Chevron Phillips Marlex D174 Polyethylene Film Grade Lldpe Hexene Copolymer

Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer

    • Product Name: Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 821017
    Productname Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Hexene
    Form Pellets
    Density 0.918 g/cm³
    Meltindex 0.90 g/10 min
    Meltingpoint 120 °C
    Vicatsofteningpoint 93 °C
    Tensilestrengthatyieldmd 1500 psi
    Tensilestrengthatbreakmd 5100 psi
    Tensilestrengthatbreaktd 4500 psi
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Dartdropimpact 120 g
    Elmendorftearmd 300 g
    Elmendorfteartd 500 g
    Haze 12%
    Gloss45 55%
    Coefficientoffriction 0.15

    As an accredited Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene-lined bags, palletized and stretch-wrapped; available in 1,000 kg quantities for safe transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading: Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer, palletized 25-kg bags, securely stowed for export.
    Shipping Chevron Phillips Marlex® D174 LLDPE is shipped as non-hazardous, odorless polyethylene pellets in 25 kg polyethylene-lined bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Store away from heat, moisture, and contamination. Keep packaging closed until use; follow manufacturer’s handling instructions. Not regulated for transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers/packaging closed and off the floor on pallets. Avoid moisture, dust, and contamination; separate from strong oxidizers. Maintain ambient temperatures and follow first-in, first-out stock rotation. Protect from prolonged UV exposure and physical damage. Use clean handling equipment to prevent cross-contamination.
    Shelf Life Typically 24 months from manufacture when stored in original unopened packaging, cool and dry below 50°C, away from direct sunlight.
    Application of Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer

    Chevron Phillips Marlex® D174 is a hexene-copolymer linear low-density polyethylene film resin supplied for blown and cast film conversion routes where the finished web must balance dart impact, tear propagation resistance, draw extensibility, and heat-seal response. The following downstream segments are limited to established polyolefin film applications: food-contact blown film, cast pallet stretch film, heavy-duty industrial sacks and FIBC liners, extrusion lamination sealant webs, and agricultural silage bale wrap. Functional additive loadings are stated as weight percent of an as-supplied masterbatch unless an active concentration is explicitly identified; all addition ratios are starting-point industrial formulations and must be re-validated on the specific monolayer or coextrusion line because screw design, die gap, cooling capacity, and downstream stretching history shift the practical balance between film optics, coefficient of friction, seal performance, and dart impact.

    What Separates a Stable Frost Line From a Melt-Fracture Episode in Food-Grade Blown Film?

    In food-contact blown film for frozen vegetable pouches, dry-mix liners, and institutional ice bags, Marlex® D174 is converted on mono- and three-layer blown film lines with extruders of 30:1 L/D or greater, barrier screws, and spiral mandrel dies. A typical monolayer formulation uses a 20 wt% active precipitated silica antiblock masterbatch at 1.5–3.0 wt%, a 5 wt% active erucamide slip masterbatch at 0.8–1.5 wt%, and a 3 wt% active fluoroelastomer processing aid masterbatch at 0.4–0.8 wt%. The resulting film is conditioned at 23 °C and 50% RH for 24 h; coefficient of friction is measured under ASTM D1894-14, and values above 0.20 on the sealant side indicate that erucamide bloom is insufficient or that the slip masterbatch carrier resin is incompatible. For frozen-food seal layers, 10–20 wt% of an LDPE homopolymer or lower-density metallocene LLDPE is incorporated to lower seal initiation to the 95–105 °C range when tested on a hot-tack instrument under ASTM F1921-12. Process aid addition is not merely a surface-quality adjustment; at die shear stress above approximately 200 kPa, unmodified hexene-copolymer LLDPE exhibits sharkskin melt fracture on the outer film surface, and the fluoroelastomer PPA at the specified loading displaces the onset of melt fracture by conditioning the die lip and reducing local shear stress.

