Chevron Phillips Marlex D252 257 Linear Low Density Polyethylene Film Resin

Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin

    • Product Name: Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 286018
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.923 g/cm3
    Meltindex 0.7 g/10 min (190 °C/2.16 kg)
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreakmd 31 MPa
    Tensilestrengthatbreaktd 28 MPa
    Elongationatbreakmd 700%
    Elongationatbreaktd 800%
    Flexuralmodulus 276 MPa
    Dartdropimpact 100 g
    Elmendorftearmd 200 g
    Elmendorfteartd 400 g
    Haze 14%
    Gloss 50%
    Coefficientoffriction 0.2
    Blocking 30 g
    Filmgauge 1 mil (25 µm)

    As an accredited Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Marlex D252/257 is typically packaged in 25 kg (55 lb) bags, 40 bags per 1,000 kg pallet; also available in bulk.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of Chevron Phillips Marlex® D252/257 LLDPE film resin, palletized, shrink-wrapped, and secured.
    Shipping Chevron Phillips Marlex D252/257 LLDPE film resin is shipped as non-hazardous solid pellets in 25 kg polyethylene bags, stretch-wrapped pallets, supersacks, or bulk trucks/railcars. Store in a dry, cool, well-ventilated area away from heat, sunlight, and ignition sources. Protect packaging from damage and moisture.
    Storage Store Marlex® D252/257 LLDPE film resin indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep bags or containers closed to prevent moisture and contamination. Avoid dust generation and static discharge; ground handling equipment. Maintain stable stacks and follow first-in, first-out inventory practices. Consult the SDS for detailed storage requirements.
    Shelf Life Marlex® D252/257 LLDPE film resin typically has a 24-month shelf life when stored cool, dry, and sealed in original packaging.
    Application of Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin

    At cast film line speeds above 300 m/min, the D252 member of the Marlex D252/257 resin family is processed on single-screw extruders with 30:1 L/D barrier screws and Maddock mixing heads; the resin family is characterised by a nominal density of 0.923 g/cm³ per ASTM D792 and a melt index of 2.0 g/10 min for D252 at 190°C/2.16 kg per ASTM D1238-20. In cast pallet stretch film, the formulation loads D252/257 at 80-95 wt% with LDPE at 5-20 wt% to maintain cling after 150-250% pre-stretch without external tackifier; silica antiblock is added at 0.1-0.3 wt% and erucamide slip at 0.2-0.5 wt%, with slip migration to the film surface requiring 48-72 h at 23°C before stable coefficient of friction is recorded. Industry compliance for non-food pallet stabilisation is anchored to REACH Regulation (EC) No 1907/2006 SVHC screening and CONEG heavy metal model legislation; where the wrap may contact food in secondary packaging, FDA 21 CFR 177.1520(c)3.2a and EU Regulation (EU) No 10/2011 apply, with overall migration below 10 mg/dm² under the regulatory test condition. Downstream processing uses a coat-hanger die with 0.8-1.2 mm die gap, melt temperature 230-280°C, a chrome chill roll held at 15-25°C, air-knife and vacuum-box pinning, and corona treatment to 38-42 dyn/cm; draw resonance becomes visible as transverse thickness bands when the draw ratio exceeds 12:1 or when chill-roll speed oscillation exceeds ±2%, so the line speed is maintained within 300-600 m/min. Terminal product types include hand pallet wrap, machine pallet wrap, pre-stretched film, and agricultural pallet stabilisation film.

    When High-Stalk Blown Film Systems Exceed a 3.5:1 Blow-Up Ratio, What Limits Bubble Stability in Heavy-Duty Sack Applications?

