| HS Code | 610151 |
| Product Name | Chevron Phillips Marlex® D170DK Polyethylene Film Grade LLDPE Hexene Copolymer |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene-1 |
| Density | 0.917 g/cm3 |
| Melt Index | 0.9 g/10 min (190°C/2.16 kg) |
| Melting Point | 123 °C |
| Vicat Softening Point | 94 °C |
| Tensile Strength At Break Md | 40 MPa |
| Tensile Strength At Break Td | 34 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 12% |
| Gloss 60 | 60 |
| Coefficient Of Friction | 0.2 |
| Low Temperature Brittleness | < -70 °C |
As an accredited Chevron Phillips Marlex® D170DK Polyethylene Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® D170DK Polyethylene Film Grade LLDPE Hexene Copolymer is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL: Marlex D170DK LLDPE in 25 kg bags, approx. 17 MT net, palletized, shrink-wrapped, securely loaded. |
| Shipping | Chevron Phillips Marlex® D170DK is a non-hazardous, solid LLDPE hexene copolymer resin shipped as pellets. Standard packaging: 25-kg polyethylene bags, palletized and stretch-wrapped, or bulk trucks/railcars. Not DOT/IMDG/IATA regulated. Store in a dry, cool area away from direct sunlight and ignition sources. |
| Storage | Store Chevron Phillips Marlex® D170DK in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers closed, safely palletized, and protected from moisture, dust, and contamination. Avoid strong oxidizers, prolonged UV exposure, and incompatible materials. Do not stack excessively. Follow local regulations, supplier SDS, and good housekeeping practices. |
| Shelf Life | No specific shelf life; stable under normal storage. Store cool, dry, well-ventilated, away from heat, sparks, and sunlight. |
Blown-film conversion of Marlex® D170DK is established on heavy-duty form-fill-seal sack lines where the film must survive drop loading, tear propagation, and low-temperature flexing without gauge extension at seal zones. The resin is characterized by a nominal density of 0.917 g/cm³ per ASTM D1505 and a nominal melt index of 0.75 g/10 min per ASTM D1238 at 190°C and 2.16 kg. On a 75 mm single-screw extruder with a 30:1 L/D barrier screw and Maddock mixing section, melt temperature measured at the adapter is typically held between 190°C and 210°C. The die gap is maintained at 2.0–2.5 mm because narrower gaps drive shear rate upward and may produce sharkskin melt fracture at screw speeds above 80 rpm. A spiral mandrel die with blow-up ratio of 2.5:1 to 3.0:1 is used for gusseted open-mouth sacks, and frost-line height is controlled at 6–8 die diameters to retain dart impact while limiting excessive machine-direction orientation. Film produced at 125–150 µm gauge is converted into polymer granulate and fertilizer sacks with seal-bar temperatures between 150°C and 170°C. Food-contact compliance is routinely declared under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 when the finished film contains only approved stabilizers and meets overall migration limits. Hexene comonomer distribution contributes to the tear and puncture performance required in this application; dart drop is measured by ASTM D1709, Elmendorf tear by ASTM D1922, and tensile properties by ASTM D882.
Cast stretch line trials with D170DK encounter a measurable process conflict because conventional cast stretch grades are formulated at melt indices between 2.0 g/10 min and 4.0 g/10 min for low melt pressure and stable draw at high line speed. The 0.75 g/10 min melt index of D170DK raises melt pressure in flat-die systems and increases motor load on 30:1 L/D extruders. Published data for this specific configuration is limited. Melt temperature must be raised to 220–240°C to reduce viscosity, but the upper limit is set at 250°C because prolonged residence time above that threshold initiates oxidation gel formation in the melt film. Chill roll temperature is maintained at 15–25°C with an air gap of 150–250 mm to control edge bead and film width. D170DK is inherently non-tack; cling is generated by adding a tackifier masterbatch, commonly an EVA or polyisobutylene-based system, at converter-validated dosages in the 1–3 wt% range. Formulation tolerance is narrow because excess tackifier reduces film modulus and blocks unwind, while insufficient tackifier fails pallet-load retention. Machine-direction stretch force is tested by ASTM D5459, and cling strength is measured by ASTM D5458. The lower melt index also limits cast draw stability. Edge bead formation becomes more pronounced when film thickness is below 15 µm, and bubble-breathing control used in blown stretch is not available because the cast process has no internal air pressure. Converters selecting D170DK for cast stretch should verify melt pressure and ampacity margins on the die and extruder before production.