    Food-contact compliance rests on U.S. FDA 21 CFR 177.1520(c) for olefin polymers, Commission Regulation (EU) No 10/2011 Annex I with an overall migration limit of 10 mg/dm², and GB 4806.7-2016 for polyethylene food-contact materials in China; converters must verify that all masterbatch carrier resins and migratory additives carry equivalent food-contact declarations before the finished film is placed on the market. The blown film die gap is held at 1.8–2.2 mm for finished film between 40 µm and 75 µm; blow-up ratio is set at 2.2–2.8, and frost line height is maintained between 250 mm and 450 mm above the die. Melt temperature measured in the adapter is controlled at 198–220 °C, internal bubble cooling air exchange is held at 15–25%, and dual-lip air ring pressure is set between 4 mbar and 8 mbar. Attempts to run blow-up ratios above 3.0 without increasing air-ring flare produced bubble flapping, visible gauge bands in the haul-off, and gauge variation of 4–8%; this upper boundary is a consequence of the lower melt tension of hexene-copolymer LLDPE relative to high-pressure LDPE, and it is not overcome by raising melt temperature alone because elevated stock temperature further reduces melt strength.

    The extruded web is corona-treated to 38–42 dyn/cm for reverse printing or adhesive lamination, then slit into pillow pouches, side-seal bags, gusseted freezer bags, and wicket bags for dry-food operations. Terminal products include 40–75 µm frozen vegetable pouches, dry-mix liners, and institutional ice bags in which the critical film attributes are dart impact resistance, low coefficient of friction for automated bag insertion, and consistent heat-seal response across packaging line speeds of 30–80 bags/min.

    At cast-film line speeds above 600 m/min, Marlex® D174 functions as the core and skin resin in pallet unitization stretch film, blended with 10–30 wt% of a metallocene or octene-LLDPE to suppress draw resonance in the air gap. A 20 wt% active polyisobutylene cling masterbatch is introduced into the skin extruder at 1.0–3.0 wt%, resulting in 0.2–0.6 wt% active PIB in the finished film; below 1.0 wt% skin-layer masterbatch, peel cling under ASTM D5458-95 falls below the level required for high-speed palletizing, while above 3.0 wt% PIB transfer to pallet decks and blocking in warm warehouses become recurrent field complaints. Where the wrap contacts food in secondary packaging, compliance with EU Regulation (EU) No 10/2011 is required only for direct food-contact layers; industrial pallet wrap is otherwise assessed under REACH and the converter’s internal packaging waste compliance program.

    The film is produced on five-layer cast lines with extruders of 30:1 L/D, screen packs at 30/60/100 mesh, melt temperatures of 235–250 °C at the feedblock, and a die gap of 0.6–1.0 mm. Air gap is maintained at 40–80 mm before a matte-finished chill roll at 18–24 °C; finished thickness is 15–30 µm. Tensile properties are tested under ASTM D882-18, peel cling under ASTM D5458-95, puncture propagation resistance under ASTM D5748-95(2019), and stretch force characteristics under ASTM D4649-20. On a high-speed pallet wrapper applying 200–300% pre-stretch, the film must retain at least 85% of its clamped width during elongation; neck-down above 15% causes edge failure at pallet corners. Terminal products include 15–23 µm hand stretch film, 20–30 µm machine stretch film, and tinted or printed pallet wrap used for load identification and tamper evidence.

    Heavy-Duty Sacks and FIBC Liners at 180 µm: Gauge Uniformity, Dart Impact, and Seal Integrity

    Published data for D174 in FIBC liner configurations is limited; the following ratios are starting-point formulations derived from polyolefin film extrusion practice rather than resin-supplier certifications. For dry bulk packaging of hygroscopic powders, construction chemicals, and resin pellets, D174 is used in three-layer blown film structures at total thickness 120–200 µm. The core layer contains 60–80 wt% D174, 20–40 wt% high-pressure LDPE for bubble stability, and 2.5–4.0 wt% of a 40 wt% carbon black masterbatch when outdoor storage or ultraviolet exposure is expected. The skin layers may include a 20 wt% antiblock masterbatch at 1.5–2.5 wt% to prevent blocking on the gusseted roll. Gravimetric hopper loading is preferred; volumetric dosing below 3% additive loading has produced coefficient-of-variation shifts above 5% in dart impact on production sacks.

