Chevron Phillips Marlex D350 M Lldpe Linear Low Density Polyethylene

Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene

    • Product Name: Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 267148
    Productname Chevron Phillips Marlex D350 m-LLDPE Linear Low Density Polyethylene
    Polymertype Metallocene Linear Low Density Polyethylene
    Comonomer Hexene-1
    Density 0.935 g/cm³
    Meltindex 0.5 g/10 min
    Meltingpoint 124 °C
    Vicatsofteningpoint 108 °C
    Tensilestrengthatyield 16 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 600%
    Flexuralmodulus 550 MPa
    Dartimpact 180 g
    Elmendorftearmd 200 g
    Elmendorfteartd 400 g
    Haze 10%
    Gloss45 60
    Coefficientoffriction 0.2

    As an accredited Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg (55 lb) polyethylene-lined paper bags, palletized and stretch-wrapped; bulk quantities available in 1,000 kg (2,205 lb) supersacks.
    Container Loading (20′ FCL) 20′ FCL container loading for Chevron Phillips Marlex® D350 m-LLDPE: 25 kg bags, floor-loaded, 1,000 bags, approx. 25 MT net weight.
    Shipping Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene is shipped as non-hazardous resin pellets. Standard packaging includes 25 kg bags, bulk boxes, and bulk trucks or railcars. It is not DOT-regulated. Store and transport dry, cool, and away from direct sunlight, heat, and ignition sources.
    Storage Store Chevron Phillips Marlex® D350 m-LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and oxidizing agents. Keep original containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Maintain clean, segregated storage and use first-in, first-out rotation. Follow local regulations, the manufacturer’s safety data sheet, and no smoking or ignition sources nearby.
    Shelf Life Stable under normal storage conditions; no defined shelf life. Store in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene

    Flat-die extrusion of hexene-based m-LLDPE D350 into geomembrane sheet requires carbon black masterbatch letdown at 2.0–3.0 wt% to meet weathering resistance for exposed installations. The carbon black is incorporated prior to sheet extrusion through a twin-screw compounding step. Dispersion quality is monitored by ISO 18553, with an acceptable rating of A1–A2. The compounded resin is fed through a single-screw extruder with L/D ratio of 30:1, barrel zones 180–240 °C, and a flat sheet die maintained at 240 °C. Chill roll temperatures are held at 60–80 °C to limit crystallinity gradients across 1.5 mm sheet. Thickness is verified under ASTM D5199. Low-temperature brittleness is measured by ASTM D746 with a failure point commonly below −70 °C for m-LLDPE geomembrane grades. Tear resistance is evaluated by ASTM D1004, and puncture resistance by ASTM D4833. For landfill liner service, the sheet is joined by hot-wedge welding at 350–400 °C seam temperature. Seam peel strength is verified by ASTM D6392. Field performance is tied to stress crack resistance measured by ASTM D5397, with notch constant tensile load testing under 2.5 MPa net section stress. The resin is not recommended for extended contact with aromatic hydrocarbon solvents. Published permeation data for this specific configuration is limited. Sheet edge trim is recycled at 15–20 wt% into the core layer of a three-layer coextruded structure without loss of impact, provided the recycled fraction is dried below 0.03 wt% moisture. Screen packs of 20/40/60 mesh are installed ahead of the die to capture carbon black agglomerates that would otherwise form pinholes under hydraulic pressure.

    Test methodPropertyRelevance to geomembrane fabrication
    ASTM D5199Sheet thicknessControls weld window and puncture resistance
    ASTM D1505DensityDetermines crystallinity and chemical resistance
    ASTM D6693Tensile yield and breakValidates long-term slope stability
    ASTM D1004Tear resistanceAffects handling and seam integrity
    ASTM D4833Puncture resistanceRelevant during aggregate placement

    What Process Window Governs Rotational Molding of D350 for Chemical Storage Tanks?