Frozen-food film converters typically run D170DK in a three-layer coextrusion where the resin forms the core or outer layers, with a food-contact sealant skin. The hexene short-chain branching of this grade lowers the crystalline plateau compared with butene-copolymer LLDPE of equivalent density, which translates into improved low-temperature impact resistance. Film gauge for frozen vegetable, seafood, and meat packaging is generally between 30 µm and 75 µm. After conditioning at −30°C for 24 h, dart impact is measured by ASTM D1709; the specific value depends on layer thickness and frost-line settings, but hexene copolymer films typically retain a higher percentage of room-temperature dart impact than butene-copolymer films at the same density and melt index. The resin’s 0.917 g/cm³ nominal density provides flexibility at freezer temperatures without the low-modulus limpness of lower-density ethylene copolymers. Heat sealing is evaluated by ASTM F88/F88M at sealing temperatures between 120°C and 150°C. The hot-tack window is relevant for vertical form-fill-seal equipment where the filled pouch drops immediately after sealing. Compliance with FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 applies only when the finished structure uses food-approved tie layers and sealants. D170DK is not an organoleptic barrier; strongly odorous frozen products may require an additional barrier layer unless sensory evaluation under EN 1230-1 demonstrates pack compliance.
| Regulation or standard | Scope | Test method or clause | Typical limit |
|---|---|---|---|
| FDA 21 CFR | Olefin polymers for food contact | 177.1520(c) | Specified extractives by polymer type |
| Regulation (EU) No 10/2011 | Plastic food contact materials | Annex I | Overall migration < 10 mg/dm² |
| REACH | Substances of very high concern | EC 1907/2006 | SVHC < 0.1% w/w |
| RoHS Directive | Heavy-metal restrictions in electrical equipment | 2011/65/EU | Pb 1000 ppm, Cd 100 ppm, Hg 1000 ppm, Cr(VI) 1000 ppm |
In silage baling operations, D170DK is evaluated as a blown-film layer for wrap protection where puncture resistance during bale rotation and cling after stretching are the primary mechanical requirements. Typical film thickness is 25–50 µm, but D170DK alone does not provide an oxygen barrier comparable to EVOH or polyamide; oxygen transmission must be measured by ASTM D3985 for the final film structure. UV stabilization is mandatory for outdoor storage because the base resin contains no long-term UV inhibitor. A HALS stabilizer masterbatch is introduced at the converter’s validated let-down ratio, often in the 1–3 wt% range. The blown-film process uses a die gap of 1.8–2.5 mm, a blow-up ratio of 2.0:1 to 2.5:1, and melt temperatures between 190°C and 215°C to prevent thermal degradation of the UV additive. End-use puncture resistance is assessed by ASTM D5748, and tear resistance by ASTM D1922. The hexene comonomer reduces stress whitening in stretched film, but cling is formulated with a tackifier because D170DK has no inherent cling. Bale wrap exposed beyond one season to ultraviolet radiation must be evaluated for retained tensile and elongation per ASTM D882.