    Mechanical acceptance is evaluated against ASTM D1709-15 dart drop for 180 µm film, ASTM D882-18 tensile properties, ASTM D1922-15 Elmendorf tear resistance, and ISO 21898:2020 for flexible intermediate bulk containers for non-dangerous goods when the liner is integrated into an FIBC. If the sack is used as an inner liner in UN-certified packagings, the complete package is tested under UN Model Regulations Chapter 6.5, not the film alone; the film supplier’s data cannot be used to infer UN performance level. Extrusion uses a triple-layer line with 350–600 mm spiral mandrel die, die gap 2.0–2.5 mm, blow-up ratio 1.8–2.2, and frost line height 350–550 mm above the die. Melt temperatures are set to 200–225 °C in the core and 195–215 °C in the skins. Inline gusseting, perforation, and surface printing run at 60–120 m/min; gauge variation across the collapsed bubble is maintained below ±6% because off-spec gauge in the crease region is the primary cause of split sacks during drop loading.

    Terminal products include block-bottom valve sacks, open-mouth sacks, pinch-bottom sacks, and FIBC liners for hygroscopic powders; the finished sack structure is specified by filled-sack drop impact performance on the converter’s drop-test rig rather than by film tensile data alone.

    Extrusion lamination of biaxially oriented polyester, biaxially oriented polypropylene, and aluminum foil to produce dry-food and frozen-food laminates uses Marlex® D174 as the sealant web at coating weights of 18–25 g/m². In this operation, 10–20 wt% of an autoclave LDPE is added to D174 to reduce neck-in and edge-bead formation, and a polyolefin antioxidant masterbatch is incorporated at 0.3–0.6 wt% if the coated structure is intended for long-laminate inventory or high-temperature drying. Maleic anhydride tie layers are not required when the sealant is joined to ethylene-based primers or corona-treated foil; adhesion to polyester and foil is improved by ozone treatment of the melt curtain and by maintaining the substrate surface treatment above 42 dyn/cm.

    The sealant layer must comply with U.S. FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm², and GB 4806.7-2016 for food-contact polyethylene. Process conditions on the coater are set to melt temperature 295–315 °C at the die, die gap 0.5–0.8 mm, air gap 150–250 mm, and chill roll temperature 15–20 °C; line speed is limited by draw resonance and is typically 120–250 m/min. Neck-in is measured before the metal edge bead slitter; when the air gap exceeds 200 mm, neck-in above 25 mm/side produces a non-coatable edge band, and the converter must either increase LDPE content or decrease melt temperature within the specified window. Terminal products include stand-up pouch sealant webs, four-side-seal sachet laminates, and tube laminates for dry mix and frozen food applications, where the D174 sealant layer provides the heat-seal interface against polyolefin inner surfaces.

    When Bale Wrap Must Hold 60% Pre-Stretch Without Tear Propagation in the Field

    Agricultural silage bale wrap manufactured from Marlex® D174 is a five-layer cast film in which the two outer skins carry the cling function and the three internal layers provide puncture and tear resistance. A 20 wt% active PIB masterbatch is added to each skin extruder at 1.5–3.0 wt%, and a 60 wt% titanium dioxide white masterbatch is introduced at 4.0–7.5 wt% overall to reduce solar heat absorption. A UV stabilizer masterbatch containing hindered amine light stabilizers and a benzotriazole absorber is compounded at 0.8–1.5 wt%; films without this stabilizer package begin to show tensile elongation loss after 12 months of outdoor exposure, while stabilized film is qualified for 24–36 months field use according to EN 13207:2018.

