| HS Code | 292594 |
| Polymer Type | Metallocene Linear Low Density Polyethylene (m-LLDPE) |
| Comonomer | Hexene-1 |
| Catalyst Type | Metallocene |
| Molecular Weight Distribution | Narrow |
| Comonomer Distribution | Uniform |
| Form | Pellets |
| Color | Natural |
| Density | 0.916 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.90 g/10 min |
| Melting Point | 116 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 1,300 psi |
| Tensile Strength At Break | 7,000 psi |
| Elongation At Break | 600% |
| 1 Secant Modulus | 30,000 psi |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength | 300 g/mil |
| Haze | 6% |
| Gloss 45 | 80 |
| Coefficient Of Friction | 0.20 |
| Low Temperature Brittleness | < -70 °C |
| Heat Seal Initiation Temperature | 105 °C |
As an accredited Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Marlex D143 m-LLDPE comes in 25 kg (55.1 lb) polyethylene-lined bags on pallets; bulk truck and railcar options are available. |
| Container Loading (20′ FCL) | 20′ FCL typically holds 25 kg bags of Marlex® D143 m-LLDPE, palletized, stretch-wrapped, approx. 25 MT net, secured for transport. |
| Shipping | Chevron Phillips Marlex® D143 m-LLDPE ships as non-hazardous, free-flowing polyethylene pellets in sealed 25-kg bags, bulk sacks, or bulk trucks/railcars. Transport in cool, dry, shaded conditions away from moisture, UV, and ignition sources. Keep containers closed, palletized, and secured to prevent spillage or contamination. |
| Storage | Store Chevron Phillips Marlex® D143 m-LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags closed and palletized to prevent contamination and moisture ingress. Avoid contact with strong oxidizers. Maintain good housekeeping and follow supplier SDS and local regulations. Protect from UV exposure and excessive stacking. |
| Shelf Life | Chevron Phillips Marlex D143 m-LLDPE has no defined shelf life if stored sealed, cool, dry, protected from UV and moisture. |
In frozen food webs that require low haze, high dart impact, and low-temperature heat-seal integrity, Marlex® D143 m-LLDPE is processed on three-layer blown film equipment with a dual-lip air ring, internal bubble cooling, and an oscillating haul-off. The resin, characterized by a nominal density of 0.916 g/cm³ and a melt index of 1.0 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg, is charged as the sole resin at 100 wt% for maximum clarity; where bubble fluttering occurs at high frost-line settings, high-pressure LDPE is added at 10–25 wt%, which raises ASTM D1003 haze from the 5–7% range to above 10% but stabilizes the web. A silica-based antiblock masterbatch is dosed at 1,500–3,000 ppm active silica, and erucamide slip is held at 400–900 ppm to maintain coefficient of friction below 0.40 under ISO 8295; excessive slip above 1,200 ppm can cause blocking in warm warehouses. For direct food contact, the film falls under FDA 21 CFR 177.1520(c) item 3.2a and EU Regulation (EU) No 10/2011 Annex I, with overall migration not exceeding 10 mg/dm²; the supplier formulation is supported for food-contact use subject to end-use testing under the specified simulants. Downstream conversion includes in-line corona treatment to 42–48 mN/m, slitting, and horizontal or vertical form-fill-seal operations. Terminal finished products include frozen vegetable pillow packs, dry-mix carton liners, resealable zipper pouches, and clear produce bags. The dominant processing limit is seal-temperature control: jaw temperatures above 135–145 °C at dwell times of 0.5–1.0 s produce tail-tear failures on high-speed HFFS machines, so converters must map seal curves rather than transfer settings from conventional LLDPE.
