Chevron Phillips Marlex D139fk Metallocene Linear Low Density Polyethylene Blown Film

Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film

    • Product Name: Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 178173
    Product Name Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
    Manufacturer Chevron Phillips Chemical Company
    Grade D139FK
    Polymer Type Metallocene Linear Low Density Polyethylene
    Form Blown Film
    Density 0.916 g/cm³
    Melt Index 0.85 g/10 min
    Melt Flow Ratio 16
    Melting Point 118 °C
    Vicat Softening Point 91 °C
    Tensile Strength At Yield 12 MPa
    Tensile Strength At Break 34 MPa
    Elongation At Break 600 %
    Dart Drop Impact 250 g
    Elmendorf Tear Md 180 g
    Elmendorf Tear Td 350 g
    Haze 6 %
    Gloss 70 %
    Coefficient Of Friction 0.2
    Blocking 50 g

    As an accredited Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene blown film resin supplied in 25 kg polyethylene-lined bags.
    Container Loading (20′ FCL) Typically 20′ FCL: 20 pallets (800 x 25 kg bags), totaling 20 MT of Marlex D139FK metallocene LLDPE blown-film resin.
    Shipping Chevron Phillips Marlex® D139FK is typically shipped as non-hazardous polyethylene resin pellets in 25 kg bags, octabins, or bulk trucks/railcars. No UN hazard class or transport placarding is normally required. Keep packages dry, clean, and intact; store away from heat and direct sunlight. Standard handling PPE is recommended.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep the resin in original sealed bags or packaging on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Store at ambient temperature, protect packaging from punctures, and follow local regulations and supplier recommendations.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film

    D139FK is processed within the metallocene LLDPE blown film envelope; nominal density is 0.918 g/cm³ and melt index is 1.0 g/10 min when measured under ASTM D1238 at 190°C/2.16 kg. The grade is non-hygroscopic; pre-drying is not required at ambient relative humidity, but surface condensate on outdoor-stored resin sacks should be removed by an air knife before hopper loading. The following scenarios are separated by extrusion configuration, additive chemistry, and final test methodology.

    In frozen food packaging lines running vertical form-fill-seal machinery, D139FK is coextruded as the sealant skin over a stiffer core of conventional linear low density polyethylene or high-density polyethylene on a three-layer blown film line. The core layer carries 80–85% of the total thickness, and the D139FK skins are split 7.5–10% per side. This structure shifts the seal initiation temperature into the 85–95°C range when measured by ASTM F2029 on a 25.4 µm specimen, allowing vertical form-fill-seal jaw temperatures to be reduced by 10–15 K relative to an LDPE-rich sealant. The reduction in heat input is not uniform across machine designs; rotary VFFS lines with 0.4–0.6 s seal dwell times impose higher hot tack demand, which is evaluated by ASTM F1921. Film structures for frozen vegetables, seafood, and ice cream pouches are designed for puncture resistance at −20°C; the metallocene chain architecture provides a lower ductile-to-brittle transition temperature than butene-based LLDPE when tested in accordance with ASTM D3420. In blown film conversion, the die gap is not reduced below 1.8 mm because the narrow molecular weight distribution raises die lip pressure; a 2.0–2.5 mm die gap coupled with a 2.0:1–2.5:1 blow-up ratio suppresses melt fracture. Frost line height is maintained between 3 and 5 die diameters to stabilize the bubble before collapse. Direct food contact compliance requires that the hexane-soluble extractable fraction remains within the limits described in 21 CFR 177.1520(c) and that the overall migration limit under EU Regulation No 10/2011 does not exceed 10 mg/dm² after simulant testing for frozen food. A thin slip/anti-block package is incorporated only at the level required for film opening; excess slip agent migrates during frozen storage and may reduce seal strength.

    What Bubble Stability Limits Govern High-Gauge Industrial Sack Films?

    Extrusion of 150–250 µm monolayer or three-layer heavy-duty sack film on a 75 mm single-screw extruder with 30:1 L/D and a Maddock mixing section encounters two competing constraints. At the lower end of the melt temperature range, 193°C, bubble stability improves because draw resonance is damped, but the die lip pressure rises and may exceed 280–350 bar when the die gap is narrower than 2.0 mm. At the upper end, 216°C, the melt is easier to pump but the lower melt strength causes the bubble to wander when the blow-up ratio is pushed above 2.5:1. The practical formulation used on production lines therefore includes 10–20 wt% high-pressure LDPE to add shear thinning and melt elasticity. This let-down reduces the critical shear rate for melt fracture and allows a 2.2–2.5 mm die gap without sacrificing gauge uniformity. A fluoropolymer processing aid is dosed at 300–600 ppm to reduce die lip fouling when the line is operated at the maximum screw speed available for the 200 µm gauge. For fertilizer and resin pellet sacks, the film is tested against ISO 7965-1 for drop resistance and ASTM D1709 for dart drop impact; converter-specific target failure masses are not part of the resin datasheet, and published D139FK-specific drop data for this configuration is limited. The tear propagation resistance in both machine and transverse directions is measured by ASTM D1922; cross-direction Elmendorf tear values tend to be the limiting factor because blown film orientation concentrates stress in the machine direction.

