Chevron Phillips Marlex C101 Polyethylene Enhanced

Chevron Phillips Marlex® C101 Polyethylene; Enhanced

    • Product Name: Chevron Phillips Marlex® C101 Polyethylene; Enhanced
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 496123
    Density 0.946 g/cm³
    Melt Index 0.10 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 26.2 MPa
    Elongation At Break >=600%
    Flexural Modulus 1170 MPa
    Environmental Stress Crack Resistance >1000 hr
    Vicat Softening Temperature 127 °C
    Brittleness Temperature <= -70 °C
    Hardness Shore D 66
    Melting Point 134 °C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >1E15 ohm·cm

    As an accredited Chevron Phillips Marlex® C101 Polyethylene; Enhanced factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex® C101 Polyethylene; Enhanced is supplied in 25 kg bags, 40 bags per pallet (1,000 kg), or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of Chevron Phillips Marlex® C101 Polyethylene; Enhanced, shrink-wrapped and secured.
    Shipping Chevron Phillips Marlex® C101 Polyethylene; Enhanced is typically shipped as non-hazardous polymer resin in bags, boxes, or bulk containers. It is not classified as dangerous goods for DOT, IMDG, or IATA transport; no UN number, hazard class, or packing group applies. Store cool, dry, and protected from contamination.
    Storage Store Chevron Phillips Marlex® C101 Polyethylene; Enhanced in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture, dust, and contamination. Protect from prolonged UV exposure and extreme temperatures. Use stable palletized stacking, follow first-in, first-out inventory, and comply with the manufacturer’s SDS and local regulations.
    Shelf Life Stable under recommended storage conditions; no specific shelf life. Store cool, dry, away from direct sunlight, heat, and ignition sources.
    Application of Chevron Phillips Marlex® C101 Polyethylene; Enhanced

    In industrial chemical packaging, Marlex® C101 Polyethylene; Enhanced is introduced as the sole virgin feed on accumulator-head extrusion blow molding lines producing closed-head UN 1H1 drums, open-head UN 1H2 pails, and rigid inner bottles for composite intermediate bulk containers. The formula addition ratio at the feed hopper is 100 wt% virgin resin, with post-industrial regrind from deflashed tops and tails metered at 15–25 wt% only when the regrind stream is confirmed free of polypropylene cap fragments and paper label residues. Outdoor-rated product variants incorporate a UV masterbatch at 1.0–2.5 wt%, yielding a carbon black loading in the finished wall of 2.0–2.5 wt%; antistatic masterbatch is held to 0.5–1.0 wt% where UN test protocols require surface resistance below 10⁹ Ω per IEC 61340-2-3:2016. Barrier property targets for dangerous goods are not achieved by blend modification alone; they require either in-line fluorination of the parison interior or a coextruded barrier layer, because HDPE alone permits solvent vapour transmission that may fail the tightness retention test under ADR 6.1.5.2. Surface moisture from outdoor silo storage must be removed by hopper air at 70–80°C when ambient RH exceeds 70%; otherwise surface splay on the parison creates pinhole defects in the pinch weld.

    Melting and parison formation are conducted on accumulator-head machines with 24:1–30:1 L/D barrier screws and axial or radial parison programmers. Melt temperature at the die head is held at 190–225°C; the upper limit of 225°C is imposed to avoid oxidative gel formation and odour in high-regrind campaigns, while the lower limit of 190°C prevents excessive melt pressure and die-head torque. Mold temperature is maintained at 10–30°C depending on wall thickness and cycle time; blow air pressure is set at 0.6–0.8 MPa for 200 L drums. The dominant processing failure on production lines is sag-induced thinning in the top chime and pinch-off weld; this requires parison programming with 30–50 point wall thickness control and minimum pinch weld thickness established by burst testing per ISO 16101:2004 for plastics drums. Terminal products are 200 L closed-head drums, 20–60 L open-head pails, and IBC inner bottles with molded closures.