Barrier coextrusions for modified atmosphere packaging use D143 as the sealant skin, a maleic anhydride-grafted polyolefin tie, and an ethylene-vinyl alcohol copolymer core; the process conflict arises from dissimilar melt curves and layer-ratio limits. At a die gap of 1.8–2.4 mm and blow-up ratio of 2.0:1–2.8:1, the D143 skins are each set at 25–35 wt% of total film, the tie layers at 8–12 wt%, and the EVOH core at 5–10 wt%, producing a barrier layer of 3–10 μm in a total gauge of 50–120 μm. The D143 layer can exhibit interfacial encapsulation and gauge bands when the skin layer falls below 15 wt% or when the melt temperature at the die exit is below 204 °C; separate extruder profiles are therefore maintained at 204–221 °C for D143, 193–210 °C for tie resin, and 200–225 °C for EVOH. Compliance for food contact includes FDA 21 CFR 177.1520(c) item 3.2a for the D143 skin, FDA 177.1360 for EVOH, and EU 10/2011 overall migration limits for the converted film. Terminal products include gas-flushed pouches for meat, cheese, and shredded bakery mixes, vacuum pouches for fresh red meat, and thermoformed barrier lidding webs. Long-run production experience shows that fluoropolymer processing aid at 200–600 ppm is required to suppress melt fracture in the D143 skins if grooved-feed extruders of 30:1 L/D are operated above 120 kg/h on 400 mm diameter dies; published data for this specific coextrusion configuration are limited, and pilot-scale layer stability trials are advised before commercial freezing.
Agricultural greenhouse films formulated with D143 target three-year to five-year installation life and depend on a UV-stabiliser masterbatch, an anti-drip wetting agent, and a high EVA fraction for thermal retention. A three-layer blown film structure with a blow-up ratio of 2.8:1–3.2:1 and die gap 2.0–2.4 mm is run with melt temperatures of 200–226 °C; the skin layers contain 50–80 wt% D143, 10–25 wt% ethylene-vinyl acetate with 14–18% vinyl acetate, 3–6 wt% anti-drip masterbatch, and 0.5–1.5 wt% hindered amine light stabiliser masterbatch. The film is classified under EN 13206:2017 for agricultural covering applications, and accelerated weathering is assessed under ISO 4892-2 for UV exposure and ISO 527-3 for tensile properties; REACH Regulation EC 1907/2006 applies to substances of very high concern in the compounding stage. After blown film extrusion, the film is corona-treated to 38–42 mN/m on one side, folded with anti-block spacers, and slit into widths for gothic-arch or tunnel greenhouses. Terminal products include multi-season greenhouse covers, low tunnel films, and shade-hall cladding. The main formulation constraint is additive partition: at EVA loadings above 25 wt%, anti-drip agents migrate to the surface within weeks and can reduce light transmission below the EN 13206 class thresholds; at D143 loadings above 80 wt%, the film retains tensile strength but loses infrared retention needed for night-time thermal stability. Published data for this specific additive partition at multi-year exposure is limited, and the usual field practice is to validate one full season under the target climate before commercial specification.
For 50–100 μm industrial sacks converted into block-bottom and valve formats, D143 is blended rather than run neat because tear-propagation resistance and stiffness must be balanced against bubble stability. The blown film line is operated at a die gap of 2.0–2.5 mm, blow-up ratio of 2.0:1–2.6:1, and melt temperatures of 204–232 °C on upstream grooved-feed extruders with 30:1 L/D; the formulation consists of 65–85 wt% D143, 10–25 wt% butene-based LLDPE, 5–15 wt% high-pressure LDPE, 2–4 wt% carbon black masterbatch, and 200–500 ppm fluoropolymer processing aid. The D143 fraction contributes dart impact under ASTM D1709 and puncture resistance, while the LDPE fraction stabilises the frost line at high production outputs. The finished sacks are tested under EN ISO 7965-2 for drop resistance and ISO 527-3 for tensile properties; when the sack is intended for packaging non-hazardous chemical powders, the structure must also meet REACH EC 1907/2006 for the packaging material itself and the converter’s declaration for food-contact status is not required. Terminal products include heavy-duty shipping sacks for polymer pellets, mineral fillers, construction adhesives, and bulk food ingredients packed in 25–50 kg quantities. The processing bottleneck is not extrusion output but edge-trim reprocessing: reground D143-heavy film above 15 wt% in the feed blend increases gel count and lowers bubble stability, so converters must limit recycled edge trim or route it into the middle layer only.
