Chevron Phillips Marlex D139 M Lldpe Linear Low Density Polyethylene

Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene

    • Product Name: Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 323379
    Density 0.918 g/cm³
    Melt Index 0.9 g/10 min
    Melting Point 121 °C
    Vicat Softening Point 98.9 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 34.5 MPa
    Elongation At Break 700%
    Flexural Modulus 207 MPa
    Dart Drop Impact 250 g
    Elmendorf Tear Strength Md 240 g
    Elmendorf Tear Strength Td 390 g
    Haze 12%
    Gloss 55%

    As an accredited Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex D139 m-LLDPE is supplied in 25 kg polyethylene bags on pallets and 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL: 25-kg bags; approximately 25 metric tons of Chevron Phillips Marlex® D139 m-LLDPE per container, subject to weight limits.
    Shipping Chevron Phillips Marlex® D139 m-LLDPE ships as non-hazardous polyethylene pellets, typically in 25 kg bags, stretch-wrapped pallets, bulk boxes, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Store and transport in a dry, cool area away from ignition sources, excessive heat, and moisture to prevent contamination.
    Storage Store Chevron Phillips Marlex® D139 m-LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep material in original, sealed packaging on pallets, off the floor, to prevent moisture, dirt, and contamination. Avoid excessive stacking and prolonged UV exposure. Maintain good housekeeping to prevent slipping on spilled pellets. Follow the SDS and local regulations.
    Shelf Life Stored cool, dry, sealed, and protected from sunlight/contaminants, Marlex D139 m-LLDPE has no defined shelf life and remains usable indefinitely.
    Application of Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene

    Before monolayer or three-layer blown film structures are qualified for frozen vegetable pouches and fresh-cut produce packaging, Marlex D139 m-LLDPE is introduced as the primary hexene-based component at a nominal density of 0.918 g/cm³ (ASTM D1505) and a melt index of 0.90 g/10 min (ASTM D1238, 190 °C/2.16 kg). A production outer-layer formulation combines 70–80 wt% D139, 10–20 wt% LDPE with melt index 0.25–0.35 g/10 min, and 5–10 wt% silica-based antiblock masterbatch; the core layer adds 1–3 wt% slip masterbatch to adjust coefficient of friction. Blending is performed on 75 mm grooved-feed extruders with 30:1 L/D barrier screws equipped with Maddock mixing sections, feeding a 250–400 mm spiral mandrel die with a 2.0–2.4 mm die gap. Blow-up ratio is maintained at 2.0–2.8, melt temperature at 195–220 °C, and frost line height at 15–25 cm above the die exit. Finished film thickness ranges from 35–70 µm. Melt pressure upstream of the screen pack is typically held at 25–35 MPa; values exceeding 38 MPa indicate insufficient melting in the Maddock section and require a reduction in screw speed or an increase in barrel set-point. Haze is evaluated to ASTM D1003, tensile modulus and elongation to ASTM D882, and dart impact to ASTM D1709 Method A. For direct food contact, the fabricated film must comply with FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011 Annex I, with total migration not exceeding 10 mg/dm² under the intended food simulant and time-temperature exposure. Terminal products include pillow packs for washed leafy greens, side-gusseted frozen vegetable pouches, and bakery overwrap requiring low seal initiation temperature and high puncture resistance.

    What Limits Heat Seal Initiation in High-Speed VFFS Laminates?

    Seal initiation temperature, rather than ultimate seal strength, limits laminate performance on vertical form-fill-seal units running at 80–120 pouches/min. The narrow molecular weight distribution and hexene comonomer placement of D139 permit seal initiation at lower jaw temperatures than Ziegler-Natta C4 LLDPE of similar density. A production laminate may combine biaxially oriented polyester print web, a polyurethane adhesive, and a blown or cast D139 sealant layer at 25–40 µm. The sealant layer is compounded with 75–85 wt% D139, 10–15 wt% LDPE for bubble stability, and 5–10 wt% slip/antiblock masterbatch; if coefficient of friction must remain below 0.25 on automated feed tracks, the slip concentrate portion is raised within the upper bound after ASTM D1894 measurements. Seal jaw setpoints range from 115–135 °C with dwell times of 0.3–0.6 s and jaw pressure of 2–3 N/mm². Seal strength is evaluated to ASTM F88, hot tack to ASTM F1921, and seal initiation temperature to ASTM F2029. Published D139-specific hot-tack curves for this exact laminate configuration are limited; therefore seal window validation on the target VFFS machine is required before commercial qualification. Terminal articles are snack bar wrappers, frozen seafood pouches, and cereal bag-in-box liners where a 25 mm seal must survive 0.5–1.0 N pack-off force at the jaw release point.