    When D139FK is let down into a three-layer greenhouse film at 20–30 wt% of the total blend, the improvement in puncture resistance is accompanied by a reduction in melt elasticity that must be offset by a high-pressure LDPE carrier. The film is processed on lines equipped with internal bubble cooling and external cooling rings; the internal bubble pressure is trimmed to hold a 2.0:1 blow-up ratio within ±0.1 because the metallocene phase has a narrower orientation window. The additive package includes a hindered amine light stabilizer at 0.4–0.6 wt%, a UV absorber at 0.2–0.4 wt%, and an antifog concentrate at 0.8–1.2 wt% in the inner skin. Failures on high-temperature greenhouse lines occur when the film is pulled through collapsing frames at high speed with insufficient slip; the kinetic coefficient of friction against a steel surface should be maintained below 0.35 when measured by ASTM D1894. The final 180 µm film is used for long-season greenhouse tunnels in Mediterranean climate zones; the UV resistance is validated by EN 13206 or equivalent national specifications for covering films. In this application, the metallocene chain architecture increases low-temperature impact resistance, but the resin does not provide UV stabilisation by itself; a masterbatch of UV stabilisers is mandatory for service lifetimes beyond one growing season.

    When D139FK Replaces Conventional LLDPE Sealant Webs in Extrusion Lamination

    Extrusion lamination of oriented PET or BOPP to aluminum foil or metallized film uses D139FK at a coat weight of 15–25 g/m² as the sealant layer. The lower shear viscosity of metallocene LLDPE is not always beneficial in this process because the resin experiences draw-down ratios of 20:1–40:1 between the slot die and the chill roll. D139FK has less long-chain branching than high-pressure LDPE, so neck-in is higher unless the melt temperature is lowered to 290–305°C and the air gap is kept below 150 mm. A blend of 70–80 wt% D139FK with 20–30 wt% LDPE is typical; this moves the neck-in value closer to that of a conventional lamination-grade LDPE while preserving seal performance. The chill roll is maintained at 15–20°C to quench the sealant at a rate that minimizes excessive crystallinity and maintains hot tack. Adhesion to aluminum foil requires ozone treatment of the melt web in the air gap; without ozonation, peel strength measured by ASTM F904 may drop below the converting requirement of 400 g/25 mm. End structures include hot-fill stand-up pouches, lidding film for dairy cups, and dry-soup pouches. For direct food contact, the structure must meet 21 CFR 177.1520 and, in the EU, the migration testing matrix of Regulation (EU) No 10/2011. Published D139FK-specific peel strength data for hot-fill lamination configurations is limited, so converter trials should establish the appropriate ozonation intensity and LDPE let-down for the specific foil substrate.

    Industrial Liner Film Toughness and Dart Impact Reserve

    Industrial liners for construction debris, agricultural bulk goods, and chemical packaging are converted from 75–120 µm blown film with a high molecular weight high-alpha-olefin comonomer distribution. On a 60 mm extruder with 25:1 L/D, screen changer, and spiral mandrel die, D139FK is run with a barrel profile that holds melt temperature between 190°C and 205°C. The bubble is quenched with a dual-lip air ring; an internal bubble cooling system is not required for this thickness range, but without IBC the line speed is limited by heat transfer, not by the resin. The critical quality variable is dart impact reserve: converters periodically test ASTM D1709 Method A or B depending on the gauge and compare the failure energy to the minimum specification. For waste sack applications, the specification often requires a mean failure mass not less than 300 g for 100 µm film, but such values are converter-specific and not part of the resin datasheet. Tear strength in the machine direction is reduced when the blow-up ratio is below 2.0:1, so the line is kept at 2.2:1 to balance MD and TD Elmendorf tear values recorded under ASTM D1922. Because industrial liners are often stored in warm warehouses, an anti-block masterbatch is added at 1–2 wt% to prevent blocking when the film surface temperature reaches 35–40°C; the static coefficient of friction should stay below 0.50 measured under ASTM D1894.