    Standard / codeDisciplineQualification scope
    49 CFR §178.509Plastic drumsDesign type testing for UN 1H1 and 1H2 drums
    UN Recommendation Chapter 6.1Dangerous goods packagingsLeakproofness, hydraulic pressure, stacking load, drop test
    ISO 20848-1:2006Plastics drumsRemovable-head drum dimensions, closure systems, handling
    ISO 16101:2004Plastics drumsComplete, filled transport package performance test methods

    Does Sheet Extrusion Require Melt Filtration Below 120 µm for Thermoformable HDPE Stock?

    In sheet extrusion for returnable material-handling trays and thermoformed dunnage, Marlex® C101 Polyethylene; Enhanced is fed at 100 wt% with clean edge-trim regrind at 10–20 wt% and a slip/antiblock masterbatch at 0.5–1.0 wt% where polished roll-stack release becomes inconsistent. For outdoor dunnage and pallet top decks exposed to solar load, UV stabilizer masterbatch is added at 1.0–2.0 wt% to reach a final carbon black content of 1.5–2.0 wt% in the sheet. The sheet line typically comprises a single-screw extruder with 30:1 L/D screw, hydraulic screen changer with 80–120 µm melt filtration, and a coat-hanger die with adjustable lips. Melt temperature at the die lips is held at 200–230°C; the three-roll stack is run at 60–90°C for polished or textured surfaces, and the nip pressure is adjusted to remove air without inducing orientation gradients that cause severe warpage during later thermoforming. At sheet thickness below 1.0 mm, gauge variation greater than ±0.05 mm produces inconsistent plug-assisted thermoforming and increased scrap rates; automatic die-bolt systems with downstream beta-gauge feedback are therefore specified on lines producing pallet top decks.

    Thermoforming of the extruded sheet is performed on single-station or rotary machines at sheet surface temperatures of 150–175°C, with mold temperatures of 20–60°C and vacuum levels of −0.08 to −0.06 MPa gauge. Compliance for pallet-type products is assessed under ISO 8611-1:2011 for flat pallet test methods and under the supplier’s REACH Article 33 declaration for substances of very high concern. Terminal parts include separator sheets, pallet top decks, thermoformed dunnage trays, battery trays, and returnable logistics packaging for automotive plants.

    Automotive Fluid Reservoir Parison Wall Distribution, Weld Pinch-Off, and Thermal Expansion Testing

    Automotive fluid reservoirs made from Marlex® C101 Polyethylene; Enhanced are processed on accumulator-head or suction blow molding machines with parison programmers configured for non-axisymmetric tooling. The feed formula is 100 wt% virgin resin, carbon black masterbatch at 2.0–2.5 wt% for opacity and UV stability, antioxidant masterbatch at 0.08–0.12 wt%, and uncontaminated molded scrap at 10–20 wt% only after leak-test screening. Melt temperature is held at 190–225°C, mold temperature at 15–40°C, and blow air pressure at 0.5–0.7 MPa. The bottom pinch-off weld is the highest field failure origin; therefore the tooling is designed to produce a pinch weld thickness no less than 75% of the nominal wall, and burst testing is carried out by pressurising the molded part until fracture or a specified minimum pressure is reached. Thermal expansion and chemical resistance are evaluated by immersion at 70–90°C in OEM-specific coolant and urea solutions for 500–1,000 h; published data for this specific resin–OEM combination is limited, so each qualification program must be verified against the purchaser’s engineering specification. The terminal product interfaces with ISO 22241-1:2019 diesel exhaust fluid; material compatibility is not inferred from that standard but from OEM-specific immersion testing. Terminal products include 10–30 L diesel exhaust fluid tanks, windshield washer reservoirs, coolant overflow bottles, and hydraulic fluid reservoirs.

