MPa maintained to control inner wall collapse during vacuum formation. Formulation addition includes carbon black masterbatch at 2.0–3.0 wt% for UV stabilization corresponding to ASTM D3350 cell class C, hindered phenol/phosphite antioxidant at 0.10–0.20 wt%, and external lubricant at 0.05–0.10 wt% to prevent screw slip in grooved feed sections. The material is qualified under ASTM D3350 for cell classification, ASTM F2648 for dual-wall drainage pipe, and ASTM D3212 for gasketed joint performance; it is not specified for potable pressure service under ISO 4427. Terminal products include agricultural field drainage pipe, highway edge drain, cable conduit, and stormwater detention chamber shells.

    Blow molding of selective catalytic reduction urea tanks and coolant expansion reservoirs uses Marlex® HHM TR-232 in single-layer and three-layer configurations on accumulator-head machines with 60–100 mm extruders. Melt temperature is controlled at 205–220°C, mold temperature at 12–20°C, and blow pressure at 0.7–1.0 MPa. For urea service, three-layer HDPE / regrind / HDPE structures are common, with regrind introduced at 20–35 wt% of the wall and carbon black masterbatch at 2.0–2.5 wt% for UV protection. Copper-containing stabilizers and unreacted amine-bearing additives are excluded from the formulation because localized urea decomposition can raise pH above 9.5 and accelerate stress cracking at pinch-off weld lines. Compliance includes ISO 22241-1 for urea quality compatibility, SAE J2659 for tank material validation, and OEM pressure-vacuum cycling tests; material performance is checked using ASTM D1693 Condition A in 50°C urea solution and ASTM D638 tensile after 1,000 h heat aging. Terminal products include diesel exhaust fluid storage tanks, coolant reserve bottles, and windshield washer reservoirs.

    Free Quote

    Competitive Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced is a bimodal high-density hexene-1 copolymer supplied primarily for pressure pipe and industrial piping extrusion. The resin carries an ASTM D3350 cell classification of 445574 C and is listed as a PE 4710 pressure-rated material. The PE 4710 designation corresponds to a hydrostatic design basis of 1600 psi at 73 °F and 1000 psi at 140 °F under the listings maintained in PPI TR-4. Representative manufacturer-published values include a nominal density of 0.947 g/cm³ determined by ASTM D1505 and a melt mass-flow rate of 0.06 g/10 min determined by ASTM D1238 at 190 °C with a 2.16 kg load. These values place the resin in the high-molecular-mass, low-melt-index extrusion envelope required for thick-wall pipe where sag resistance and melt strength control the upper line-speed limit.

    The enhanced designation refers to a bimodal molar mass distribution created by cascade reactor polymerisation. The low-molar-mass mode provides shear thinning that lowers extruder torque and die-head pressure; the high-molar-mass mode contributes chain entanglement and resistance to slow crack growth. Hexene-1 incorporation shortens the average ethylene sequence length, increases tie-molecule concentration, and modifies lamellar thickness distribution. Compared with a conventional unimodal high-density polyethylene of similar density and melt index, this architecture produces a steeper shear-viscosity curve and higher elongational melt strength at pipe-forming temperatures. The practical consequence is a processing envelope for maintaining wall-thickness uniformity without excessive parison sag in large-diameter pipe.

    Rheological characterisation of bimodal high-density polyethylene pipe grades indicates pronounced non-Newtonian behaviour. At the low shear rates encountered in sag and parison forming, the molar-mass distribution produces high zero-shear viscosity; at high shear rates inside the die land, shear viscosity decreases steeply. This shear-thinning characteristic lowers extruder torque relative to a unimodal resin of equivalent melt index. Pipe producers using melt-pump-assisted lines can run barrel temperatures at the lower end of the processing window to preserve antioxidant package activity and reduce carbon-black degradation. Because published capillary rheometry data for this specific commercial grade is limited, processing trials should establish the shear-viscosity curve and extruder operating line before committing to a production campaign.

    How Does the Bimodal Molar Mass Distribution Affect Slow Crack Growth Resistance?

    Slow crack growth in pressurised polyethylene pipe is governed by the disentanglement of tie molecules in the amorphous phase under sustained hoop stress. A bimodal distribution with a high-molar-mass tail increases the probability that one chain participates in multiple crystalline lamellae, thereby increasing the number of load-bearing tie chains per unit cross-section. In this resin, the Pennsylvania notch test under ASTM F1473 exceeds 1000 h at 80 °C and 2.4 MPa. That threshold is widely used to separate PE 4710 pressure-pipe compounds from older PE 3408 or PE 3608 materials. Environmental stress-cracking resistance under ASTM D1693 condition C exceeds 5000 h with 100% Igepal CO-630, indicating resistance to slow crack growth in the presence of a surface-active environment.