    Heavy-duty sack production shifts to the higher melt strength member of the D252/257 family, typically D257 with a melt index of approximately 0.5 g/10 min at 190°C/2.16 kg per ASTM D1238-20, because elongational melt strength at the frost line controls bubble stability when blow-up ratios exceed 3.0:1. The base formulation combines D257 at 70-90 wt% with LDPE or recycled LLDPE at 10-30 wt%; carbon black masterbatch at 2-4 wt% is added for outdoor storage bags, and a fluoropolymer processing aid at 0.03-0.08 wt% is introduced only when die lip deposits are observed after 48 h of continuous extrusion. Compliance for heavy-duty industrial sacks is verified by ASTM D1709-22 Method B for dart impact, ASTM D882-18 for tensile elongation, and ISO 4593 for thickness tolerance; where the sack is used for chemical packaging under UN certified conditions, the complete package must pass the UN Model Regulations drop test and stacking test under the applicable packing group. Downstream high-stalk blown film conversion uses a 250-350 mm spiral mandrel die with a 1.8-2.4 mm die gap, melt temperature 190-210°C, blow-up ratio 2.5:1-4.0:1, and internal bubble cooling holding the frost line at 6-9 die diameters above the die. Gauge variation is held below ±8% by controlling dew point and exhaust air temperature; batch-to-batch melt index variation outside ±0.2 g/10 min is corrected by die gap adjustment because stalk height and bubble tension are highly sensitive to molecular weight shift. Terminal product types include 25 kg and 50 kg export sacks, FIBC inner liners, construction aggregate sacks, and salt/fertilizer bags.

    Low-temperature dart impact in frozen seafood and IQF vegetable pouches is measured by ASTM D1709-22 Method A at -18°C on films with thickness 40-80 µm; the resin family’s low gel count and α-olefin comonomer distribution permit processing without melt temperature exceeding 200°C, which limits oxidative degradation during extended runs. The formulation uses D252/257 at 80-100 wt%, with 0-20 wt% metallocene LLDPE for improved dart impact, antiblock masterbatch at 0.2-0.5 wt%, and slip additive at 0.05-0.15 wt%; no plasticiser is used, maintaining food-contact compliance under FDA 21 CFR 177.1520(c)3.2a and EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² at 20°C/10 days for frozen storage. Downstream conversion uses a 150-200 mm blown film die, die gap 1.2-1.8 mm, blow-up ratio 2.0:1-3.0:1, dual-lip air-ring cooling, and corona treatment to 38-42 dyn/cm for laminating or print. Terminal products include frozen vegetable pouches, ice cream liners, IQF poultry bags, and seafood vacuum package base web.

    Silage Film Oxygen Barrier and UV Stabilization Under ISO 527-3 Tensile Limits

    Agricultural bale-wrap film based on D252/257 is specified under EN 13206:2017 for agricultural/horticultural film and ISO 527-3:2018 for tensile properties of film and sheeting; the film must retain ≥80% of original machine-direction tensile elongation after outdoor weathering exposure, which is why HALS stabilizer at 0.3-0.8 wt% and carbon black masterbatch at 2-4 wt% are compounded into the base resin. The formulation loads D252/257 at 70-90 wt% with LDPE at 5-20 wt% for melt strength; total masterbatch content is kept below 8 wt% to prevent tensile rupture in bale wrapper pre-stretch units operating at 50-70% extension. Downstream blown film extrusion uses a 1,200-2,000 mm annular die with 1.8-2.5 mm die gap, high-stalk internal bubble cooling, melt temperature 190-210°C, blow-up ratio 2.5:1-3.5:1, and final film thickness 25-40 µm; gauge variation is controlled to ±6% and corona treatment is set to 36-40 dyn/cm for adhesion of print and adhesive. Published data for the specific weathering degradation curve of Marlex D252/257 in 25 µm bale wrap under Northern European UV exposure is limited; therefore UV masterbatch loadings are validated by field trial rather than extrapolated from accelerated QUV testing alone. Terminal product types include silage bale wrap, silage clamp covers, greenhouse side curtains, and grain storage liners.

    Application zoneStandard designationParameter controlledRegulatory anchor
    Cast stretch wrapASTM D882-18 / ISO 527-3:2018Tensile elongation at breakREACH, FDA 21 CFR 177.1520(c)3.2a, EU (EU) No 10/2011
    Heavy-duty sacksASTM D1709-22 Method BDart impact resistanceUN Model Regulations applicable packing group
    Frozen food packagingASTM D1709-22 Method ALow-temperature dart impactFDA 21 CFR 177.1520(c)3.2a, EU (EU) No 10/2011
    Silage filmEN 13206:2017 / ISO 527-3:2018Weatherability and tensile retentionEN 13206:2017
    Dry food pouch sealantASTM F1249-20 / ASTM D3985-21WVTR and oxygen transmission rateFDA 21 CFR 177.1520(c)3.2a, EU (EU) No 10/2011