    On palletizing lines that apply stretch hoods over stacked construction panels or bagged bulk solids, D139FK is coextruded as the outer skin of a 150–200 µm blown film with a core of lower-density metallocene plastomer. The film is slit to gusseted tubing and drawn over the load by a stretch hood machine that can apply 50–80% elongation in the transverse direction during the stretching cycle. The blown film line must be configured with a 2.5 mm die gap and a 2.0:1 blow-up ratio to preserve machine-direction tear resistance; if the die gap is reduced to 1.8 mm, MD tear measured by ASTM D1922 drops sharply because the orientation in the machine direction is no longer balanced by the transverse stretching cycle. The film's elastic recovery and hoop force are evaluated by load retention tests based on ASTM D5459 with cycle times of 1 h, 4 h, and 24 h; residual force retention determines pallet stability during transport. The outer skin is compounded with 0.5–1.0 wt% slip agent to facilitate film opening on the forming head, but excessive slip agent migration reduces the coefficient of friction below 0.15 and causes the hood to slip on the load. For UV-sensitive products stored outdoors, a UV-stabilised skin is used, but the resin alone does not provide UV resistance; the converter adds a masterbatch in compliance with EN 13206 only when the final load is stored outside. This application is sensitive to batch-to-batch gel levels: a single large gel in the outer skin can initiate a tear during the transverse stretching cycle, so the film is inspected with a continuous vision system at the winder.

    Low Seal Initiation Is the Primary Selection Criterion in Powder Packaging

    Low seal initiation temperature is the primary selection criterion when D139FK is used in horizontal form-fill-seal lines for dry powder products such as cake mixes, instant coffee, and detergent powders. The sealant film is run at 25–35 µm as a polyethylene layer in a lamination with BOPP or cellulose-based sheets; the seal jaws are operated between 85°C and 105°C and the dwell time is compressed to 0.3–0.8 s to maintain line speeds above 80 pouches/min. Powder contamination on the seal area is the main failure mode. The metallocene sealant lowers the heat-seal initiation enthalpy requirement compared with conventional LLDPE, but the seal-through-contamination window is not unlimited; trials are performed with controlled corn starch dust levels of 0.05–0.15 mg/cm² across the seal area to map the limiting jaw temperature. Hot tack force is measured by ASTM F1921 at a 0.5 s dwell and 0.2 s cool time; converters generally require the hot tack force to remain above 1.5 N/15 mm during the fill cycle. The low molecular weight fraction in D139FK can migrate to the film surface during storage; this reduces blocking but may also lower the oxygen barrier of the substrate. For dry powder packaging, the oxygen transmission rate is tested by ASTM D3985 at 23°C and 0% RH; the final package specification is determined by the product shelf life, not by the resin source. Compliance is established through 21 CFR 177.1520 for US food contact and EU Regulation No 10/2011 for EU markets. When powders contain high fat levels, the film is additionally screened for extractives under FDA 21 CFR 177.1520(c) to confirm that the hexane solubles remain within the stated limit.

    For dry bulk mail order bag film, D139FK is converted at 40–60 µm with 1–2 wt% anti-block masterbatch and tested only for MD Elmendorf tear under ASTM D1922.

    ApplicationPrimary StandardTest ParameterControl Range
    Frozen food packaging21 CFR 177.1520(c), EU Regulation No 10/2011Seal initiation temperature85–95°C
    Heavy-duty sacksISO 7965-1, ASTM D1709Dart drop mean failure massConverter-specific
    Greenhouse filmEN 13206UV weathering retentionSeason-dependent
    Lamination sealant21 CFR 177.1520, ASTM F904Bond peel strength≥400 g/25 mm
    Industrial linersASTM D1709, ASTM D1894Dart impact and static COF≥300 g/100 µm; COF <0.50
    Stretch hood filmASTM D5459Residual hoop force retentionCycle-dependent
    Powder packagingASTM F1921, ASTM D3985Hot tack force, OTRHot tack >1.5 N/15 mm
    Free Quote

    Competitive Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product designation Chevron Phillips Marlex® D139FK identifies a metallocene-catalyzed linear low density polyethylene supplied as pelletized blown film extrusion resin. The nominal density is 0.918 g/cm³ when determined by ASTM D1505; the nominal melt index is 1.0 g/10 min when measured at 190 °C and 2.16 kg load according to ASTM D1238. These values place the grade in the low-density segment of LLDPE film resins, where downgauging potential and seal performance are tied to a narrow composition distribution. The resin is intended for monolayer and coextruded blown film structures requiring optical clarity, high dart impact resistance, and low-temperature seal initiation. Because the single-site catalyst produces a narrower short-chain branching distribution than conventional Ziegler-Natta LLDPE, the resin typically generates lower solvent-extractable fractions and more uniform crystal thickness. At ambient relative humidity below 60 %, pre-drying is not required for pellet handling. On production-scale lines, melt index variability is typically controlled within a range of ±0.05 g/10 min, reducing layer-ratio drift in coextruded structures.

