| HS Code | 622916 |
| Productname | Chevron Phillips Marlex D173 Film Grade LLDPE |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
| Density | 0.923 g/cm3 |
| Meltindex | 1.0 g/10 min |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 100 °C |
| Brittlenesstemperature | < -70 °C |
| Tensilestrengthatyield | 11 MPa |
| Tensilestrengthatbreak | 30 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 240 MPa |
| Dartdropimpact | 120 g |
| Elmendorftearmd | 250 g |
| Elmendorfteartd | 400 g |
| Haze | 10% |
| Gloss45 | 70% |
| Coefficientoffriction | 0.20 |
As an accredited Chevron Phillips Marlex® D173 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® D173 Film Grade LLDPE comes in 25 kg polyethylene-lined bags, palletized, with 1,000 kg bulk bags available. |
| Container Loading (20′ FCL) | Chevron Phillips Marlex D173 film-grade LLDPE in 20′ FCL: 25 kg bags, palletized, approx. 24–25 MT net, dry container, secured. |
| Shipping | Marlex D173 Film Grade LLDPE is shipped as non-hazardous resin pellets in moisture-barrier 25 kg bags, 500–1000 kg bulk bags, or bulk truck/rail hopper cars. Store dry and cool, away from heat, sunlight, punctures, and contamination. Follow supplier SDS and local transport regulations. |
| Storage | Store Chevron Phillips Marlex® D173 Film Grade LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, palletized off the floor, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Follow first-in, first-out stock rotation. Maintain ambient temperature; protect from weather and mechanical damage. |
| Shelf Life | Shelf life is typically 24 months when stored in unopened original packaging in a cool, dry, well-ventilated area away from heat and sunlight. |
Marlex D173 is a film-grade linear low density polyethylene with a nominal density of 0.917 g/cm³ per ASTM D1505 and a melt index of 1.0 g/10 min at 190°C/2.16 kg per ASTM D1238. In single-screw extrusion, barrier screws with 24:1 to 30:1 L/D are preferred because the resin’s molecular weight distribution can raise melt pressure at screw speeds below 25 rpm. Pre-drying is generally not required when silo and hopper moisture remain below 50% RH, but hopper dryers set at 60°C to 70°C should be used if condensation risk exists above 70% RH. Cast film conversion typically imposes melt temperatures of 220°C to 250°C, whereas blown film lines operate more effectively at 185°C to 215°C to maintain bubble geometry. Gravimetric dosing is necessary when masterbatch density differs from the resin by more than 0.15 g/cm³ to prevent pellet segregation in the feed throat.
| Downstream segment | Primary compliance reference | Mechanical validation standard | Critical process boundary |
|---|---|---|---|
| Cast stretch film | Directive 94/62/EC | ASTM D1709-A | Melt temperature ≤ 260°C |
| Frozen food packaging | 21 CFR 177.1520(c)(3.2a); EU 10/2011 | ASTM F88/F88M; ASTM F1921 | Frost line height 5 to 8 die diameters |
| Silage film | EN 13207:2018 | ISO 527-3; ISO 6383-2; ISO 7765-2 | Blow-up ratio 2.4:1 to 3.2:1 |
| Heavy-duty sacks | 94/62/EC; 21 CFR 177.1520(c) if food contact | ASTM D1709-A; ASTM D1922 | Screen changer 80 mesh above 5 wt% recyclate contamination |
| Lamination sealant web | 21 CFR 177.1520; EU 10/2011 | ASTM F1921; ASTM F904 | Melt temperature 230°C to 245°C |
| Refuse sacks and liners | 94/62/EC | ISO 527-3; ASTM D5748 | Gauge variation ≤ ±5% |
On a three-layer cast stretch film line, D173 is typically assigned to the core layer at 60 wt% to 75 wt% of total mass flow, with the cling skin composed of a metallocene LLDPE and 2 wt% to 5 wt% polyisobutylene masterbatch, while the release skin carries 0.5 wt% to 1.2 wt% erucamide slip and 1000 ppm to 3000 ppm silica antiblock. The die gap is set at 0.5 mm to 0.8 mm because D173 exhibits less neck-in than butene-based LLDPE at equivalent melt temperature. Melt temperature at the feedblock is held at 235°C to 245°C. The chill roll temperature is maintained at 18°C to 22°C with an air knife positioned to quench the web within 5 mm to 10 mm of the die exit. Line speed is typically 250 m/min to 600 m/min, producing final film thicknesses from 10 µm to 20 µm. Operational boundary: increasing melt temperature above 260°C to improve clarity may volatilize low-molecular-weight fractions and increase die-lip build-up rates; chill roll temperatures above 25°C reduce pre-stretch retention. Industrial pallet wrap is not placed in direct food contact, but it falls under the European Packaging and Packaging Waste Directive 94/62/EC with a maximum total concentration of lead, cadmium, mercury, and hexavalent chromium below 100 ppm. Terminal products include 12 µm to 23 µm machine-grade pallet wrap and 8 µm to 10 µm hand-applied wrap after down-gauging. Dart impact after pre-stretching should be validated in-line using ASTM D1709-A, because published data for this specific configuration is limited.