    Test or compliance scopeStandard/codeParameter controlled
    Resin densityASTM D15050.918 g/cm³ nominal
    Melt indexASTM D12380.90 g/10 min at 190 °C/2.16 kg
    Food contactFDA 21 CFR 177.1520(c) 3.2aOlefin polymer identity and extractable limits
    EU food contactEU Regulation (EU) No 10/2011 Annex ITotal migration < 10 mg/dm²
    Seal strengthASTM F88Force per width on VFFS seal
    Hot tackASTM F1921Peak force during seal cooling
    Dart impactASTM D1709Impact failure mass at film thickness

    Stretch Hood Cast Film Processing and Puncture Propagation Control

    At line speeds above 350 m/min on stretch hood cast coextrusion lines, D139 is processed in multi-layer A/B structures at 50–120 µm. The skin layers typically contain 80–90 wt% D139 and 10–20 wt% propylene-based elastomer or C8 plastomer to moderate clamp slip; the core layer may be 90–100 wt% D139 with processing stabilizer masterbatch at 1–2 wt%. Slot dies of 2.5–3.0 m width are operated with chilled roll temperatures of 16–24 °C, melt temperatures of 205–235 °C, and line speeds of 350–650 m/min. Puncture propagation resistance is measured to ASTM D5748, force retention and elongation to ASTM D882 and ASTM D5458. The high hexene content and metallocene catalyst reduce gel particles that otherwise initiate puncture tears at the film edge during pallet transit. A processing conflict exists above 500 m/min where chill roll release must be balanced against cling agents; line trials above 550 m/min have required air knife placement at 20–30 mm from the die exit to control film flutter and prevent edge fold-over. Terminal products include elastic pallet hoods for glass bottle crates, cold-chain beverage trays, and appliance logistics.

    Heavy-duty sack production for polymer granulate and fertilizer logistics feeds D139 into three-layer blown film structures of 120–200 µm. A production formulation contains 55–70 wt% D139, 10–20 wt% HDPE with density 0.955–0.965 g/cm³, 5–15 wt% LDPE, and 3–5 wt% carbon black masterbatch. The screw configuration is a 90 mm grooved-feed unit with 30:1 L/D and a barrier metering section; the die gap is set at 2.2 mm to reduce shear stress below the sharkskin threshold. The blow-up ratio is 1.8–2.5, and the melt temperature is constrained to 195–215 °C. Below 195 °C the narrow molecular weight distribution raises screw backpressure and die melt pressure; above 215 °C dart impact and Elmendorf tear decline due to oxidative chain scission of metallocene polyethylene. Dart impact is tested to ASTM D1709 Method B, Elmendorf tear to ASTM D1922, slow puncture to ASTM D5748, and filled bag drop resistance to ISO 7965-2. Terminal articles are 25 kg polymer granulate sacks, mineral fertilizer bags, and cement bag liners, where a 1.2 m drop onto a concrete surface at 23 °C is the routine field acceptance test.

    Greenhouse covers require accelerated weathering validation before extrusion scale-up.

    After resin blending for multi-season agricultural greenhouse films of 150–220 µm, D139 is coextruded as the inner or core layer in three-layer blown film structures. A typical formulation includes 65–80 wt% D139, 10–20 wt% C8 linear low-density polyethylene, 0.3–0.8 wt% HALS masterbatch, 0.2–0.5 wt% UV absorber masterbatch, and 0.5–1.5 wt% antifog concentrate. The line uses a 2.4 mm die gap, blow-up ratio 2.5–3.0, and melt temperature 190–215 °C. Accelerated weathering is carried out to ISO 4892-2, tensile properties are measured to ISO 527-3, and tear propagation to ISO 6383-2; EN 13206 governs covering films for agricultural multi-span tunnels. The film must retain at least 50% of original elongation after 5,000 h of accelerated weathering, and UV transmission in the 280–400 nm band is controlled by spectral radiometry. Hindered amine stabilizer concentration is the principal operational boundary: exceeding 0.8 wt% in the D139-containing layer increases the risk of die lip build-up on spiral mandrel dies, requiring shutdown at intervals shorter than 8 h. Terminal uses include three-season greenhouse covers, low tunnel films, and solarization films where thermal retention in the 7–14 µm infrared window is obtained by the coextruded EVA or mineral-filled inner layer.