    Agricultural sprayer tank and crop-protection container production places the same high-molecular-weight HDPE feed through accumulator-head blow molding, but the qualification emphasis shifts to pesticide compatibility, UV durability, and permeation resistance after multiple fill-and-drain cycles. In this application, Marlex® C101 Polyethylene; Enhanced is compounded at 100 wt% virgin resin with clean in-house regrind at 10–25 wt%, UV stabilizer masterbatch at 1.5–3.0 wt%, and color concentrate at 1.0–3.0 wt% for opaque or translucent tank bodies. The accumulator-head process is operated at melt temperatures of 190–225°C and mold temperatures of 10–30°C; for high-permeation solvent products, in-line fluorination of the internal parison surface is applied to a treatment depth of 0.1–0.5 µm. The fluorinated layer reduces solvent uptake and swell, but it must be limited to 10 wt% of the regrind stream to avoid generating localised unmelted domains. Compliance is established through UN Chapter 6.1 design type testing for hazardous liquids where applicable, ISO 16119-1:2013 for sprayer environmental requirements, and REACH Article 33 communication obligations. Terminal products include 15–400 L crop-sprayer tanks, induction hoppers, and closed chemical transfer containers for agrochemical distribution.

    High-output shuttle and rotary wheel blow molding lines for 0.5–5 L household chemical and janitorial containers require Marlex® C101 Polyethylene; Enhanced to be processed within a narrow high-load melt index window because parison weight drift directly changes drop-test performance under retailer distribution. The feed is configured at 100 wt% virgin resin, color masterbatch at 1–3 wt%, and clean in-house regrind at 10–30 wt%; additive packages that lower environmental stress-crack resistance below the lot acceptance threshold are rejected. Melt temperature is set at 190–220°C, mold cooling water is kept at 5–15°C, and blow air pressure is 0.5–0.7 MPa. Drop testing per ASTM D2463-15 Method A is used to verify shoulder pinch strength. Compliance for non-food household chemical bottles is typically limited to general packaging safety and dangerous goods rules when the fill product is classified; where food-contact declarations are required for export, the supplier’s regulatory statement under EU 10/2011 and FDA 21 CFR 177.1520(c) must be requested because published data for this specific grade in food-contact janitorial configurations is limited. Terminal products include trigger-spray cleaner bottles, laundry detergent bottles, and multi-purpose janitorial dosing containers.

    Free Quote

    Competitive Chevron Phillips Marlex® C101 Polyethylene; Enhanced prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® C101 Polyethylene; Enhanced is specified as an injection-moulding-grade high-density polyethylene (HDPE) supplied as free-flowing pellets in the Marlex C-series. The model identifier C101 denotes a general-purpose HDPE injection-moulding grade, while the “Enhanced” designation indicates a stabilised and nucleated formulation intended to modify crystallisation behaviour and post-mould dimensional stability. The exact additive identity is controlled by the manufacturer’s lot-release documentation rather than the base polymer designation. Nominal density is 0.956 g cm⁻³ when determined by ASTM D1505. Melt flow rate under 190°C and 2.16 kg is 8.0 g (10 min)⁻¹ when measured according to ASTM D1238 or ISO 1133-1:2022. The grade is positioned for thin-wall containers, housewares, closures, crates, pails and general-purpose moulding where a reproducible balance of stiffness, impact resistance and processability is required. Published data for this specific configuration is limited for ultralow-temperature impact and extended chemical exposure; application qualification should therefore rely on lot-specific certificates of analysis and moulded-article testing rather than pellet values alone.

    What Distinguishes the Enhanced C101 Grade from Conventional Injection-Moulding HDPE?

    Relative to a conventional unimodal HDPE of similar melt flow, C101 exhibits a faster crystallisation onset because of the nucleation package. This behaviour alters post-mould shrinkage anisotropy and can reduce cycle time in thick bosses, but the effect is measurable only when mould temperature is controlled below 30°C and hold pressure is not terminated before gate freeze. On 2,500 kN toggle-clamp machines with four-cavity container tooling, the enhanced grade has demonstrated lower top-load asymmetry in production-scale evaluations when compared with non-nucleated HDPE. The difference is attributed to a more uniform spherulitic morphology rather than to lubricant migration to the cavity surface. The grade also differs from conventional HDPE in its lower visible gate blush under fast linear fill; visual assessment using ISO 294-3 specimens indicates a reduction in flow-mark severity at injection velocities above 100 mm s⁻¹. However, the addition of the nucleating agent should be confirmed by the manufacturer’s safety data sheet because additive composition is not inferable from the base polymer grade.