    The cast line runs with 30:1 L/D extruders, melt temperatures 230–250 °C, die gap 0.8–1.2 mm, air gap 50–90 mm, and chill roll temperature 18–22 °C. Film thickness is controlled at 25–35 µm; on a round-bale wrapper applying 55–70% pre-stretch, the film must retain tear-propagation resistance after the outer layers have been thinned by stretching. PIB-rich skins above 3.0 wt% masterbatch cause dust adhesion in dry field conditions, and white masterbatch above 7.5 wt% reduces film toughness because inorganic loading dilutes the polymer matrix. Terminal products include black, white, and green round-bale silage wrap for 1.2–1.5 m diameter bales, supplied in 750 mm and 500 mm roll widths, and the film is not biodegradable; collection and disposal obligations under applicable agricultural plastic waste schemes remain with the end user.

    Free Quote

    Competitive Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® D174 Polyethylene Film Grade LLDPE Hexene Copolymer is a pelletized linear low-density polyethylene resin designated by the manufacturer as a hexene copolymer for blown film and cast film conversion. The nominal melt index is 1.0 g/10 min determined by ASTM D1238 at 190°C with a 2.16 kg load, and the nominal density is 0.918 g/cm³ determined by ASTM D1505. The polyethylene CAS registration is 9002-88-4. The resin is typically evaluated in film thicknesses from 12 µm to 125 µm, although the practical lower and upper gauge limits are controlled by die-gap uniformity, bubble cooling capacity, and downstream converting tension.

    These values are nominal targets rather than release limits. A converter should obtain the lot-specific certificate of analysis because additive package, melt-flow ratio, and density can vary within the manufacturer specification window. For incoming lot verification, a thermal analysis check may be run at 10°C/min under nitrogen according to ISO 11357-3. A broad melting endotherm between 100°C and 125°C with a peak melting temperature near 110°C to 115°C is characteristic of this density class; a shift greater than 2°C from the established lot average may indicate comonomer distribution drift or contamination.

    Why does comonomer selection alter the tear and impact balance measured on D174 film?

    Hexene incorporation produces butyl branches along the polyethylene backbone, whereas butene-copolymer LLDPE contains ethyl branches. The longer branches are less efficiently incorporated into the crystallites, creating a wider distribution of lamellar thickness and altering the number of tie molecules that connect adjacent crystallites. In film testing, this molecular difference can shift failure from brittle crack propagation toward ductile yielding. A direct comparison must be made at the same gauge, density, melt index, and extrusion orientation because melt draw and frost-line height influence molecular alignment.

    Laboratory conditions for film testing should follow ASTM D618 conditioning at 23°C ± 2°C and 50% ± 10% RH for 40 h. Dart impact is measured by ASTM D1709-15 Method A; Elmendorf tear is measured by ASTM D1922-15; puncture resistance is measured by ASTM D5748-19; tensile properties are measured by ASTM D882-18 at a jaw separation rate of 500 mm/min. Because D174-specific comonomer content is not disclosed on the public data sheet, absolute property values must be generated on production film rather than inferred from resin density alone.

    PropertyTest methodNominal value
    Melt indexASTM D12381.0 g/10 min at 190°C/2.16 kg
    DensityASTM D15050.918 g/cm³
    ComonomerManufacturer designationHexene

    On a conventional air-cooled blown film line equipped with a 63.5 mm single-screw extruder with a 30:1 L/D ratio and a barrier screw, D174 is normally processed with a barrel temperature profile from 180°C at the feed throat to 220°C at the die. The die gap is typically set between 1.5 mm and 2.5 mm. A wider gap increases melt residence time and can reduce gel formation risk, while a narrower gap reduces melt strength and may destabilize the bubble at high blow-up ratios. Operators commonly run a blow-up ratio of 2.0:1 to 3.5:1 with a frost-line height of 250 mm to 600 mm. Published data for D174-specific bubble stability limits across all die geometries is limited, so these ranges should be taken as starting points on a monolayer line of similar geometry.