    Rotational molding of D350 begins with grinding to 35 mesh nominal particle size, approximately 500 µm. Dry blending of UV stabilizer at 0.1–0.3 wt% and pigment at 0.5–2.0 wt% is preferred over melt compounding to preserve particle shape and flow. The mold is charged, clamped, and heated in a clamshell oven operating at 280–300 °C. Internal air temperature measured by a through-axle thermocouple reaches 190–205 °C for complete densification. At 6 mm nominal wall thickness, oven residence time is typically 12–18 min. Molds with tapered corners and venting at 0.5–1.0 mm diameter reduce trapped gas porosity. The peak internal air temperature must remain below 215 °C; above this threshold oxidative degradation increases, producing yellowing and a measurable drop in impact strength. Cooling rate is the main lever for warpage control. Forced-air cooling produces higher density and more shrinkage, while water mist cooling at 40–60 °C increases impact toughness but may induce bowing in flat panels. Wall thickness is checked by ultrasonic gage at 5–8 points per tank. Environmental stress crack resistance is measured by ASTM D1693, condition C, and notched constant tensile load by ASTM D5397. Food-contact tanks are tested under FDA 21 CFR 177.1520, olefin polymer clearance. Potable water tanks must meet NSF/ANSI 61. The mold release agent must not contain fatty amines; residual amine-class additives can cause surface oxidation and interfere with adhesion in multi-layer rotomolding.

    Blown Film Bubble Stability and Impact Resistance in Heavy-Duty Sack Applications

    Blown film conversion of D350 into heavy-duty sacks runs on a monolayer or coextruded line with die diameter 200–250 mm and die gap 1.4–2.0 mm. Melt temperature is set at 200–230 °C, with frost line height 500–900 mm above the die. The bubble is maintained at a blow-up ratio of 2.2:1–2.8:1. Internal bubble cooling becomes necessary above 80 µm gauge to control bubble flutter. Thick film of 80–150 µm requires low stalk height and a dual-lip air ring. Slip additive is incorporated at 500–1500 ppm, antiblock at 1000–3000 ppm, and polymer processing aid at 200–500 ppm when melt pressure exceeds 35 MPa at the breaker plate. The narrow molecular weight distribution of m-LLDPE increases melt pressure compared with conventional LLDPE. Barrier flight screws with L/D of 30:1 are standard for this resin class. Mechanical verification includes Dart impact by ASTM D1709, Elmendorf tear by ASTM D1922, and probe puncture by ASTM D5748. Heavy-duty sack end products of 25–50 kg capacity are tested under ISO 21898 for drop and stacking performance. Heat sealing uses jaw temperature 130–160 °C and dwell 0.5–1.0 s. Melt temperature above 240 °C should be avoided because alkoxylated additive degradation accelerates gel and odour formation during extended residence time.

    Low-pressure drip irrigation laterals extruded from D350 rely on high environmental stress crack resistance and flexibility at wall thicknesses of 0.6–2.0 mm. Pipe extrusion uses a grooved-feed extruder with L/D 24:1–30:1, barrel profile 190–240 °C, and a spiral mandrel pipe die. The melt is calibrated in a vacuum tank at −20 to −40 kPa, with water temperature 20–40 °C. Carbon black masterbatch is added at 2.0–2.5 wt% for UV stabilization. Dispersion is assessed under ISO 18553 to avoid microvoids that reduce burst strength. Burst pressure is measured by ISO 1167 with end caps and water pressurization. Slow crack growth is evaluated by ASTM F1473 on notched pipe. The final lateral withstands a bending radius of 8–10 times outside diameter at 23 °C without kinking. Emitters are inserted by hot-punch at 180–220 °C; the hole edge must show no melt fracture or radial cracking. Compatibility with fertilizer solutions is limited to pH 3–9. Strong oxidizing agents such as sodium hypochlorite above 10 ppm free chlorine accelerate oxidative degradation unless the compound includes stabilizer at the upper end of supplier recommendations. For buried installations, external load deflection is evaluated under ASTM D2412, with pipe stiffness dependent on wall thickness and outside diameter.