Industrial can liners are converted from D170DK on heavy-gauge blown-film lines producing film between 100 µm and 250 µm. The resin’s hexene copolymer architecture supports high environmental stress crack resistance, which is measured by ASTM D1693 and is required for liners holding solvent-contaminated solids or alkaline cleaning residues. Extrusion conditions include a die gap of 2.0–3.0 mm, a blow-up ratio of 2.0:1 to 2.5:1, and melt temperatures between 190°C and 220°C. Puncture resistance is evaluated by ASTM D5748, and tear resistance by ASTM D1922. The film is not inherently UV stable; outdoor service requires carbon black at 2.0–2.5 wt% dispersion, and the dispersion quality is checked by ISO 18553. Heavy-metal and SVHC restrictions are verified under REACH and, when applicable, local landfill and incineration permits. The absence of plasticizers and migratory slip additives in D170DK simplifies compliance with many waste-containment specifications, but converters must confirm that welding or side-gusset sealing temperatures do not exceed 230°C to prevent polymer degradation at the seal fold. Bags which are stacked outdoors must be tested after UV exposure because surface oxidation can reduce tensile at break and increase tear propagation.
Coextrusion of D170DK as a sealant layer requires melt temperature control between 200°C and 230°C because the 0.75 g/10 min melt index increases viscosity relative to high-MI sealant grades. The resin is used in sealant webs for heavy packaging laminates where seal strength and stiffness are prioritized over low-temperature sealing. Sealant layer thickness is typically 10–25 µm. Heat-seal initiation is measured by ASTM F2029, and hot-tack strength is measured by ASTM F1921. D170DK has a hot-tack plateau at sealing temperatures above 120°C in most coextruded structures, but specific seal initiation depends on the adjacent tie resin and substrate. Adhesion to EMA- and EBA-based tie layers is generally stronger than to acid-modified EVA systems; converter trials determine the precise peel failure mode. The resin is not recommended for high-speed packaging lines requiring seal initiation below 100°C. Coextruded films must be checked for interfacial gel formation because temperature overshoot above 250°C in the sealant layer can generate oxidized specks that produce weak seal regions. Film clarity is measured by ASTM D1003, and haze values depend on layer distribution and die-lip surface condition.
Competitive Chevron Phillips Marlex® D170DK Polyethylene Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical Marlex® D170DK is a linear low-density polyethylene film resin supplied as a 1-hexene copolymer for blown-film extrusion. Nominal lot-release properties include melt flow index 0.75 g/10 min measured under ASTM D1238 at 190 °C/2.16 kg, and solid-state density 0.917 g/cm³ measured under ASTM D1505. The resin is typically converted into heavy-duty shipping sacks, industrial liners, agricultural film, stretch-hood film, and frozen-food packaging where thickness reduction, tear propagation resistance, and low-temperature dart impact are controlled by ASTM D1922, ASTM D1709A, and ASTM D882. The product is supplied as free-flowing pellets and is not formulated as a ready-to-use film compound; slip, antiblock, and processing aid masterbatches are normally metered at the extruder throat to adjust coefficient of friction, blocking, and die lip buildup.
Single-point tensile, tear, haze, and dart values are not inherent resin constants; they are functions of film thickness, die gap, blow-up ratio, frost line height, and downstream cooling. The supplier’s certificate and blown-film datasheet provide nominal values for a defined film structure, but converter validation is required for specification writing. This is particularly relevant for ASTM D1922 Elmendorf tear and ASTM D1709A dart drop impact, which respond nonlinearly to comonomer type and melt orientation.
In ethylene copolymers, comonomer selection changes the short-chain branch identity and crystalline organization. Butene-based LLDPE introduces ethyl branches; hexene-based LLDPE introduces butyl branches. At equivalent density 0.917 g/cm³ and equivalent melt flow index, the longer butyl branch disrupts lamellar thickening more efficiently, increasing tie-chain probability between adjacent lamellae. Under Elmendorf tear testing per ASTM D1922, the resulting film usually shows higher fracture energy in both machine and transverse directions. Published comparative data for the hexene LLDPE product class commonly show machine-direction tear values 20–50% higher and dart drop impact values 15–30% higher than butene LLDPE at equivalent gauge and extrusion conditions. D170DK therefore enters applications where a butene-based resin fails tear specification or requires excessive thickness.