    What Distinguishes D139FK from Conventional Ziegler-Natta and High-Pressure LDPE Resins?

    The principal structural difference lies in catalytic control of comonomer insertion. Conventional Ziegler-Natta LLDPE synthesized with heterogeneous active sites displays a broad interchain comonomer distribution: the low-molecular-weight fraction tends to be highly branched while the high-molecular-weight fraction is more linear, producing a wider melting range and a measurable crystalline fraction that persists at elevated sealing temperatures. D139FK belongs to a metallocene and/or single-site catalyst class in which the active sites are more uniform; consequently, the hexene-1 comonomer is distributed across the molecular weight distribution with less composition drift. Differential scanning calorimetry under ASTM D3418 typically shows a lower peak melting temperature and a narrower melting endotherm than an equivalent-density Ziegler-Natta LLDPE, while the cold extraction fractions measured by 21 CFR 177.1520 extraction protocols are generally reduced. In blown film, this molecular structure shifts the property balance relative to conventional LLDPE: for a comparable density and melt index, haze development from crystalline scattering is lower, while dart impact values under ASTM D1709A are typically higher because the more uniform crystal network delays crack propagation. Compared with high-pressure LDPE, D139FK does not possess the same degree of long-chain branching; therefore, melt tension and bubble stability are lower. The trade-off is partly offset by higher elongation at break and improved puncture resistance, but converters routinely blend 10–20 wt% LDPE into the formulation when enhanced melt strength is required.

    Compared with high-density polyethylene film resins, D139FK has lower density and therefore lower stiffness and lower yield strength, but it provides higher dart impact and better puncture resistance at equivalent thickness. Compared with metallocene plastomers in the 0.895–0.910 g/cm³ range, D139FK has higher secant modulus and lower blocking tendency, while retaining sufficient low-temperature sealing for refrigerated packaging. The melt index of 1.0 g/10 min is higher than that of fractional-melt blown film grades, meaning it can be processed at lower head pressures but may require more bubble support at high blow-up ratios. These distinctions are measurable by ASTM D1709A, ASTM D1922, ASTM D882, and ASTM D1003.

    Tensile, Tear, and Impact Response in 25 µm Blown Film

    In a 25 µm monolayer blown film produced at a blow-up ratio of 2.5:1 and a die gap of 1.2 mm, the following property ranges are observed in industrial evaluations and manufacturer technical literature. The tensile properties reflect orientation balance and crystallinity; machine-direction orientation generally increases tensile strength at break while transverse-direction orientation is governed by blow-up ratio. Values in Table 1 are reported as typical ranges rather than specification limits.

    PropertyTest MethodTypical Range
    DensityASTM D15050.918 g/cm³
    Melt IndexASTM D12381.0 g/10 min
    Melting PeakASTM D3418117–121 °C
    Vicat Softening TemperatureASTM D1525100–104 °C
    Film HazeASTM D10036–12 %
    Gloss at 45°ASTM D245770–80
    Dart Impact F50, 25 µmASTM D1709A400–700 g
    Elmendorf Tear, MD/TDASTM D1922250–450 / 350–550 g
    Tensile Strength at Break, MD/TDASTM D88240–60 / 35–50 MPa
    Elongation at Break, MD/TDASTM D882450–650 / 550–750 %

    Elmendorf tear data under ASTM D1922 reveal an anisotropic response. Transverse-direction tear values are commonly higher than machine-direction tear values because the film is more oriented in the machine direction. The dart impact F50 value under ASTM D1709A is a rapid failure test used to rank film toughness; for mLLDPE films of this density, values between 400 g and 700 g at 25 µm are typical. Haze under ASTM D1003 and 45° gloss under ASTM D2457 are optical properties influenced by surface roughness and internal scattering. The low density and uniform crystallinity of D139FK produce haze values between 6 % and 12 %, making the film suitable for display packaging if the bubble is maintained without excessive melt temperature fluctuations. In coextruded structures, the skin layers can be adjusted to further reduce total haze or to shift coefficient of friction values measured by ASTM D1894.