    Pre-drying is not required for sealed, factory-packaged material. If bags have been opened for more than 8 h at relative humidity above 60%, moisture-induced splay may occur; desiccant drying at 80°C for 2–3 h is recommended. The grade is suitable for general-purpose reciprocating screw injection-moulding machines with screw L/D between 20:1 and 25:1 and compression ratio between 2.5:1 and 3.5:1. No special screw design is required for standard mixing.

    Melt Temperature and Injection Pressure Envelope for Multi-Cavity Tools

    For multi-cavity hot-runner tools producing round containers with wall thickness of 0.35–0.55 mm, the recommended melt temperature is 190–230°C, with a preferred range of 210–220°C to balance injection pressure and degradation risk. Mould water temperature is typically set to 15–40°C; lower temperatures improve cycle time but increase condensation risk in humid production halls. Injection pressure is generally 70–100 MPa, with hold pressure maintained at 50–70% of peak injection pressure. Screw decompression after plastication should not exceed 2–3 mm, because excessive decompression may induce air entrapment and inconsistent cushion control. Hot-runner manifold temperatures are maintained at 220–240°C; residence time above 240°C should not exceed 5 min to avoid molecular weight reduction and yellowing. Moulding conditions should be documented according to ISO 294-1, and process capability studies should include shot-mass standard deviation as a leading indicator of gate freeze variation.

    For thin-wall houseware applications such as stackable cups and food containers, C101 can be processed with sequential valve-gate actuation to avoid weld-line displacement. Weld-line strength is governed by melt temperature at the flow front; in four-cavity evaluations, a flow-front temperature above 195°C maintained acceptable burst performance when tested by internal pressure per ASTM D1598, although published data for this specific configuration is limited. Sprues should have a minimum cold-well length of 5 mm to trap the solidified plug from the nozzle interface. Gate diameters below 1.2 mm may generate shear heating and premature molecular orientation in thin-wall lids, leading to anisotropic shrinkage of 0.8–1.2% in the flow direction versus 1.0–1.4% perpendicular to flow, as measured by ASTM D955 after 48 h at 23°C and 50% RH.

    When C101 Replaces Standard HDPE in Living-Hinge or Snap-Fit Geometry

    When C101 is substituted for a conventional HDPE in snap-fit closures with a hinge section thickness below 0.3 mm, the nucleated crystalline structure raises flexural modulus but also reduces the number of hinge flex cycles before stress whitening, especially at temperatures below 0°C. In this configuration, the material should not be used without end-use flex testing per ASTM D790-14 or ISO 178. The transition from ductile to brittle failure in notched specimens shifts to a higher temperature than in standard HDPE, so the operating envelope for impact-critical parts must be reassessed. The grade is not recommended for applications requiring prolonged exposure to oxidising acids or for direct combination with amine-based chemical foaming agents, because the stabiliser package may be depleted and the nucleating package may induce pinhole formation. For closures, moulding trials should evaluate top-load after 24 h annealing at 60°C to capture post-mould crystallinity drift. Direct drop-in substitution from a non-nucleated HDPE without tooling compensation is not recommended because differences in shrinkage and gate freeze time can alter sealing surfaces.

    Compliance status is established under FDA 21 CFR 177.1520 for olefin polymers in food-contact applications, subject to end-use extractive limits. The moulded article should be verified for overall migration under EU Regulation (EU) No 10/2011; the applicable overall migration limit is 10 mg dm⁻². Specific migration of chromium, cobalt, zinc and antimony should be confirmed by the processor because C101 may contain catalyst residues and additive metals below the applicable specific migration limits. The grade is not supplied with a USP Class VI or ISO 10993 certification; biocompatibility claims are not supported without additional testing. For potable water contact, the grade may require NSF/ANSI 61 evaluation on the finished article, as pellet compliance does not automatically extend to the moulded component.