    Because linear low-density polyethylene has a steeper shear-viscosity curve than long-chain-branched LDPE at the same melt index, screw drive current and melt pressure should be monitored carefully. At a shear rate near 100 s⁻¹, generic LLDPE of 0.918 g/cm³ density may generate apparent viscosity values between 300 Pa·s and 800 Pa·s at 190°C; D174-specific pressure-drop calculations should use the lot melt-flow data. A screen pack with 60/80/100 mesh may be used to maintain melt-compression and trap contaminants, but the resulting pressure increase must remain below the extruder barrel pressure limit.

    When D174 is used as a drop-in replacement for a C4 LLDPE on high-output blown film equipment

    Direct replacement is not automatic. A C4 grade may have a different molecular weight distribution and catalyst package, so switching to D174 can change the crystallization rate and bubble cooling demand. On short-stalk lines, a drop-in change may produce bubble sagging or helical instability. In such cases, output may need to be reduced by 5% to 15% until the frost-line position is re-established. The melt temperature should not be raised above 220°C without verification of the stabilizer package, because oxidative degradation accelerates above 220°C, increasing melt-pressure fluctuation and gel defects. Gel defects can be inspected according to ASTM D7310-20.

    If bubble stability is insufficient, high-pressure LDPE may be blended in the range of 5 wt% to 20 wt%. This addition improves bubble stability but generally lowers tear resistance measured by ASTM D1922. A converter should compare at least 0 wt%, 10 wt%, and 20 wt% LDPE fractions at film gauges of 25 µm and 50 µm, using ASTM D1709, ASTM D1922, ASTM D1003 for haze, and ASTM F88/F88M-21 for seal strength. The optimum LDPE fraction is the level that satisfies the minimum machine-direction tear, seal strength, and bubble stability requirements.

    When a line shutdown occurs with molten resin in the barrel, residence time above 220°C should not exceed 10 min. Longer residence may generate low-molecular-weight species that alter organoleptic properties in food packaging. The extruder should be purged with a low-viscosity polyethylene such as a 2.0 g/10 min LDPE until the discharge is clear. The screen pack should then be inspected for gel content and metal contamination.

    Compared with metallocene-catalyzed LLDPE grades of similar density, D174 generally occupies a broader processing window. Metallocene grades can show lower melt strength and require more LDPE addition on older air-cooled lines, while D174 may maintain a stable bubble at lower LDPE fractions. However, the exact molecular weight distribution of D174 is not published on the standard technical data sheet. The comparative processing window should therefore be evaluated on the target line rather than assumed from nominal melt index and density.

    In non-food applications such as agricultural silage covers, temporary construction films, and industrial can liners, film qualification is usually based on total thickness, dart impact by ASTM D1709, Elmendorf tear by ASTM D1922, tensile strength at break by ASTM D882, and puncture resistance by ASTM D5748. A qualification run should collect roll sets from the start, middle, and end of the extrusion campaign to capture lot-to-lot variability. On a converting bag line, the film coefficient of friction and slip-agent distribution affect seal-bar tracking and bag-opening force; these values should be measured according to ASTM D1894. If the slip package is changed, the coefficient of friction can shift from 0.10 to 0.40, altering the settings required for feed rollers and sealing jaws.

    Optical properties are measured on production film, not resin pellets. Haze is evaluated by ASTM D1003-21, and gloss is evaluated by ASTM D2457-21 at a 45° angle. For clear food-contact films, a haze below 10% and a 45° gloss above 60 gloss units are common targets; however, the actual values are controlled by die gap, frost-line height, and the slip and antiblock additive package. Blending with high-pressure LDPE in the range of 5 wt% to 20 wt% may reduce clarity by increasing surface haze and lowering gloss. These trade-offs should be evaluated at the production frost-line setting using film samples collected from the same location on the bubble circumference.

    For cast film lines, D174 can be processed on a 90 mm extruder with a slot die and chill-roll temperatures between 15°C and 30°C. Cast film typically produces lower machine-direction orientation and better optical uniformity than blown film, but tear balance is more isotropic. In a cast-film structure, the draw ratio between die and chill roll controls the final gauge; the line speed may be set to produce a thickness of 20 µm to 80 µm. Neck-in and edge bead formation should be monitored because high draw can create thickness nonuniformity outside a ±5% gauge variation target. Published D174-specific cast-film data is limited; starting conditions should be developed with a design-of-experiments approach that varies melt temperature, line speed, and chill-roll temperature.