Extrusion lamination sealant webs based on D143 are produced at coating weights of 15–30 μm on polyester, aluminium foil, and kraft paper substrates where the mLLDPE layer must provide hot-tack strength, flex-crack resistance, and sealant integrity. The extrusion coating line uses a 26:1 L/D single-screw extruder with a slot die opening of 0.5–0.7 mm, a chill roll temperature of 15–20 °C, and melt temperatures of 290–320 °C; at these temperatures, D143 contributes low gel formation but must be blended with 5–15 wt% high-pressure LDPE to reduce neck-in and edge bead. For direct food contact, the sealant layer falls under FDA 21 CFR 177.1520(c) item 3.2a and EU 10/2011 overall migration limits; the laminated structure is also covered by FDA 177.1395 for laminates with food-contact layers. In-line corona treatment is set to 42–48 mN/m before lamination; downstream products include retortable pouches for wet food, beverage powder sachets, snack laminates, and pharmaceutical strip packaging. The principal operational boundary is adhesion: D143 requires either a primer or the higher melt-temperature window with controlled air gap to generate sufficient substrate wetting; if chill roll haze exceeds 2% or seal strength falls below 15 N/15 mm under ASTM F88/F88M, the melt temperature and nip pressure must be corrected before continuing.
Cast film production of hygiene and overwrap webs uses D143 in the skin or core to provide low gel levels and high elongation, but at line speeds above 250 m/min, additive migration can produce chill roll plate-out and web slip inconsistencies. The cast line is configured with a 30:1 L/D extruder, a flat die gap of 0.4–0.6 mm, a chill roll temperature of 18–24 °C, and melt temperatures of 220–260 °C. The formulation includes 70–90 wt% D143, 10–30 wt% a higher-MI cast-film-grade LLDPE to reduce melt pressure, 200–600 ppm fluoropolymer processing aid, 500–1,200 ppm erucamide slip, and 1,000–3,000 ppm synthetic silica antiblock. The film is assessed under ASTM D1003 for haze, ASTM D882 for tensile elongation, and ISO 8295 for coefficient of friction. Food-contact conversion falls under FDA 21 CFR 177.1520(c) item 3.2a and EU 10/2011; non-food hygiene backsheets require REACH EC 1907/2006 but no food-contact migration testing. Terminal products include stretch wrap for hand application, diaper backsheet films, feminine hygiene outer covers, and general protective overwrap. The critical threshold is chill roll condensation: in high-humidity production halls exceeding 60% relative humidity, the chill roll surface temperature should be kept above the dew point to avoid additive plate-out; if haze increases by more than 1–2% across a production shift, the roll temperature must be raised or the slip package reformulated. Published data for this specific configuration is limited, and plant trials should map the plate-out onset against dew point and additive concentration.
Competitive Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene is a metallocene-catalyzed ethylene-hexene copolymer supplied in pellet form for blown film and cast film structures. The nominal density is 0.916 g/cm³ when measured under ASTM D1505, and the nominal melt index is 1.0 g/10 min at 190 °C and 2.16 kg when measured under ASTM D1238. The resin is typically converted into monolayer and coextruded films for food packaging, heavy-duty bags, lamination film, and sealant webs. Food-contact status is stated by the manufacturer under FDA 21 CFR 177.1520(c), with final article compliance dependent on temperature, food type, migration testing, and the finished converter’s food-contact documentation. D143 is distinguished from conventional butene- and hexene-based LLDPE resins by its single-site catalyst architecture, which produces a narrower molecular weight distribution and a more uniform short-chain branch distribution at the same nominal density.
The density of 0.916 g/cm³ places D143 near the lower density range for linear low density polyethylene film grades, where impact toughness measured by ASTM D1709 on a falling dart apparatus is typically favored over the stiffness of 0.920 g/cm³ or higher resins. The 1.0 g/10 min melt index is selected to balance drawdown on film lines with bubble stability. Because single-site resins exhibit lower melt elasticity than long-chain-branched low density polyethylene, D143 should be started on a low-stalk bubble configuration with a frost line height of 2–4 die diameters. Published data for this specific configuration is limited for some film structures; converter trials should be confined to single-parameter changes until the bubble and die-pressure response is established.
The primary structural differences exist at the catalyst active site and in the resulting molecular architecture. A conventional Ziegler-Natta LLDPE is produced on multiple active sites that generate chains with a broad distribution of molecular weights and a non-uniform distribution of comonomer. In a multi-site resin, low-molar-mass fractions can contain a disproportionate share of the hexene or butene comonomer, leaving the higher-molar-mass chains more linear. D143 is produced with a single-site metallocene catalyst that yields a more homogeneous distribution of both molecular weight and hexene incorporation. This structural homogenization reduces the concentration of low-molar-mass oligomers that are extractable under FDA 21 CFR 177.1520(c) extraction protocols and that can contribute to organoleptic transfer in sensitive food packaging. It also reduces the number of broad-composition domains that melt at low temperatures, which shifts seal initiation temperature and hot-tack response measured under ASTM F1921 and seal strength measured under ASTM F88 toward a narrower and more reproducible range.