Blown coextrusion for frozen vegetable, seafood, and bakery bags positions D173 in the sealant layer at 30 wt% to 45 wt% of total film mass, with the outer layer composed of HDPE or MDPE for abuse resistance and the core carrying a D173-rich blend to preserve interlayer adhesion. The sealant layer is dry-blended with 70 wt% D173, 20 wt% metallocene LLDPE, and 10 wt% LDPE to shift the seal initiation temperature below 110°C on jaw sealers with 0.3 s to 0.5 s dwell time. Die gap is set at 1.8 mm to 2.2 mm. Blow-up ratio is maintained at 2.2:1 to 2.8:1, and frost line height is held at 5 to 8 die diameters to stabilize the bubble without excessive machine-direction orientation. Melt temperature is 190°C to 205°C. Layer distribution is verified by transmission IR rather than weight-based calculation, because the melt density difference between HDPE and D173 can distort layer ratio estimates. Compliance for direct food contact is governed by 21 CFR 177.1520(c)(3.2a) for olefin polymers, and by Regulation EU 10/2011 with an overall migration limit of 10 mg/dm² under simulant D2 for frozen aqueous foods. Terminal films range from 40 µm to 80 µm, and bags are filled at −20°C to −30°C. The seal strength after freezer storage should be checked by ASTM F88/F88M at an initial peel speed of 300 mm/min, because cold-temperature crystallization can reduce interfacial seal strength if the film is quenched too rapidly; published data for this specific configuration is limited.
For silage bale wrap and clamp sheet, D173 is compounded with a HALS/benzotriazole ultraviolet package at 0.4 wt% to 0.8 wt% total stabilizer, together with 2 wt% to 4 wt% rutile titanium dioxide masterbatch in the white skin of a white/black/white coextrusion. The black core uses 2 wt% to 3 wt% carbon black masterbatch to block ultraviolet penetration and suppress fungal growth on wet forage. In this configuration, D173 is used at 100 phr base resin in each layer, with the black core thickness at 20% to 30% of total thickness and the white skins equally divided. The blown film die gap is set at 1.4 mm to 2.0 mm, blow-up ratio at 2.4:1 to 3.2:1, and melt temperature at 190°C to 210°C. Frost line height is raised to 9 to 12 die diameters to reduce orientation and improve tear resistance, which matters when wrap is stretched around angled bale corners. Compliance is evaluated against EN 13207:2018 for silage films. Tensile yield and elongation are measured under ISO 527-3 at 500 mm/min, tear resistance under ISO 6383-2, and dart impact under ISO 7765-2. Terminal products include 50 µm to 75 µm white/black/white bale wrap and 150 µm pit cover sheets. Dispersion quality is checked by optical microscopy on cast film prints at 100× because local UV masterbatch depletion can produce photodegradation punctures after 12 months of outdoor exposure.
For heavy-duty industrial sacks loaded with polymer granules or mineral fillers, a monolayer blown film made from 70 wt% to 90 wt% D173 and 10 wt% to 30 wt% recycled LLDPE is run on a high-stalk bubble with a die gap of 2.0 mm to 2.5 mm. Blow-up ratio is kept at 2.0:1 to 2.5:1, and frost line height is raised to 10 to 12 die diameters to produce a balanced machine-direction and transverse-direction tear profile after bag sealing. Melt temperature is held at 185°C to 205°C; if the recycled fraction contains more than 5 wt% of mixed-film contamination, a screen changer with 80 mesh filtration is installed before the die to prevent gel streaks. The formulation includes 0.5 wt% to 1.0 wt% hindered phenol/phosphite antioxidant masterbatch and 2000 ppm to 5000 ppm silica antiblock, with slip additive limited to 500 ppm to 1000 ppm to avoid heat-seal strength loss on hot-bar sealers. Drop impact is evaluated under ASTM D1709-A, and tear resistance under ASTM D1922. Terminal products include 50 µm to 120 µm polymer granule sacks, mineral filler sacks, and industrial dust bags. When the sack is used to package food-grade raw materials, the inner layer must comply with 21 CFR 177.1520(c) and EU 10/2011; otherwise the application remains non-food industrial packaging under 94/62/EC.