    In coextruded barrier structures, D174 may serve as a seal-layer component because the lower density and hexene comonomer can depress seal initiation temperature relative to a high-density polyethylene seal layer. The interlayer adhesion between the seal layer and the core must be measured with a peel or shear method; if the structure fails at the interlayer before the seal peels, the coextrusion temperature profile is insufficient. A die temperature of 220°C is often used, but the actual interfacial melt temperature depends on the entire adapter and die history. Processing aids may be required to reduce surface melt fracture when the seal layer is coextruded with a high-viscosity core at a viscosity ratio exceeding 1:3.

    Field failures in heavy-duty sacks and agricultural films are usually tear propagation failures rather than tensile yield failures. A film with high tensile strength at break may still split easily if the Elmendorf tear value is low. The tear balance between machine direction and transverse direction is controlled by the bubble geometry. A high blow-up ratio increases transverse orientation and may increase machine-direction tear; a low blow-up ratio has the opposite effect. The frost-line height further modifies the orientation state. The converter should record blow-up ratio, die gap, frost-line height, and output when correlating laboratory tear data with field performance.

    Seal initiation, hot-tack, and vertical form-fill-seal rate limits

    On vertical form-fill-seal lines, D174 films are sealed at jaw temperatures typically between 120°C and 150°C, but seal initiation is affected by film thickness, contact time, and clamping pressure. Hot-tack strength is measured by ASTM F1921-18; final seal strength is measured by ASTM F88/F88M-21. Technical literature indicates that hexene grades can provide a wider hot-tack window than C4 grades under equivalent thermal load; however, published D174-specific hot-tack curves across different mono- and coextruded structures are limited. Each converter must generate hot-tack data at the exact film gauge and line speed used in production.

    For packages sealed at high speed, the hot-tack force must be sufficient to hold the product weight before the seal solidifies. A minimum hot-tack value should be defined in newtons per 25 mm width using ASTM F1921-18; if the measured value drops below the specified minimum, the jaw temperature or dwell time must be adjusted without exceeding the film thermal stability limit.

    Residual surface moisture in bulk-truck transfers produces steam-induced bubble defects

    Although polyethylene does not undergo hydrolytic degradation, surface moisture from outdoor silo storage or bulk-truck transfer can produce steam bubbles in blown film. If condensation is visible, the resin can be dried for 2 h to 4 h at 70°C to 80°C with a desiccant dryer having a dew point of -40°C. Higher drying temperatures are not recommended because pellet softening can lead to agglomeration in the hopper. Transfer lines should be cleaned to prevent cross-contamination with polypropylene, which melts at a higher temperature and can form unmelted domains in the film. Metal detection upstream of the extruder should be used, and the screen pack should be examined after every silo change.

    Regulatory compliance is end-use specific. Polyethylene film resins are generally covered under FDA 21 CFR 177.1520, but the clearance is not a finished-film approval. The converter must confirm that the final film meets extractable fraction limits and intended-use temperature conditions in 21 CFR 177.1520(c). In the European Union, plastic food-contact materials must comply with EU Regulation 10/2011, including overall migration limits and specific migration limits. A supplier regulatory statement is not a substitute for validation of the final package.

    JurisdictionRegulationConverter verification burden
    United StatesFDA 21 CFR 177.1520Extractable fraction limits; intended-use temperature
    European UnionEU Regulation 10/2011Overall migration limit 10 mg/dm²; specific migration limits
    REACHEC 1907/2006Monomer/polymer registration and exemption verification

    For fat-containing food simulants, migration testing must be performed using the assigned simulant in EU Regulation 10/2011. Dry-film non-food applications such as geomembrane temporary covers may instead be specified by ASTM D882 tensile properties, ASTM D1709 impact, and ASTM D5748 puncture. Lot-specific certificates of analysis and processing records should be retained for traceability.

    Top