    When Extrusion Lamination onto Polypropylene Woven Fabric Demands Puncture Resistance Without Tie-Layer Delamination

    Adhesion between D350 and polypropylene woven fabric in extrusion lamination depends on fabric surface energy after corona treatment. The corona discharge unit is set to 38–42 dyn/cm as measured by wetting tension test solutions according to ASTM D2578. The m-LLDPE melt is extruded through a slot die at 300–330 °C to promote thermal fusion to the PP surface. Coating weight is controlled at 15–30 g/m². Nip pressure is held at 15–25 N/mm across the roll width. Line speed varies from 100–250 m/min depending on coat weight and fabric denier. Without a tie layer, adhesion loss occurs when corona treatment drops below 34 dyn/cm; online treatment after preheating is therefore required. The resulting flexible intermediate bulk container fabric is tested under ISO 21898 for UV resistance and safe working load. Coating tear strength is measured by ASTM D882. Puncture resistance is measured by ASTM D4833. Melt temperature above 340 °C causes chain scission of D350 at extended residence times and generates gels in the coating. For food-contact packaging, the coated fabric must comply with FDA 21 CFR 177.1520 and EU Regulation 10/2011. Incompatibility with fatty amines in printing inks may require a cleaning step to avoid odour and delamination at the coating interface. The extruder is typically equipped with a 30:1 L/D screw and a gear pump to stabilize coat weight across the web.

    Injection Molding of Thick-Walled Intermediate Bulk Container Fittings

    Thick-walled IBC valve bodies and caps molded from D350 are processed with ram injection pressures of 60–120 MPa and melt temperatures of 210–250 °C. Mold temperature is kept at 15–30 °C with turbulent water cooling. Screw back pressure is set at 0.5–1.5 MPa to avoid additive degradation. Packing pressure is held at 60–80% of peak injection pressure for 20–45 s on 10 mm wall sections; early gate freeze results in sink marks and dimensional drift. Hot runner valve gates are preferred for multi-cavity tools. D350 is processed with color masterbatch letdown at 1–3 wt% and UV stabilizer at 0.1–0.3 wt%. The molded fittings are tested under ISO 16101 for IBC compatibility and under UN 31HA1 drop test conditions for dangerous goods packaging. Environmental stress crack resistance is evaluated by ASTM D1693 and tensile impact by ASTM D1822. Mold filling simulation uses a shear rate limit of 10 000 s⁻¹; exceeding this in gate regions produces flow marks. The m-LLDPE resin resists cracking in notched sections under sustained stress, but injection speed must be reduced if short shots occur below 220 °C melt temperature.

    Free Quote

    Competitive Chevron Phillips Marlex® D350 m-LLDPE Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® D350 is a metallocene-catalyzed linear low-density polyethylene (m-LLDPE) resin supplied in pellet form for blown and cast film conversion. The grade is produced with single-site catalyst chemistry that provides a narrow molecular weight distribution and a homogeneous short-chain branching profile relative to Ziegler-Natta LLDPE. Nominal resin specifications reported in the manufacturer’s published data include a density of 0.933 g/cm³ determined under ASTM D1505 and a melt index of 0.50 g/10 min determined at 190 °C with a 2.16 kg load under ASTM D1238. These values place the material in the upper-density segment of the LLDPE classification, where film modulus and thermal resistance are higher than those of 0.918 g/cm³ conventional LLDPE grades, while the 0.50 g/10 min melt index indicates a comparatively high-molecular-weight product with lower flow than 1.0 g/10 min film grades. Because the resin is an ethylene-α-olefin copolymer produced with single-site catalysis, the incorporation of comonomer along the polymer chain is more controlled than in multi-site Ziegler-Natta ethylene polymerization.

    What Distinguishes Metallocene-Catalyzed Short-Chain Branching from Ziegler-Natta Architectures?

    In Ziegler-Natta LLDPE, multiple catalytic site populations generate a broad distribution of molecular weights and a non-uniform intermolecular comonomer distribution. The high-molecular-weight fraction in Ziegler-Natta resins often contains a higher concentration of short-chain branches, while the low-molecular-weight fraction is comparatively linear; this heterogeneity contributes to increased haze, broader seal-initiation behavior, and higher extractable mass. The single-site metallocene system used for D350 produces a narrower molecular weight distribution and a more uniform placement of short-chain branches across the molecular weight range. The resulting solid-state morphology after solidification contains smaller and more uniform lamellar crystals, which lowers primary light scattering and improves optical clarity without requiring high loadings of nucleating additives.