D173 is used as a heat-seal web for dry-food and snack laminations when the structure is 12 µm PET adhesive-laminated to 7 µm aluminum foil followed by a 20 µm to 30 µm D173 sealant film. The sealant web is produced on a three-layer cast line with a die gap of 0.6 mm to 0.9 mm, chill roll temperature 18°C to 23°C, and melt temperature 230°C to 245°C. The layer formulation comprises 80 wt% to 90 wt% D173 and 10 wt% to 20 wt% metallocene plastomer to reduce seal initiation temperature for high-speed vertical form-fill-seal machines running at 80 to 140 bags/min. Slip and antiblock loadings are tuned to 800 ppm to 1200 ppm erucamide and 3000 ppm to 6000 ppm synthetic silica to maintain kinetic coefficient of friction below 0.25 on horizontal form-fill-seal guides. Hot-tack force is measured by ASTM F1921 at 120°C to 135°C seal bar temperature with 0.2 s dwell and 0.5 N/mm² sealing pressure. Lamination bond strength after solventless adhesive cure is tested under ASTM F904, and food-contact compliance is verified against 21 CFR 177.1520 and EU 10/2011 with an overall migration limit of 10 mg/dm². Terminal products include stand-up pouches for nuts, dried fruits, and confectionery, where the sealant layer must survive 30 mm drops at −5°C without longitudinal seal rupture. If the sealant web is run below 220°C melt temperature, melt curtain sag can disrupt gauge uniformity; above 250°C, die-lip build-up tends to increase after 4 h of continuous operation.
In municipal refuse and commercial can liner conversion, D173 is dry-blended with post-industrial recyclate at 60 wt% to 80 wt% and extruded on grooved-feed single-screw machines with 30:1 L/D at 180°C to 200°C. Die gap is set at 1.2 mm to 1.6 mm, blow-up ratio is 2.5:1 to 3.5:1, and frost line height is maintained at 4 to 6 die diameters to preserve the higher machine-direction modulus required for bottom-seal packaging lines. The formulation includes 0.5 wt% to 2.0 wt% zeolite or silica antiblock and 500 ppm to 1200 ppm slip masterbatch. Film gauge is monitored in-line via capacitive sensors because variations greater than ±5% cause roll deformation in high-speed converter unwind stands. Melt pressure at the screen changer is limited to 350 bar to prevent excessive shear heating, and if pressure exceeds this boundary, the recycled fraction is reduced by 5 wt% increments. Tensile properties are checked by ISO 527-3 at 100 mm/min, and puncture resistance by ASTM D5748 or equivalent. Terminal products include 30 L to 120 L refuse sacks and 20 L to 40 L can liners for commercial kitchens.
Competitive Chevron Phillips Marlex® D173 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® D173 Film Grade LLDPE is a linear low-density polyethylene resin intended for blown film and cast film conversion in which gauge reduction, tear resistance, and controlled processability are specified. The grade is released against a nominal density of 0.918 g/cm³ measured by ASTM D1505 and a nominal melt index of 1.0 g/10 min at 190 °C under a 2.16 kg load determined by ASTM D1238. These values align with film extrusion rather than injection molding, blow molding, or rotational molding. Because the lot release specification may differ from promotional literature, conversion parameters must be verified against the certificate of analysis issued for the specific batch.
From a molecular perspective, D173 is a linear low-density polyethylene produced by low-pressure catalytic polymerization. Unlike high-pressure tubular or autoclave LDPE, which contains long-chain branches and a broadened molecular weight distribution, the linear architecture of D173 has a less shear-thinning melt. This characteristic is measured indirectly by melt flow ratio from ASTM D1238 conditions such as 190 °C/21.6 kg versus 190 °C/2.16 kg, although the manufacturer may report that ratio only in the technical bulletin. The consequence is that a direct substitution into an LDPE-designed screw running at high screw speed may increase die pressure and backflow in the feed section. Grooved-feed extruders with L/D ratios above 24:1 are commonly used for this class of material.
For film property development, monolayer blown film is typically evaluated at 25 µm thickness after conditioning at 23 °C and 50 % relative humidity according to ASTM D618 or ISO 291. The linear low-density backbone yields a more uniform yielding region than LDPE at equivalent density, but the measured dart impact under ASTM D1709 Method A remains highly sensitive to gauge uniformity, frost-line height, and oscillation-induced thinning. In Elmendorf tear testing under ASTM D1922, machine-direction and transverse-direction values are not equivalent because the bubble induces preferential chain orientation. Transverse-direction tear values are typically higher than machine-direction values after the film is oriented. Published data for this specific configuration is limited; film properties must be taken from the manufacturer’s grade-specific data sheet at the intended gauge and blow-up ratio rather than interpolated from resin pellet data.