    A processing window narrower than that of high-pressure LDPE is observed on standard blown film lines. On a 55 mm groove-fed extruder with 25:1 L/D, a barrier screw, and a die gap of 1.2 mm, a practical barrel profile begins at 180 °C in the feed zone and rises to 215 °C at the adapter and die. A screen pack consisting of 40/60/40 mesh protects the die and raises back pressure sufficiently to homogenize the melt. The melt temperature measured at the die should remain below 230 °C to avoid oxidative degradation during prolonged residence times; typical melt temperatures are 204–216 °C. A dual-lip air ring with chilled air at 10–15 °C stabilizes the bubble, and the frost line height is maintained at 1–2 die diameters to manage machine-direction orientation. Blow-up ratios between 2.0:1 and 3.0:1 provide adequate transverse-direction tear strength while maintaining bubble symmetry. The film gauge can be drawn from 12 µm to 75 µm on this configuration without requiring a polymer gear pump, although pump-assisted lines reduce surging at high screw speeds. The low melt strength of mLLDPE relative to LDPE becomes apparent at high output rates: bubble oscillation and edge wander increase when the monolayer contains no LDPE. Addition of 10–20 wt% high-pressure LDPE raises the bubble stability floor and widens the operating window, but it raises haze and reduces the dart impact increment at the same gauge.

    Coextruded blown film lines using D139FK in the skin layer with a metallocene plastomer sealant layer can shift the seal initiation temperature lower while retaining stiffness from a higher-density core. In a five-layer line with a 250 mm spiral die and 2.8:1 blow-up ratio, the resin typically occupies the outer skins, while HDPE or high-stiffness LLDPE constitutes the core. The viscosity mismatch among layers must be controlled by selecting adjacent-layer resins within 0.5 melt index units; wider gaps can produce interfacial instability and optical haze at the layer boundaries. A gear pump equipped with 10 µm melt filtration improves layer uniformity and reduces the incidence of gel streaks. Published data for this specific configuration is limited, but the practice is common for low-seal-initiation mLLDPE grades.

    When Seal Initiation and Optical Uniformity Are Critical on Vertical Form-Fill-Seal Lines

    In vertical form-fill-seal equipment running at 60–120 cycles/min, the film enters a heated seal bar zone while carrying product, and sealing dwell times are often below 0.5 s. The lower seal initiation temperature of D139FK relative to Ziegler-Natta LLDPE is a measurable processing advantage. Differential scanning calorimetry shows that the resin has a high proportion of crystals that melt below the usual jaw set point, enabling seal strength to develop at seal bar temperatures 5–10 °C lower than a conventional LLDPE of equivalent density. Hot tack measurements under ASTM F1921 typically show a wider plateau for metallocene resins, reducing leaker rates when product falls into the seal area during jaw opening. In practice, seal bar temperatures can be reduced from 115 °C to 105 °C on some lines, lowering thermal stress on the film and reducing surface distortion. Optical uniformity is equally important on display packaging; local thickness variations produce visible dark spots or streaks. The uniform comonomer distribution of D139FK reduces melt-flow irregularities compared with high-density polyethylene blends, but it does not eliminate them if the die gap is mismatched or the frost line is unstable. Film blocking can be managed with a suitable slip/antiblock additive package; actual coefficient of friction values should be verified by ASTM D1894 because additive bloom kinetics vary with aging temperature.

    Operational boundaries for D139FK follow from its molecular architecture and additive composition. The resin is not intended for applications requiring long-term outdoor UV exposure unless UV stabilizers are compounded into the film; the base polymer itself does not provide weathering resistance. If pellets are stored in unheated warehouses and ambient relative humidity exceeds 60 %, surface moisture condensation can produce bubble instability and die-line defects; pre-drying in a desiccant dryer at 60–70 °C for 4–6 h is recommended before processing. The grade should not be mixed with heavily cross-linked reclaim or with additives that generate free radicals at normal processing temperatures. Food-contact applicability is governed by FDA 21 CFR 177.1520 for olefin polymers; the resin meets the composition and extractables provisions of that section when used under the end-use limitations described in paragraph 177.1520(c). EU food-contact assessment follows Commission Regulation (EU) No 10/2011, with compliance dependent on finished-structure migration testing. REACH registration is maintained for the polymer substance, and the grade does not contain intentionally added heavy metal stabilizers covered by RoHS 2011/65/EU restrictive thresholds. Published data for high-speed coextrusion of this specific resin with polyamide or EVOH barrier layers is limited; tie-layer selection and interlayer adhesion should be validated on the target line.