Octene LLDPE grades extend this effect by creating hexyl branches with greater tie-chain efficiency, and metallocene octene grades add narrow composition distribution that improves optical properties and reduces extractables. The trade-off appears in extrusion: metallocene LLDPE typically generates higher backpressure and lower melt extension viscosity than conventional hexene grades, which can destabilize the bubble on older low-output blown-film lines. D170DK differs from these products by retaining a broader molecular weight distribution and lower melt elasticity than LDPE, while providing better toughness than butene LLDPE without requiring the higher cost or higher torque often associated with metallocene octene grades. Comparative claims should be verified on the target line because die design, air ring, and collapse frame geometry affect final tear and impact balance.
Compared with LDPE, D170DK has a linear backbone without the long-chain branching distribution of autoclave LDPE. The absence of long-chain branching lowers melt strength and strain-hardening in extensional flow, which means the bubble is less forgiving under high blow-up ratios and high frost line conditions. However, the solid-state mechanical response is different: D170DK exhibits better dart impact and tear at equivalent gauge than general-purpose LDPE because the short-chain branches reduce large crystalline domains while retaining substantial elongation under ASTM D882. For applications requiring deep-draw thermoforming or high melt strength, LDPE is often blended with the LLDPE rather than replacing it.
On a production blown-film line built around a 45 mm single-screw extruder with a 24:1 L/D barrier screw and a 150 mm spiral mandrel die, D170DK is typically run at barrel temperatures from 177 °C in the feed zone to 204 °C at the adapter, with melt temperature maintained at 199–216 °C. Die gap is set between 1.5 mm and 2.5 mm. LLDPE melts exhibit less shear thinning and lower melt extension viscosity than LDPE; therefore a die gap that is too narrow at high output produces shark-skin melt fracture at the die lip. If surface melt fracture appears on the bubble, increasing the die gap to 2.5 mm or reducing screw speed is the standard corrective action. Blow-up ratio is normally controlled at 2.0:1–2.5:1. Frost line height is positioned at 3–5 die diameters. A frost line set too low increases quench-induced surface roughness and haze measured under ASTM D1003; a frost line set too high increases transverse direction shrinkage and makes the bubble sensitive to ambient air temperature fluctuations. Internal bubble cooling systems improve heat removal and permit higher throughput at equivalent frost line height, but they require stable air balance and close control of lower nip pressure to avoid stalk oscillation.
No predrying is required for moisture control because LLDPE is not hygroscopic. Condensation on cold pellet surfaces must nevertheless be avoided when pellets move from outdoor silos into a warm feed hopper, because surface water can destabilize feeding and create steam bubbles in the melt. A fluoropolymer processing aid masterbatch is used on some lines when high-output conditions cause die lip buildup; typical addition levels are 200–800 ppm of active polymer processing aid in the final film. The additive package must be verified for food-contact compliance under FDA 21 CFR 177.1520(c) if the finished film falls under that regulation.
Film blocking is controlled by antiblock masterbatch. Without antiblock, tack on wound rolls rises with storage temperature and unwind tension. Slip additives reduce coefficient of friction measured under ASTM D1894, typically targeting 0.10–0.30 for automated bag converting. The specific addition level depends on film gauge and storage time because migrating erucamide reaches the film surface over hours to days. Converters should qualify the coefficient of friction after aging because slip migration kinetics vary with film crystallinity, ambient temperature, and roll pressure.
Downgauging below 25 µm places D170DK film in a regime where minor thickness variation creates large local stress concentration effects. At 12–25 µm, the resin is commonly converted into heavy-duty shipping sacks and industrial liners. In this range, Elmendorf tear measured under ASTM D1922 and dart impact measured under ASTM D1709A are the limiting specifications because gels, die lines, or inconsistent frost line control produce notch-like defects. Extruders often compensate by raising blow-up ratio within the 2.0:1–2.5:1 range and shifting to a low-stalk bubble configuration to preserve machine-direction tear. Reducing thickness from 25 µm to 18 µm without adjusting frost line, air ring, or die gap usually decreases F50 dart impact by more than the linear gauge ratio because the molten film at the frost line is quenched faster and orientation is locked before complete lamellar reorganization. Published data for this specific gauge response on D170DK are limited; converter trials on the actual die and tower are required to establish the exact thickness-impact curve.