    The hexene-1 co-monomer also influences the crystalline morphology. Short-chain branches excluded from the crystal lattice create tie chains and reduce critical lamellar thickness. This is not equivalent to reducing overall density; the material retains sufficient crystallinity to provide a flexural modulus of 1.10 GPa by ASTM D790. The combination of high modulus and high slow crack growth resistance is a key distinction from traditional unimodal resins, which often require a compromise between stiffness and stress-cracking resistance.

    Pipe-extrusion lines running this material typically use grooved-feed single-screw extruders with 30:1 to 36:1 L/D ratios and a barrier or Maddock mixing section. The feed throat is water-cooled to maintain a solid bed and control torque during start-up. Barrel temperatures are often set in a reverse profile, with the feed zone near 180 °C and the die zone at 190 °C to 220 °C. Melt temperature at the die entrance should be maintained at or below 230 °C, and excursions above 240 °C are not recommended because oxidative degradation lowers retained slow crack growth resistance. A gear pump between the extruder and die reduces melt-pressure pulsation and allows die-head pressures above 300 bar without excessive shear heating. Screen packs of 40/60 mesh are common, with finer filtration used for small-diameter pressure pipe where carbon-black agglomerates or gels must be removed before the calibration sleeve.

    Thermal Processing Window and Barrel Temperature Profiles

    High-molecular-mass high-density polyethylene exhibits shear heating that can raise melt temperature beyond the set point. Therefore, screw speed, back pressure, and barrel cooling must be controlled simultaneously. Melt temperature should be measured with a flush-mounted thermocouple at the adapter, not inferred from the die-zone set point alone. If the adapter melt temperature exceeds 230 °C, antioxidant consumption increases and the oxidative-induction time measured by ASTM D3895 may decrease. For black carbon-black-stabilised grades, dispersion quality is influenced by screw design and melt temperature; poor dispersion can produce carbon-black agglomerates that reduce elongation at break and slow crack growth resistance. Production-scale failure modes observed on high-output lines include wall-thickness eccentricity, surface melt fracture at the inner die lip, and resin degradation during hot shutdowns. Purging with a lower-molecular-mass polyethylene before shutdown and maintaining a nitrogen blanket on the feed hopper reduce gel formation.

    The flexural modulus of 1.10 GPa measured by ASTM D790 contributes to pipe ring stiffness; however, flexible pipe design relies on soil-pipe interaction rather than rigid beam strength. For buried pressure pipe, the designer uses the pipe dimension ratio and the hydrostatic design basis to determine pressure class, while external load calculation uses pipe stiffness and soil-structure interaction models. At 73 °F, the material has sufficient ductility to resist brittle crack propagation. The brittleness temperature of less than -75 °C measured by ASTM D746 indicates that embrittlement is not expected under normal storage conditions, but impact testing on finished pipe should follow the applicable product standard.

    Table 1 compiles representative physical and mechanical property values used for pipe design and extrusion simulation. These are manufacturer-published typical values, not specification minima.

    Property Test method Typical value Unit
    Density ASTM D1505 0.947 g/cm³
    Melt mass-flow rate ASTM D1238 / ISO 1133-1:2022 0.06 g/10 min
    Tensile strength at yield ASTM D638 24 MPa
    Elongation at break ASTM D638 >600 %
    Flexural modulus ASTM D790 1.10 GPa
    Hardness Shore D ASTM D2240 64 —
    Environmental stress-cracking resistance ASTM D1693 condition C >5000 h
    Pennsylvania notch test ASTM F1473 >1000 h
    Brittleness temperature ASTM D746 <-75 °C
    Vicat softening temperature ASTM D1525 124 °C

    Materials with this density and flexural modulus are used in municipal water, industrial process water, mining slurry, and sewer force-main service. Potable-water contact requires pipe and fittings to comply with NSF/ANSI/CAN 61. Pressure pipe produced to AWWA C906, ASTM F714, or ASTM D3035 may be manufactured from this resin when the product standard permits PE 4710 materials. In buried service, pipe stiffness and soil-pipe interaction should be evaluated according to AWWA M55 or ASTM D2321 because the low flexural modulus of polyethylene relative to metallic pipe alters deflection and buckling calculations.