    Because the molecular weight distribution of D350 is narrow, the resin exhibits less shear thinning than broad-MWD LLDPE at equivalent melt index. At typical die shear rates, this can produce higher head pressure and melt temperature than a broad-MWD Ziegler-Natta LLDPE of the same nominal melt index. Extrusion lines equipped with shallow-metering screws or undersized die filtration may therefore require throughput derating or die-gap adjustment. Published data for this exact grade across all available extruder configurations is limited, but comparative rheology of metallocene LLDPE shows lower extensional thickening and lower melt elasticity than high-pressure LDPE.

    Comparison of resin architecture and typical processing characteristics
    ParameterMarlex D350 m-LLDPEZiegler-Natta LLDPEHigh-pressure LDPE
    Nominal density0.933 g/cm³ (ASTM D1505)0.916–0.940 g/cm³0.912–0.925 g/cm³
    Melt index0.50 g/10 min (ASTM D1238)0.50–1.0 g/10 min typical0.20–0.80 g/10 min typical
    Molecular weight distributionNarrowBroadBroad
    Short-chain branch distributionHomogeneousHeterogeneousHeterogeneous with long-chain branching
    Long-chain branchingLowLowHigh
    Shear thinning at high extrusion ratesLimitedModeratePronounced
    Melt strength at 190 °CLower than LDPEModerateHigh

    Film converters comparing D350 with a 0.918 g/cm³ conventional LLDPE should not infer final mechanical performance from nominal density alone. Orientation generated during film production exerts a substantial effect on machine-direction and transverse-direction modulus, tear, and dart impact. Comparative trials are typically run on a single film line at fixed gauge, blow-up ratio, frost-line height, and melt temperature; tensile properties are measured under ASTM D882, dart impact under ASTM D1709, and Elmendorf tear under ASTM D1922. In such evaluations, the higher density of D350 generally shifts the balance toward higher modulus and yield stress while reducing low-temperature toughness and tear at equal gauge. The magnitude of the shift depends on molecular orientation and cannot be predicted from resin density alone.

    Extrusion Melt Temperature and Bubble Geometry Are Determined by Melt Index and Density.

    In blown film conversion, melt temperature for this density class is generally maintained between 190 °C and 220 °C, with die temperatures at 215 °C to 230 °C. A die gap of 1.0–1.5 mm is commonly used; the narrow molecular weight distribution of m-LLDPE makes the film less tolerant of excessive drawdown than conventional LLDPE, so a blow-up ratio of 2.0:1 to 3.0:1 is typical. Frost-line height must be controlled to stabilize bubble geometry because the relatively low melt strength can produce bubble wander and instability on single-air-ring lines. Adding 10–30 wt% high-pressure LDPE is a standard process adjustment for increasing melt strength and reducing bubble flutter, but this addition lowers film modulus and optical clarity in proportion to the LDPE content.

    Pre-drying of the bulk resin is generally not necessary because polyethylene is not appreciably hygroscopic. However, pellets stored in cold, high-humidity environments can carry surface condensation into the hopper at relative humidity above 60 %; this condensation can generate surface defects and should be prevented by allowing sacks to reach ambient temperature before use. Filtration of the melt is normally performed through breaker plate screens; because head pressure is already elevated by the low melt index and narrow MWD, screen packs and feed-section geometry should be reviewed before increasing throughput. Screw speed should be increased in moderate increments to limit excessive shear heating.

    For cast film, D350 requires attention to neck-in and oxidative stability at elevated melt temperatures. Cast film lines with die-to-chill-roll gaps greater than approximately 25 mm may show wider edge trim generation when the resin is run at lower melt temperatures. Because m-LLDPE is less elastic than LDPE, edge pinning and vacuum-box settings must be adjusted; processors often raise melt temperature in 5 °C increments within the supplier’s recommended range to reduce neck-in. Chill-roll temperatures are typically maintained between 15 °C and 35 °C depending on gauge and line speed, and final film is tested for coefficient of friction under ASTM D1894, haze under ASTM D1003, and gloss under ASTM D2457.