Frozen-food packaging lines require low-temperature dart impact validation at −20 °C rather than room temperature. The hexene comonomer generally improves low-temperature impact retention compared with butene LLDPE at equivalent density, but the final film must be tested under the converter’s own packaging specifications. Film structures containing recycled LLDPE or thermally degraded rework can lose low-temperature impact faster than virgin D170DK, and the rework addition level should be limited by lot-to-lot dart impact testing under ASTM D1709A.
The upper melt temperature limit is set by oxidative degradation and gel formation rather than by moisture-related hydrolysis. Sustained melt temperatures above 232 °C generate oxidized species and crosslinked gel particles that appear as visible defects in film and raise reject rates. Residence time in the adapter, melt pipe, and die should be minimized when operating near the upper limit; local hot spots and dead zones can produce batch-to-batch gel variation even when the barrel setpoint remains unchanged. The lower practical melt temperature is approximately 193 °C. Below that point, backpressure rises quickly and may exceed the drive-torque limit on shallow-groove feed extruders. The resin is not recommended for coextrusion with barrier polymers requiring melt temperatures above 260 °C unless the melt streams are thermally isolated and combined only in a feedblock with short residence time.
Operational incompatibilities include strong oxidizers and chlorinated hydrocarbons in the melt, which generate free radicals and accelerate degradation. If the film is intended for continuous exposure above 60 °C or for outdoor service, long-term oxidative stability should be confirmed by oxidative induction time testing under ASTM D3895 with an appropriate stabilization package. The resin should not be considered autoclavable at 121 °C without film property verification, because dimensional stability and seal strength are not guaranteed by the base material alone.
The resin is manufactured by Chevron Phillips Chemical and is typically supported by a food-contact compliance statement for olefin polymers under FDA 21 CFR 177.1520(c). For the European market, the converter must demonstrate conformity with EU Regulation 10/2011, including overall migration limit 10 mg/dm² or 60 mg/kg depending on the packaging form, and any specific migration limits for downstream additives. REACH registration is the responsibility of the legal entity importing the resin into the EU, and the current candidate list for SVHC should be checked before specification. The resin is not marketed as a medical-grade material; applications requiring USP Class VI or ISO 10993 should be cleared through the supplier and appropriate regulatory testing.
| Regulation or Standard | Designation | Scope or Property |
|---|---|---|
| FDA | 21 CFR 177.1520(c) | Olefin polymers for food-contact use |
| EU | Regulation 10/2011 | Plastic materials and articles in contact with food |
| ASTM | D1238 | Melt flow index, 190 °C/2.16 kg |
| ASTM | D1505 | Density by gradient column |
| ASTM | D882 | Tensile properties of thin plastic sheeting |
| ASTM | D1922 | Elmendorf tear resistance |
| ASTM | D1709A | Dart drop impact, F50 |
| ASTM | D1003 | Haze and luminous transmittance |
| ASTM | D1894 | Static and kinetic coefficient of friction |
| ASTM | D3895 | Oxidative induction time |
Heavy-duty shipping sack lines running D170DK often set the extrusion line to the upper end of the recommended temperature profile and use a 2.2:1 blow-up ratio to balance machine-direction and transverse-direction tear. The film is sealed on rotary heat-sealing equipment; seal strength and hot-tack performance are evaluated under ASTM F88 and ASTM F1921 because the coefficient of friction and slip additive level affect bag filling speed. Agricultural film service-life assessments use ultraviolet stabilization masterbatches and weathering standards such as ASTM D4329 or ISO 4892-2. Published D170DK-specific weathering data are limited to formulated film structures rather than neat resin, and field performance must be validated on the targeted extrusion line.