    When D139 Is Coextruded as the Core Layer in Three-Layer Twist Wrap for Confectionery

    D139 is placed in the core of three-layer cast coextrusions for twist wrap where deadfold and twist retention are controlled by skin-layer HDPE. A representative structure uses skin layers of HDPE with melt index 0.7–1.2 g/10 min at 8–12 µm each, and a D139 core at 20–30 µm containing 60–80 wt% D139 and 20–40 wt% LDPE with slip and antiblock masterbatch at 2–4 wt%. The cast line runs at melt temperature 205–230 °C, chill roll temperature 15–25 °C, and line speed 150–300 m/min. Twist retention is evaluated by a 180° twist recovery fixture on 25 mm strips after 24 h at 23 °C and 50% RH; secant modulus is measured to ASTM D882, tear propagation to ASTM D1922, and coefficient of friction to ASTM D1894. Published data for this exact D139 layer ratio is limited, so pilot-scale cast coextrusion trials are used to fix the HDPE skin thickness that prevents splitty twist-off on high-speed candy wrapping machines. Terminal articles include cut-and-wrap confectionery wraps, chocolate bite twists, and seasonal foil-replacement lamination backings.

    Extrusion lamination of metallized BOPET to linear low-density sealant webs uses D139 as the sealant layer on a coextrusion coating line with a 100–150 mm single-screw extruder at 30:1 L/D and a deckled slot die set to 0.6–0.8 mm land length. Coating melt temperature is elevated to 280–310 °C to reduce neck-in and promote oxidative adhesion to the metal surface; coat weight is maintained at 15–25 g/m² on line speeds of 150–300 m/min. Formulation includes 85–95 wt% D139 and 5–15 wt% LDPE, with optional anti-block masterbatch at 2–4 wt% when the laminate enters horizontal form-fill-seal tracks. Adhesion is measured to ASTM F904 or an equivalent internal peel fixture, seal strength to ASTM F88, and water vapor transmission to ASTM F1249. Polyethylene is non-hygroscopic, so pre-drying is unnecessary even at relative humidity above 60%, but condensation on chilled incoming metallized web must be prevented by maintaining web temperature at least 3 °C above the dew point. Terminal articles are dry-food pouches with metallized barrier, detergent refill packs with laminated sealant strips, and personal care sachets requiring a 0.5–1.0 N/15 mm seal opening force.

    Free Quote

    Competitive Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® D139 is a hexene-based metallocene linear low density polyethylene (m-LLDPE) supplied as pelletized film resin for blown film and cast film conversion. The nominal density is 0.918 g/cm³ as determined by ASTM D1505, and the nominal melt index is 1.0 g/10 min at 190°C under 2.16 kg load using ASTM D1238. The single-site metallocene catalyst produces a narrow molecular weight distribution and homogeneous short-chain branching distribution compared with conventional Ziegler–Natta LLDPE. That structural uniformity is associated with reduced low-molecular-weight extractables, lower heat seal initiation temperature, and higher dart impact strength at equivalent film gauge. On production lines, D139 is used in monolayer and multilayer flexible packaging including form-fill-seal pouches, stretch wrap, heavy-duty sacks, and frozen food packaging, where film uniformity, seal performance, and tear resistance are tested respectively by ASTM D1003, ASTM F88, and ASTM D1922.

    Comparative evaluation against butene-based Ziegler–Natta LLDPE of the same 0.918 g/cm³ density shows that D139 produces higher Elmendorf tear resistance and dart impact at 25 µm because the hexene comonomer introduces longer short-chain branches that increase tie-molecule density during strain-induced crystallization at the frost line. The absence of a broad high-molecular-weight tail reduces melt elasticity and gel-like optical defects, observed as lower haze in ASTM D1003 tests. Against LDPE film grades with densities of 0.920 g/cm³ to 0.925 g/cm³, D139 has lower melt strength and reduced shear thinning, so bubble stability, die lip cleanability, and air ring control become the controlling process variables rather than melting capacity. Published data for this specific configuration is limited, but standard film comparisons generally report the trade-off between LDPE bubble stability and D139 impact toughness.

    Rheological Benchmarks and Die Configuration Limits

    In blown film conversion, the apparent viscosity at shear rates between 100 s⁻¹ and 1,000 s⁻¹ determines the melt pressure profile across the die gap. On grooved-feed extruders with screw diameters of 40 mm to 75 mm and L/D of 30:1, melt pressure before the screen changer is typically maintained below 350 bar with melt temperatures of 200°C to 220°C. Die gaps of 1.8 mm to 2.5 mm, blow-up ratios of 2.2:1 to 2.8:1, and frost line heights of 2.5 to 4.0 die diameters serve as initial operating windows for monolayer film. Specific energy input on such lines generally falls between 0.20 kWh/kg and 0.28 kWh/kg, with drive motor load increasing when melt temperature is reduced below 190°C. Because D139 has lower melt strength than LDPE, the air ring venturi must be tuned to avoid bubble collapse at high draw-down ratios; bubble kickback is more likely when the die lip accumulates oxidized resin.