    Sealant Web Rheology and Low Seal Initiation in Dry Food Pouch Lamination

    In cast film coextrusion for dry food pouch sealant webs, the D252 member of the resin family is used as the sealant layer at 20-40 µm thickness; the low seal initiation temperature reduces dwell time on vertical form-fill-seal machines running 80-140 packages per minute, while the melt index of 2.0 g/10 min permits thin-gauge distribution at line speeds up to 400 m/min. The sealant layer formulation blends D252/257 at 60-100 wt% with mLLDPE or LDPE at 0-40 wt%, adding antiblock masterbatch at 0.2-0.5 wt% and erucamide slip at 0.05-0.15 wt%; silicone-based slip additives are avoided because they increase surface adhesion defects after corona treatment. Food-contact compliance is governed by FDA 21 CFR 177.1520(c)3.2a and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² and specific migration limits listed in Annex I Table 1 of the EU regulation. Downstream processing uses a 0.8-1.0 mm die gap, melt temperature 230-270°C, chrome chill roll at 15-25°C, corona treatment to 40-44 dyn/cm, and air-gap lengths below 120 mm to minimise draw resonance and neck-in. Terminal product types include stand-up pouches, dry food sachets, stick packs, and lamination sealant webs for snack packaging.

    Free Quote

    Competitive Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® D252/257 linear low density polyethylene film resin is supplied as a pelletized ethylene copolymer intended for blown film and cast film conversion. The dual D252/D257 designation denotes a product family controlled under two closely related manufacturing set points; lot-specific verification against the supplier certificate of analysis is required before campaign changeover because melt flow and density are controlled to narrow internal tolerances under ASTM D1238 at 190 °C/2.16 kg and ASTM D1505. Incoming resin evaluation for extrusion qualification typically records pellet size distribution, apparent density under ASTM D1895, and oxidative induction time under ASTM D3895 to establish acceptable residence time in the extruder and heat-history tolerance.

    What distinguishes D252/257 from commodity butene LLDPE film resins?

    Commodity butene LLDPE grades often show lower dart impact and lower Elmendorf tear at equivalent density and melt flow than resins synthesized with higher alpha-olefin comonomers. The D252/257 family is engineered to shift the balance between bubble stability and solid-state toughness; converters benchmark it under ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D882 for tensile properties. In comparative evaluations on a 65 mm diameter extruder with a 250 mm spiral mandrel die, gauge variation at 25 µm target thickness was maintained within ±5% when frost-line height was set between 8 and 10 die diameters. The resin is supplied as fully compounded pellets, so high-shear dispersion of the base polymer is not the limiting variable; however, masterbatch distribution can affect tear variance if letdown ratio exceeds 4% without a static mixer.

    Processors blending up to 20% edge trim with virgin D252/257 do not typically exceed an extruder melt temperature of 232 °C when the recycle stream is ground below 10 mm and fed through a side-arm vented extruder. Stabilizer retention is monitored by oxidative induction time under ASTM D3895 at 200 °C; a drop below the converter’s incoming-resin specification indicates additive consumption and requires reducing reclaim ratio or raising antioxidant masterbatch addition. This practice becomes critical on high-output lines where post-consumer or edge-trim content is increased without proportional adjustment of the primary antioxidant package.

    Thermal, rheological, and melt-curtain limitations in cast and blown film conversion

    The melt flow band for the D252/D257 family is typically controlled to 0.8–1.0 g/10 min under ASTM D1238. That flow range produces moderate shear viscosity in a 63.5 mm diameter barrier-screw extruder with a 24:1 L/D ratio. Barrel profiles are generally set from 180 °C at the feed throat to 215 °C at the adapter; melt pressure before the screen pack is held between 25 MPa and 35 MPa. Die gaps below 1.2 mm increase melt shear heating by more than 4 °C per 10 rpm screw-speed increase, while die gaps above 2.0 mm increase low-output gauge scatter unless nip speed is controlled to within ±0.5 m/min. On lines equipped with gear pumps, pump inlet pressure should be kept between 5 MPa and 10 MPa to prevent cavitation. Screen pack construction of 20/40/60 mesh is typical; pressure drop across the screen pack should not exceed 10 MPa, because excessive shear heating can shift melt flow measured after processing by more than 0.2 g/10 min.