| Test function | Standard designation | Reported or reference value | Unit |
|---|---|---|---|
| Density, compression-molded or pellet | ASTM D1505 | 0.918 | g/cm³ |
| Melt index, 190 °C/2.16 kg | ASTM D1238 | 1.0 | g/10 min |
| Film tensile yield strength | ASTM D882 | gauge-dependent | MPa |
| Elmendorf tear | ASTM D1922 | orientation-dependent | g/25 µm |
| Dart impact | ASTM D1709 | gauge-dependent | g |
| Haze and light transmittance | ASTM D1003 | gauge- and screw-dependent | % |
Thermal characterization of D173 by differential scanning calorimetry under ISO 11357-3 typically identifies a crystalline melting peak in the 120–125 °C range for LLDPE of this density. This is a technique-dependent value, not a processing setpoint. For converters, the melting peak is less relevant than the melt temperature measured at the die and the cooling rate of the bubble. On a 50 mm extruder with L/D 24:1, barrel temperatures from 160 °C to 190 °C are typical for this melt-index class, while die temperatures are held above 190 °C to limit excessive die pressure and surface defects.
Production-scale blown film lines processing D173 at melt temperatures below 200 °C can exhibit sharkskin melt fracture if the die gap is narrower than 1.0 mm and the output rate exceeds the critical shear stress for the resin. The critical shear stress under ASTM D3835 capillary rheometry at 190 °C is not a fixed material property for LLDPE film resins; it shifts with die geometry, melt temperature, and additive package, especially when polymer processing aids or fluoroelastomer-based additives are present. The onset of melt fracture is therefore not controlled by melt index alone. A converter operating a 65 mm grooved-feed extruder with L/D 27:1, a 150 mm spiral mandrel die, and a die gap between 1.5 mm and 2.0 mm often observes improved surface finish at melt temperatures of 193–210 °C, but the exact barrel profile must be validated on the line because screw wear, die lip quality, and air ring condition affect the result.
The same linear architecture that limits shear thinning also affects bubble stability in high-stalk configurations. A high-stalk film tower with a stalk height above 4 die diameters may depress the frost line below the point where the molten tube achieves uniform strain. Under these conditions, bubble fluttering and asymmetric cooling stripes appear before complete collapse. Reducing the die gap to improve output can move the process toward melt fracture, while widening the die gap increases melt residence time and can reduce throughput. Processors therefore balance three competing constraints: die gap, frost-line height, and blow-up ratio. The optimum blow-up ratio for this grade is commonly reported in the supplier’s processing guide in the range of 2.0:1 to 3.0:1, with a frost-line height between 5 and 8 die diameters; however, line-specific variations require confirmation.
In monolayer food packaging, D173 is used for produce bags, freezer films, and carrier bags where a thickness reduction from 40 µm to 25 µm is specified without a proportional loss in impact resistance. The resin is also coextruded as a sealant layer in structures where heat-seal initiation is measured by ASTM F1921 and hot-tack strength is measured by ASTM F2029. Seal initiation temperatures for LLDPE film of this density class typically fall between 100 °C and 115 °C, but slip and antiblock additive packages shift this range. Organoleptic neutrality and migration must be confirmed under the intended food type and use conditions. In the United States, compliance is assessed against 21 CFR 177.1520; in the European Union, compliance is assessed against EU 10/2011 with relevant food simulants. These regulations do not automatically cover all food-contact structures; migration testing is required for fatty foods, high-temperature pasteurization, or prolonged shelf life.
Compared with high-pressure LDPE of identical density, D173 has lower melt tension under elongational flow because the linear chains do not exhibit the same degree of strain hardening as long-chain branched LDPE. This reduces bubble stability in certain high-stalk processes but improves drawdown in cast film and thin-gauge blown film. Relative to a butene-copolymer LLDPE of the same melt index, D173 is positioned in the Chevron Phillips product line as a differentiated film grade. If the grade is a higher-alpha-olefin copolymer, the tear and dart impact ratings at equivalent density and melt index differ from butene-based grades because branch length and distribution affect tie molecule concentration. The precise comonomer type and branching distribution should be clarified with the manufacturer’s technical bulletin, since not all LLDPE resins with 0.918 g/cm³ density and 1.0 g/10 min melt index produce the same film properties.
Operational boundaries include avoiding melt temperatures above 250 °C without verifying additive degradation, because slip and antiblock packages may plate out on the die lip or form deposits in the air ring. Pre-drying is generally unnecessary unless condensation has formed on cold pellets; surface moisture can generate bubbles or surface defects when the pellets are introduced into a hot blending area. Incompatibility with high-acid or high-peroxide purge compounds should be assessed before purging. Halogen-containing flame-retardant masterbatches are not typical for this film grade and may compromise food-contact status. Film gels are evaluated by internal lot qualification rather than by universal specification, because defect counts depend on film thickness, screw geometry, and filtration level.