Typical polydispersity indices for metallocene LLDPE are reported in the range 2.0–3.0, whereas conventional Ziegler-Natta LLDPE often displays values from 3.5 to 5.0 by gel permeation chromatography. D143 follows this structural pattern; the lower polydispersity index is a primary reason why the resin exhibits a smaller shear-thinning gradient. This does not mean that D143 is free of high-molar-mass chains, but that the fraction of chains above the critical entanglement molecular weight is distributed differently than in a conventional LLDPE. The resulting change in relaxation time distribution influences bubble stability and the rate of film stress decay after the die exit.
The structural difference also affects solid-state mechanical properties. In blown film, Elmendorf tear measured by ASTM D1922 using an Elmendorf tearing tester and tensile yield and break properties measured by ASTM D882 are influenced by bubble geometry. For D143, the more uniform branching tends to increase the machine-direction tear component relative to a butene-LLDPE of similar density, but the exact tear anisotropy depends on blow-up ratio, frost line height, and gauge. The lower concentration of branched low-molar-mass species also reduces haze and increases gloss when evaluated under ASTM D1003 and ASTM D2457. However, the improvement is not identical at all film thicknesses, and published data for this specific configuration is limited.
On a grooved-feed single-screw extruder with 25:1 to 30:1 L/D, the narrow molecular weight distribution generates less shear thinning than a conventional Ziegler-Natta LLDPE of the same melt index. This can appear as higher melt pressure and higher motor load at equal screw speed. Barrel temperature profiles from 170 °C to 190 °C in the feed zone, increasing to 210 °C to 230 °C at the adapter and die, are typical starting conditions for D143. A die gap of 1.5 mm to 2.5 mm and a blow-up ratio of 2.0:1 to 2.5:1 are used to control film mechanical balance. At throughputs above 2.0 kg per hour per mm of die circumference, die-lip deposit formation can become visible on extended runs. The use of a fluoropolymer processing aid at 200–500 ppm is common to delay deposit accumulation and to suppress melt fracture in the die land region. Reducing the die gap below 1.2 mm is not advised unless the melt temperature and die pressure are monitored closely, because the higher shear rate can raise localized melt temperature enough to initiate oxidative degradation.
The processing window for D143 is influenced less by the melting range than by the elongation behavior of the narrow molecular weight distribution. On high-stalk bubble configurations, the reduced melt elasticity can cause sagging and pulsing unless the frost line is held low. A dual-lip air ring with internal bubble cooling is more effective than a single-lip air ring for stabilizing the bubble at high throughput. If a line has only a single-lip air ring, the blow-up ratio should be reduced from 2.5:1 to 2.0:1 until the bubble shape is stable. Melt temperatures at the die should be maintained between 210 °C and 225 °C; increasing the die temperature above 230 °C improves melt strength but accelerates the oxidation of unstabilized or low-additive blends. The extruder back pressure on a 40 mm grooved-feed machine is typically higher than with an equal-melt-index conventional LLDPE and should be kept below the extruder manufacturer’s rated barrel pressure, often 350–500 bar for standard barrels. If the pressure approaches the rated limit, the feed section temperature can be raised slightly to delay melting and reduce torque, but this may change solid-conveying pressure stability.
Die-lip deposit formation on multi-layer dies is observed as a gradual loss of film edge quality or as streak lines in the machine direction. With D143, the lower concentration of low-molar-mass waxes reduces one mechanism of die-lip deposit, but the higher die shear stress can promote degradation products from the polymer or from additive packages. A fluoropolymer processing aid at 200–500 ppm is effective in reducing die-lip shear stress and delaying deposit accumulation. Compatibility of the processing aid with the resin and with any slip or antiblock masterbatch should be confirmed under production-scale conditions, because some migratory slip additives increase initial die-lip wetting. When the processing aid is used, it may require 30–60 minutes to condition the die and stabilize melt pressure.