    Film optical properties are sensitive to crystalline morphology and processing history. Haze is measured under ASTM D1003, and gloss at 45° under ASTM D2457. For the D252/257 family, a frost-line height increase of 200 mm generally raises haze by 1–2 percentage points and lowers gloss by 5–10 units on a 38 µm monolayer film; these values are line-specific and should be reconfirmed before color-critical packaging is approved. Cast film lines running the same resin often report lower haze because chill-roll cooling produces a smaller crystalline morphology, but the difference is more pronounced at thicknesses above 50 µm.

    When oxygen transmission or seal initiation limits flexible package performance

    In flexible packaging structures where oxygen transmission rate is critical, D252/257 is not selected as the barrier layer. Linear low density polyethylene of this density class transmits oxygen at rates far above EVOH or nylon at equivalent thickness. Seal initiation is characterized on a gradient heat sealer under ASTM F2029. For monolayer films of D252/257, seal-bar temperatures below 115 °C generally produce incomplete fusion at 0.5 s dwell and 0.2 MPa jaw pressure; converters often set the sealing range between 120 °C and 150 °C to obtain seal strength above 10 N/25 mm under ASTM F88. Heat-seal strength is not solely a resin property; orientation, film gauge, and contamination at the seal surface influence the measured value more strongly than melt index differences across the D252/D257 flow range.

    Regulatory compliance matrix and waste-stream compatibility

    FrameworkStandard/ClauseRelevance for D252/257 film applications
    US food contact21 CFR 177.1520(c)Establishes olefin polymer status for food-contact articles when end-use extraction conditions are met.
    EU food contactRegulation (EU) No 10/2011Requires overall migration testing of the final film or package; specific migration limits apply to additives.
    United States PharmacopeiaUSP 661.1May apply to packaging systems for pharmaceutical dosage forms; suitability depends on extractables profile.
    Heavy metals in packagingDirective 2011/65/EU Annex IIRelevant only when packaging is integrated into electrical and electronic equipment; not a general film requirement.

    Compared with high-density polyethylene film resins having density above 0.941 g/cm³, D252/257 exhibits lower modulus and higher impact resistance. The lower crystallinity of the LLDPE family reduces yield stress but improves puncture resistance. A converter replacing HDPE with D252/257 in grocery sacks or can liners should reduce the die gap by 0.2–0.4 mm and lower the melt temperature by 10–15 °C to prevent bubble instability from the lower melt strength. This substitution also increases film extensibility, which can alter bag length control on form-fill-seal equipment unless the draw ratio is recalculated.

    On a 40-inch diameter blown film die with a 2.5:1 blow-up ratio, D252/257 runs without melt fracture when the die gap is maintained above 1.2 mm and melt temperature is between 199 °C and 216 °C. Gauge variation measured by a capacitance thickness scanner remains below ±4% at net output above 15 kg/h per linear die inch; below 10 kg/h, the melt curtain can sag and produce thickness bands. The observed failure mode on that line geometry is not melt fracture but periodic gauge bands associated with insufficient melt stiffness. The same mechanism can appear on cast film lines if the air gap exceeds 50 mm at low take-off speed.

    Why does D252/257 retain dart impact better than some commodity LLDPE films?

    Solid-state impact resistance is governed by tie-molecule concentration, spherulite size, and the distribution of short-chain branches. Resins with a more uniform short-chain branch spacing exhibit a more homogeneous crystal network, which delays crack propagation under ASTM D1709. In comparative tests at 25 µm, the D252/257 family typically shows higher dart impact than a 0.918 g/cm³ butene LLDPE at equivalent melt flow; the difference narrows when films are run at high frost-line heights above 12 die diameters because orientation effects dominate. The producer’s published data for the D257 designation indicates a lower melt index than D252, which tends to raise impact and lower extrusion output; converters balance this by increasing screw speed within the thermal limit specified for the stabilizer system.

    Processing of D252/257 is not recommended at melt temperatures above 232 °C for residence times beyond 5 min, as oxidative degradation depletes the phenolic stabilizer package and raises melt flow beyond the original specification, producing a loss of dart impact in the net film. The resin is not hydroscopic, but storage in conditions above 60% relative humidity can retain surface moisture and lead to bubble instability when reclaim is introduced without drying. Acid-functional copolymers such as ethylene acrylic acid should be purged from the die before extrusion of D252/257, because residual acid groups accelerate degradation at LLDPE processing temperatures and can create black specks after 30–60 min of contact time.