    When D139 is used as a sealant layer in three-layer coextruded films, the metallocene architecture shifts heat seal performance toward lower jaw temperatures; this behavior is measured as a lower curve onset in ASTM F88 seal strength testing. On vertical form-fill-seal machines operating at 40 to 80 cycles/min, lower seal initiation can permit reduced jaw set points and shorter dwell times, although the magnitude depends on film gauge, layer ratio, and seal bar design. The lower extractable fraction compared with heterogeneous LLDPE is relevant for direct food contact under FDA 21 CFR 177.1520; migration evaluations follow the test conditions prescribed for fatty, aqueous, acidic, and alcoholic food simulants. In high-speed packaging, the resin’s consistent pellet conformity reduces feed bridging in gravimetric blending systems. The optimum corona level for solventless lamination is generally 38 mN/m to 42 mN/m as measured by ISO 8296, but printed or laminated structures may require higher surface energy depending on the ink system.

    What Are the Predominant Failure Modes When Melt Temperature and Frost Line Height Drift?

    Three failure modes are observed on production blown film lines when the processing window is exceeded. First, die-lip deposit accumulation increases when melt temperature exceeds 230°C; the oxidized resin fraction accumulates at the lip and transfers to the film as gel-like optical defects detected in ASTM D1003 haze measurements. Second, bubble instability appears as low-frequency oscillation when the frost line is raised above 4.5 die diameters at melt temperatures below 190°C; the cylindrical bubble loses symmetry under the air ring venturi, and film gauge variation measured by a non-contacting capacitance gauge can exceed ±5% of nominal thickness. Third, machine-direction tear resistance decreases when the draw-down ratio is increased without proportionally raising the frost line. ASTM D1922 Elmendorf tear values on 25 µm film can drop below 150 g in the machine direction while transverse-direction values remain above 300 g. These thresholds are not absolute; they depend on die diameter, air ring type, and internal bubble cooling settings.

    If Maximum Dart Impact and Low Extractables Are Required in Direct Food Contact

    Film converters selecting between D139, butene-based Ziegler–Natta LLDPE, and LDPE for direct food contact usually compare the property set under standardized film test protocols. The table below lists typical values for films at 25 µm thickness; results depend on die gap, frost line height, blow-up ratio, and additivation.

    PropertyTest methodUnitsD139 m-LLDPEZN butene LLDPELDPE film grade
    DensityASTM D1505g/cm³0.9180.9180.922
    Melt indexASTM D1238 (190°C/2.16 kg)g/10 min1.01.01.9
    Dart impactASTM D1709Ag≥50012090
    Elmendorf tear MD/TDASTM D1922g250/380180/260140/150
    HazeASTM D1003%8146
    Gloss 45°ASTM D2457%705575
    Seal initiationASTM F88°C95104108

    The comparative matrix shows that D139’s dart impact and Elmendorf tear values are higher than those of Ziegler–Natta LLDPE and LDPE at similar density. The haze value under ASTM D1003 is intermediate between LDPE and ZN LLDPE, but the reduction in seal initiation temperature relative to LDPE is operationally relevant in high-speed packaging. Tests under ASTM F88 display a measurable lowering of the temperature at which seal strength exceeds 3 N/15 mm, although the absolute value depends on seal bar Teflon condition and dwell pressure. Converters should not transfer these values directly to a specific line without pilot-scale confirmation using the target die and air ring.

    In cast film conversion, D139 is processed at melt temperatures of 230°C to 245°C with chill roll temperatures of 15°C to 25°C. The lower viscosity at these temperatures permits higher line speeds, but die lip deposit formation becomes more likely above 245°C. The film is therefore often stabilized with a phosphite antioxidant package to reduce oxidative gel formation during edge trim recycling. In stretch wrap lines, cling performance is introduced through a coextruded tackifier layer, because D139 itself is not inherently a self-cling grade and requires surface modification or a tackified outer layer for pallet wrap applications.

    Under FDA 21 CFR 177.1520, D139 can be used in olefin polymer food-contact articles subject to the extractable fraction limits and end-use conditions described in the regulation. In the European Union, compliance with Commission Regulation (EU) No 10/2011 and its amendments requires evaluation of overall migration and specific migration of monomers and additives; the final article must respect an overall migration limit of 10 mg/dm² or 60 mg/kg according to the applicable food simulant. REACH does not require polymer registration, but the imported article provisions and SVHC communication duties under Article 33 remain applicable if the product is used in articles. RoHS 2011/65/EU compliance is typically met because polyethylene does not contain the restricted heavy metals or brominated flame retardants above the maximum concentration values; verification is required at the article level. Processing limitations include avoidance of melt temperatures above 260°C for prolonged periods to minimize oxidative chain scission and gel generation. If the resin is stored at relative humidity above 60%, pre-drying in a desiccant hopper dryer at 80°C for 2 h to 4 h is recommended before extrusion, though moisture sensitivity of polyethylene is generally low. Contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents is not recommended during heated processing.