    Evaluating the Stiffness-Toughness Shift with Standard Film Tests

    The higher density of Marlex D350 primarily affects tensile secant modulus and yield stress. The secant modulus at 1 % strain measured under ASTM D882 is frequently the first comparative property examined during down-gauging. Because film orientation created by bubble geometry and haul-off speed can alter the MD/TD balance more significantly than a small density difference, comparative testing should be performed on films produced at the same gauge and blow-up ratio. For blown film at 25 μm gauge, tensile properties are often tested with a crosshead speed of 500 mm/min under ASTM D882; dart impact is tested as F50 under ASTM D1709; Elmendorf tear is tested under ASTM D1922; haze is tested under ASTM D1003; and clarity may be checked under ASTM D1746. Differences between m-LLDPE grades with different density are observed primarily in modulus and low-temperature impact rather than in optical transmittance.

    Published data for this specific product’s film properties should be requested as a grade-specific product data sheet, because film values vary with extrusion conditions, additive masterbatch, and cooling rate. A single laboratory tensile value should not be treated as a universal film property, since gauge, die gap, orientation, and frost-line height all affect the result. Batch-to-batch release testing under ASTM D1505 and ASTM D1238 provides incoming quality control data, but film-level performance must be established on the converter’s own line.

    When a Converter Replaces Conventional LLDPE with D350 in Multi-Layer Coextrusion

    On a three-layer blown film line, D350 is often placed in the core layer to increase overall film stiffness, while lower-density m-LLDPE or LDPE is retained in the skin layers to preserve sealing performance and optics. If D350 replaces a conventional Ziegler-Natta LLDPE of similar density, the converter should expect a different pressure-flow relationship through the die. Because narrow-MWD metallocene resins show reduced shear thinning, the apparent viscosity at high die shear remains higher than a broad-MWD LLDPE at the same melt index. This can raise melt pressure and require adjustment of extruder screw rpm, die temperatures, or screen filtration. On smaller extruders with limited drive torque, this pressure increase can become a throughput constraint.

    No universal die-gap correction is appropriate because die geometry and air-ring design vary. When melt fracture appears at high line speed, the die temperature may be raised in 5 °C increments or the die gap may be widened within the die manufacturer’s mechanical limitations. Bubble stability is maintained by controlling frost-line height and using internal bubble cooling where available. The resin should not be combined with high-percentage peroxide masterbatches unless reactive modification is intended, because free-radical chemistry can promote gel formation and degrade optical quality.

    Vicat Softening, Seal Initiation, and Hot-Tack Performance in Packaging Layers

    Higher copolymer density raises the Vicat softening temperature and seal initiation temperature relative to lower-density m-LLDPE. In lamination and overwrap structures, D350 is therefore more likely to be selected for stiffness-critical layers than for low-temperature sealant layers. Seal performance is evaluated under ASTM F2029 for heatsealability and ASTM F1921 for hot-tack strength, with seal-bar temperatures set across a range to identify the film’s practical sealing window. Because the narrow composition distribution of m-LLDPE can produce a relatively sharp seal onset, the practical sealing window should be established on the packaging line rather than inferred from DSC melting data alone.

    Thermal properties are reported in the certificate of analysis by ASTM D3418 or ASTM D1525. The exact Vicat softening increment over lower-density LLDPE should be confirmed batch-by-batch, because additive packages and minor process variation can shift the value. Films containing D350 in the core layer retain LLDPE-type toughness and environmental stress crack resistance compared with HDPE, but the higher density reduces the low-temperature impact cushion that a 0.918 g/cm³ m-LLDPE can provide. Comparative dart impact testing under ASTM D1709 on fixed-gauge film is therefore required before down-gauging. Environmental stress cracking resistance can be assessed by ASTM D1693, although film-specific seal and dart testing usually dominate conversion decisions.

    Marlex D350 is suitable for industrial liners, heavy-duty overwrap, collation shrink, agricultural films requiring higher stiffness, and stiffness-enhancing layers in coextruded packaging. The material is also used in cast film structures when a balance of clarity and modulus is needed. Compliance with food-contact provisions such as FDA 21 CFR 177.1520 and EU Regulation (EC) No 10/2011 depends on the finished film formulation, additive package, and migration testing, and should be verified through the manufacturer’s product safety documentation. REACH Regulation (EC) No 1907/2006 obligations are generally addressed by the supplier registration and safety data sheet; converters should confirm SVHC status and any article-level communication duties before commercial use. Batch-to-batch density and melt index variation is controlled by manufacturer release testing under the standards cited above, and converters should retain certificates of analysis as part of incoming quality control.

    Top