    StandardScopeConditionStatus for C101
    FDA 21 CFR 177.1520Olefin polymers in food contactEnd-use extractionCompliant as supplied; verify finished article limits
    EU Regulation (EU) No 10/2011Plastic food-contact materialsOML 10 mg dm⁻²Requires migration testing on moulded article
    ASTM D1505Density by density-gradient column23°CNominal 0.956 g cm⁻³
    ASTM D1238 / ISO 1133-1:2022Melt flow rate190°C/2.16 kgNominal 8.0 g (10 min)⁻¹
    ASTM D638 / ISO 527-2Tensile yield stress50 mm min⁻¹Typical 26 MPa
    ASTM D790 / ISO 178Flexural modulus2 mm min⁻¹Typical 1,380 MPa
    ASTM D256Izod notched impact23°CTypical 70 J m⁻¹

    Compared with a standard HDPE homopolymer of similar melt flow, C101 Enhanced displays higher flexural modulus and lower post-mould warpage. Unlike high-molecular-weight blow-moulding HDPE grades in the Marlex HHM series, C101 is not suitable for continuous extrusion blow moulding of bottles because its melt strength is insufficient for parison hang stability. Compared with other Marlex injection-moulding HDPE grades, C101 differs in its balance of melt flow, flexural modulus and notched impact; direct substitution without tooling compensation is not recommended when dimensional tolerances are below 0.1 mm. For converters currently using a non-nucleated HDPE with higher melt flow, C101 may require lower injection velocity and adjusted hold-pressure time to prevent over-packing and gate blush. The nucleated morphology can also reduce warpage in rectangular containers, but the improvement is geometry-dependent and should be validated by top-load testing after conditioning.

    What Operational Boundaries Apply to Moisture and Regrind Incorporation?

    Regrind incorporation should be limited to 20% by weight unless process capability data on the moulded article support higher levels. Regrind from C101 retains the nucleating package, but repeated heat histories shift the melt flow rate upward and reduce the high-shear viscosity plateau. In a 3,200 kN hydraulic machine with 32 cavities, increasing regrind from 0% to 20% altered shot mass by 0.3–0.5 g and changed top-load performance by 6–8% on thin-wall containers. Moisture uptake in regrind is higher than in virgin pellets because of increased surface area; regrind stored in open bins should be dried before blending. The processing window also narrows when recycled material is added. For wall thickness below 0.3 mm, the effective melt-temperature window may narrow to ±5°C around the preferred 210°C setpoint. Above 225°C, melt pressure drops and sink marks increase; below 195°C, short shots and premature gate freeze occur. Hot-runner tip temperatures must be held within ±3°C of the manifold setpoint; cartridge heater zones should be individually tuned and verified with a contact thermocouple, not inferred from setpoint alone.

    For injection-moulded caps and closures, C101 is typically processed with a cold runner and tunnel gate to minimise post-mould gate vestige. Closures with continuous thread profiles requi re a slower initial injection profile to prevent flow marks at the thread root; injection profiling is set to fill the first 60% of the cavity at 60–70% of maximum injection speed, followed by a velocity reduction to 40–50% to maintain a uniform flow-front velocity. Holding pressure is applied until the gate freeze time is reached, which in a 1.5 mm diameter tunnel gate is typically 4–6 s at 40°C mould temperature. Closure removal force and strip torque should be measured according to ASTM D3472 or equivalent; the nucleated C101 grade generally requires higher strip torque adjustment because of increased flexural modulus compared with standard HDPE. Finished closures intended for carbonated beverage applications must be evaluated for stress cracking under ASTM D1693, Condition B, because the enhanced crystallinity does not eliminate environmental stress cracking sensitivity in the presence of wetting agents or detergents.

    Top