In cast film coextrusion, D143 can be processed on chill-roll lines with roll temperatures from 15 °C to 30 °C. The narrow molecular weight distribution can increase melt-curtain tension at high line speeds, so the die-to-roll distance should be minimized to preserve edge stability. In coextruded structures with polypropylene or barrier polymers, the layer adjacent to D143 should be selected to avoid interfacial instability caused by viscosity mismatch. Apparent viscosity comparisons are preferably made at the relevant shear rate using ASTM D3835 capillary rheometry rather than relying on melt index alone, because melt index does not capture the shear-thinning differences that govern die flow stability in coextrusion feedblocks.
The first measurable change in this substitution is usually an increase in die pressure and motor load at equal screw speed because the lower shear thinning of single-site LLDPE reduces the natural viscosity drop across the die. The magnitude of the increase depends on the die gap, die land length, and screw wear, but converters have observed that back pressure can approach or exceed the extruder barrel limit if the profile is not adjusted. When replacing a conventional LLDPE, the feed section should be started at 170 °C, the compression section at 190 °C, and the die at 210–225 °C. The frost line height should be lowered to 2–4 die diameters, and the blow-up ratio should be reduced to 2.0:1 until the bubble is stable. The die gap should remain at 1.8–2.5 mm. A die gap below 1.2 mm may cause melt fracture and excessive die pressure unless the die temperature is increased, which can then increase oxidation risk.
| Parameter | Method or instrument | D143 | Conventional LLDPE |
|---|---|---|---|
| Density | ASTM D1505 | 0.916 g/cm³ | 0.916–0.920 g/cm³ typical |
| Melt index (190 °C, 2.16 kg) | ASTM D1238 | 1.0 g/10 min | 0.9–1.2 g/10 min typical |
| Molecular weight distribution | Gel permeation chromatography | Narrow | Broad |
| Shear thinning at 100–500 s⁻¹ | Capillary rheometer ASTM D3835 | Lower | Higher |
| Bubble stability margin | Film line observation | Lower | Higher |
| Die-lip deposit mechanism | Production observation | Reduced low-MW wax component; higher die shear | Higher low-MW wax component |
Relative to high-pressure low density polyethylene, D143 provides higher tensile strength at break measured under ISO 527-3 or ASTM D882 and higher dart impact under ASTM D1709, but the bubble stability margin is lower because high-pressure LDPE contains long-chain branching that increases melt elasticity. Relative to butene-LLDPE, D143 provides a different impact–tear balance and a lower concentration of extractable low-molar-mass material under FDA 21 CFR 177.1520(c) extraction conditions. Relative to other metallocene LLDPE grades in the Marlex® family, the 0.916 g/cm³ density and 1.0 g/10 min melt index target film structures requiring a lower seal initiation temperature than 0.918 g/cm³ products while retaining sufficient bubble stability for monolayer and coextruded film. This does not imply that D143 is directly interchangeable with all other m-LLDPE grades; the specific die gap, haul-off speed, and air-ring type determine whether the substitution can be completed without a change in film anisotropy.
Sealant-layer performance is characterized under ASTM F88 for seal strength, ASTM F1921 for hot tack, and ASTM F2029 for heat-sealability. In form–fill–seal operations, D143 is commonly used at sealant thicknesses from 20 µm to 40 µm. The seal bar temperature required to reach a specified seal strength is a function of dwell time, pressure, and the identity of the core and tie layers. Published data for this specific configuration is limited, and converter trials should use a temperature matrix rather than a single seal-bar setpoint. In barrier laminates, the organoleptic contribution of the sealant layer is tested under ASTM E460 or internal sensory protocols; the lower extractable content of metallocene LLDPE is often cited as a reason for its selection, but the final article must be tested as a complete structure because lamination primers and inks can dominate taint and odor. Additive compatibility should be verified before production: high loadings of some amine-based stabilizers or zinc stearate can shift seal initiation temperature and cause color development during processing. Pre-drying is not normally required when the resin is stored below 60% relative humidity, but condensation on cold pellet surfaces must be avoided because it can introduce surface defects in film. Storage under dry conditions at 23 °C and relative humidity below 60% is recommended. Resin stored beyond 12 months from the manufacturer’s certification date should be re-tested for melt index, density, and film appearance before conversion.