    When PE 3408 or PE 3608 Is Replaced in Compressed Air or Water Networks

    Replacing a PE 3408 or PE 3608 resin with a PE 4710 material changes the hydrostatic design basis and the allowable pressure class at a given standard dimension ratio. The hydrostatic design basis of 1600 psi at 73 °F permits higher pressure classes at equivalent wall thickness when the design tables in PPI TR-4 are used. At 140 °F, the hydrostatic design basis of 1000 psi still exceeds the elevated-temperature ratings of many older materials, but the derating is not linear. Designers should not take an existing pressure rating and multiply by the ratio of hydrostatic design basis values without recalculating surge allowance, working pressure, fatigue life, and fitting material compatibility. Under AWWA C906, the pipe material designation and dimension ratio must be marked on the pipe, and mixed-material systems require adapters or fittings qualified for the lower-rated material if the system rating is to remain valid.

    Because this resin is a high-molecular-mass material with a 0.06 g/10 min melt index, butt fusion joining requires longer heat-soak times than lower-density or higher-melt-index polyethylene. Fusion parameters should follow ASTM F2620 with heater plate surface temperatures of 204 °C to 232 °C and interfacial bead-up pressure of 60 psi to 90 psi. Exact soak time depends on wall thickness and ambient temperature. Cold fusion, characterised by a smooth, flat interfacial bead that does not roll back onto the pipe surface, is a principal field failure mode. Electrofusion couplers should be programmed for PE 4710 resins and validated by coupler manufacturers rather than assuming compatibility with older PE 3408 fittings.

    Long-term exposure to potable water with high free-chlorine residuals at temperatures above 23 °C requires oxidative-induction-time testing under ASTM D3895 and, where specified, accelerated chlorine-resistance testing under ASTM F2263. Polyethylene pipe resins are not resistant to strong oxidising acids, warm aromatic hydrocarbons, or concentrated halogenated solvents; contact with toluene, xylene, or strong oxidisers can promote solvent swelling and environmental stress cracking. The material should not be installed in compressed oxygen service without a separate suitability evaluation because ignition and combustion behaviour differ from metallic pipe.

    Table 2 summarises the principal standards referenced for pressure pipe manufactured from this material.

    Reference Scope Design or test parameter
    ASTM D3350 Polyethylene pipe material cell classification 445574 C
    ASTM D2837 Hydrostatic design basis determination 1600 psi at 73 °F; 1000 psi at 140 °F
    ASTM D1238 / ISO 1133-1:2022 Melt mass-flow rate 0.06 g/10 min at 190 °C, 2.16 kg
    ASTM F1473 Pennsylvania notch test for slow crack growth >1000 h at 80 °C, 2.4 MPa
    ASTM D1693 Environmental stress-cracking resistance >5000 h, condition C, 100% Igepal
    ASTM F2620 Butt fusion joining Heater plate 204 °C to 232 °C
    AWWA C906 Polyethylene pressure pipe and fittings PE 4710 material designation
    NSF/ANSI/CAN 61 Drinking-water system components Health-effects compliance

    Finished pipe pressure testing is typically conducted at 1.5 times the working pressure for potable water systems, but the actual test pressure should follow AWWA C605 or ASTM F2164. Sustained hydrostatic testing of pipe specimens under ASTM D1598 or ISO 1167 at 20 °C and 80 °C confirms that extruded pipe retains the expected long-term strength. Ductile-mode failure after short-term testing is acceptable if the failure stress exceeds the material’s short-term burst requirement; brittle failure at short time or low stress indicates processing-induced thermal degradation or poor fusion of the pipe wall.

    Manufacturing consistency is monitored through melt index, density, tensile yield, and Pennsylvania notch test value on each lot. A shift of 0.01 g/10 min in melt index may alter die-head pressure and wall-thickness control; gravimetric feeding and melt-pump speed adjustment are therefore recommended. Pipe producers should retain fused-joint samples for destructive testing under ASTM F2620 and hydrostatic sustained-pressure testing under ASTM D1598 or ISO 1167. When dimensional scrap is reintroduced, regrind content above 20% should be qualified by retention of slow crack growth resistance on finished pipe, because regrind reduces the high-molar-mass fraction and can lower long-term performance even when melt index remains within specification. Published data for this specific resin at regrind levels above 20% is limited.

    Top